1.
A series of triblock co‐polymers, consisting of a poly(ethylene glycol) (PEG) central block joined to two blocks of random p‐dioxanone‐co‐L ‐lactide copolymers were synthesized by ring‐opening polymerization of p‐dioxanone (PDO) and L ‐lactide (LLA) initiated by PEG in the presence of stannous 2‐ethylhexanoate catalyst. The resulting copolymers were characterized by various techniques including 1H and 13C NMR and FTIR spectroscopies, gel permeation chromatography, inherent viscosity, wide‐angle X‐ray diffractometry (WAXD) and differential scanning calorimetry (DSC). The conversion of PDO and L ‐lactide into the polymer was studied various mole ratios and at different polymerization temperature from 1H NMR spectra. Results of WAXD and DSC showed that the crystallinity of PEG macroinitiator was greatly influenced by the composition of PDO and L ‐lactide in the copolymer. The triblock copolymers with low molecular weight were soluble in water at below room temperature. © 2003 Society of Chemical Industry  相似文献   

2.
Two enantiomeric triblock ABA copolymers composed of poly(L ‐lactide)–poly(ethylene glycol)–poly(L ‐lactide) (PLLA–PEG–PLLA) and poly(D ‐lactide)–poly(ethylene glycol)–poly(D ‐lactide) (PDLA–PEG–PDLA) were synthesized with two different middle‐block PEG chain lengths by ring‐opening polymerization of L ‐lactide and D ‐lactide in the presence of PEG, respectively. A pair of enantiomeric triblock copolymers were combined to form a stereocomplex by a solvent‐casting method. The triblock copolymers and their stereocomplexes were characterized by 1H‐ and 13C‐NMR spectroscopy and gel permeation chromatography. Their crystalline structures and crystalline melting behaviors were analyzed by the wide‐angle X‐ray diffraction method and differential scanning calorimetry. The stereocomplex formed between a pair of enantiomeric triblock copolymers exhibited a higher crystalline melting temperature with a distinctive 3/1 helical crystalline structure. PLLA–PEG–PLLA and its stereocomplex with PDLA–PEG–PDLA were used to fabricate a series of microspheres encapsulating a model protein drug, bovine serum albumin (BSA). They were prepared by a double‐emulsion solvent‐evaporation method. The morphological aspects of the microspheres were characterized and BSA release profiles from them were investigated. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 75: 1615–1623, 2000  相似文献   

3.
Three types of copolymers were synthesized and characterized. First, triblock ABA copolymers [where A is a homopolymer of ?‐caprolactone and B is poly(ethylene glycol)] were prepared by the ring‐opening polymerization of poly(ethylene glycol) with ?‐caprolactone in the presence of stannous octoate (Sn(Oct)2). The spectral, thermal, and mechanical properties of one sample of these copolymers were studied, and it was discovered that these types of copolymers were more hydrophilic, possessed lower melting points, and had superior mechanical properties (greater toughness) than poly(?‐caprolactone). Second, triblock ABA copolymers [where A is a homopolymer of L ‐lactide and B is poly(ethylene glycol)] were prepared by the ring‐opening polymerization of poly(ethylene glycol) with L ‐lactide in the presence of Sn(Oct)2. The mechanical properties of these copolymers were studied, and it was found that they were tougher and softer than poly(L ‐lactide). Third, novel ABA triblock copolymers [where A is a copolymer of ?‐caprolactone and L ‐lactide and B is poly(ethylene glycol)] were prepared, and 1H‐NMR and 13C‐NMR spectra of these copolymers indicated a microblock structure for the two end blocks. The stress–strain behavior revealed low yields and high toughness for these copolymers. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 83: 2072–2081, 2002  相似文献   

4.
The quasiliving characteristics of the ring‐opening polymerization of ?‐caprolactone (CL) catalyzed by an organic amino calcium were demonstrated. Taking advantage of this feature, we synthesized a series of poly(?‐caprolactone) (PCL)–poly(L ‐lactide) (PLA) diblock copolymers with the sequential addition of the monomers CL and L ‐lactide. The block structure was confirmed by 1H‐NMR, 13C‐NMR, and gel permeation chromatography analysis. The crystalline structure of the copolymers was investigated by differential scanning calorimetry and wide‐angle X‐ray diffraction analysis. When the molecular weight of the PLA block was high enough, phase separation took place in the block copolymer to form PCL and PLA domains, respectively. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 2654–2660, 2006  相似文献   

5.
Diblock copolymers of poly(L ‐lactide)‐block‐poly(methyl methacrylate) (PLLA‐b‐PMMA) were synthesized through a sequential two‐step strategy, which combines ring‐opening polymerization (ROP) and atom transfer radical polymerization (ATRP), using a bifunctional initiator, 2,2,2‐trichloroethanol. The trichloro‐terminated poly(L ‐lactide) (PLLA‐Cl) with high molecular weight (Mn,GPC = 1–12 × 104 g/mol) was presynthesized through bulk ROP of L ‐lactide (L ‐LA), initiated by the hydroxyl group of the double‐headed initiator, with tin(II) octoate (Sn(Oct)2) as catalyst. The second segment of the block copolymer was synthesized by the ATRP of methyl methacrylate (MMA), with PLLA‐Cl as macroinitiator and CuCl/N,N,N′,N″,N″‐pentamethyldiethylenetriamine (PMDETA) as catalyst, and dimethyl sulfoxide (DMSO) was chosen as reaction medium due to the poor solubility of the macroinitiator in conventional solvents at the reaction temperature. The trichloroethoxyl terminal group of the macroinitiator was confirmed by Fourier transform infrared spectroscopy (FTIR) and 1H‐NMR spectroscopy. The comprehensive results from GPC, FTIR, 1H‐NMR analysis indicate that diblock copolymers PLLA‐b‐PMMA (Mn,GPC = 5–13 × 104 g/mol) with desired molecular composition were obtained by changing the molar ratio of monomer/initiator. DSC, XRD, and TG analyses establish that the crystallization of copolymers is inhibited with the introduction of PMMA segment, which will be beneficial to ameliorating the brittleness, and furthermore, to improving the thermal performance. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

6.
Poly (DL ‐lactic acid‐co‐glycolic acid)‐co‐poly(ethylene glycol) was synthesized by bulk ring‐opening polymerization of DL ‐lactide/glycolide/poly(ethylene glycol) using stannous chloride as an initiator. The molecular structure of the copolymer was analyzed by IR, 1H NMR, and DSC. The degradation behavior of copolymer was assayed by the reduction of molecular weight, the loss‐in‐mass, and the changes of pH value for degradation medium. The different contents of PGA and PEG in the molecules of the copolymer could control the degradation rate of polymer. Human Serum Albumin (HSA) was chosen as the model hydrophilic drug and encapsulated in the copolymer. The HA‐loaded copolymer microspheres were characterized by the diameter, diameter distribution of the microspheres, and the loading efficiency. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 90: 3150–3156, 2003  相似文献   

7.
Ring‐opening polymerization of L ‐ or D ‐lactide was realized at 140 °C for a period of 7 days in the presence of dihydroxyl poly(ethylene glycol) (PEG), with M?n = 4000 g mol?1, using zinc lactate as initiator. The resulting poly(L ‐lactide)–PEG–poly(L ‐lactide) and poly(D ‐lactide)–PEG–poly(D ‐lactide) triblock copolymers are water soluble with polylactide (PLA) block length ranging from 11 to 17 units. Both the tube inverting method and rheological measurements were used to evaluate the gelation properties of aqueous solutions containing single copolymers or L /D copolymer pairs. Stereocomplexation between poly(L ‐lactide) and poly(D ‐lactide) blocks is observed for mixed solutions. Hydrogel formation is detected in the case of relatively long PLA blocks (DP PLA = 17), but not for copolymers with shorter PLA blocks (DP PLA = 11–13) due to partial racemization of L ‐lactyl units. Racemization is largely reduced when the reaction time is shortened to 1 day. Under these conditions, DP PLA of 8 is sufficient for the stereocomplexation of PLA–PEG block copolymers, and DP PLA above 10 leads to the formation of hydrogels of PLA–PEG block copolymers. On the other hand, racemization appears as a general phenomenon in the (co)polymerization of L ‐lactide with Zn(Lac)2 as initiator, although it is negligible or undetectable in the case of high molar mass polymers. Therefore, racemization is the limiting factor for the stereocomplexation‐induced gelation of water‐soluble PLA–PEG block copolymers where the PLA block length generally ranges from 10 to 30. Reaction conditions including initiator, time and temperature should be strictly controlled to minimize racemization. Copyright © 2010 Society of Chemical Industry  相似文献   

8.
A series of biodegradable thermo‐sensitive hydrogels were synthesized by ring‐opening polymerization of methoxy‐poly(ethylene glycol) (mPEG) and various ester monomers, i.e. D ,L ‐lactide, glycolide, β‐propiolactone, δ‐valerolactone and ε‐caprolactone. The copolymers were characterized using 1H NMR spectroscopy and gel permeation chromatography. The micelle properties were also measured. The results indicated that the diblock copolymers formed nano‐micelles at low concentrations in aqueous phase. The lower critical solution temperatures of the diblock copolymers were above 35 °C at 1 wt%. As the temperature increased above room temperature, the diblock copolymer solutions underwent a sol‐to‐gel phase transition, which was manifested in viscosity increases, indicative of the formation of a gel. The mPEG–polyester diblock copolymer solutions exhibited sol‐gel transition behavior as a function of temperature and polymer concentration. Copyright © 2010 Society of Chemical Industry  相似文献   

9.
A series of aliphatic biodegradable poly (butylene succinate‐co‐ethyleneoxide‐co‐DL ‐lactide) copolyesters were synthesized by the polycondensation in the presence of dimethyl succinate, 1,4‐butanediol, poly(ethylene glycol), and DL ‐oligo(lactic acid) (OLA). The composition, as well as the sequential structure of the copolyesters, was carefully investigated by 1H‐NMR. The crystallization behaviors, crystal structure, and spherulite morphology of the copolyesters were analyzed by differential scanning calorimetry, wide angle X‐ray diffraction, and polarizing optical microscopy, respectively. The results indicate that the sequence length of butylene succinate (BS) decreased as the OLA feed molar ratio increasing. The crystallization behavior of the copolyesters was influenced by the composition and sequence length of BS, which further tuned the mechanical properties of the copolyesters. The copolyesters formed the crystal structures and spherulites similar to those of PBS. The incorporation of more content of ethylene oxide (EO) units into the copolyesters led to the enhanced hydrophilicity. The more content of lactide units in the copolyesters facilitated the degradation in the presence of enzymes. The morphology of the copolyester films after degradation was also studied by the scanning electron microscopy. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012  相似文献   

10.
A series of novel triblock copolymers, consisting of a poly(ethylene glycol) center block joined by two blocks of random L ‐lactide/glycolide copolymers, are synthesized and their characteristics (spectral, thermal, and mechanical) determined. Polymer compositions and structures are assessed via 1H‐NMR and 13C‐NMR spectroscopies. DSC and stress–strain behavior studies demonstrate that these copolymers are generally more amorphous, more elastic, and tougher than are poly(L ‐lactides). © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 74: 2004–2009, 1999  相似文献   

11.
The goal of this study was to synthesize novel biodegradable charged polymers for medical applications. The polymers synthesized were metal‐coordinated salicylidene‐based copolymers. The linear copolymers were prepared by polycondensation of the metal‐coordinated salicylidene monomer with acyl or aryl dichloride. Structure analysis was carried out by 1H and 13C NMR, FTIR, and elemental analysis. Physicochemical evaluation was carried out using DSC and thermogravimetry. The surface properties were analyzed by contact angle measurements and the crystallinity was determined by polarizing microscopy and AFM. Finally, polymer electrical conductivity and biocompatibility were examined. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 2568–2577, 2006  相似文献   

12.
Biodegradable polymers/oligomers were successfully synthesized through a ring‐opening polymerization of ε‐caprolactone and L ,L ‐lactide, initiated by L ‐arginine and L ‐citrulline. The α‐amino acid initiators are natural, operationally simple, inexpensive, environmentally friendly and safe for human health. The polymerizations were performed with no solvents and without introducing any metal impurities. The chemical structures of the polymers obtained were elucidated using 1H NMR, 13C NMR and Fourier transform infrared spectroscopies. In addition, incorporation of α‐amino acid molecules into the polymer chain was confirmed using matrix‐assisted laser desorption ionization time‐of‐flight mass spectrometry. Due to the significant biological activity of L ‐arginine and L ‐citrulline, these α‐amino acid initiators may open a new route for the synthesis of functional polymers especially for pharmaceutical applications. Copyright © 2011 Society of Chemical Industry  相似文献   

13.
The poly(ethylene terephthalate‐co‐ethyleneoxide‐co‐DL ‐lactide) copolymers were successfully prepared by the melt reaction between poly(ethylene terephthalate), poly(ethylene glycol), and DL ‐oligo(lactic acid) without any catalysts. The transesterification between ethylene terephthalate, ethyleneoxide, and lactide segments during the reaction was confirmed by the 1H NMR analysis. The effect of reaction temperatures and the starting feed ratios on the molecular microstructures, molecular weights, solubility, thermal properties, and degradability of the copolyesters was extensively studied. The values of crystallization temperature, melting temperature, crystallization, and melting enthalpy of the copolyesters were found to be influenced by the reaction temperatures, starting feed ratios, etc. The copolyesters showed good tensile properties and were found to degrade in the soil burial experiments during the period of 3 months. The morphology of the copolyester films were also investigated by scanning electron microscopy during soil burial degradation. POLYM. ENG. SCI., 2010. © 2009 Society of Plastics Engineers  相似文献   

14.
Well‐defined multiarmed star random and block copolymers of ε‐caprolactone with l ‐lactide with controlled molecular weights, low polydispersities, and precise numbers of arms were synthesized by the ring‐opening polymerization of respective cyclic ester monomers. The polymers were characterized by 1H‐NMR and 13C‐NMR to determine their chemical composition, molecular structure, degree of randomness, and proof of block copolymer formation. Gel permeation chromatography was used to establish the degree of branching. Star‐branched random copolymers exhibited lower glass‐transition temperatures (Tg's) compared to a linear random copolymer. When the star random copolymers were melt‐blended with poly(l ‐lactic acid) (PLA), we observed that the elongation of the blend increased with the number of arms of the copolymer. Six‐armed block copolymers, which exhibited higher Tg's, caused the maximum improvement in elongation. In all cases, improvements in the elongation were achieved with no loss of stiffness in the PLA blends. © 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016 , 133, 43267.  相似文献   

15.
In this study, ring‐opening graft polymerization of l ‐lactide onto cellulose was carried out homogeneously in ionic liquid (IL)/dimethyl sulfoxide (DMSO) co‐solvent as a reaction media. Through the effective control of high viscosity and steric hindrance caused by the interaction between the IL and the hydroxyl group of cellulose by adding DMSO as a co‐solvent, cellulose‐graft‐poly(l ‐lactide) (Cell‐g‐PLLA) copolymer with higher substitution efficiency was successfully prepared, at relatively low concentration of l ‐lactide. The maximum values of molar substitution, degree of lactyl substitution, and degree of polymerization of poly(l ‐lactide) in the copolymer were 3.76, 1.74, and 2.16, respectively, determined by 1H‐NMR. The prepared cell‐g‐PLLA copolymers showed thermal plasticization with a glass transition temperature of 155°C. In addition, the thermal processibility could be improved as the amount of grafted PLLA in the copolymer increased. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015 , 132, 41331.  相似文献   

16.
With D,L ‐lactic acid and Nϵ‐carbobenzoyloxy‐L ‐lysine [Lys(Z)] as the starting monomer material and tin dichloride as the catalyst, the drug carrier material poly(lactic acid‐coNϵ‐carbobenzoyloxy‐L ‐lysine) was synthesized via direct melt polycondensation. The copolymer was systematically characterized with intrinsic viscosity testing, Fourier transform infrared spectroscopy, 1H‐NMR, gel permeation chromatography, differential scanning calorimetry, and X‐ray diffraction. The influences of different feed molar ratios were examined. With increasing molar feed content of Lys(Z), the intrinsic viscosity, weight‐average molecular weight, and polydispersity index (weight‐average molecular weight/number‐average molecular weight) gradually decreased. Because of the introduction of Lys(Z) with a big aromatic ring into the copolymer, the glass‐transition temperature gradually increased with increasing feed charge of Lys(Z), and all of the copolymers were amorphous. The copolymers, with weight‐average molecular weights from 10,500 to 6900 Da, were obtained and could reach the molecular weight level of poly(lactic acid) modified by Lys(Z) via the ring‐opening polymerization of the cyclic intermediates, such as lactide and morpholine‐2,5‐dione. However, a few terminal carboxyl groups might have been deprotected during the polymerization reaction under high temperatures. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

17.
Poly(ethylene glycol)‐poly(L ‐lactide) diblock and triblock copolymers were prepared by ring‐opening polymerization of L ‐lactide with poly(ethylene glycol) methyl ether or with poly(ethylene glycol) in the presence of stannous octoate. Molecular weight, thermal properties, and crystalline structure of block copolymers were analyzed by 1H‐NMR, FTIR, GPC, DSC, and wide‐angle X‐ray diffraction (WAXD). The composition of the block copolymer was found to be comparable to those of the reactants. Each block of the PEG–PLLA copolymer was phase separated at room temperature, as determined by DSC and WAXD. For the asymmetric block copolymers, the crystallization of one block influenced much the crystalline structure of the other block that was chemically connected to it. Time‐resolved WAXD analyses also showed the crystallization of the PLLA block became retarded due to the presence of the PEG block. According to the biodegradability test using the activated sludge, PEG–PLLA block copolymer degraded much faster than PLLA homopolymers of the same molecular weight. © 1999 John Wiley amp; Sons, Inc. J Appl Polym Sci 72: 341–348, 1999  相似文献   

18.
Star‐block copolymers comprised of poly(styrene) (S) core and four poly(ε‐caprolacton) (ε‐CL) arms were synthesized by the combination of free radical polymerization (FRP) of S and ring opening polymerization (ROP) of ε‐CL in one‐step in the presence of tetrafunctional ineferter. The block copolymers were characterized by 1H‐NMR and FTIR spectroscopy, gel permeation chromatography (GPC), and fractional precipitation method. 1H ‐NMR and FTIR spectroscopy and GPC studies of the obtained polymers indicate that star‐block copolymers easily formed as result of combination FRP and ROP in one‐step. The γ values (solvent/precipitant volume ratio) were observed between 1.04–2.72 (mL/mL) from fractional measurements. The results show that when the initial S feed increased, the molecular weights of the star‐block copolymers also increased and the polydispersities of the polymers decreased. Mw/Mn values of the products were measured between 1.4 and 2.86 from GPC. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

19.
We propose here, a novel technique to synthesize high molecular weight (MW) poly (L ‐lactic acid)‐clay nanocomposite (PLACN), via solid state polymerization (SSP). We synthesize prepolymer of PLACN (pre‐PLACN) from both, L ‐lactic acid and L ‐lactide, as starting materials. Synthesis of pre‐PLACN from L ‐lactic acid is carried out via in situ melt polycondensation (MP) of L ‐lactic acid oligomer, followed by SSP, to achieve high MW PLACN (Mw ∼ 138,000 Da). In case of L ‐lactide as the starting material, we prepare L ‐lactide–clay intercalated mixture which yields moderate MW pre‐PLACN during subsequent ring opening polymerization (ROP). Interestingly, ROP is performed by using hydroxyl functionalized ternary catalyst system (L ‐lactide–Sn(II) octoate–oligo (L‐lactic acid) complex), which provides the terminal hydroxyl end‐groups, required for step‐growth SSP. Pre‐PLACN MW is now increased to Mw ∼ 127,000 Da, by the subsequent SSP process. 1H NMR analyses confirm that these end‐groups, are indeed consumed during SSP. During SSP, the PLACN also achieves up to 90% crystallinity, which may be due to the synchronization of the slow step‐growth SSP of poly(L ‐lactic acid) (PLA) with the crystallization kinetics. Optical purity of PLACNs is similar to that of neat PLA, whereas the thermal stability of PLACNs is significantly superior. As evidenced by wide‐angle X‐ray scattering/small‐angle X‐ray scattering analyses and in line with the literature, both, intercalated and exfoliated PLACN morphologies, have been synthesized, by suitable selection of clays. We also verify the correlation between the PLA semicrystalline morphology and the PLACN morphology, which is consistent with those of PLACN synthesized by other techniques. POLYM. COMPOS., 2011. © 2011 Society of Plastics Engineers  相似文献   

20.
Novel biodegradable polylactide (PLA) copolymers bearing pendant antimicrobial agent groups were successfully fabricated with a combination of ring‐opening copolymerization and copper(I)‐catalysed azide–alkyne cycloaddition click reaction in a two‐step reaction procedure. First, biodegradable PLA copolymers bearing azido groups were synthesized by the ring‐opening copolymerization of l ‐lactide and 2,2‐ bis(azidomethyl)trimethylene carbonate in the presence of 1‐dodecanol as protic co‐initiator and tin(II) 2‐ethylhexanoate (Sn(Oct)2) as the catalyst. Then, alkyne functionalized quaternary ammonium salts were attached onto the azido groups of the copolymers via a Huisgen 1,3‐dipolar cycloaddition reaction to give PLA imparting antimicrobial activity. The chemical structure and composition of the copolymers were clearly confirmed using 1H NMR and Fourier transform infrared spectroscopies and gel permeation chromatography. Thermal phase transition temperatures (Tm and Tg) and the thermal stability of the polymers were investigated by DSC and TGA experiments, respectively. The antimicrobial activity tests were carried out against Gram‐negative (Escherichia coli) and Gram‐positive (Staphylococcus aureus) bacteria by the drop plate method. It was observed that antimicrobial agents are more active in the polymeric form than in the monomeric form. Also, the activity depends on the compositional ratio and the length of the alkyl group on the ammonium salts. © 2018 Society of Chemical Industry  相似文献   