首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 31 毫秒
1.
Poly(ethylene oxide) (PEO) monochloro macroinitiators or PEO telechelic macroinitiators (Cl‐PEO‐Cl) were prepared from monohydroxyfunctional or dihydroxyfunctional PEO and 2‐chloro propionyl chloride. These macroinitiators were applied to the atom transfer radical polymerization of styrene (S). The polymerization was carried out in bulk at 140°C and catalyzed by Copper(I) chloride (CuCl) in the presence of 2,2′‐bipyridine (bipy) ligand (CuCl/bipy). The amphiphilic copolymers were either A‐B diblock or A‐B‐A triblock type, where A block is polystyrene (PS) and B block is PEO. The living nature of the polymerizations leads to block copolymers with narrow molecular weight distribution (1.072 < Mw/Mn < 1.392) for most of the macroinitiators synthesized. The macroinitiator itself and the corresponding block copolymers were characterized by FTIR, 1H NMR, and SEC analysis. By adjusting the content of the PEO blocks it was possible to prepare water‐soluble/dispersible block copolymers. The obtained block copolymers were used to control paper surface characteristics by surface treatment with small amount of chemicals. The printability of the treated paper was evaluated with polarity factors, liquid absorption measurements, and felt pen tests. The adsorption of such copolymers at the solid/liquid interface is relevant to the wetting and spreading of liquids on hydrophobic/hydrophilic surfaces. From our study, it is observed that the chain length of the hydrophilic block and the amount of hydrophobic block play an important role in modification of the paper surface. Among all of block copolymers synthesized, the PS‐b‐PEO‐b‐PS containing 10 wt % PS was found to retard water absorption considerably. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 4304–4313, 2006  相似文献   

2.
A poly(ethylene oxide)‐block‐poly(dimethylamino ethyl methacrylate) block copolymer (PEO‐b‐PDMAEMA) bearing an amino moiety at the PEO chain end was synthesized by a one‐pot sequential oxyanionic polymerization of ethylene oxide (EO) and dimethylamino ethyl methacrylate (DMAEMA), followed by a coupling reaction between its PEO amino and a biotin derivative. The polymers were charac terized with 1H NMR spectroscopy and gel permeation chromatography. Activated biotin, biotin‐NHS (N‐hydroxysuccinimide), was used to synthesize biotin‐PEO‐PDMAEMA. In aqueous media, the solubility of the copolymer was temperature‐ and pH‐sensitive. The particle size of the micelle formed from functionalized block copolymers was determined by dynamic light scattering. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 3552–3558, 2006  相似文献   

3.
Blends of poly(3‐hydroxy butyrate‐co‐3‐hydroxy valerate) (PHBV) and poly(ethylene oxide) (PEO) were prepared by casting from chloroform solutions. Crystallization kinetics and melting behavior of blends have been studied by differential scanning calorimetry and optical polarizing microscopy. Experimental results reveal that the constituents are miscible in the amorphous state. They form separated crystal structures in the solid state. Crystallization behavior of the blends was studied under isothermal and nonisothermal conditions. Owing to the large difference in melting temperatures, the constituents crystallize consecutively in blends; however, the process is affected by the respective second component. PHBV crystallizes from the amorphous mixture of the constituents, at temperatures where the PEO remains in the molten state. PEO, on the other hand, is surrounded during its crystallization process by crystalline PHBV regions. The degree of crystallinity in the blends stays constant for PHBV and decreases slightly for PEO, with ascending PHBV content. The rate of crystallization of PHBV decreases in blends as compared to the neat polymer. The opposite behavior is observed for PEO. Nonisothermal crystallization is discussed in terms of a quasi‐isothermal approach. Qualitatively, the results show the same tendencies as under isothermal conditions. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 2776–2783, 2006  相似文献   

4.
The transparent and flexible solid polymer electrolytes (SPEs) were fabricated from polyacrylonitrile‐polyethylene oxide (PAN‐PEO) copolymer which was synthesized by methacrylate‐headed PEO macromonomer and acrylonitrile. The formation of copolymer is confirmed by Fourier‐transform infrared spectroscopy (FTIR) measurements. The ionic conductivity was measured by alternating current (AC) impedance spectroscopy. Ionic conductivity of PAN‐PEO‐LiClO4 complexes was investigated with various salt concentration, temperatures and molecular weight of PEO (Mn). And the maximum ionic conductivity at room temperature was measured to be 3.54 × 10?4 S/cm with an [Li+]/[EO] mole ratio of about 0.1. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 461–464, 2006  相似文献   

5.
The crystallization behavior of two molecular weight poly(ethylene oxide)s (PEO) and their blends with the block copolymer poly(2‐vinyl pyridine)‐b‐poly(ethylene oxide) (P2VP‐b‐PEO) was investigated by polarized optical microscopy, thermogravimetric analysis, differential scanning calorimetry, and atomic force microscopy (AFM). A sharp decreasing of the spherulite growth rate was observed with the increasing of the copolymer content in the blend. The addition of P2VP‐b‐PEO to PEO increases the degradation temperature becoming the thermal stability of the blend very similar to that of the block copolymer P2VP‐b‐PEO. Glass transition temperatures, Tg, for PEO/P2VP‐b‐PEO blends were intermediate between those of the pure components and the value increased as the content of PEO homopolymer decreased in the blend. AFM images showed spherulites with lamellar crystal morphology for the homopolymer PEO. Lamellar crystal morphology with sheaf‐like lamellar arrangement was observed for 80 wt% PEO(200M) and a lamellar crystal morphology with grain aggregation was observed for 50 and 20 wt% blends. The isothermal crystallization kinetics of PEO was progressively retarded as the copolymer content in the blend increased, since the copolymer hinders the molecular mobility in the miscible amorphous phase. POLYM. ENG. SCI., 2012. © 2011 Society of Plastics Engineers  相似文献   

6.
Polystyrene (PS)/poly(ethylene oxide) (PEO) prototype brushes were prepared by alternating free‐radical copolymerization of methacryloyl‐terminated PS and α‐vinylbenzyl‐ω‐hydroxy or α‐vinylbenzyl‐ω‐perfluoroalkyl (Rf) PEO macromonomers with the addition of Lewis acid (SnCl4). It was found from their dilute‐solution properties that PS/PEO end‐capped with Rf (PBRf), and PS/PEO having OH groups at terminal ends (PBOH) prototype brushes formed a single molecule in benzene and aggregates in chloroform, respectively. However, the brush PBOH formed a single molecule in N,N‐dimethylformamide. Such aggregation behaviors seemed to be caused by the interaction between hydroxy groups of PEO chain ends. The brush PBOH was also converted into PBRf‐type brush by chemical modification, using corresponding acid chloride. The substitution of Rf groups was ~70% due to slipping of terminal hydroxy groups into PEO internal domains. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 772–778, 2006  相似文献   

7.
In virtue of the potential biomedical application of carbon nanotube (CNT), the CNT was hybridized into a supramolecular hydrogel based on the selective inclusion of α‐cyclodextrin (α‐CD) onto poly(ethylene oxide) (PEO) segments of a triblock copolymer, i.e., PEO‐block‐poly(propylene oxide)‐block‐PEO. Different from the previous report, the content of α‐CD, in contrast to that of ethylene oxide unit, was decreased to decrease the network density in hydrogel and hence improve the diffusion of encapsulated substances. As a result, the modulus of the hydrogels climbed slightly after introducing CNT. Furthermore, as the essential properties for wound dressing, the antimicrobial activity, the skin‐adhesion, and water‐retention of such supramolecular hybrid hydrogels were also verified. On the other hand, the supramolecular hybrid hydrogels inherited the shear‐thinning property and are suitable as an injectable biomaterial. The cell viability assay confirmed the equivalent cytotoxicity of the supramolecular hybrid hydrogels to that of the native hydrogels without CNT. Consequently, such CNT‐hybridized supramolecular hydrogel shows a great potential in the biomedical application. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

8.
To study the effect of the silica content on the properties of the salt‐free and salt‐added hybrids based on poly(ethylene oxide) (PEO) and silica, two series of hybrids, PEO–silica and PEO–silica–LiClO4 (O:Li, 9:1) hybrids were prepared via the in situ acid‐catalyzed sol–gel reactions of the precursors [i.e., PEO functionalized with triethoxysilane and tetraethyl orthosilicate (TEOS)]. The morphology of the hybrids was examined by scanning electron microscopy (SEM) of the fracture surfaces of the hybrid. The results indicated that the discontinuity develops with increasing the weight percent of silica in both hybrids. The differential scanning calorimetric (DSC) analysis indicated that effects of silica content on the glass transition temperatures (Tg) of the PEO phase were different in salt‐free and salt‐added hybrids. The Tg of PEO phase increased with increasing weight percent of silica in salt‐free hybrids, whereas the curve of Tg of PEO phase and silica content had a maximum at 35 wt % of silica content in salt‐added hybrids. For both salt‐free and salt‐added hybrids, peaks of the loss tangent, determined by dynamic mechanical analysis (DMA) were gradually broadened and lowered with increasing weight percent of silica. The storage modulus, E′, in the region above Tg increases with increasing silica content for both PEO–silica and PEO–silica–LiClO4 hybrids. In the conductivity and composition curves for PEO–silica–LiClO4 hybrids, the conductivity shows a maximum value of 3.7 × 10?6 S/cm, corresponding to the sample with a 35 wt % of silica. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 81: 2471–2479, 2001  相似文献   

9.
A series of well‐defined and property‐controlled polystyrene (PS)‐b‐poly(ethylene oxide) (PEO)‐b‐polystyrene (PS) triblock copolymers were synthesized by atom‐transfer radical polymerization, using 2‐bromo‐propionate‐end‐group PEO 2000 as macroinitiatators. The structure of triblock copolymers was confirmed by 1H‐NMR and GPC. The relationship between some properties and molecular weight of copolymers was studied. It was found that glass‐transition temperature (Tg) of copolymers gradually rose and crystallinity of copolymers regularly dropped when molecular weight of copolymers increased. The copolymers showed to be amphiphilic. Stable emulsions could form in water layer of copolymer–toluene–water system and the emulsifying abilities of copolymers slightly decreased when molecular weight of copolymers increased. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 727–730, 2006  相似文献   

10.
In this article, a series of poly(N‐isopropylacrylamide) (PNIPAM)‐based hydrogels were prepared under microwave irradiation using poly(ethylene oxide)‐600 (PEO‐600) as reaction medium and microwave‐absorbing agent as well as pore‐forming agent. All of the temperature measurements, gel fractions, and FTIR analyses proved that the PNIPAM hydrogels were successfully synthesized. Within 1 min, the PNIPAM hydrogel with a 98% yield was obtained under microwave irradiation. The PNIPAM hydrogels thus prepared exhibited controllable properties such as pore size, equilibrium swelling ratios, and swelling/deswelling rates when changing the feed weight ratios of monomer (N‐isopropylacrylamide, NIPAM) to PEO‐600. These properties are well adapted to the different requirements for their potential application in many fields such as biomedicine. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102:4177–4184, 2006  相似文献   

11.
Homogeneous solutions of syndiotactic polystyrene (sPS) in diglycidylether of bisphenol A (DGEBA), containing 2.5, 5 and 7.5 wt % of thermoplastic with or without 0.5 and 1 wt % of poly(styrene‐b‐ethylene oxide) (PS‐b‐PEO) block copolymer, were polymerized using a stoichiometric amount of an aromatic amine hardener, 4,4′‐methylene bis (3‐chloro‐2,6‐diethylaniline) (MCDEA). The dynamic‐mechanical properties and morphological changes of sPS‐(DGEBA/MCDEA) compatibilized with different amount of PS‐b‐PEO have been investigated in this paper. The addition of the block copolymer produced significant changes in the morphologies generated. The size of the dispersed spherical sPS spherulites does not change significantly, but less spherulites of sPS appeared upon network formation in the systems with compatibilizer, what means that addition of compatibilizer in this system delayed crystallization of sPS in sPS‐(DGEBA/MCDEA) systems and change phase separation mechanism from crystallization‐induced phase separation (CIPS) and reaction‐induced phase separation (RIPS) almost only to RIPS. Moreover, PS‐b‐PEO with higher molecular weight of PS block seems to be a more effective compatibilizer than one with lower molecular weight of PS block. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 479–488, 2006  相似文献   

12.
Polymer electrolyte membranes based on blends consisting of polyethylene oxide (PEO) grafted polyether sulfone (PES‐g‐PEO) and sulfonated polysulfone (SPSF(Na)) are prepared and their electrochemical and mechanical properties are investigated with respect to water electrolysis operation. The prepared blends are amorphous; they exhibit high glass transition temperatures and high thermal stability, thus ensuring the dimensional stability under electrolysis cell operation. Because of the presence of the water soluble constituent PES‐g‐PEO, the prepared blend membranes show very high water uptakes, reaching up to 370 wt %. Membrane electrode assemblies are fabricated and evaluated in single cells demonstrating that proton conductivity depends on the PEO‐g‐PES content as well as the PEO molecular weight. Namely, the increased concentration of PES‐g‐PEO leads to increased number of charge carriers, thus result in enhanced ionic conductivity. The use of longer PEO units (MW 5000), due to their improved chain mobility, facilitates the fast proton conduction as well. The maximum proton conductivity value is achieved (1.4 × 10?2 S cm?1, 80°C) for the blend with the higher PEO‐g‐PES content (20 wt %) and the higher PEO molecular weight (5000). Under electrolysis cell operation, the above‐mentioned membrane with the lower ohmic resistance shows the best performance, although it is still poor mainly due to the use of Pt as anode. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014 , 131, 39922.  相似文献   

13.
The AB type diblock PS‐b‐PEO and ABA type triblock PS‐b‐PEO‐b‐PS copolymers containing the same proportions of polystyrene (PS) and poly(ethylene oxide) (PEO) but different connection sequence were synthesized and investigated. Using the sequential living anionic polymerization and ring‐opening polymerization mechanisms, diblock PS‐b‐PEO copolymers with one hydroxyl group at the PEO end were obtained. Then, using the classic and efficient Williamson reaction (realized in a ‘click’ style), triblock PS‐b‐PEO‐b‐PS copolymers were achieved by a coupling reaction between hydroxyl groups at the PEO end of PS‐b‐PEO. The PS‐b‐PEO and PS‐b‐PEO‐b‐PS copolymers were well characterized by 1H NMR spectra and SEC measurements. The critical micelle concentration (CMC) and thermal behaviors were also investigated by steady‐state fluorescence spectra and DSC, respectively. The results showed that, because the PEO segment in triblock PS‐b‐PEO‐b‐PS was more restricted than that in diblock PS‐b‐PEO copolymer, the former PS‐b‐PEO‐b‐PS copolymer always gave higher CMC values and lower crystallization temperature (Tc), melting temperature (Tm) and degree of crystallinity (Xc) parameters. © 2015 Society of Chemical Industry  相似文献   

14.
Poly(lactide‐co‐glycolide) (PLGA 75 : 25), IV 0.94 dL/g was chosen as the matrix of the microparticles. Bovine serum albumin (BSA) (Fraction V) as the model drug was incorporated in the microparticles by a W/O/W emulsification and solvent evaporation technique. The effect of the various preparation parameters on particle morphology, drug loading efficiency, and drug release profiles of the resultant microparticles were examined. Particle size varied from 5 to 60 μm. The final morphology of the microparticles varied dramatically with preparation variables such as equipment used to produce the primary emulsion (W1/O) and the water‐to‐oil ratio (W1/O) in the primary emulsion. In general, the viscosity of the primary emulsion had a significant effect on the porosity of particles produced. The release of BSA showed a strong relationship with the preparation parameters of microparticles, partly due to the morphological effects. For example, microparticles made from the vortex mixer that was used to disperse inner aqueous phase (W1) to oil phase (O) showed a lower burst effect than that made from the homogenizer because of its better surface morphology. W1/O ratio, speed of dispersing the primary emulsion into W2, PLGA concentration, and different matrix materials also affected the drug release profiles. In all the samples studied here, only diffusion‐controlled release was observed. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 3053–3061, 2006  相似文献   

15.
In this work, we have synthesis nylon‐6/polyethylene oxide (PEO) copolymer system based on feed ratio of PEO (0~ 10 wt %) through condensation polymerization in a pilot scale. The structure of copolymer was confirmed by Fourier transform infrared (FTIR) spectroscopy and verified by 1H nuclear magnetic resonance (1HNMR). The thermal properties were investigated by differential scanning calorimetry (DSC) and indicated both melting temperature (Tm) and cold crystallization temperature (Tc) appearing unapparent decreased while increased PEO content in copolymers. The incorporation of PEO into the nylon‐6 chain reduced its tensile strength, modulus, and heat distortion temperature (HDT). The notched Izod impact strength of and ductility of the copolymers improved significantly as the PEO content was increased. The plasticizing effect was caused by the soft segments from PEO, which increases the mobility of the molecular chain in the copolymers. The results of mechanical tests agree closely with dynamic mechanical analysis (DMA) measurements. A rheological investigation revealed that neat nylon‐6 and its copolymer displayed similar behavior. The crystalline structure was examined by wide‐angle X‐ray diffraction (WAXD). The results demonstrate that the addition of a little PEO altered the crystallization from the α form to the γ form, mainly owing to the breaking parts of the original H‐bonds by the incorporation of ether groups. A mechanism of interaction between the amide and the ether group in nylon‐6/PEO copolymers is proposed. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

16.
A series of MC nylon‐6/ polyethylene oxide (PEO) blends were prepared via in situ polymerization. It was found that addition of PEO delayed the polymerization process of caprolactam. The apparent activation energy and pre‐exponential factor increased, indicating that the polymerization reaction became difficult with increasing PEO content. The stress–strain curves of the blends presented strain hardening behavior and increasing elastic deformation stress plateau at low PEO content. Nonisothermal DSC and XRD tests indicated that addition of PEO led to a decrease of the crystallization ability of the nylon‐6 matrix by reducing crystal grain size and crystallinity, whereas the crystallization ability of the PEO phase was improved. No co‐crystal formed between the two phases. PEO with low content only existed as amorphous state, while with increasing PEO content, PEO can crystallize gradually, forming interfibrillar segregation first, and then forming interspherilute segregation of the blend independently. By addition of PEO, the fracture surface of the blend became rough, displaying character of tough fracture. The interface between nylon‐6 phase and PEO phase was diffused, and the nylon‐6 matrix around the PEO particles presented fibrous structure, indicating the good compatibility between them. The toughening mechanism of the blend corresponded to the crazing‐shear banding mechanism. POLYM. ENG. SCI., 55:589–597, 2015. © 2014 Society of Plastics Engineers  相似文献   

17.
Viscometric behaviors of dextran (Dx), poly(N‐vinyl‐2‐pyrrolidone) (PVP), and poly(ethylene oxide) (PEO) with bovine serum albumin (BSA) in aqueous solutions have been studied at 25, 30, and 35°C. The reduced viscosity and intrinsic viscosity have been experimentally measured for the polymer/water and polymer/BSA/water systems by classical Huggins equation. Measurements of reduced viscosities of the Dx, PVP, and PEO in water have been calculated and all intrinsic viscosities of PEO([η]PEO) are larger than that of Dx([η]Dx), and PVP([η]PVP) in aqueous solutions, at all temperatures. The intrinsic viscosities of PVP, PEO, and Dx were found to be dependent on the concentration of BSA. The presence of BSA (0.05, 0.10, and 0.30 wt %) led to a decrease in the intrinsic viscosities of polymers, at 25, 30, and 35°C. The concentration difference of BSA (Δ[BSA]) is most effective in decreasing the intrinsic viscosities of Dx at 25°C and PEO at 30 and 35°C. In other words, Δ[η] (%) order followed as Dx > PEO > PVP at 25°C and PEO > Dx > PVP at 30 and 35°C. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1554–1560, 2006  相似文献   

18.
The electron spin resonance (ESR) spectra of end‐group spin labelled poly(ethylene oxide) (SLPEO) using 2,2,6,6‐tetramethyl‐piperdine‐1‐oxyl nitroxide and its blends with poly(styrene‐co‐4‐vinylphenol) (STVPhs) of different hydroxyl contents were recorded over a wide temperature range. For a blend of SLPEO and pure polystyrene (PS), the ESR spectrum was composed of a single motion component, indicating that PS was immiscible with PEO. For blends composed of SLPEO and different‐hydroxyl‐content STVPhs, two spectral components with different motion rates were observed over a certain temperature range. The difference between the motion rates should be attributed to micro‐heterogeneity in the blends, with the faster rate corresponding to a nitroxide radical motion trapped in the PEO‐rich domain and the slower rate corresponding to a nitroxide radical motion trapped in the STVPh‐rich domain. Variations in the values of a number of the ESR parameters (Ta, Td and T50G) and the apparent activation energy (Ea) with hydroxyl content in the blends indicated that the miscibility of the blends increased with increasing hydrogen‐bonding density due to specific interactions between the hydroxyl groups in STVPh and the ether oxygens in PEO. Copyright © 2004 Society of Chemical Industry  相似文献   

19.
A crystalline block copolymer of poly(ethylene‐block‐ethylene oxide) (PE‐b‐PEO) was successfully grafted onto a carbon black surface by direct condensation of its terminal hydroxyl groups with carboxyl groups on the surface using N,N′‐dicyclohexylcarbodiimide as a condensing agent. The electric resistance of the composite from PE‐b‐PEO (PEO content is above 50 wt %)‐grafted carbon black drastically increased to 104–106 times of the initial resistance in a vapor of dichloromethane, chloroform, tetrahydrofuran, and carbon tetrachloride, which are good solvents for PE‐b‐PEO, and returned immediately to the initial resistance when the composite was transferred in dry air. However, the change of the electric resistance of these composites was less than one‐tenth in a poor solvent vapor at the same condition. The response of the electric resistance was reproducible and stable even after exposure to a good solvent vapor and dry air with 30 cycles or exposure to the vapor over 24 h. The effect of PEO content on the vapor response was also investigated. The composite from PE‐b‐PEO‐grafted carbon black responded to the low vapor concentration with a linear relationship between the electric resistance and the concentration of the vapor in dry air. This indicates that the composite can be applied as a novel gas sensor. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 77: 2437–2447, 2000  相似文献   

20.
This study covers the crosslinking of poly(ethylene oxide) (PEO) and its composite with calcium hydroxyapatite (HA), their mechanical and swelling properties, and morphology. Sheets of the composites of PEO (two different grades with Mv: 5 × 106 and 2 × 105) and HA and neat PEO were prepared by compression molding. The prepared composite and PEO (0.1‐mm‐thick) sheets were crosslinked with exposure of UV‐irradiation in the presence of a photoinitiator, acetophenone (AP). This simple method for crosslinking, induced by UV‐irradiation in the presence of AP, yielded PEO with gel content up to 90%. Gel content, equilibrium swelling ratio, and mechanical and morphological properties of the low molecular weight polyethylene oxide (LMPEO)–HA crosslinked and uncrosslinked composites were evaluated. Although the inclusion of HA into LMPEO inhibits the extent of crosslinking, the LMPEO–HA composite with 20% HA by weight shows the highest gel content, with appreciable equilibrium swelling and mechanical strength. The growth of HA in simulated body fluid solutions on fractured surfaces of LMPEO and also LMPEO–HA was found to be very favorable within short times. The dimensional stability of these samples was found to be satisfactory after swelling and deposition experiments. The good compatibility between the filler hydroxyapatite and poly(ethylene oxide) makes this composite a useful tissue‐adhesive material. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 90: 488–496, 2003  相似文献   