A series of novel poly(trimethylene terephthalate‐co‐1,4‐cyclohexylene dimethylene terephthalate) (PTCT) with various compositions were synthesized by melt polycondensation of 1,3‐propanediol, 1,4‐cyclohexanedimethanol and dimethyl terephthalate. The resulting copolyesters were characterized using 13C and 1H nuclear magnetic resonance. The average length of both trimethylene terephthalate (TT) and cyclohexylene dimethylene terephthalate (CT) sequences varies from 1 to 10, and the chain structure is statistically random. The crystallization was investigated using wide angle X‐ray diffractometer (WAXD) and differential scanning calorimeter. The WAXD patterns can be divided in two groups according to the composition: copolyesters with less than 35 mol % CT content exhibit PTT‐type lattice, and those with CT unit content higher than 42 mol % crystallize with the PCT‐type lattice. The crystallizability of CT sequence is higher than that of TT sequence. Thermodynamic analysis shows that the comonomer is excluded from the PTT‐type or PCT‐type crystal of the copolyesters. The thermal decomposition temperature of copolyesters increases with increasing CT content, and their thermal stability is improved as compared to that of PTT. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

2.
Poly(butylene terephthalate‐co‐2‐methyl‐ethylene terephthalate) (PBT/MET) was synthesized by incorporating 1,2‐propandiol(1,2‐PDO) into PBT chains. The molar composition and chemical structure of PBT/MET copolyesters were confirmed by means of FT‐IR and 1H‐NMR. To investigate the effect of 1,2‐PDO on the thermal properties of PBT/MET copolyesters, the copolymerizations were carried out by varying various contents of MET units, and the prepared materials were evaluated by differential scanning calorimetry and thermogravimetric analysis. Results suggested that with the increase of the content of 1,2‐PDO, the amount of crystallinity and the melting temperature decline, while the glass transition temperature increases and the copolyesters become more transparent and brittle with respect to PBT homopolymer. In addition, the Tg‐composition and Tm‐composition data are well subjected to the Wood equation and Flory's equation, respectively. All these copolyesters are found to consist of the general trend displayed by copolymers reported elsewhere. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

3.
Differential scanning calorimetry (DSC) was used to evaluate the thermal behavior and isothermal crystallization kinetics of poly(ethylene terephthalate) (PET) copolymers containing 2‐methyl‐1,3‐propanediol as a comonomer unit. The addition of comonomer reduces the melting temperature and decreases the range between the glass transition and melting point. The rate of crystallization is also decreased with the addition of this comonomer. In this case it appears that the more flexible glycol group does not significantly increase crystallization rates by promoting chain folding during crystallization, as has been suggested for some other glycol‐modified PET copolyesters. The melting behavior following isothermal crystallization was examined using a Hoffman–Weeks approach, showing very good linearity for all copolymers tested, and predicted an equilibrium melting temperature (Tm0) of 280.0°C for PET homopolymer, in agreement with literature values. The remaining copolymers showed a marked decrease in Tm0 with increasing copolymer composition. The results of this study support the claim that these comonomers are excluded from the polymer crystal during growth. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 2592–2603, 2006  相似文献   

4.
A series of random copolymers were synthesized by the bulk polycondensation of dimethyl terephthalate with ethylene glycol (EG) and propane‐1,3‐diol (PDO) in various compositions. Their composition and thermal properties were investigated. The copolymers with 57.7 mol % or more PDO or 14.4 mol % or less PDO were crystallizable, but those with 36–46.2 mol % PDO were amorphous. The nonisothermal crystallization behavior was investigated with varying cooling rates by DSC. Poly(ethylene terephthalate) (PET) and poly(trimethylene terephthalate) (PTT) homopolymers have relatively lower activation energy than their copolymers. PET‐rich copolymers (EG > 85.9%) exhibited PET crystal structure, and exhibited no PTT crystal structure; and PTT‐rich copolymers (PDO > 41.7%) exhibited PTT crystal structure, and exhibited no PET crystal structure. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007  相似文献   

5.
A series of aliphatic–aromatic poly(carbonate‐co‐ester)s poly(butylene carbonate‐co‐terephthalate)s (PBCTs), with weight‐average molecular weight of 113,000 to 146,000 g/mol, were synthesized from dimethyl carbonate, dimethyl terephthalate, and 1,4‐butanediol via a two‐step polycondensation process using tetrabutyl titanate as the catalyst. The PBCTs, being statistically random copolymers, show a single Tg over the entire composition range. The thermal stability of PBCTs strongly depends on the molar composition. Melting temperatures vary from 113 to 213°C for copolymers with butylene terephthalate (BT) unit content higher than 40 mol %. The copolymers have a eutectic melting point when about 10 mol % BT units are included. Crystal lattice structure shifts from the poly(butylene carbonate) to the poly(butylene terephthalate) type crystal phase with increasing BT unit content. DSC and WAXD results indicate that the PBCT copolymers show isodimorphic cocrystallization. The tensile modulus and strength decrease first and then increase according to copolymer composition. The enzymatic degradation of the PBCT copolymers was also studied. © 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015 , 132, 41952.  相似文献   

6.
The effects of incorporating 5‐tert‐butylisophthalic acid (tBI) and 1‐3/1‐4 cyclohexanedimethanol (CHDM) in the polymer chain of poly(ethylene terephthalate) (PET) on the crystallization behavior and thermal, optical and tensile properties of this polyester (PETGB) were evaluated. These random copolyesters that contained between 0 and 20 mol % of CHDM and between 0 and 10 mol % of tBI units were prepared by esterification followed by melt copolycondensation. The compositions and molecular weights of the copolyesters were determined by 1H‐NMR spectroscopy and viscometry, respectively. The composition of the polyester was consistent with the composition of the feed. The intrinsic viscosities of the copolymers ranged between 0.62 and 0.74 dL/g. The thermal behaviors were investigated over the entire range of copolymer compositions, using DSC under the heating and cooling rate of 20°C/min and TGA. The copolyesters with tBI and CHDM of < 20 mol % were crystallizable, whereas the copolyesters with tBI and CHDM of ≥ 20 mol % were amorphous. They appeared to be stable up to 395°C. The optical transmissions of the amorphous polyesters were more than 88% in the visible region. The mechanical behavior was investigated by performing a tensile test. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 104: 279–285, 2007  相似文献   

7.
Poly(ethylene isophthalate‐co‐ethylene terephthalate) (PEIPET) copolymers of various compositions and molecular weights were synthesized by melt polycondensation and characterized in terms of chemical structure and thermal and rheological properties. At room temperature, all copolymers were amorphous and thermally stable up to about 400°C. The main effect of copolymerization was a monotonic increase of glass transition temperature (Tg) as the content of ethylene terephthalate units increased. The Fox equation accurately describes the Tg–composition data. The presence of ethylene terephthalate units was found to influence rheological behavior in the melt, with the Newtonian viscosity increasing as the content of ethylene terephthalate units increased. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 186–193, 2004  相似文献   

8.
The conformational changes, crystal structure and melting behavior of poly(ethylene/trimethylene terephthalate) (ET) copolyesters were investigated using in situ Fourier transform infrared (FTIR) spectroscopy, wide‐angle X‐ray diffraction (WAXD), transmission electron microscopy (TEM) and differential scanning calorimetry (DSC) under isothermal crystallization conditions. The results show that the minimum melting temperature was observed in ET53, in which the relative amount of ethylene glycol (EG) to 1,3‐propanediol (PDO) was 52.68/47.32 and the PDO‐dimethyl terephthalate (DMT)‐PDO segments in the molecular chain dominated the crystal formation. The minimum crystallinity of ET copolyesters was found in ET66, in which the relative amount of EG/PDO was 65.91/34.09 and the EG‐DMT‐EG segments in the molecular chain dominated the crystal formation. A rapid and continuous conformational transition in ET copolyesters was observed using in situ FTIR in the first 10 min under isothermal crystallization conditions. The continuously adjusting conformation in the molecules reflects the crystallization of ET copolyesters. Based on the DSC and the X‐ray analyses of the crystallization behavior in the ET copolyesters, crystalline conformation transitions of molecules in ET copolyesters take place rapidly and early. Copyright © 2012 Society of Chemical Industry  相似文献   

9.
A series of biodegradable aliphatic‐aromatic copolyester, poly(butylene terephthalate‐co‐butylene adipate‐co‐ethylene terephthalate‐co‐ethylene adipate) (PBATE), were synthesized from terephthalic acid (PTA), adipic acid (AA), 1,4‐butanediol (BG) and ethylene glycol (EG) by direct esterification and polycondensation. The nonisothermal crystallization behavior of PBATE copolyesters was studied by the means of differential scanning calorimeter, and the nonisothermal crystallization kinetics were analyzed via the Avrami equation modified by Jeziorny, Ozawa analysis and Z.S. Mo method, respectively. The results show that the crystallization peak temperature of PBATE copolyesters shifted to lower temperature at higher cooling rate. The modified Avrami equation could describe the primary stage of nonisothermal crystallization of PBATE copolyesters. The value of the crystallization half‐time (t1/2) and the crystallization parameter (Zc) indicates that the crystallization rate of PBATE copolyesters with more PTA content was higher than that with less PTA at a given cooling rate. Ozawa analysis was not suitable to study the nonisothermal crystallization process of PBATE copolyesters, but Z.S. Mo method was successful in treatingthis process. POLYM. ENG. SCI., 2011. © 2011 Society of Plastics Engineers  相似文献   

10.
Two series of amorphous copolyesters, PETGN and PETGS, were synthesized by the copolymerization of 2,6‐naphthalene dicarboxylic acid (NDA) (0–40%), succinic acid (SA) (0–40%), 1,3/1,4‐cyclohexanedimethanol (1,3/1,4‐CHDM) (10–50%), ethylene glycol (EG), and terephthalic acid (TPA). The compositions and molecular weights of the copolyesters were determined by 1H NMR spectroscopy and viscometry, respectively. The thermal behaviors were studied over the entire range of copolymer compositions, using DSC and TGA. The optical characteristics, heat‐shrinkable effects and tensile properties of these polymers were also determined. Experimental results indicated that the thermal, optical, tensile, and shrinkage properties of PETGN and PETGS were functions of NDA or SA content. DSC and X‐ray analysis demonstrated that both PETGN and PETGS series were amorphous. Incorporating NDA and SA influenced the Tg values of those polymers, from about 37°C for PETG30S40 to 89°C for PETG30N40. Furthermore, the shrinkage of these amorphous copolyesters was more than 40% when the heating temperature was higher than the corresponding Tg. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008  相似文献   

11.
Poly(trimethylene terephthalate‐co‐2‐methyl‐ ethylene terephthalate) random copolymers of various compositions were synthesized via traditional two‐step polycondensation by incorporating of 1,2‐propanediol. The molar composition of trimethylene terephthalate and 2‐methyl‐ethylene terephthalate units and chemical structure were confirmed by means of 1H‐NMR and Fourier transform infrared. The thermal properties of the copolyesters were evaluated by DSC and TGA. As far as the thermal properties is concerned, the main effect of incorporation of 1,2‐propanediol was a lowering in the melting temperature, and an increment of glass transition temperature compared to homopolymer PTT. Due to the effect of the lateral methyl groups in the polymeric chain, the thermal stability is slightly decreased as the amount of the MET units is increased. Furthermore, the crystals of PTT/MET copolyesters were observed by hot‐stage optical polarizing microscopy at the indicated crystallization temperatures. As expected, the incorporation of MET units in the polymer chain of PTT was found to decrease the dimension of the crystals. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

12.
With the aim to develop novel biodegradable materials with good flexibility and fast degradation rate, random copolymers of ?‐caprolactone (CL) and p‐dioxanone (PDO) with a full range of compositions were synthesized in bulk using stannous octoate as the ring‐opening catalyst. The chemical composition and number average sequence lengths of CL and PDO units determined by 1H‐NMR were used to correlate with various properties of the copolymers. Although both CL and PDO are crystalline components, only one crystalline phase could be present for each copolymer. The low limit of average block length for the copolymers that could crystallize is 3.22 for LCL and 3.43 for LPDO, respectively. The crystallinity and crystalline morphology of the copolymers are dependent on the crystalline component as well as its number average sequence length. Irrespective of composition, all the copolymers have good solubility in chloroform with glass transition temperature much below room temperature, implying good flexibility of the materials. The incorporation of PDO component could significantly increase the water wettability of the copolymer surfaces and thereby accelerate the degradation rate of the materials. In conclusion, flexible biodegradable polymers with adjustable degradation and crystalline properties were acquired by random copolymerization of CL and PDO, which are expected to use in tissue engineering and drug delivery fields. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 130: 2978–2986, 2013  相似文献   

13.
In this study, a series of aliphatic–aromatic poly(butylene terephthalate‐co‐ε‐caprolactone) (PBTCL) copolyesters were synthesized from various monomeric compositions of terephthalic acid (TPA), 1,4‐butanediol (BDO), and ε‐caprolactone (CL) in the presence of tetrabutyl titanate (Ti(Obu)4) and stannous octoate (Sn(Oct)2) as catalysts through a combination of polycondensation and ring opening polymerization. A significant increase in the melting temperature (Tm) of copolyesters was observed by increasing the TPA/(CL+TPA) molar ratio, starting from the low end (Tm 66.2°C) of pure poly‐ε‐caprolactone PCL upward. We found that PBTCL‐50, which has a TPA/(CL+TPA) 50% molar ratio and polycondensation at 260°C for 1.5 h, resulted in a proper Tm of 139.2°C that facilitates thermal extrusion from biomass or other biodegradable polymers of similar Tm. The number–average molecular weight (Mn) of 7.4 × 104 for PBTCL‐50 was determined from the intrinsic viscosity [η] by using the Berkowitz model of Mn = 1.66 × 105[η]0.9. Good mechanical properties of PBTCL‐50 have been shown by tensile stretching experiment that indicates tensile strength, elongation, and Young's modulus are 11.9 MPa, 132%, and 257 MPa, respectively. Polymers with aforementioned properties are suitable for manufacturing biodegradable plastic films for downstream agricultural applications or merely for trash bag. This article reveals that the PBTCL‐50 contains all five monomers with different molar ratios and characteristical linkages between each other. The novel structure was furthermore analyzed by 1H‐ and 13C‐NMR spectroscopy. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

14.
Segmented copolymers with telechelic poly(2,6‐dimethyl‐1,4‐phenylene ether) (PPE) segments and crystallizable bisester tetra‐amide units (two‐and‐a‐half repeating unit of nylon‐6,T) were studied. The copolymers were synthesized by reacting bifunctional PPE with hydroxylic end groups with an average molecular weight of 3500 g/mol and bisester tetra‐amide units via an ester polycondensation reaction. The bisester tetra‐amide units had phenolic ester groups. By replacing part of the bisester tetra‐amide units with diphenyl terephthalate units (DPT), the concentration of tetra‐amide units in the copolymer was varied from 0 to 11 wt%. Polymers were also prepared from bifunctional PPE, DPT, and a diaminediamide (6T6‐diamine). The thermal and thermal mechanical properties were studied by DSC and DMA and compared with a copolymer with flexible spacer groups between the PPE and the T6T6T. The copolymers had a high Tg of 180–200°C and a melting temperature that increased with amide content of 220–265°C. The melting temperature was sharp with monodisperse amide segments. The TmTc was 39°C, which suggests a fast, but not very fast, crystallization. The crystallinity of the amide was ~ 20%. The copolymers are semicrystalline materials with a high Tg and a high Tg/Tm ratio (> 0.8). © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 103: 512–518, 2007  相似文献   

15.
Short‐segmented block copolymers of poly(butylene succinate‐co‐butylene fumarate) were synthesized and their crystallinity and crosslinking behavior were investigated. 1H NMR was used to characterize the microstructure and composition of the copolyesters. Molecular weight determination was performed using gel permeation chromatography. Based on the DSC results all copolyesters were crystalline and the degree of crystallinity of the copolymers did not change with butylene fumarate mole fraction due to co‐crystallization of the butylene succinate and butylene fumarate groups. Crosslinked copolyesters showed a lower crystallization rate and degree of crystallinity while the crystallization temperature shifted to higher temperatures compared with uncrosslinked copolyesters due to the formation of nucleating agents by crosslinkages. Photo‐DSC was used to investigate the crosslinking kinetics for UV‐initiated photo‐curing. Three kinetics parameters including the rate constant (k) and the orders of the initiation and propagation reactions (m and n, respectively) were determined for the quenched and unquenched copolymers. © 2016 Society of Chemical Industry  相似文献   

16.
Poly(butylene adipate‐co‐succinate) (PBAS), an aliphatic polyester, is known for its excellent biodegradability, but its physical and mechanical properties are poor. To improve the physical properties, stiff aromatic rings were added to PBAS through transesterification with poly(ethylene terephthalate) (PET). New biodegradable copolyesters were prepared by the intermolecular ester‐exchange reactions between molten PBAS and PET. The transesterification reaction was carried out at 280°C without a catalyst. The newly synthesized copolyesters were characterized with 1H‐NMR spectroscopy, differential scanning calorimetry, and thermogravimetric analysis. The mechanical properties were measured with a universal test machine, and the biodegradability was also investigated. By the new peaks appearing in 1H‐NMR spectra of the copolyesters, the occurrence of the transesterification reaction between PBAS and PET was confirmed. A reduction of the melting temperature was observed for the copolyesters. The elongations at break of the new copolyesters increased for all compositions and reaction times, in comparison with PBAS. However, the tensile strength decreased with the induction of terephthalate units in the copolyesters. The biodegradability of the copolyesters also depended on the number of terephthalate units. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 3266–3274, 2004  相似文献   

17.
Poly(p‐dioxanone) (PPDO) has received significant attention due to its good biocompatibility and fast biodegradation profiles. In addition, PPDO is a polymer with high potential in biomedical applications. However, the conventional syntheses of PPDO via the ring‐opening polymerization (ROP) of p‐dioxanone (PDO) often use a metallic catalyst, which significantly limits its biorelated applications. This investigation was focused on the synthesis of metal‐free PPDO by using phosphazene base t‐BuP4 as the catalyst. The effects of the reaction conditions including temperature, reaction time, initiators, and feed molar ratios were studied in detail by nuclear magnetic resonance spectroscopy, viscosimetry, differential scanning calorimetry, and thermogravimetric analysis. The results showed that t‐BuP4 exhibited especially high activity in catalyzing alcohol or aniline to initiate the ROP of PDO, consequently resulting in metal‐free PPDOs. The polymerization was optimum at a reaction temperature of approximately 100°C and 88.7% of PDO was consumed. The viscosity–average molecular weights of the resulting polymer reached as high as 2.09 × 104 g/mol. The molar ratios of [PDO]/[t‐BuP4] also had an obvious effect on both the polymerization and the resulting polymer. Increasing [PDO]/[t‐BuP4] ratios facilitated the molecular weight growth, whereas the conversions of PDO significantly decreased. © 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016 , 133, 43030.  相似文献   

18.
The crystallization kinetics of poly(butylene terephthalate) (PBT), poly(ethylene terephthalate) (PET), and their copolymers poly(1,4‐butylene‐co‐ethylene terephthalate) (PBET) containing 70/30, 65/35 and 60/40 molar ratios of 1,4‐butanediol/ethylene glycol were investigated using differential scanning calorimetry (DSC) at crystallization temperatures (Tc) which were 35–90 °C below equilibrium melting temperature . Although these copolymers contain both monomers in high proportion, DSC data revealed for copolymer crystallization behaviour. The reason for such copolymers being able to crystallize could be due to the similar chemical structures of 1,4‐butanediol and ethylene glycol. DSC results for isothermal crystallization revealed that random copolymers had a lower degree of crystallinity and lower crystallite growth rate than those of homopolymers. DSC heating scans, after completion of isothermal crystallization, showed triple melting endotherms for all these polyesters, similar to those of other polymers as reported in the literature. The crystallization isotherms followed the Avrami equation with an exponent n of 2–2.5 for PET and 2.5–3.0 for PBT and PBETs. Analyses of the Lauritzen–Hoffman equation for DSC isothermal crystallization data revealed that PBT and PET had higher growth rate constant Go, and nucleation constant Kg than those of PBET copolymers. © 2001 Society of Chemical Industry  相似文献   

19.
The aim of the study was to investigate the mechanical properties and biodegradability of poly(trimethylenecarbonate‐ε‐caprolactone)‐block‐poly(p‐dioxanone) [P(TMC‐ε‐CL)‐block‐PDO] in comparison with poly(p‐dioxanone) and poly(glycolide‐ε‐caprolactone) (Monocryl®) monofilaments in vivo and in vitro. P(TMC‐ε‐CL)‐block‐PDO copolymer and poly(p‐dioxanone) were prepared by using ring‐opening polymerization reaction. The monofilament fibers were obtained using conventional melt spun methods. The physicochemical and mechanical properties, such as viscosity, molecular weight, crystallinity, and knot security, were studied. Tensile strength, breaking strength retention, and surface morphology of P(TMC‐ε‐CL)‐block‐PDO, poly(p‐dioxanone), and Monocryl monofilament fibers were studied by immersion in phosphate‐buffered distilled water (pH 7.2) at 37°C and in vivo. The implantation studies of absorbable suture strands were performed in gluteal muscle of rats. The polymers, P(TMC‐ε‐CL)‐block‐PDO, poly(p‐dioxanone), and Monocryl, were semicrystalline and showed 27, 32, and 34% crystallinity, respectively. Those mechanical properties of P(TMC‐ε‐CL)‐block‐PDO were comparatively lower than other polymers. The biodegradability of poly(dioxanone) homopolymer is much slower compared with that of two copolymers. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 737–743, 2006  相似文献   

20.
A series of new aliphatic/aromatic copolyesters [poly(hexylene terephthalate‐co‐hexylene adipate) (PHTA)] were synthesized on the bases of 1,6‐hexanediol, adipic acid, and dimethyl terephthalate and characterized by gel permeation chromatography, 1H‐NMR, wide‐angle X‐ray diffraction (WAXD), differential scanning calorimetry (DSC), and compost testing. 1H‐NMR results show that the compositions of the copolyesters were in accordance with the feed molar ratios. The WAXD patterns indicated that the crystal structures of the PHTA copolyesters were determined by the dominant crystal units, and the copolyesters became less crystallizable, even amorphous, with increasing comonomer content. The DSC curves showed that the glass‐transition temperatures (Tg′s) of the PHTA copolyesters decreased linearly, and both the melting temperature (Tm) and heat of fusion decreased first and then increased with increasing hexylene adipate unit content. Under compost conditions, PHTA copolyesters with less than 60 mol % aromatic units were biodegradable. Particularly, compared with the copolyester poly(butylene terephthalate‐co‐butylene adipate), the PHTA copolyester with the same aliphatic/aromatic composition possessed a lower Tg and Tm and better biodegradability. Additionally, the biodegradability of the copolyesters could be predicted by the number‐average sequence length of aromatic units, Tg, and the temperature difference between Tm and the temperature at which biodegradation took place. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   