1.
The adhesively bonded tubular single lap joint shows nonlinear torque transmission capability and deformation characteristics under static torsional loading because of nonlinear properties of the adhesive. However, the dynamic or fatigue torque transmission capability can be calculated with linear, analysis because the stress-strain relation under torsional fatigue loading is linear, due to the small dynamic transmission capability compared with the static torque transmission capability.

In this paper, a failure model for the adhesively bonded tubular single lap joint under torsional fatigue loading was developed with respect to the adhesive thickness, which is the critical factor for the static torque transmission capability. Also, a design method for the adhesively bonded tubular single lap joint under torsional fatigue loading was proposed.  相似文献   

2.
Calculated torque transmission capability of adhesively bonded tubular lap joints using linear elastic material properties is usually much less than the experimentally-determined one because the majority of the load transfer of the adhesively bonded joints is accomplished by the nonlinear behavior of rubber-toughened epoxy adhesives.

Although the adhesively bonded tubular double lap joint has better torque transmission capability and reliability than the single lap joint, the nonlinear analytic or numerical analysis for the adhesively bonded tubular double lap joint has not been performed because of numerical complications.

An iterative solution that includes the nonlinear shear behavior of the adhesive was derived using the analytic solution. Since the iterative solution can be obtained very quickly due to the simplicity of the algorithm, it is an attractive method of designing adhesively bonded tubular single and double lap joints.  相似文献   

3.
The adhesively bonded tubular double lap joint has better torque transmission capability and reliability in bonding than the single lap joint.

In this paper, an analytic solution for the torque transmission capability and stress distribution of the adhesively bonded tubular double lap joint was derived assuming linear properties of the adhesive.

From the analytic solution, it was found that the torque transmission capability of the double lap joint was more than 40% larger than that of the single lap joint.  相似文献   

4.
The accurate calculation of the stresses and torque capacities of adhesively bonded joints is not possible without understanding the failure phenomena of the adhesive joints and the nonlinear behavior of the adhesive.

In this paper, an adhesive failure model of the adhesively bonded tubular single lap joint with steel-steel adherends was proposed to predict the torque capacity accurately.

The model incorporated the nonlinear behavior of the adhesive and the different failure modes in which the adhesive failure mode changed from bulk shear failure, via transient failure, to interfacial failure between the adhesive and the adherend, according to the magnitudes of the residual thermally-induced stresses from fabrication.  相似文献   

5.
The adhesively-bonded tubular single lap joint shows large nonlinear behavior in the load-displacement relationship, because structural adhesives for the joint are usually rubber-toughened, which endows adhesives with nonlinear shear properties. Since the majority of load transfer of the adhesively-bonded tubular single lap joint is accomplished by the nonlinear behavior of the adhesive, its torque transmission capability should be calculated using nonlinear shear properties. However, both the analytic and numerical analyses become complicated if the nonlinear shear properties of the adhesive are included during the calculation of torque transmission capabilities.

In this paper, in order to obtain the torque transmission capabilities easily, an iterative solution which includes the nonlinear shear properties of the adhesive was derived using the analytic solution with the linear shear properties of the adhesive. Since the iterative solution can be obtained very quickly due to its simplicity, it has been found that it can be used in the design of the adhesively-bonded tubular single lap joint.  相似文献   

6.
When an adhesively bonded joint is exposed to a high environmental temperature, the tensile load capability of the adhesively bonded joint decreases because the elastic modulus and failure strength of the adhesive decrease. In this paper, the elastic modulus and failure strength of the adhesive as well as the tensile load capability of the tubular single lap adhesively bonded joint were experimentally and theoretically investigated with respect to the volume fraction of filler and the environmental temperature. Two types of fillers - Al2O3 (alumina) and chopped fiber E glass - were used. From the experiment, it was found that the elastic modulus and failure strength of the adhesive increased in accordance with the increase of volume fraction of the filler and decreased with the environmental temperature rise. It was also found that the tensile load capability of the tubular single lap adhesively bonded joint decreased as the environmental temperature increased; however, it had no correlation with the volume fraction of filler because of the effect of the fabrication thermal residual stresses generated by the CTE difference between the adherend and adhesive.  相似文献   

7.
With the wide application of fiber-reinforced composite materials in aircraft, space structures and robot arms, the design and manufacture of composite joints have become a very important research area because they are often the weakest areas in composite structures.

In this paper, the stress and torque transmission capabilities of the adhesively-bonded tubular single lap joint and the double lap joint were experimentally tested. In order to compare the experimental results with the calculated results, the stress and torque transmission capabilities were analyzed by the 3-dimensional finite element method taking into consideration the nonlinear properties of the adhesive.

From the experiments it was found that the torque transmission capabilities of the adhesively-bonded double lap joint was 2.7 times as large as that of the single lap joint. Also, it was found that the fatigue limit of the double lap joint was 16 times as large as that of the single lap joint.  相似文献   

8.
The majority of the load transfer of an adhesively-bonded joint is accomplished by the nonlinear behavior of the adhesive. In this paper, the torque transmission capability and shear stress distribution of the tubular single lap joint were calculated by incorporating the nonlinear shear properties of the adhesive. The nonlinear shear properties were represented by three different mathematical models such as two-parameter exponential, linear perfectly-plastic and multilinear strain-softening approximations.

From the analyses and experiments, it was found that all the analyses with nonlinear approximations predicted the torque transmission capabilities accurately, but the two-parameter exponential approximation gave the best predictions with the simplest form for use in numerical calculation.  相似文献   

9.
The static tensile load bearing capability of adhesively-bonded tubular single lap joints calculated using linear mechanical adhesive properties is usually far less than the experimentally-determined one because the majority of the load transfer of adhesively-bonded joints is accomplished by the nonlinear behavior of the rubber-toughened epoxy adhesive

In this paper, both the nonlinear mechanical properties and the residual thermal stresses in the adhesive resulting from joint fabrication were included in the stress calculation of adhesively-bonded joints. The nonlinear tensile properties of the adhesive were approximated by an exponential equation which was represented by the initial tensile modulus and ultimate tensile strength of the adhesive.

From the tensile tests and the stress analyses of adhesively-bonded joints, a failure model for adhesively-bonded tubular single lap joints under axial loads was proposed.  相似文献   

10.
An investigation of an adhesively bonded composite joint with a brittle adhesive was conducted to characterize both the static and fatigue debond growth mechanism under mode I and mixed mode I-II loadings. The bonded system consisted of graphite/epoxy adherends bonded with FM-400 adhesive. Two specimen types were tested: (1) a double-cantilever-beam specimen for mode I loading and (2) a cracked-lap-shear specimen for mixed mode I-II loading. In all specimens tested, failure occurred in the form of debond growth either in a cohesive or adhesive manner. The total strain-energy-release rate is not the criterion for cohesive debond growth under static and fatigue loading in the birttle adhesive as observed in previous studies with the ductile adhesives. Furthermore, the relative fatigue resistance and threshold value of cyclic debond growth in terms of its static fracture strength is higher in the brittle adhesive than its counterpart in the ductile adhesive.  相似文献   

11.
The tensile load bearing capability of adhesively-bonded tubular single lap joints which is calculated under the assumption of linear mechanical adhesive properties is usually much less than the experimentally-determined because the majority of the load transfer of adhesively-bonded joints is accomplished by the nonlinear behavior of rubber-toughened epoxy adhesives. Also, as the adhesive thickness increases, the calculated tensile load bearing capability with the linear mechanical adhesive properties increases, while, on the contrary, the experimentally-determined tensile load bearing capability decreases.

In this paper, the stress analysis of adhesively-bonded tubular single lap steel-steel joints under tensile load was performed taking into account the nonlinear mechanical properties and fabrication residual thermal stresses of the adhesive. The nonlinear tensile properties of the adhesive were approximated by an exponential equation which was represented by the initial tensile modulus and ultimate tensile strength of the adhesive.

Using the results of stress analysis, the failure criterion for the adhesively-bonded tubular single lap steel-steel joints under tensile load was developed, which can be used to predict the load-bearing capability of the joint. From the failure criterion, it was found that the fracture of the adhesively-bonded joint was much influenced by the fabrication residual thermal stresses.  相似文献   

12.
Optimal Design of the Adhesively-Bonded Tubular Single Lap Joint   总被引:1,自引:0,他引:1  
In this paper, a method for the optimal design of the adhesively-bonded tubular single lap joint was proposed based on the failure model of the adhesively-bonded tubular single lap joint. The failure model incorporated the nonlinear mechanical behavior of the adhesive as well as the different failure modes in which the adhesive failure mode changed from bulk shear failure, via transient failure, to interfacial failure between the adhesive and the adherend, according to the magnitudes of the residual thermal stresses induced by fabrication.

The effects of the design parameters for the adhesively-bonded tubular single lap joint, such as the thicknesses of adhesive layer and adherends, the bonding length, and the scarfs of adherends, on the torque transmission capability and the efficiency of the adhesive joint were investigated.  相似文献   

13.
Adhesively bonded joints can support a longer fatigue life if compared to conventional joining techniques, provided that a set of requirements is fulfilled. One of the most important requirements is the mechanical preparation of the bonded joint surface, which improves the joint interface adhesion. The aim of this work is to investigate the influence of surface roughness of mild steel substrates on fatigue behavior in adhesive bonded plates. To accomplish this objective, three different surface treatments were used on A36 steel substrate specimens, namely sand blasting, grit blasting, and bristle blasting. Bonded plate specimens, using end-notched flexure format, with a thin adhesive epoxy layer were manufactured and tested, under mode II loading condition, in both static and dynamic tests. The results confirm the importance of surface treatment of the substrate on the fatigue life, confirming that adhesively bonded joints have significant performance differences when subjected to static and dynamic loadings.  相似文献   

14.
An experimental–computational fracture-mechanics approach for the analysis and design of structural adhesive joints under static loading is demonstrated by predicting the ultimate fracture load of cracked lap shear and single lap shear aluminum and steel joints bonded using a highly toughened epoxy adhesive. The predictions are then compared with measured values. The effects of spew fillet, adhesive thickness, and surface roughness on the quasi-static strength of the joints are also discussed. This fracture-mechanics approach is extended to characterize the fatigue threshold and crack growth behavior of a toughened epoxy adhesive system for design purposes. The effects of the mode ratio of loading, adhesive thickness, substrate modulus, spew fillet, and surface roughness on the fatigue threshold and crack growth rates are considered. A finite element model is developed to both explain the experimental results and to predict how a change in an adhesive system affects the fatigue performance of the bonded joint.  相似文献   

15.
Better fatigue performance of adhesively bonded joints makes them suitable for most structural applications. However, predicting the service life of bonded joints accurately remains a challenge. In this present study, nonlinear computational simulations have been performed on adhesively bonded single lap ASTM-D1002 shear joint considering both geometrical and material nonlinearities to predict the fatigue life by judiciously applying the modified Coffin-Manson equation for adhesive joints. Elasto-plastic material models have been employed for both the adhesive and the adherends. The predicted life has close agreement in the high cycle fatigue (HCF) regime with empirical observations reported in the literature.  相似文献   

16.
An investigation of an adhesively bonded composite joint with a brittle adhesive was conducted to characterize both the static and fatigue debond growth mechanism under mode I and mixed mode I-II loadings. The bonded system consisted of graphite/epoxy adherends bonded with FM-400 adhesive. Two specimen types were tested: (1) a double-cantilever-beam specimen for mode I loading and (2) a cracked-lap-shear specimen for mixed mode I-II loading. In all specimens tested, failure occurred in the form of debond growth either in a cohesive or adhesive manner. The total strain-energy-release rate is not the criterion for cohesive debond growth under static and fatigue loading in the birttle adhesive as observed in previous studies with the ductile adhesives. Furthermore, the relative fatigue resistance and threshold value of cyclic debond growth in terms of its static fracture strength is higher in the brittle adhesive than its counterpart in the ductile adhesive.  相似文献   

17.
This paper discusses the static and fatigue behavior of adhesively bonded single lap joints in SMC-SMC composites. Effects of lap length and adhesive thickness on the static and fatigue strength of SMC-SMC adhesive joints are studied. Effects of SMC surface preparation and test speed on the joint performance are evaluated. Finally, the effect of water exposure on the joint durability is also investigated. Results show that the static behavior of adhesive joints in SMC-SMC composites is significantly influenced by the lap length and adhesive thickness. With an increase in lap length from 12.7 mm to 38.1 mm, the joint failure load increases by 37%. The joint failure load also increases with the adhesive thickness, but it reaches a maximum at an adhesive thickness of 0.33 mm and then decreases. However, lap length and adhesive thickness have negligible effect on the ratio of fatigue strength to static strength. The fatigue strength at 106 cycles is approximately 50% to 54% of the static strength for various adhesive thicknesses and lap lengths investigated in this study. Adhesive failure, fiber tear or combination of these two failure modes are observed during both static and fatigue tests.  相似文献   

18.
In this paper, a method for the optimal design of the adhesively-bonded tubular single lap joint was proposed based on the failure model of the adhesively-bonded tubular single lap joint. The failure model incorporated the nonlinear mechanical behavior of the adhesive as well as the different failure modes in which the adhesive failure mode changed from bulk shear failure, via transient failure, to interfacial failure between the adhesive and the adherend, according to the magnitudes of the residual thermal stresses induced by fabrication.

The effects of the design parameters for the adhesively-bonded tubular single lap joint, such as the thicknesses of adhesive layer and adherends, the bonding length, and the scarfs of adherends, on the torque transmission capability and the efficiency of the adhesive joint were investigated.  相似文献   

19.
Since the surface roughness of adherends greatly affects the strength of adhesively bonded joints, the effect of surface roughness on the fatigue life of adhesively bonded tubular single lap joints was investigated analytically and experimentally by a fatigue torsion test. The stiffness of the interfacial layer between the adherends and the adhesive was modelled as a normal statistical distribution function of the surface roughness of the adherends. From the investigation, it was found that the optimum surface roughness of the adherends for the fatigue strength of tubular single lap joints was dependent on the bond thickness and applied load.  相似文献   

20.
In order to improve the tensile lap shear strength of adhesively bonded joints, nano-particles were dispersed in the adhesive using a 3-roll mill. The dispersion states of nano-particles in the epoxy adhesive were observed with TEM (Transmission Electron Microscopy) with respect to the mixing conditions, and the effect of nano-particles on the mechanical properties of the adhesive was measured with respect to dispersion state and weight content of nano-particles. Also the static tensile load capability of the adhesively bonded double lap joints composed of uni-directional glass/epoxy composite and nano-particle-reinforced epoxy adhesive was investigated to assess the effect of nano-particles on the lap shear strength of the joint. From the experimental and FE analysis results, it was found that the nano-particles in the adhesive improved the mechanical properties of the adhesive. Also the increased failure strain and the reduced CTE (coefficient of thermal expansion) of the nano-particle-reinforced adhesive improved the lap shear strength of adhesively bonded joints.  相似文献   