1.
35钢45钢化学成分与机械性能的关系   总被引:1,自引:0,他引:1  
通过两种钢数据的统计分析,结果表明,控制化学成分范围可使机械性能得到较大的提高,从而对现有的钢号标准有进一步探讨的必要。  相似文献   

2.
根据普通碳素钢的反弯矫直计算方法,对高速钢棒材的反弯矫直压下量进行了修正,并通过矫直实验进行了验证。  相似文献   

3.
概述了美国钢铁工业的发展历程、生产布局的演化,强调了在这一进程中电炉钢发展的重要性;对2000年以来美国钢铁工业的发展进行了简单分析,表明美国钢铁工业目前处于一个平稳发展阶段;最后总结了1998年前后美国钢铁工业的能源消耗水平,并对当前美国钢铁工业的能耗统计体系(MECS)和内容进行介绍,认为美国在节能工作方面取得了重大进展,但在节能技术方面仍有较大的潜力。  相似文献   

4.
为了提高A333Gr.3低温用无缝钢管的冲击韧性,对三种低温用无缝钢管进行了化学成分、有害元素、气体含量、轧态力学性能、热处理后的金相组织和力学性能分析对比.碳含量对钢管低温冲击韧性有明显的影响,碳含量越低,冲击韧性越高.钢中磷含量可显著提高钢的脆性转变温度,应进一步降低钢中磷含量,同时控制钢管轧制温度,降低钢管终轧温度,提高钢管冷却速度,细化晶粒度,这些措施都有助于提高无缝钢管低温冲击韧性.  相似文献   

5.
Metallographic data are presented for manganese steel before and after ladle treatment—specifically, treatment with calcium–strontium carbonate or argon injection in the ladle or both. Quantitative analysis of the nonmetallic inclusions is undertaken. The position of the inclusions relative to the grain boundaries is determined. Electron microscopy permits detailed study of the composition and form of the inclusions that appear during ladle treatment and without such treatment. The influence of various types of ladle treatment on the impact strength of manganese steel is discussed. Alloying of the manganese steel with vanadium is considered. Practical data regarding the influence of alloying with vanadium on the impact strength of the manganese steel are presented.  相似文献   

6.
李伯华 《包钢科技》2005,31(Z1):1-3
概述了美国对旧有大型钢铁联合企业的改造,提出了大力发展短流程钢厂的创新思路,显现了大力发展电炉新工艺的优越性.  相似文献   

7.
郑向东  代媛 《包钢科技》2007,33(1):68-70
随着我国钢铁行业产能的不断扩张,对供应链的建立和完善已日趋为钢铁业所重视,并纷纷着手建立了产品的供应链运作模式.今后的钢材市场竞争将是供应链与供应链之间的竞争.因此,对于包钢来说也应重点研究供应链的建立和完善.  相似文献   

8.
The hydrogen embrittlement resistances of 35KhGM steel in states of different strengths are compared. The effect of strength on the fracture mechanism and kinetics in the steel during hydrogen embrittlement is demonstrated using a joint analysis of acoustic emission signals and stress-strain diagram during tension, metallography, and fractography.  相似文献   

9.
张立峰  李燕龙  任英 《钢铁》2013,48(11):1-10
 从几个方面对多年来在钢中非金属夹杂物基础研究方面做的工作做简单介绍:钢中夹杂物和钢水洁净度的评估方法、稳态浇注和非稳态浇注的定义、非稳态浇注过程中形成的大颗粒夹杂物、总氧和大颗粒夹杂物的对应关系、脱氧过程夹杂物形成的热力学基础、钢水中夹杂物形核及长大的动力学研究和钢水中流体流动和夹杂物的运动、去除及被凝固前沿的捕捉。并讨论了钢中夹杂物研究下一步应该继续进行的工作,对洁净钢的生产提出了一些指导性意见。  相似文献   

10.
王国华  李建民 《山西冶金》2006,29(1):37-38,43
太钢第二炼钢厂以转炉、连铸机高效化生产为主线进行了一系列的技术改遣和项目建设,主要技术经济指标大幅度提高。具备了年产240万t碳钢的生产能力,成为一个具有竞争力的现代化炼钢厂。  相似文献   

11.
 介绍了特厚临氢设备用12Cr2Mo1R(HIC)钢板的生产工艺和技术指标,详细研究了钢板热处理工艺与组织对模拟焊后热处理和回火脆化倾向等性能的关系。以118mm厚钢板为例,给出了化学成分及力学性能结果,结果表明该特厚临氢设备用12Cr2Mo1R钢板成分均匀、杂质元素含量低、综合力学性能优良、回火脆化敏感性低。  相似文献   

12.
本文叙述企业在"八五”至"九五”期间依靠技术进步,为适应市场经济和广州市城市建设发展需要,进-步实施技术改造和搬迁,使企业在原有基础上获得了新的发展.  相似文献   

13.
研究了0.16C-10Ni-14Co-1Cr-1Mo(16NiCo)钢在510℃和0.23℃-12Ni-14Co-3Cr-1Mo(23NiCo)钢在482℃回火的组织与性能。随回火时间的延长,强度、硬度的降低主要是由于M_2C的粗化及与基体共格性降低所致。M_2C的粗化速度23NiCo钢要小于16NiCo钢。  相似文献   

14.
??The hot compression tests of 2. 25Cr1Mo steel at 950-1200??, 0. 01-10s-1, and deformation of 60% were carried out on a Gleeble- 1500D simulator. The effects of deformation temperature and strain rate on the dynamic recrystallization of 2. 25Cr1Mo steel were investigated. The models for dynamic recrystallization critical strains and dynamic recrystallization fraction were established. The results show that 2. 25Cr1Mo steel is more likely to undergo dynamic recrystallization at high temperature and high strain rate. The deformation activation energy and critical strains in dynamic recrystallization as well as dynamic recrystallization fraction model of 2. 25Cr1Mo steel were obtained. The constitutive equation of 2. 25Cr1Mo steel was constructed and the dynamic recrystallization physical metallurgical model of finite element software data interface was established. The model provides the basic conditions for the forging microscopic simulation of large forgings.  相似文献   

15.
The elemental and phase composition and defect structure of the surface layer on 5140 steel is considered after alloying by melting of a film–substrate (5140 steel) system under irradiation by intense pulsed electron beam; the film consists of aluminum or titanium. Treatment of the titanium–5140 steel system results in alloying to the depth of the molten layer (about 15 μm); polycrystalline structure (with submicron grains) based on α-phase hardened by titanium-carbide nanoparticles is formed. For the aluminum–5140 steel system, only a thin surface layer (about 2 μm) is alloyed, on account of the evaporation of aluminum from the steel surface. Martensit structure hardened by iron-aluminide nanoparticles is formed.  相似文献   

16.
通过理论计算确定氢离子辐照下武钢产SA738Gr.B钢位移损伤峰值的深度,对不同剂量辐照(0.2、0.5、1.0dpa)前后微观组织的特征和元素分布情况进行分析,判定离子辐照对SA738Gr.B钢的显微组织的影响.结果表明,通过高倍TEM观察以及STEM技术的分析,在SA738Gr.B钢基体中并未发现氢泡和大尺寸空位团,氢离子辐照下材料肿胀很小.通过对比0.5 dpa位移损伤量的微观组织与1.0 dpa位移损伤量的微观组织,可以明显看出,位移损伤量低的SA738Gr.B钢中的位错密度、位错环数量都大大降低.随着辐照剂量的提高,钢中位错密度和位错环数逐步增多,可以初步判定钢的辐照硬化效应程度.  相似文献   

17.
按酒钢炼钢一工序2007年实际情况,对钢铁料消耗进行了测算,结合2006年、2007年实际控制情况进行了对比分析,提出了在炼钢一工序现状条件以及目前钢铁料消耗核算制度下,主要影响钢铁料消耗指标的因素,并对进一步降低钢铁料消耗提出了建议。  相似文献   

18.
采用可控速热处理炉对核压力容器用SA508Gr.4N钢消除组织遗传性现象进行研究。为模仿大锻件锻后不同位置晶粒尺寸差异较大现象,对试验钢进行不同温度预粗化处理。设计了A和B两种方案消除试验钢的组织遗传性,结果表明:经方案A即等温退火+亚温正火+正火处理后,得到细小且均匀的晶粒,晶粒等级由2~9级细化为7.5~8.0级,该方案可有效消除SA508Gr.4N钢的组织遗传性现象。观察了等温退火、亚温正火和高温回火后试验钢组织的变化,分析了微观组织变化对消除试验钢组织遗传性的影响。  相似文献   

19.
对三钢厂结晶器振动参数的探讨   总被引:1,自引:0,他引:1  
主要介绍了结晶器振动参数及工艺效果 ,振动参数与拉速匹配关系 ,对三钢厂结晶器振动参数的设定进行了探讨  相似文献   

20.
太钢生产轴承钢已有较长时间并有过灿烂的历史,但近年日渐衰退,差距明显。通过开发新的冶炼生产工艺,拓宽产品规格、缩短工艺流程,改善外观质量,使太钢轴承钢生产再现辉煌。  相似文献   