The poly(2‐methacryloyloxyethyl phosphorylcholine)‐block‐poly(D ,L ‐lactide) (PMPC‐b‐PLA) was specially designed to develop biomimetic giant vesicles (GVs) and giant large compound vesicles via a simple spontaneous assemble in aqueous solution. The weight fraction of the hydrophilic PMPC block (fPC) was proved to play an important role in the size and morphology control of the self‐assembled aggregates. The GVs with controlled micrometer size and biomimetic PMPC corona have great potential as artificial cell models. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

2.
Poly[2‐(methacryloyloxy)ethyl phosphorylcholine](PMPC) with one pendant tocopheryl moiety at the polymer terminus (PMPC‐Toco) was prepared by the radical polymerization of 2‐(methacryloyloxy)ethyl phosphorylcholine (MPC) initiated with 4,4′‐azobis[(3‐tocopheryl)‐4‐cyanopentanoate] in the presence of 2‐mercaptoethanol as a chain transfer reagent. The self‐organization of PMPC‐Toco was analyzed with fluorescence and 1H‐NMR measurements. The critical micelle concentrations of PMPC‐Toco with [η] = 0.25, 0.13, 0.10, and 0.05 dL g?1 were found to be 200, 100, 100, and 90 mg L?1, respectively. The blood compatibility of PMPC‐Toco was evaluated from the Michaelis constant (Km) for the enzymatic reaction of thrombin and a synthetic substrate, S‐2238, in the presence of PMPC‐Toco. The Km values were 0.21, 0.23, 0.36, and 0.21 for PMPC‐Toco‐1, 2, 3, and PMPC ([η] = 0.56 dL g?1), respectively. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

3.
The thermal degradation of poly(3‐hydroxybutyrate) (PHB) and poly(3‐hydroxybutyrate‐co‐3‐hydroxyvalerate) [P(HB‐HV)] was studied using thermogravimetry (TG). In the thermal degradation of PHB, the temperature at the onset of weight loss (To) was derived by To = 0.97B + 259, where B represents the heating rate (°C/min). The temperature at which the weight loss rate was maximum (Tp) was Tp = 1.07B + 273, and the final temperature (Tf) at which degradation was completed was Tf = 1.10B + 280. The percentage of the weight loss at temperature Tp (Cp) was 69 ± 1% whereas the percentage of the weight loss at temperature Tf (Cf) was 96 ± 1%. In the thermal degradation of P(HB‐HV) (7:3), To = 0.98B + 262, Tp = 1.00B + 278, and Tf = 1.12B + 285. The values of Cp and Cf were 62 ± 7 and 93 ± 1%, respectively. The derivative thermogravimetric (DTG) curves of PHB confirmed only one weight loss step change because the polymer mainly consisted of the HB monomer only. The DTG curves of P(HB‐HV), however, suggested multiple weight loss step changes; this was probably due to the different evaporation rates of the two monomers. The incorporation of 10 and 30 mol % of the HV component into the polyester increased the various thermal temperatures (To, Tp, andTf) by 7–12°C (measured at B = 20°C/min). © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 80: 2237–2244, 2001  相似文献   

4.
This article investigates the effects of electron beam (EB) radiation on poly(D ,L ‐lactic acid)‐b‐poly (ethylene glycol) copolymer (PLA‐b‐PEG‐b‐PLA). The copolymer films were EB irradiated at doses from 0 to 100 kGy. The degradation of these films was studied by measuring the changes in their molecular weight, mechanical and thermal properties. The dominant effect of EB radiation on PLA‐b‐PEG‐b‐PLA is chain‐scission. With increasing irradiation dose, recombination reactions or partial crosslinking may occur in addition to chain scission. The degree of chain scission Gs and crosslinking Gx of sample are calculated to be 0.213 and 0.043, respectively. A linear relationship is also established between the decreases in molecular weight with increasing irradiation dose. Elongation at break of the irradiated sample decreases significantly, whereas its tensile strength decreases slightly. The glass transition temperature (Tg) is basically invariant as a function of irradiation dose. Thermogravimetric analysis shows that its thermal stability decreases with increasing dose. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

5.
A series of copolymers of poly(2‐methacryloyloxyethyl phosphorylcholine)‐b‐poly(butylene succinate)‐b‐poly(2‐methacryloyloxyethyl phosphorylcholine) (PMPC‐b‐PBS‐b‐PMPC) were synthesized by atom transfer radical polymerization. The structure of the polymers was characterized by 1H NMR and infrared spectroscopy, and their thermal properties were described using TGA and DSC. In aqueous solutions, the PMPC‐b‐PBS‐b‐PMPC could form micelles with sizes ranging from 108 to 170 nm. In vitro release studies showed that acidic media and a longer PMPC chain benefited doxorubicin (DOX) release. 3‐(4,5‐dimethylthiazol‐2‐yl)‐2,5‐diphenyltetrazolium bromide (MTT) assays indicated that the micelles had low cytotoxicity to HeLa and L929 cells. DOX‐loaded micelles exhibited high cytotoxicity to HeLa cells. Flow cytometry results demonstrated that DOX‐loaded micelles could be internalized by HeLa cells. The in vitro phagocytosis results showed 3.9‐fold and 5.5‐fold reductions compared with poly(lactic acid) (PLA) nanoparticles and PDS55 micelles. These results demonstrate that PMPC‐b‐PBS‐b‐PMPC block copolymer micelles have great promise for cancer therapy. © 2017 Society of Chemical Industry  相似文献   

6.
A donor copolymer Poly{2,6‐4,8‐bis(2‐ethylhexyl)benzo[1,2‐b:3,4‐b′]dithiophene‐5,8‐2,3‐bis(5‐octylthiophen‐2‐yl)quinoxaline} (PBDTThQx) with benzo[1,2‐b:4,5‐b′]dithiophene and quinoxaline derivatives was synthesized and characterized with NMR, ultraviolet–visible spectroscopy, thermogravimetric analyses, and cyclic voltammetry. Photovoltaic devices with the configuration indium tin oxide–poly(3,4‐ethylenedioxythiophene)–poly(styrene sulfonate)–PBDTThQx–[6,6]‐phenyl‐C61‐butyric acid methyl ester (PC61BM)–LiF–Al were fabricated, in which PBDTThQx performed as the electron donor and PC61BM was the electron acceptor in the active layer. The device presented reasonable photovoltaic properties when the weight ratio of PBDTThQx:PC61BM reached 1:3. The open‐circuit voltage, fill factor, and power conversion efficiency were gauged to be 0.75 V, 0.59, and 0.74%, respectively. The experimental data implied that PBDTThQx would be a promising donor candidate in the application of polymer solar cells. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014 , 131, 40279.  相似文献   

7.
To develop conjugated polymers with low bandgap, deep HOMO level, and good solubility, a new conjugated alternating copolymer PC‐DODTBT based on N‐9′‐heptadecanyl‐2,7‐carbazole and 5, 6‐bis(octyloxy)‐4,7‐di(thiophen‐2‐yl)benzothiadiazole was synthesized by Suzuki cross‐coupling polymerization reaction. The polymer reveals excellent solubility and thermal stability with the decomposition temperature (5% weight loss) of 327°C. The HOMO level of PC‐DODTBT is ‐5.11 eV, indicating that the polymer has relatively deep HOMO level. The hole mobility of PC‐DODTBT as deduced from SCLC method was found to be 2.03 × 10?4 cm2/Versus Polymer solar cells (PSCs) based on the blends of PC‐DODTBT and [6,6]‐phenyl‐C71‐butyric acid methyl ester (PC71BM) with a weight ratio of 1:2.5 were fabricated. Under AM 1.5 (AM, air mass), 100 mW/cm?2 illumination, the devices were found to exhibit an open‐circuit voltage (Voc) of 0.73 V, short‐circuit current density (Jsc) of 5.63 mA/cm?2, and a power conversion efficiency (PCE) of 1.44%. This photovoltaic performance indicates that the copolymer is promising for polymer solar cells applications. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

8.
A series of new 5,6‐bis(tetradecyloxy)‐2,1,3‐benzoselenadiazole‐based copolymers ( PBDT‐DTBSe, PC‐DTBSe , and PF‐DTBSe) have been first synthesized by Stille or Suzuki coupling polymerization reaction. The synthesized copolymers show good solubility in common organic solvents, such as chloroform, tetrahydrofuran, and chlorobenzene with excellent film‐forming properties. The molecular weight was determined by gel permeation chromatography and the thermal properties were investigated by thermogravimetric analysis. All the copolymers exhibited broad absorption from 350 to 700 nm. The preliminary results showed the device based on the structure of indium tin oxide/PEDOT : PSS/ PC‐DTBSe : PC61BM (1 : 2, w/w)/Ca/Al displayed the best photovoltaic performance with a power conversion efficiency of 1.35%, a Voc of 0.87 V, a Jsc of 3.84 mA/cm2 and a fill factor of 40.4%, under illumination of AM 1.5 G (100 mW/cm2). © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

9.
Magnetic star‐shaped amphiphilic copolymers (S‐Fe3O4‐PLA‐b‐MPEG) consisting of Fe3O4 as the core, poly(L ,D ‐lactide) (PLA) as the inner layer, and monomethyl polyethylene glycol (MPEG) as the out shell were synthesized. The syntheses included ring‐opening polymerization of L ,D ‐lactide initiated by hydroxyl modified Fe3O4 (Fe3O4‐(OH) n), followed by the esterification of the PLA with MPEG. The structure of the star block copolymers were characterized by Fourier Transform infrared spectroscopy, thermogravimetric analysis, X‐ray diffraction, transmission electron microscopy, nanoparticle size analyzer, and vibrating sample magnetometer. The nanoparticles in aqueous solution were made from the amphiphilic star copolymer. The average size of the nanoparticles was adjustable and increased with the increase of the PLA segments in the copolymer. The cytotoxicity grade of the nanoparticles was zero determined by the analysis of cytotoxicity. The nanoparticles could potentially be used as the drug vehicles for magnetic‐response controlled release. POLYM. COMPOS., 2012. © 2012 Society of Plastics Engineers  相似文献   

10.
A thermosensitive amphiphilic triblock copolymer, poly(d,l ‐lactide) (PLA)‐b‐poly(N‐isopropyl acrylamide) (PNIPAAM)‐b‐PLA, was synthesized by the ring‐opening polymerization of d,l ‐lactide; the reaction was initiated from a dihydroxy‐terminated poly(N‐isopropyl acrylamide) homopolymer (HO‐PNIPAAM‐OH) created by radical polymerization. The molecular structure, thermosensitive characteristics, and micellization behavior of the obtained triblock copolymer were characterized with Fourier transform infrared spectroscopy, 1H‐NMR, gel permeation chromatography, dynamic light scattering, and transmission electron microscopy. The obtained results indicate that the composition of PLA‐b‐PNIPAAM‐b‐PLA was in good agreement with what was preconceived. This copolymer could self‐assemble into spherical core–shell micelles (ca. 75–80 nm) in aqueous solution and exhibited a phase‐transition temperature around 26 °C. Furthermore, the drug‐delivery properties of the PLA‐b‐PNIPAAM‐b‐PLA micelles were investigated. The drug‐release test indicated that the synthesized PLA‐b‐PNIPAAM‐b‐PLA micelles could be used as nanocarriers of the anticancer drug adriamycin (ADR) to effectively control the release of the drug. The drug‐delivery properties of PLA‐b‐PNIPAAM‐b‐PLA showed obvious thermosensitive characteristics, and the release time of ADR could be extended to 50 h. This represents a significant improvement from previous PNIPAAM‐based drug‐delivery systems. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017 , 134, 45304.  相似文献   

11.
The synthesis, characterization, photophysical and photovoltaic properties of two 5,6‐bis(octyloxy)benzo[c][1,2,5]thiadiazole‐containing wide‐band‐gap donor and acceptor D‐π‐A alternating conjugated polymers (HSD‐a and HSD‐b) have been reported. These two polymers absorb in the range of 300–700 nm with a band gap of about 1.88 and 1.97 eV. The HOMO energy levels were ?5.44 eV for HSD‐a and ?5.63 eV for HSD‐b. Polymer solar cells with HSD‐b :PC71BM as the active layer demonstrated a power conversion efficiency (PCE) of 2.59% with a high Voc of 0.93 V, a Jsc of 7.3 mA/cm2, and a comparable fill factor (FF) of 0.38 under simulated solar illumination of AM 1.5G (100 mW/cm2) without annealing. In addition, HSD‐a :PC71BM blend‐based solar cells exhibit a PCE of 2.15% with a comparable Voc of 0.64 V, Jsc of 8.75 mA/cm?2, and FF of 0.40. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015 , 132, 41587.  相似文献   

12.
Ferrocene‐substituted conducting polymer namely poly(trans‐1‐(4‐methyl‐3′‐thienyl)‐2‐(ferrocenyl)ethene‐co‐3,4‐ethylenedioxythiophene) [P(MTFE‐co‐EDOT)] was synthesized and its electrochromic properties were studied. Monomer, MTFE, was obtained using 2‐(ferrocenyl)ethene and 3‐methyl‐4‐bromothiophene. The structure of monomer was determined via Fourier transform infrared spectroscopy (FTIR), 1H‐NMR, and 13C‐NMR techniques. The copolymer was synthesized using this monomer and EDOT. The resulting copolymer P(MTFE‐co‐EDOT) was characterized by cyclic voltammetry, FTIR, scanning electron microscopy, atomic force microscopy, and UV–vis spectroscopy. The conductivity measurements of copolymer and PEDOT were accomplished by the four‐probe technique. Although poly(trans‐1‐(4‐methyl‐3′‐thienyl)‐2‐(ferrocenyl)ethene) [P(MTFE)] reveals no electrochromic activity, its copolymer with EDOT has two different colors (violet and gray). Band gap (Eg) and λmax of P(MTFE‐co‐EDOT) were determined. © 2012 Wiley Periodicals, Inc. J Appl Polym Sci, 2012  相似文献   

13.
Poly(styrene)‐poly(lactide) (PS‐PLA), poly (tert‐butyl styrene)‐poly(lactide) (PtBuS‐PLA) diblocks, and poly(tert‐butyl styrene)‐poly(styrene)‐poly(lactide) (PtBuS‐PS‐PLA) segmented and tapered triblocks of controlled segment lengths were synthesized using nitroxide‐mediated controlled radical polymerization. Well‐defined PLA‐functionalized macromediators derived from hydroxyl terminated TEMPO (PLAT) of various molecular weights mediated polymerizations of the styrenic monomers in bulk and in dimethylformamide (DMF) solution at 120–130°C. PS‐PLA and PtBuS‐PLA diblocks were characterized by narrow molecular weight distributions (polydispersity index (Mw/Mn) < 1.3) when using the PLAT mediator with the lowest number average molecular weight Mn= 6.1 kg/mol while broader molecular weight distributions were exhibited (Mw/Mn = 1.47‐1.65) when using higher molecular weight mediators (Mn = 7.4 kg/mol and 11.3 kg/mol). Segmented PtBuS‐PS‐PLA triblocks were initiated cleanly from PtBuS‐PLA diblocks although polymerizations were very rapid with PS segments ~ 5–10 kg/mol added within 3–10 min of polymerization at 130°C in 50 wt % DMF solution. Tapering from the PtBuS to the PS segment in semibatch mode at a lower temperature of 120°C and in 50 wt % DMF solution was effective in incorporating a short random segment of PtBuS‐ran‐PS while maintaining a relatively narrow monomodal molecular weight distribution (Mw/Mn ≈ 1.5). © 2008 Wiley Periodicals, Inc. J Appl Polym Sci 2008  相似文献   

14.
A biodegradable block copolymer, poly‐D ,L ‐lactide (PLA)‐co‐poly(ethylene glycol) (PEG), was prepared by the ring‐opening polymerization of lactide with stannous caprylate [Sn(Oct2)] as a catalyst; then, the PLA–PEG copolymer was made into nanoparticles by nanoprecipitation under different conditions. The average molecular weight and structure of PLA–PEG were detected by 1H‐NMR and gel permeation chromatography. The sizes and distributions of the nanoparticles were investigated with a laser particle‐size analyzer. The morphologies of the nanoparticles were examined by transmission electron microscopy. The effects of the solvent–nonsolvent system, operation conditions, and dosage of span‐80 on the sizes and distributions of the nanoparticles are discussed. The results show that acetone–water was a suitable solvent–nonsolvent system and the volume ratio of the nonsolvent phase to the solvent phase (O/W) (v/v), the concentration of PLA–PEG in the solvent phase, and the dosage of span‐80 had important effects on the particle sizes and distributions. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 98: 1884–1890, 2005  相似文献   

15.
Commercial EIA‐Y5V base‐metal‐electrode multilayer ceramic capacitors (BME‐MLCCs) made of (CaO+ZrO2)‐doped BaTiO3 are analyzed for the microstructure and investigated for its relation to dielectric properties. The characteristic diffuse scattering (DS) intensities observed in BaTiO3 ceramics and the featureless “solid‐solution” grains in Y5V capacitor chips are originated from multiple Ti sites in the dynamic BaTiO3 structure. The pseudo‐cubic (PC)‐grains retaining the overall cubic (C‐) symmetry metastably at room temperature are embedded with polar nanoregions (PNRs) in the ferroelectric (FE) tetragonal (T‐), and rhombohedral (R‐) phases, as revealed by high‐resolution transmission electron microscopy (HRTEM). The presence of PNRs contributes effectively to large relative permittivity εr ≈ 13 200 at 25°C. The FE T‐domains grow from within PC‐grains at the expense of embedded PNRs after prolonged annealing by extending “oxidizing firing” at 950°C in pO2 = 10?7 atm. These domains contain less Zr with otherwise homogeneously distributed solutes in PNR‐dispersed PC‐grains. Although preserving the relaxors characteristics, εr is reduced to ~11 000 after 12 h, and then to ~9000 after 24 h annealing. The reduction in εr is attributed to the annealing‐induced FE T‐domains grown at the expense of PNRs in PC‐grains. The Vögel–Fulcher analysis indicates that Y5V ceramics are in the relaxor FE category, containing PNRs derived from polarization frustration.  相似文献   

16.
Poly(3‐hydroxybutyrate‐co‐3‐hydroxyvalerate) (PHBV) was irradiated by 60Co γ‐rays (doses of 50, 100 and 200 kGy) under vacuum. The thermal analysis of control and irradiated PHBV, under vacuum was carried out by thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). The tensile properties of control and irradiated PHBV were examined by using an Instron tensile testing machine. In the thermal degradation of control and irradiated PHBV, a one‐step weight loss was observed. The derivative thermogravimetric curves of control and irradiated PHBV confirmed only one weight‐loss step change. The onset degradation temperature (To) and the temperature of maximum weight‐loss rate (Tp) of control and irradiated PHBV were in line with the heating rate (°C min?1). To and TP of PHBV decreased with increasing radiation dose at the same heating rate. The DSC results showed that 60Co γ‐radiation significantly affected the thermal properties of PHBV. With increasing radiation dose, the melting temperature (Tm) of PHBV shifted to a lower value, due to the decrease in crystal size. The tensile strength and fracture strain of the irradiated PHBV decreased, hence indicating an increased brittleness. Copyright © 2004 Society of Chemical Industry  相似文献   

17.
The isothermal crystallization kinetics of biodegradable blends made of poly(lactic acid) (PLA) and poly(ε‐caprolactone) (PCL) compatibilized with two different low molecular weight block copolymers, that is, ε‐caprolactone/tetramethylene ether glycol and ε‐caprolactone/aliphatic polycarbonate (CB), was done. Blends were prepared by melt mixing in an extruder, while isothermal crystallization kinetics and morphologies were investigated by thermal (differential scanning calorimetry) and thermo‐optical (quantitative polarized light optical microscopy [qPLOM]) quantitative methods. Data were analyzed using the Avrami equation, revealing 2D and 3D growth and simultaneous heterogeneous nucleation. The presence of low molecular weight compatibilizers, that is, 2,000 g mol?1, accelerated the PLA crystallization rate by two to threefold when compared with neat PLA, with high degrees of crystallinity (40–43%) as confirmed by PLOM images. The activation energy (Ea) showed that PCL inhibits PLA crystallization; however, the addition of block copolymers used as compatibilizers of the blends reduced Ea values, increasing the chain mobility of PLA and thus increasing the crystallization rate. POLYM. ENG. SCI., 59:E161–E169, 2019. © 2018 Society of Plastics Engineers  相似文献   

18.
Poly(lactic acid) (PLA) was reinforced halloysite nanotubes (HNTs) in this study. To improve dispersion and interfacial adhesion of HNTs within the PLA matrix, HNTs were surface modified with 3‐aminopropyltriethoxysilane (ASP) prior to compounding with PLA. PLA/ASP‐HNTs nanocomposites were characterized by differential scanning calorimetry (DSC), Fourier transfer infrared spectroscopy (FTIR), surface wettability, thermogravimetric analysis, transmission electron microscopy (TEM), and tensile testing. The hemocompatibility and cytocompatibility of PLA and PLA composites were investigated and the in vitro degradation process of PLA/ASP‐HNTs composites was investigated for a period of 6 months by gel permeation chromatography, FTIR, weight loss measurement, DSC, and tensile testing. PLA and all PLA composites were blood compatibile and non‐cytotoxic. TEM analysis revealed that HNTs agglomeration in PLA matrix was reduced by surface treatment with ASP. ASP‐HNTs had better reinforcing effect than unmodified HNTs evidenced by tensile testing. ASP‐HNTs appeared to increase the hydrolytic degradation process as measured by weight measurement. PLA/ASP‐HNTs composites displayed 12.1% weight loss and 30.6% average molecular weight reduction while retaining 74% of Young's modulus by the 24th week of degradation. Based on this data, the reinforcement of PLA using ASP‐HNTs may prove beneficial for applications such as biodegradable stents. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018 , 135, 46521.  相似文献   

19.
Polylactide (PLA) and a block copolymer, poly‐DL ‐lactide–poly(ethylene glycol) (PELA) were synthesized by bulk ring‐opening polymerization initiated by stannous chloride. A linear DNA molecule, λDNA, was used as the model DNA. PLA, PELA, λDNA‐loaded PLA and PELA microspheres were prepared by the solvent‐extraction method based on the formation of multiple w1/o/w2 emulsion. The particle‐size distribution, surface morphology, and DNA loading characterized the microspheres. The mean diameter of λDNA‐loaded PELA microspheres was proved to be 3.5 μm. The integrity of the λDNA molecules, after preparing the microspheres, was determined by agarose gel electrophoresis. The result suggested that most of the λDNA molecules could retain their integrity after being encapsulated by PELA. The PELA microspheres could also prevent λDNA from being degraded by DNase. The in vitro degradation and release of PLA, PELA, and λDNA‐loaded PELA microspheres were carried out in a pH 7.4 buffer solution at 37°C. Quantitatively, evaluating the molecular weight reduction, the mass loss, the particle‐size changes, and the particle‐size distribution changes also monitored the degree of degradation. The release profile was assessed by measurement of the amount of λDNA present in the release medium at determined intervals. The degradation profiles of the PELA microspheres were quite different from those of the PLA microspheres. The introduction of the hydrophilic poly(ethylene glycol) domain in PLA and the presence of λDNA within the microspheres exhibit the apparent influence on the degradation and release profiles. A biphasic release profile was proved, that is, an initial burst release during the first days, then a gradual release. It was demonstrated that the PELA microspheres could be used potentially as a controlled release‐delivery system for λDNA. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 2557–2566, 2002  相似文献   

20.
In this work, novel biodegradable crystalline silk nano‐discs (CSNs) having a disc‐like morphology have been utilized for fabrication of poly(lactic acid) (PLA) nanocomposites by melt‐extrusion. The main focus is to investigate the effect of CSN on isothermal melt crystallization kinetics, spherulitic growth rates, morphology, and hydrolytic degradation of PLA. Spherulitic morphology and growth rates are examined over a wide range of crystallization temperatures (90–120 °C). With incorporation of CSN, the isothermal crystallization kinetics of PLA/CSN increases, however, the crystallization mechanism remains unaltered. The apparent activation energy and surface energy barrier for crystallization process decreases upon addition of CSNs. At lower isothermal crystallization temperatures (Tc) viz. (90–100 °C), reduced growth rates of PLA spherulites is observed. Both PLA and PLA/CSN exhibit highest crystallization rates at around ~107 °C. The hydrolytic degradation rates calculated from molecular weight reduction shows that PLA/CSN nanocomposites' degradation rates are lower as compared to PLA in acidic, neutral, and alkaline media at pH = 2, 7, and 12, respectively, due to hydrophobic nature of CSN. Scanning electron microscopy study demonstrated the surface erosion mechanism of hydrolytic degradation of PLA and PLA/CSN nanocomposites. This work provides valuable insight for the application and reclamation of PLA/CSN bionanocomposites in moist and wet working environments. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018 , 135, 46590.  相似文献   