1.
Chao Deng  Xiabin Jing 《Polymer》2005,46(3):653-659
A biodegradable amphiphilic triblock copolymer of poly(ethylene glycol)-b-poly(l-lactide)-b-poly(l-glutamic acid) (PEG-b-PLLA-b-PLGA) was obtained by catalytic hydrogenation of poly(ethylene glycol)-b-poly(l-lactide)-b-poly(γ-benzyl-l-glutamic acid) (PEG-b-PLLA-b-PBLGA) synthesized by the ring-opening polymerization (ROP) of N-carboxyanhydride of γ-benzyl-l-glutamate (BLG-NCA) with amino-terminated MPEG-b-PLLA-NH2 as a macroinitiator. MPEG-b-PLLA-NH2 converted from MPEG-b-PLLA-OH first reacted with tert-Butoxycarbonyl-l-phenylalanine (Phe-NBOC) and dicyclohexylcarbodiimide (DCC) and then deprotected the tert-butoxycarbonyl group. MPEG-b-PLLA-OH was prepared by ROP of l-lactide with monomethoxy poly(ethylene glycol) in the presence of stannous octoate. The triblock copolymer and its diblock precursors were characterized by 1H NMR, FTIR, GPC and DSA (drop shape analysis) measurements. The lengths of each block polymers could be tailored by molecular design and the ratios of feeding monomers. The triblock polymer PEG-b-PLLA-b-PLGA containing carboxyl groups showed obviously improved hydrophilic properties and could be a good potential candidate as a drug delivery carrier.  相似文献   

2.
Poly(γ-benzyl l-glutamate)-block-poly(l-phenylalanine) was prepared via the ring opening polymerization of γ-benzyl l-glutamate N-carboxyanhydride and l-phenylalanine N-carboxyanhydride using n-butylamine·HCl as an initiator for the living polymerization. Polymerization was confirmed by 1H-nuclear magnetic resonance spectroscopy and matrix assisted laser desorption ionization time of flight mass spectroscopy. After deprotection, the vesicular nanostructure of poly(l-glutamic acid)-block-poly(l-phenylalanine) particles was examined by transmission electron microscopy and dynamic light scattering. The pH-dependent properties of the nanoparticles were evaluated by means of ζ-potential and transmittance measurements. The results showed that the block copolypeptide could be prepared using simple techniques. Moreover, the easily prepared PGA-PPA block copolypeptide showed pH-dependent properties due to changes in the PGA ionization state as a function of pH; this characteristic could potentially be exploited for drug delivery applications.  相似文献   

3.
Copolymers of N-vinyl-2-pyrrolidone and 2-phenyl-1, 1-dicyanoethene were studied. Infrared, proton, and carbon-13 spectra of the copolymers are discussed by comparison with poly(N-vinyl-2-pyrrolidone), model compounds, and various copolymers. Thermal behavior of the copolymers was investigated by using DSC, TMA, and TGA methods. Thermal as well as thermooxidative stability of the copolymers was found to be lower than those of poly(N-vinyl-2-pyrrolidone).  相似文献   

4.
Chang-Hong Ho  Yu-Der Lee 《Polymer》2010,51(7):1639-1647
This investigation characterizes the molten morphologies following isothermal crystallization of poly(l-lactide-block-dimethyl siloxane-block-l-lactide) triblock copolymers, which were synthesized by ring-opening polymerization of l-lactide using hydroxyl-telechelic PDMS as macroinitiators, via small-angle X-ray scattering (SAXS) and transmission electron microscopy (TEM). The break-out and preservation of the nanostructure of the triblock copolymer depended on the segregation strength, which was manipulated by varying the degree of polymerization. The crystallization kinetics of these semicrystalline copolymers and the effect of isothermal crystallization on their melting behaviors were also studied using DSC, FT-IR and WAXS. The exclusive presence of α-phase PLLA crystallite was verified by identifying the absence of the WAXS diffraction signal at 2θ = 24.5° and the presence of IR absorption at 1749 cm−1 when the PLLA segment of the block copolymers was present as a minor component. The dependence of the crystallization rate (Rc) on the chemical composition of the triblock copolymers reveals that the Rc of the triblock copolymers was lower than that of PLLA homopolymer and the Rc were substantially reduced when the minor component of the crystallizable PLLA domains was dispersed in the PDMS matrix.  相似文献   

5.
Xiaoyi Sun  Xiaohua Huang  Qi-Feng Zhou 《Polymer》2005,46(14):5251-5257
The synthesis of ABC triblock copolymer poly(ethylene oxide)-block-poly(methyl methacrylate)-block-polystyrene (PEO-b-PMMA-b-PS) via atom transfer radical polymerization (ATRP) is reported. First, a PEO-Br macroinitiator was synthesized by esterification of PEO with 2-bromoisobutyryl bromide, which was subsequently used in the preparation of halo-terminated poly(ethylene oxide)-block-poly(methyl methacrylate) (PEO-b-PMMA) diblock copolymers under ATRP conditions. Then PEO-b-PMMA-b-PS triblock copolymer was synthesized by ATRP of styrene using PEO-b-PMMA as a macroinitiator. The structures and molecular characteristics of the PEO-b-PMMA-b-PS triblock copolymers were studied by FT-IR, GPC and 1H NMR.  相似文献   

6.
In previous papers, we studied the hydrolytic degradation of six poly(ester-ether-ester) block copolymers, i.e. three poly(ε-caprolactone)-block-poly(oxyethylene)-block-poly(ε-caprolactone) copolymers and three poly(l-lactide)-block-poly(oxyethylene)-block-poly(l-lactide) copolymers. Their degradation products, 6-hydroxyhexanoic acid and l-lactic acid, have now been found to modulate endothelin release by human umbilical vein endothelial cells, with no significant alteration of the vasoconstrictor-vasodilator balance previously determined. The influence of the same degradation products on the cell proliferation has also been determined and discussed. Received: 13 January 1997/Revised: 2 May 1997/Accepted: 3 May 1997  相似文献   

7.
The adhesion strength of an adhesive is affected by two factors: the development of interfacial adhesion and the cohesive strength of the adhesive. In order to evaluate the relative contributions of these two factors, the tack of polyacrylic block copolymer-based adhesives was measured using a probe tack test. For this purpose, three model adhesives were prepared: poly(methyl methacrylate)-block-poly(n-butyl acrylate)-block-poly(methyl methacrylate) triblock copolymer (A), a mixture of the triblock and poly(methyl ethacrylate)-block-poly(n-butyl acrylate) diblock copolymer (7/3, w/w) (B), and a mixtureof the triblock and poly(n-butyl acrylate) oligomer (8/2, w/w) (C). The tack measured at room temperature was in the order B ≈ C > A and increased gradually with an increase in the contact time. The temperature dependence of tack showed peak tack values above room temperature, and the peak tack temperature was in the order A > B > C. The storage and loss moduli measured by dynamic mechanical analysis were also in the order A > B > C. The molecular mobility of the poly(n-butyl acrylate) unit in the block copolymer measured by H-pulse NMR was in the order C> B > A. It was concluded from these results that the relative contribution of interfacial adhesion to the tack of the different systems was in the order C > B > A.  相似文献   

8.
We demonstrated here a facile method to synthesize novel double crystalline poly(butylene terephthalate)-block-poly(ethylene oxide)-block-poly(butylene terephthalate) (PBT-b-PEO-b-PBT) triblock copolymers by solution ring-opening polymerization (ROP) of cyclic oligo(butylene terephthalate)s (COBTs) using poly(ethylene glycol) (PEG) as macroinitiator and titanium isopropyloxide as catalyst. The structure of copolymers was well characterized by 1H NMR and GPC. TGA results revealed that the decomposition temperature of PEO in triblock copolymers increased about 30 °C to the same as PBT copolymers, after being end-capped with PBT polymers. These triblock copolymers showed double crystalline properties from PBT and PEO blocks, observed from DSC and WAXD measurements. The melting and crystallization peak temperatures corresponding to PBT blocks increased with PBT content. The crystallization of PBT blocks showed the strong confinement effects on PEO blocks due to covalent linking of PBT blocks with PEO blocks, where the melting and crystallization temperatures and crystallinity corresponding to PEO blocks decreased significantly with increment of PBT content. The confinement effect was also observed by SAXS experiments, where the long distance order between lamella crystals decreases with increasing PBT length. For the triblock copolymer with highest PBT content (PBT54-b-PEO227-b-PBT54), this effect shows a 30 °C depression on PEO crystals' melting temperature and 77% on enthalpy, respectively, compared to corresponding PEO homopolymer. The crystal morphology was observed by POM, and amorphous-like spherulites were observed during PBT crystallization.  相似文献   

9.
Jingru Sun  Xiabin Jing 《Polymer》2004,45(17):5969-5977
Crystallization behavior, structural development and morphology evolution in a series of diblock copolymers of poly(l-lactide)-block-poly(ethylene glycol) (PLLA-b-PEG) were investigated via differential scanning calorimetry, wide-angle X-ray diffraction, polarized optical microscopy and atomic force microscopy. In these copolymers, both blocks are crystallizable and biocompatible. It was interesting that these PLLA-b-PEG diblock copolymers could form spherulites with banded textures, which was undercooling dependent. Single crystals with an abundance of screw dislocations were also observed via AFM. Such results indicated that these ringed spherulites and single crystals were formed during the crystallization of the PLLA blocks.  相似文献   

10.
We present the synthesis of fluorescein isothiocyanate (FITC)-labeled poly(ethylene oxide)-block-poly(?-caprolactone)-block-poly(ethylene oxide) (PEO-PCL-PEO) triblock copolymers and their applications for tracking the penetration behavior of FITC-labeled copolymers in the hairless mouse skin. In the first step, PEO-PCL diblock copolymers with different ratios of PCL to PEO (i.e., [CL]/[EO]) were prepared by ring opening polymerization of ?-caprolactone (CL), where monomethoxy poly(ethylene glycol) (mPEG, Mn = 2000 g mol−1) was used as a macro-initiator. FITC was successively reacted with octadecylamine, isophorone diisocyanate (IPDI), and then used as a linker to obtain PEO-PCL-PEO triblock copolymers from the PEO-PCL diblock copolymers. In aqueous solution, both FITC-labeled triblock copolymers show two UV absorption peaks at 489 and 455 nm, attributed to the monomeric FITC and H-aggregated FITC moieties, respectively. Due to the strong H-aggregation of FITC in the copolymer of high [CL]/[EO], fluorescent emission intensities considerably decreased at high concentrations of the copolymer. FITC-labeled copolymers exhibited more sharper polarized optical and fluorescence microscopic images compared to the mixtures of FITC and unlabeled copolymer in both solid crystalline and multiple emulsion state. Furthermore, the Frantz diffusion cell test was carried out to demonstrate the penetration behavior of the FITC-labeled copolymers in the hairless mouse skin.  相似文献   

11.
In this work, we investigated the effect of formation mechanisms of nanophases on the morphologies and thermomechanical properties of the nanostructured thermosets containing block copolymers. Toward this end, the nanostructured thermosets involving epoxy and block copolymers were prepared via self-assembly and reaction-induced microphase separation approaches, respectively. Two structurally similar triblock copolymers, poly(ε-caprolactone)-block-poly(butadiene-co-styrene)-block-poly(ε-caprolactone) (PCL-b-PBS-b-PCL) and poly(ε-caprolactone)-block-poly(ethylene-co-ethylethylene-co-styrene)-block-poly(ε-caprolactone) (PCL-b-PEEES-b-PCL) were synthesized via the ring-opening polymerization of ε-caprolactone (CL) with α,ω-dihydroxyl-terminated poly(butadiene-co-styrene) (HO-PBS-OH) and α,ω-dihydroxyl-terminated poly(ethylene-co-ethylethylene-co-styrene) (i.e., HO-PEEES-OH) as the macromolecular initiators, respectively; the latter was obtained via the hydrogenation reduction of the former. Both the triblock copolymers had the same architecture, the identical composition and close molecular weights. In spite of the structural resemblance of both the triblock copolymers, the formation mechanisms of the nanophases in the thermosets were quite different. It was found that the formation of nanophases in the thermosets containing PCL-b-PBS-b-PCL followed a reaction-induced microphase separation mechanism whereas that in the thermosets containing PCL-b-PEEES-b-PCL was in a self-assembly manner. The different formation mechanisms of nanophases resulted in the quite different morphologies, glass transition temperatures (Tg's) and fracture toughness of the nanostructured thermosets.  相似文献   

12.
13.
We recently achieved quantitative synthesis of an amphiphilic coil-rod-coil triblock copolymer, poly(2-vinylpyridine)-b-poly(n-hexyl isocyanate)-b-poly(2-vinylpyridine), by coupling in situ living diblock copolymer poly(2-vinylpyridine)-b-poly(n-hexyl isocyanate) (P2VP-b-PHIC) using malonyl chloride in the presence of pyridine. This led to the introduction of an active methylene group that is a site for further functionalization in the rod block. The Michael addition reaction of the triblock copolymer with 7-(4-trifluoromethyl) coumarin acrylamide led to copolymer bearing a fluorescent pendent in the rod block. The fluorescent labeled copolymers were isolated in ∼94% yields. Similarly C60 pendent was introduced to the rod block by the Bingel reaction. The yields of C60 functionalized copolymers were ∼54%. The precursor and functionalized amphiphilic coil-rod-coil copolymer show diverse morphologies, such as micelles and vesicles by simply changing the solvent. For the C60 functionalized block copolymer, structural constraints in micelles and vesicles prevented C60 pendents to aggregate.  相似文献   

14.
Two novel triblock copolymers poly(hydroxypropyl acrylate)-b-poly (methyl methacrylate)-b-poly(N,N-dimethylaminoethyl methacrylate) and poly(hydroxypropyl acrylate)-b-poly(methyl methacrylate)-b-poly(acrylic acid) were successfully synthesized. In acetone media, using the electrostatic interactions between N,N-dimethylaminoethyl methacrylate and acrylic acid units, they could form spherically shaped multilayer micelles with pH-responsive, and have a mean diameter around 110 nm. The critical micelle concentration of it was determined to be 2.42 mg/L. In vitro release experiments, the folic acid-loaded micelles exhibited sustained release behavior and the drug release rate was affected by the pH value of release media. These results indicate that the multilayer micelles may serve as a novel intelligent drug delivery system.  相似文献   

15.
A facile approach is offered to synthesize well‐defined amphiphilic ABC triblock copolymers composed of poly(ethylene glycol) monomethyl ether (MPEO) as A block, poly(L ‐lysine) (PLLys) as B block, and poly(ε‐caprolactone) (PCL) as C block by a combination of ring‐opening polymerization (ROP) and click reactions. The propargyl‐terminated poly(Z‐L ‐lysine)‐block‐poly(ε‐caprolactone) (MPEO‐PzLLys‐PCL) diblock copolymers were synthesized via the ring‐opening polymerization of Nε‐carbobenzoxy‐L ‐lysine N‐carboxyanhydride (Z‐L ‐Lys NCA) in DMF at room temperature using propargyl amine as an initiator and the resulting amino‐terminated poly(Z‐L ‐lysine) then used in situ as a macroinitiator for the polymerization of ε‐caprolactone in the presence of stannous octoate as a catalyst. The triblock copolymers poly(ethylene glycol) monomethyl ether –block‐poly(Z‐L ‐lysine)‐block‐poly(ε‐caprolactone) (MPEO‐PzLLys‐PCL) were synthesized via the click reaction of the propargyl‐terminated PzLLys‐PCL and azido‐terminated poly(ethylene glycol) monomethyl ether (PEO‐N3) in the presence of CuBr and 1,1,4,7,7‐pentamethyldiethylenetriamine (PMDETA) catalyst system. After the removal of Z groups of L ‐lysine units, amphiphilic and biocompatible ABC triblock copolymers MPEO‐PLLys‐PCL were obtained. The structural characteristics of these ABC triblock copolymers and corresponding precursors were characterized by NMR, IR, and GPC. These results showed the click reaction was highly effective. Therefore, a facile approach is offered to synthesize amphiphilic and biocompatible ABC triblock copolymers consisting of polyether, polypeptide and polyester. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

16.
The electrochemical behaviour of N-acetyl-l-cysteine (NAC) has been investigated by linear and cyclic voltammetry on gold electrode at room temperature. The results showed two oxidation peaks under acid and neutral conditions and only one in basic medium. For each oxidation, as many electron was exchanged as proton. The influence of both the concentration and the potential scan rate on the peak currents highlighted a diffusion-controlled phenomenon for the first peak and an adsorption-limited reaction rate for the second one. The diffusion coefficient of NAC in solution and the surface concentration of the adsorbed species at pH 3 and 7 were close to 2 × 10−4 to 2 × 10−5 cm2 s−1 and 6 × 10−9 to 6 × 10−10 mol cm−2, respectively. Film transfer experiments resulted in an irreversible adsorption of NAC on gold electrode, and the formation of a self-assembled monolayer (SAM).  相似文献   

17.
A series of ABA type triblock copolymers [Poly(lactide)-block-poly(hexamethylene 2,3-O-isopropylidene tartarate)-block-poly(lactide)] PLA-b-PHIT-b-PLA based on renewable monomers l-tartaric acid and l-lactide have been synthesized and the effect of the PLA chain length on the properties of the triblock copolymers has been systematically investigated. The block nature of the copolymers was established by differential scanning calorimetry (DSC) which showed two glass transition temperatures (Tg) corresponding to PHIT and PLA blocks. Solution cast films of these triblock copolymers turned out to be brittle in nature and to overcome this, ε-caprolactone was copolymerized with l-lactide to generate a separate series of triblock copolymers [PLA-ran-PCL]-b-PHIT-b-[PLA-ran-PCL]. Our study systematically demonstrates that the PLA-to-PCL ratio in the outer block composition influences the mechanical properties via a delayed post-yield stress drop phenomenon. The study further elaborates the time-synchronized strain-field analysis of the novel triblocks to be a convincing approach for the characterization of micro-deformation modes.  相似文献   

18.
High-velocity sedimentation, translational isothermal diffusion, and viscometry in H2O and DMF are used to investigate the samples and fractions of poly(N-methyl-N-vinylacetamide) synthesized by free-radical polymerization and fractionated in a chloroform-diethyl ether system. Molecular masses M and the Mark-Kuhn-Houwink-Sakurada relations are obtained for the fractions in the molecular mass range M × 10−3 = 3.5−540.0. The negative temperature coefficient of intrinsic viscosity is revealed for both solvents. The length of the Kuhn statistical segment and the hydrodynamic diameter of poly(N-methyl-N-vinylacetamide) macromolecules are estimated; the hydrodynamic volumes occupied by water-soluble poly(N-methyl-N-vinylacetamide), poly(1-vinyl-2-pyrrolidone), poly(vinylformamide), and pullulan molecules are compared.  相似文献   

19.
Summary The triblock copolymers of poly(p-dioxanone)-b-poly(tetrahydrofuran)-b-poly(p-dioxanone) were synthesized by ring-opening polymerization of p-dioxanone in the presence of dihydroxyl poly(tetrahydrofuran)(PTHF) using stannous octoate (SnOct2) as a catalyst. The effects of feed ratio, reaction time and reaction temperature on the copolymerization were investigated. It was found that the optimal reaction temperature and time were 80 °C and 42 hours, respectively, and the molar ratio of p-dioxanone/SnOct2 (PDO/cat.) had little influence on the inherent viscosity of the copolymers. The triblock copolymers were characterized by various analytical techniques such as 1H-NMR and DSC.  相似文献   

20.
The sequential ring-opening polymerizations (ROP) of ε-caprolactone (ε-CL) and L-lactide (LLA) with benzo-12-crown-4-imidazole carbene (B-12-C-4imY) as the catalyst have been performed. Using either benzyl alcohol or ethylene glycol as an initiator, the corresponding poly(ε-caprolactone)-poly(L-lactide) (PCL-b-PLLA) diblock or poly(L-lactide)-poly(ε-caprolactone)-poly(L-lactide) (PLLA-PCL-PLLA) triblock copolymers were easily prepared. The results indicated that B-12-C-4imY was quite effective for the copolymerization. The diblock copolymerization of ε-CL with LLA could only be achieved when ε-CL was first polymerized followed by LLA. Feeding the two monomers simultaneously, however, only resulted in the formation of LLA homopolymers. Thermogravimetric analysis (TGA) measurements demonstrated that block copolymers exhibited the decomposition temperature lower than the PCL homopolymer. The copolymers were characterized by 1H NMR and 13C NMR, FT-IR, GPC, and DSC analyses. 20?×?10 mm2 rectangular specimens made of the triblock copolymer were allowed to degrade in a pH?=?7.4 phosphate buffer at 37 °C. Degradation was monitored by various analytical techniques such as GPC, IR, and ESEM.  相似文献   