首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 265 毫秒
1.
Five kinds of polytetrafluoroethylene (PTFE)-based composites were prepared: PTFE, PTFE + 30 vol % SiC, PTFE + 30 vol % Si3N4, PTFE + 30 vol % BN, and PTFE + 30 vol % B2O3. The friction and wear properties of these ceramic particle filled PTFE composites sliding against GCr15 bearing steel under both dry and liquid paraffin lubricated conditions were studied by using an MHK-500 ring-block wear tester. The worn surfaces and the transfer films formed on the surface of the GCr15 bearing steel of these PTFE composites were investigated by using a scanning electron microscope (SEM)and an optical microscope, respectively. The experimental results show that the ceramic particles of SiC, Si3N4, BN, and B2O3 can greatly reduce the wear of the PTFE composites; the wear-reducing action of Si3N4 is the most effective, that of SiC is the next most effective, then the BN, and that of B2O3 is the worst. We found that B2O3 reduces the friction coefficient of the PTFE composite but SiC, Si3N4, and BN increase the friction coefficients of the PTFE composites. However, the friction and wear properties of the ceramic particle filled PTFE composites can be greatly improved by lubrication with liquid paraffin, and the friction coefficients of the PTFE composites can be decreased by 1 order of magnitude. Under lubrication of liquid paraffin the friction coefficients of these ceramic particle filled PTFE composites decrease with an increase of load, but the wear of the PTFE composites increases with a load increase. The variations of the friction coefficients with load for these ceramic particle filled PTFE composites under lubrication of liquid paraffin can be properly described by the relationship between the friction coefficient (μ) and the simplified Sommerfeld variable N/P as given here. The investigations of the frictional surfaces show that the ceramic particles SiC, Si3N4, BN, and B2O3 enhance the adhesion of the transfer films of the PTFE composites to the surface of GCr15 bearing steel, so they greatly reduce the wear of the PTFE composites. However, the transfer of the PTFE composites onto the surface of the GCr15 bearing steel can be greatly reduced by lubrication with liquid paraffin, but the transfer still takes place. Meanwhile, the interactions between the liquid paraffin and the PTFE composites, especially the absorption of liquid paraffin into the surface layers of the PTFE composites, create some cracks on the worn surfaces of the ceramic particle filled PTFE composites; the creation and development of these cracks reduces the load-supporting capacity of the PTFE composites. This leads to the deterioration of the friction and wear properties of the PTFE composites under higher loads in liquid paraffin lubrication. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 73: 2611–2619, 1999  相似文献   

2.
Four kinds of polytetrafluoroethylene(PTFE)-based composites, such as pure PTFE, PTFE+30%(v)PbO, PTFE+30%(v)Pb3O4, and PTFE+30%(v)Cu2O composite, were prepared. The friction and wear properties of these metal oxides filled PTFE composites sliding against GCr15 bearing steel in both dry and lubricated conditions were studied by using an MHK-500 ring-block wear tester. Then the worn surfaces of these PTFE composites and the transfer films of these PTFE composites formed on the surface of GCr15 bearing steel were examined by using a Scanning Electron Microscope (SEM) and an Optical Microscope, respectively. Experimental results show that the friction and wear properties of these metal oxide-filled PTFE composites can be greatly improved by liquid paraffin lubrication, and the friction coefficients can be decreased by one order of magnitude. Meanwhile, the interactions between liquid paraffin and metal oxide-filled PTFE composites, especially the absorption of liquid paraffin into the surface layers of these PTFE composites, reduce the mechanical strength and the load-carrying capacity of these metal oxide-filled PTFE composites. This leads to the deterioration of the friction and wear properties of these PTFE composites. Investigations of the frictional surfaces show that Pb3O4, Cu2O, and PbO enhance the adhesion of the transfer films to the surface of GCr15-bearing steel, and thus promote the transfer of the PTFE composites onto the surface of GCr15-bearing steel. Therefore, they greatly reduce the wear of the PTFE composites. However, the transfer of these PTFE composites onto the counterfaces can be greatly reduced by lubrication with liquid paraffin. © 1997 John Wiley & Sons, Inc. J Appl Polym Sci 66: 85–93, 1997  相似文献   

3.
Four kinds of polytetrafluoroethylene (PTFE)-based composites, such as pure PTFE, PTFE + 30(v)%Cu, PTFE + 30(v)%Cu2O, and PTFE + 30(v)%CuS composite, were prepared. Then the friction and wear properties of the PTFE composites filled with Cu, Cu2O, or CuS sliding against GCr15-bearing steel under both dry and liquid paraffin-lubricated conditions were studied by using an MHK-500 ring-block wear tester. Finally, the worn surfaces and the transfer films of these PTFE composites formed on the surface of GCr15-bearing steel were investigated by using a scanning electron microscope (SEM) and an optical microscope, respectively. Experimental results show that the antiwear properties of these PTFE composites can be greatly improved by filling Cu, Cu2O, or CuS to PTFE, and the wear of these PTFE composites can be decreased by two orders of magnitude compared to that of pure PTFE under dry friction conditions. Meanwhile, CuS increases the friction coefficient of the PTFE composite, but Cu and Cu2O reduce the friction coefficients of the PTFE composites. However, the friction and wear properties of Cu, Cu2O, or CuS-filled PTFE composites can be greatly improved by lubrication with liquid paraffin. The friction coefficients of these PTFE composites can be decreased by one order of magnitude compared to those under dry friction conditions, while the wear of these PTFE composites can be decreased by one to two orders of magnitude. The PTFE + 30(v)%Cu composite exhibits excellent friction and wear-reducing properties under higher loads in liquid paraffin-lubricated conditions, so the PTFE + 30(v)%Cu composite is much more suitable for application under oil-lubricated conditions in practice. Optical microscope investigation of transfer films shows that Cu, Cu2O, and CuS enhance the adhesion of the transfer films to the surface of GCr15-bearing steel, so they greatly reduce the wear of the PTFE composites. However, the transfer of the PTFE composites onto the surface of GCr15-bearing steel can be greatly reduced by lubrication with liquid paraffin, but the transfer still takes place. SEM examination of worn surfaces shows that the interaction between liquid paraffin and the PTFE composites, especially the absorption of liquid paraffin into the surface layers of the PTFE composites, creates some cracks on the worn surfaces of Cu2O or CuS-filled PTFE composites, the creation and development of the cracks reduces the load-carrying capacity of the PTFE composites; this leads to the deterioration of the friction and wear properties of the PTFE composites under higher loads in liquid paraffin lubrication. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 70: 1455–1464, 1998  相似文献   

4.
Five kinds of polytetrafluoroethylene (PTFE)‐based composites, pure PTFE, PTFE + 30(v)% MoS2, PTFE + 30(v)% PbS, PTFE + 30(v)% CuS, and PTFE + 30(v)% graphite (GR) composites, were first prepared. Then the friction and wear properties of these PTFE composites, sliding against GCr15‐bearing steel under both dry and liquid paraffin‐lubricated conditions, were studied by using an MHK‐500 ring‐on‐block wear tester. Finally, the worn surfaces and the transfer films of the PTFE composites formed on the surface of GCr15 bearing steel were investigated by using a scanning electron microscope (SEM) and an optical microscope, respectively. Experimental results show that filling with MoS2, PbS, CuS, or graphite to PTFE can reduce the wear of the PTFE composites by two orders of magnitude compared to that of pure PTFE under dry friction conditions. However, the friction and wear‐reducing properties of these PTFE composites can be greatly improved by lubrication with liquid paraffin. Investigations of transfer films show that MoS2, PbS, CuS, and graphite promote the transfer of the PTFE composites onto the surface of GCr15‐bearing steel under dry friction conditions, but the transfer of the PTFE composites onto the surface of GCr15‐bearing steel can be greatly reduced by lubrication with liquid paraffin. SEM examinations of worn surfaces show that with lubrication of liquid paraffin, the creation and development of the cracks occurred on the worn surfaces of the PTFE composites under load, which reduces the load‐supporting capacity of the PTFE composites. This would lead to the deterioration of the friction and wear properties of the PTFE composites under higher loads (>600N). © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 72: 751–761, 1999  相似文献   

5.
The effects of lubricating‐oil additive zinc dialkyldithiophosphate (ZDDP) on the friction and wear properties of polymers and their composites sliding against GCr15 bearing steel were studied by using an MHK‐500 ring‐on‐block wear tester (Timken wear tester). Then the frictional surfaces of the friction pairs were examined by using electron probe microanalysis (EPMA). Experimental results show that the ZDDP contained in liquid paraffin has little effect on the friction coefficients of the polyimide (PI) or polyamide 66 (PA66) against GCr15 bearing steel friction pairs compared with that under the lubrication of liquid paraffin, but it slightly reduces the friction coefficients of polytetrafluoroethylene (PTFE) or its composites against GCr15 bearing steel friction pairs. Under lubrication of liquid paraffin containing 2 wt % ZDDP, the ZDDP film absorbed on the frictional surfaces of the PTFE composites–GCr15 bearing steel friction pairs exhibits obvious antiwear properties; it greatly reduces the wear of pure PTFE and the PTFE composites filled with Pb, PbO, and MoS2; and the wear of the PTFE composites can be reduced by one order of magnitude compared with that under lubrication of pure liquid paraffin. Meanwhile, the inorganic fillers Pb, PbO, and MoS2 contained in PTFE have little effect on the absorption of ZDDP to the frictional surfaces, so they have little effect on the friction coefficients of the PTFE composites–GCr15 bearing steel friction pairs under the lubrication of liquid paraffin containing 2 wt % ZDDP. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 76: 1240–1247, 2000  相似文献   

6.
Polytetrafluoroethylene (PTFE)‐based composites, filled with CeO2, CeF3, and La2O3 in volume contents of 5, 10, 15, 20, and 30%, were prepared. Then, the friction and wear behavior of these PTFE composites sliding against GCr15 bearing steel under both dry and liquid paraffin‐lubricated conditions was evaluated using an MHK‐500 ring‐on‐block wear tester. Finally, the worn surfaces and the transfer films of these PTFE composites were investigated using a scanning electron microscope (SEM) and an optical microscope. Experimental results showed that filling CeO2, CeF3, and La2O3 into PTFE can reduce the wear of the PTFE composites by 1–2 orders of magnitude. When the content of CeO2 in PTFE is 15%, the friction and wear properties of the CeO2‐filled PTFE composite are the best. Meanwhile, when the content of La2O3 in PTFE is between 15 and 20%, the PTFE composite filled with La2O3 exhibits excellent friction and wear‐reducing properties. However, the friction coefficient of the CeF3‐filled PTFE composite increases but its wear decreases with increase in the content of CeF3 from 5 to 30%. The friction and wear‐reducing properties of CeO2‐, CeF3‐, and La2O3‐filled PTFE composites can be greatly improved by lubrication with liquid paraffin, but the limit loads of the PTFE composites decrease with increase in the content of CeO2, CeF3, and La2O3 in PTFE (from 5 to 30%) under the same conditions. Investigations of worn surfaces show that the interaction between liquid paraffin and the CeO2‐, CeF3‐, and La2O3‐filled PTFE composites, especially the absorption of liquid paraffin into the microdefects of the PTFE composites, creates some cracks on the worn surfaces of the PTFE composites and that the creation and development of the cracks reduces the mechanical strength and the load‐supporting capacity of the PTFE composites. However, with increase of the content of CeO2, CeF3, and La2O3 in the PTFE, the microdefects in the PTFE composites also increase, which would lead to increase in the number of the cracks on the worn surfaces of the PTFE composites under load and, so, in turn, lead to the reduction of the limit loads of the CeO2‐, CeF3‐, and La2O3‐filled PTFE composites under lubrication with liquid paraffin. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 78: 797–805, 1999  相似文献   

7.
The friction and wear properties of polytetrafluoroethylene (PTFE), polyimide (PI), and polyamide 66 (PA66) sliding against GCr15 bearing steel under both dry and oil-lubricated conditions were studied by using an MHK-500 ring-block wear tester (Timken wear tester), and then Stribeck's curves of PTFE, PI, and PA66 under lubrication of the oil were given out. The worn surfaces of these polymers and the transfer films formed on the counterfaces were examined by using a scanning electron microscope (SEM) and an optical microscope, respectively. Experimental results show that the friction and wear-reducing properties of PTFE, PI, and PA66 can be greatly improved by lubrication with liquid paraffin, and the friction coefficients can be decreased by 1 order of magnitude compared to those in dry friction condition. Under lubrication of liquid paraffin, the friction coefficients of PTFE, PI, and PA66 decrease with the increase of load, but the wear increases with the increase of load. The variations of friction coefficients with load for PTFE, PI, and PA66 under lubrication of liquid paraffin can be described properly by the Stribeck's curves, as given out in this article. Under higher loads and sliding speeds in liquid paraffin lubrication, the friction and wear reducing properties of PA66 are the best, and those of PTFE are the worst; therefore, PA66 is also very suitable for applications in oil-lubricated conditions. Meanwhile, SEM and optical microscope investigations show that the wear and transfer of PTFE, PI, and PA66 can be greatly reduced by lubrication of liquid paraffin, but they still take place. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 68: 2175–2182, 1998  相似文献   

8.
Polytetrafluoroethylene (PTFE)‐based composites filled with various inorganic fillers in a volume fraction of 30% were prepared. The tribological behavior of the PTFE composites sliding against AISI52100 steel under dry and liquid paraffin‐lubricated conditions was investigated on an MHK‐500 model ring‐on‐block test rig. The morphologies of worn surfaces and wear debris were observed with a scanning electron microscope (SEM) and an optical microscope. As the results, different fillers show different effects on the tribological behavior of the PTFE composites, while the composite shows much different tribological behavior under lubricated conditions as compared with dry sliding. The tribological behavior of the PTFE composites under dry sliding is greatly related to the uniformity and thickness of the transfer films. Only the PTFE composites with a transfer film of good uniformity and proper thickness may have excellent tribological behavior. The PTFE composites show much better tribological behavior under lubrication of liquid paraffin than under dry sliding, namely, the friction coefficients are decreased by 1 order of magnitude and the wear rate by 1–3 orders of magnitude. Observation of the worn composite surfaces with SEM indicates that fatigue cracks were generated under lubrication of liquid paraffin, owing to the absorption and osmosis of liquid paraffin into the microdefects of the PTFE composites. The creation and development of the fatigue cracks led to fatigue wear of the PTFE composites. This would reduce the mechanical strength and load‐supporting capacity of the PTFE composites. Therefore, the tribological behavior of the PTFE composites under lubrication of liquid paraffin is greatly dependent on the compatibility between the PTFE matrix and the inorganic fillers. In other words, the better is the compatibility between PTFE and fillers the better is the tribological behavior of the composites. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 80: 1891–1897, 2001  相似文献   

9.
SiC whisker-reinforced polyetheretherketone (PEEK) composites with different filler proportions were made into block specimens by compression molding. The friction and wear properties of the composites were investigated on a block-on-ring machine by running a plain carbon steel (AISI 1045 steel) ring against the composite block under ambient conditions. The morphologies of the wear traces and wear debris were observed by scanning electron microscopy (SEM). It was found that SiC whisker-reinforced PEEK exhibited considerably lower friction coefficient compared with pure PEEK, while SiC whisker as a filler at a content of 1.25 to 2.5 wt % was very effective in reducing the wear rate of PEEK. Especially, the lowest wear rate was obtained with the composite containing 1.25 wt % SiC whisker. The SEM pictures of the wear traces indicated that PEEK composites undertook abrasive wear that was enhanced with increasing SiC whisker content, while for the frictional couple of carbon steel ring/composite block (reinforced with 1.25 wt % filler), a thin, uniform, and tenacious transfer film was formed on the ring surface. It was also supposed that the differences in the content of SiC whisker as filler could cause the differences in the wear mechanisms of SiC whisker-reinforced PEEK composites. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 69: 2341–2347, 1998  相似文献   

10.
Three‐dimensional (3D) braided carbon fiber reinforced polyetheretherketone (denoted as CF3D/PEEK) composites with various fiber volume fractions were prepared via hybrid woven plus vacuum heat‐pressing technology and their tribological behaviors against steel counterpart with different normal loads at dry sliding were investigated. Contrast tribological tests with different lubricants (deionized water and sea water) and counterparts made from different materials (epoxy resin, PEEK) were also conducted. The results showed that the incorporation of 3D braided carbon fiber can greatly improve the tribological properties of PEEK over a certain range of carbon fiber volume fraction (Vf) and an optimum fiber loading of ∼54% exists. The friction coefficient of the CF3D/PEEK composites decreased from 0.195 to 0.173, while the specific wear rate increased from 1.48 × 10−7 to 1.78 × 10−7 mm3 Nm−1 with the normal load increasing from 50 to 150 N. Abrasive mechanism was dominated when the composites sliding with GCr15 steel counterpart under dry and aqueous lubrication conditions. Deionized water and sea water lubricants both significantly reduced the wear of the CF3D/PEEK composites. When sliding with neat PEEK counterpart, the CF3D/PEEK composites possess lower friction coefficient than those against epoxy resin and GCr15 steel counterparts. In general, CF3D/PEEK composites possess excellent tribological properties and comprehensive mechanical performance, which makes it become a potential candidate for special heat‐resisting tribological components. POLYM. COMPOS., 36:2174–2183, 2015. © 2014 Society of Plastics Engineers  相似文献   

11.
The composites of polytetrafluoroethylene (PTFE) filled with expanded graphite (EG), poly(p‐oxybenzoyl) (POB), and basalt fiber (BF) were prepared by heating compression and sintering molding. The tribological behavior of PTFE composites was investigated with a pin‐on‐disk tester under dry conditions and seawater lubrication. The worn surface of PTFE composites and the transfer film on the counterface were observed with a scanning electron microscope. The results indicated that the incorporation of EG and POB improved the hardness of PTFE composites, and addition of BF led to greater load‐carrying capacity. Compared to pure PTFE, the coefficients of friction of PTFE composites slightly increased, but the wear rates were significantly reduced (the wear rate of composite with 3% EG being only 10.38% of pure PTFE). In addition, all the composites exhibited a lower coefficient of friction (decreases of about 0.03–0.07) but more serious wear under seawater lubrication than under dry sliding. The wear mechanism changed from serious abrasive wear of pure PTFE to slight adhesion wear of PTFE composites under both conditions. A transfer film was obviously found on the counterface in seawater, but it was not observed under dry conditions. Among all the materials tested, the PTFE‐based composite containing 20% POB (mass fraction), 2% EG, and 3% BF exhibited the best comprehensive performance. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 130: 2523–2531, 2013  相似文献   

12.
The wear-resistant polyamide 66 (PA66) composites were prepared and the mechanical properties, friction and wear properties were inspected. Results show that GF, PTFE and MoS2 can improve the mechanical, friction and wear properties of PA66 composites. PTFE is more effective on the friction and wear properties than MoS2 when GF is 30%wt. The best effect of the modification is 35%wt GF when both PTFE and MoS2 were added. Friction coefficient first increase, then reduce to be stable as sliding time increases. Friction coefficient and wear mass loss increase as load increases. The main wear mechanisms are fatigue and abrasion wears.  相似文献   

13.
不同介质中聚四氟乙烯复合材料的摩擦磨损性能   总被引:1,自引:0,他引:1       下载免费PDF全文
汪怀远  冯新  史以俊  何鹏  陆小华 《化工学报》2007,58(4):1053-1058
分别在碱液、水、油和干摩擦条件下考察了碳纤维和玻璃纤维填充聚四氟乙烯复合材料的摩擦磨损性能。利用SEM观察了不同介质中磨损面和对摩面的形貌,并探讨了其磨损机理。结果表明,不同介质中摩擦系数的大小关系是μ干>μ水或油>μ碱,磨损率是W水>W干>W碱或油。水、碱和油都不同程度地阻止了转移膜的形成。碱液和油具有很好的冷却与润滑作用,摩擦系数低,磨损小;然而水分子降低了填料和基体的界面粘接强度,造成犁削和磨粒磨损加重。  相似文献   

14.
Nano‐micro hierarchical porous polyphenylene sulfide/polytetrafluoroethylene (PPS/PTFE) composites were prepared by mold‐leaching and vacuum melting process under high temperature condition. The tribological behaviors of porous PPS/PTFE composites and the synergism as a result of incorporation of both micro‐porogen (NaCl) and mesoporous TiO2 whiskers were investigated. The effects of mesoporous TiO2 whiskers and nonperforated TiO2 whiskers on the friction and wear properties of PPS/PTFE composites were comparatively studied, respectively. Results indicated that the wear rate of porous PPS/PTFE composites with 30 wt % NaCl and 7 wt % mesoporous TiO2 whiskers obtained the lowest values under the load of 100 N. Compared with pure PPS, the wear resistance of nano‐micro porous PPS/PTFE composite was enhanced by 6.45 × 103 times, showing outstanding wear resistance. During sliding condition, grease could be squeezed through the nano‐micro pores under the coupling effect of load and friction heat, and formed a lubricanting layer on friction surface, providing self‐lubricating effect and high wear resistance. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

15.
The friction and wear behaviors of aramid-filled PA 6 composites filled with and without nano-MoS2 were investigated on an end-face tribometer through rubbing against ASTM 1045 steel under dry friction. The experimental results indicated that the wear rate and the friction coefficient of PA 6 decreased with the addition of nano-MoS2. The friction coefficients of PA 6 composites filled with aramid fiber are lower than those without nano-MoS2. The main wear mechanisms under dry sliding condition are the plastic deformation and mechanical microploughing. For best combination of friction coefficient and wear rate, the optimal volume content of MoS2 in the composites appears to be 10 vol %.  相似文献   

16.
PTFE/BaSO4复合材料摩擦磨损性能研究   总被引:1,自引:0,他引:1  
用M-2000型摩擦磨损试验机研究了干摩擦条件下BaSO4用量,载荷,对磨时间对聚四氟乙烯(PTFE)复合材料摩擦磨损性能的影响。在本实验条件下,PTFE/BaSO4复合材料的摩擦系灵敏随着BaSO4含量的增加而增大,抗磨损能力则有一个最佳含量;随着载荷的增加,材料的摩擦系数,磨损量和磨痕宽度也随之增大,磨损量随着对磨时间的延长而波动变小并趋于稳定。  相似文献   

17.
In this work, the influence of polytetrafluoroethylene (PTFE) filler size and testing conditions (i.e., air, water, and lubricating oil) on the tribological properties of poly(arylene ether nitrile) (PEN) was systematically investigated. The results showed that the addition of PTFE was beneficial to improve the tribological properties of PEN-based composites which was related to the easier formation of transfer film on the surface of friction pair. Samples which were tested in water demonstrated a relatively higher friction coefficient (μ) and wear loss when compared with those tested in dry air and lubricating oil scenarios, which was attributed to the fact that friction induced heat and wear debris could be timely removed by water. In addition, the infiltration of water further reduced the interaction between PTFE filler and PEN, which aggravated the wear loss of sample blocks. When tested in lubricating oil, pure PEN showed the lowest wear loss when compared with that of PEN/PTFE composites. At a given content (20 wt%) of PTFE fillers, PEN/PTFE1.5μm exhibited the lowest μ in lubricating oil whereas PEN/PTFE5μm demonstrated the lowest specific wear loss in air condition (1.18 × 10−6 mm3/N·m). This work provided some useful information for the design and application of PTFE-containing polymer composites that can be targeted in different lubrication scenarios in industrial fields.  相似文献   

18.
Micrometer and nanometer TiO2 particle‐filled poly(phthalazine ether sulfone ketone) (PPESK) composites with various filler volume fractions from 0.5 to 7.5 vol % were prepared by heating compression molding. The friction and wear behaviors of the PPESK composites were evaluated using the block‐on‐ring test rig by sliding PPESK‐based composite blocks against a mild carbon steel ring under dry friction conditions. The wear debris and the worn surfaces of the PPESK composites filled with micrometer and nanometer TiO2 particles were investigated by using a scanning electron microscope (SEM), while the structures of PPESK composites and wear debris were analyzed with IR spectra. Experimental results show that antiwear properties of the PPESK composites can be improved greatly by filling nanometer TiO2 particles, and the friction coefficient decreases when the filler volume fraction is below 2.5%, but when the filler volume fraction is above 2.5% the friction coefficient increases gradually with increasing filler volume fraction. In the case of micrometer TiO2 filler, wear rates increase with increasing filler volume fractions under identical test conditions, and the friction coefficients are less sensitive to the filler volume fraction. It was also found that the wear mechanism of micrometer TiO2 particle‐filled PPESK is mainly severe adhesion and abrasive wear, while that of nanometer TiO2 particle‐filled PPESK is mainly slight abrasive wear. In the former case, there are no transfer film formed on the surface of the counterpart steel, and wear debris are in the form of long and large ribbon. While in the latter case, the wear debris was granule and their size was about 10 μm. In case of 1 vol % nanometer TiO2 particle‐filled PPESK composites, the transfer film was fairly thinner and smoother, and the transfer film provided better coverage on the surface of steel ring, while that of 7.5 vol % was thicker and discrete. These account for the different friction and wear behavior of micrometer and nanometer TiO2 particle‐filled PPESK composite. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 906–914, 2004  相似文献   

19.
Al2O3/PTFE复合材料的磨损性能研究   总被引:2,自引:0,他引:2  
用机械共混、冷压成型烧结的方法制备了Al2O3/PTFE复合材料试样。用MM-200型磨损试验机测试了在干摩擦定载荷条件下各试样的磨损性能;用扫描电子显微镜(SEM)对磨损试样的表面形貌和磨屑的形貌进行了观察和分析;用光学显微镜对磨损后偶件环的表面形貌作了观察分析。结果表明:在实验条件下,Al2O3/PTFE复合材料的抗磨损性能,随Al2O3用量的增大逐渐增强,当Al2O3用量大于35%后,抗磨损性能增强的趋势明显减缓;在干摩擦条件下Al2O3/PTFE复合材料主要发生粘着磨损和磨粒磨损,且随Al2O3用量的增加,磨粒磨损所起的作用也增大。  相似文献   

20.
利用冷压烧结法制备了不同含量的聚四氟乙烯/纳米碳化硅(PTFE/纳米SiC)复合材料。采用MM-200型摩擦磨损试验机在干摩擦条件下考察了纳米SiC含量及载荷对PTFE/纳米SiC复合材料摩擦磨损性能的影响,借助于扫描电子显微镜观察分析了试样磨损表面形貌,并探讨了其磨损机理。结果表明,纳米SiC能够提高PTFE/纳米SiC复合材料的硬度和耐磨性,当纳米SiC质量分数为7%时,PTFE/纳米SiC复合材料的磨损量最小,摩擦系数也最小;随纳米SiC含量的增加,其摩擦系数有所增大;随着载荷的增大,PTFE/纳米SiC复合材料的磨损量增加。  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏