正中国地质科学院矿产综合利用研究所分别对拉拉铜铝多金属矿、炉霍铜锑矿以及代石沟低品位氧化铜矿开展了多金属矿分离新技术研究。拉拉铜钼多金属矿最终确定采用铜钼混合浮选一选钴一选铁一铜钼分离工艺流程,并进行了扩大试验,取得的技术指标为:铜精矿品位20.57%、回收率92.21%;钼精矿品位47.75%、回收率53.26%;铁精矿品位62.85%、回收率20.47%;钴精矿品位0.33%、回收率21.90%。铜  相似文献   

2.
正中国地质科学院矿产综合利用研究所分别对拉拉铜钼多金属矿、炉霍铜锑矿以及代石沟低品位氧化铜矿开展了多金属矿分离新技术研究。拉拉铜钼多金属矿最终确定采用铜钼混合浮选—选钴—选铁—铜钼分离工艺流程,扩大试验取得的技术指标为:铜精矿品位20.57%、回收率92.21%;钼精矿品位47.75%、回收率53.26%;铁精矿品位62.85%、  相似文献   

3.
某钼、锌、铁复杂多金属矿的选矿工艺研究   总被引:3,自引:0,他引:3  
李崇德  陈金中 《铜业工程》2006,(1):15-18,10
针对某钼、锌、铁复杂多金属矿石中含有可浮性极好的滑石、蛇纹石等特点,采用选择性捕收剂优先反浮选影响钼浮选的脉石,然后选钼,再锌、硫混选;浮选尾矿弱磁选铁。采用该工艺,试验获得了钼品位45.54%、回收率82.29%的钼精矿和锌品位48.07%、回收率84.14%的锌精矿,以及铁品位65.20%、对原矿全铁回收率53.46%(对原矿磁铁矿回收率81.30%)的铁精矿,同时获得了硫品位为38.75%、回收率为60.42%的硫精矿,使钼、锌、铁、硫都得到了综合回收。  相似文献   

4.
某选铁尾矿低碱度铜硫分离试验研究   总被引:1,自引:0,他引:1  
针对某选铁尾矿矿石性质,进行铜硫混合浮选,混合精矿再磨后铜硫分离的选别工艺,以乙黄药+丁胺黑药为组合捕收剂,新型抑制剂DT-4与石灰为铜硫分离抑制剂,进行铜硫浮选试验,最终获得铜品位26.68%,回收率80.39%铜精矿;硫品位47.68%,回收率74.82% 硫精矿,实现了铜硫的分离及铜硫的综合回收。  相似文献   

5.
《黄金》2015,(9)
新疆某铜铅锌矿属于难选低品位多金属硫化矿,原矿铜品位0.15%、铅品位3.52%、锌品位1.24%。针对该矿石性质,试验采用铜铅混合浮选—铜铅分离—铜铅尾矿选锌—锌尾矿再磁选铁的浮选流程,可获得铜品位22.30%、铜回收率68.63%的铜精矿,铅品位58.67%、铅回收率86.83%的铅精矿,锌品位42.85%、锌回收率65.32%的锌精矿,及品位67.0%的铁精矿,全铁回收率62.97%(对磁性铁的回收率为97.52%),闭路产品全部达到国家质量标准要求。  相似文献   

6.
斑岩型低品位铜钼矿石工艺矿物学研究   总被引:4,自引:0,他引:4  
采用显微镜研究、X-射线衍射分析、电子探针分析等手段,查明了某斑岩型低品位铜钼矿石矿物组成,铜、钼的赋存状态及主要矿物的嵌布特性。根据工艺矿物学研究结果,针对该矿石的性质特点,选矿试验采用铜钼硫混合浮选-铜钼浮选-铜钼分离的原则流程,最终得到良好指标:钼精矿钼品位46.28%,回收率70.26%;铜精矿铜品位22.31%,回收率84.19%;硫精矿硫品位30.24%,回收率69.60%。为了提高矿山的资源利用率,在浮选富集金属矿物之后,应在尾矿中回收钾长石、钠长石。  相似文献   

7.
西藏某铜钼矿矿石性质复杂多变,常常伴生有黄铁矿、方铅矿、闪锌矿,并且矿石矿泥含量波动较大。采用黄药作为捕收剂进行混合浮选能够取得较好的铜钼混合浮选指标,但在铜钼分离工艺流程难以实现有效的铜钼分离,尤其是黄铁矿、大量矿泥的进入往往造成钼精矿不合格。在铜钼分离过程中采用多种手段抑制黄铁矿、分散矿泥无果的情况下[1-6],为解决此问题,技术组采用煤油、丁基黄药对铜钼矿进行捕收的混合浮选工艺,在混合浮选目的矿物回收率指标不受影响的同时,铜钼分离指标得以明显改善。小型试验钼精矿钼品位由41.02%提升到49.12%。  相似文献   

8.
内蒙古某钼铋多金属硫化矿,含钼0.65 %,含铋1.12 %,钼铋品位较高,有较大的工业回收价值.采用“混合浮选—钼铋分离”的选矿工艺回收该矿石中的有用矿物,以乙硫氮和煤油作为捕收剂进行混合浮选,以硫化钠和亚硫酸钠作为组合抑制剂,煤油为捕收剂进行钼铋分离,最终实验室小型闭路试验可以获得含钼47.31 %,钼回收率89.52 %的钼精矿以及含铋42.64 %,铋回收率86.04 %的铋精矿,较好地实现了钼铋分离.   相似文献   

9.
铜、铅、锌、铁复杂多金属矿综合回收研究   总被引:2,自引:0,他引:2  
福建闽北某矿山复杂多金属矿含有铜、铅、锌、铁等多种有价金属矿物,综合利用价值高。通过对该矿石进行选矿试验研究,采用先浮后磁、部分混合浮选的流程,选出铜铅混合精矿、再进行铜、铅分离,然后浮选锌、硫,浮选尾矿经过磁选选铁,得出了铜精矿、铅精矿、锌精矿和铁精矿四种产品。为该矿多金属矿的综合利用提供了可行的方案。  相似文献   

10.
《中国钨业》2020,(1):29-35
某难选高硫含铜白钨矿中钨主要以白钨矿的形式存在,硫化铁主要以磁黄铁矿的形式存在。为给该矿石的开发利用提供技术支持,采用磁选-铜硫混合浮选-白钨浮选原则流程进行条件试验。结果表明,原矿磨矿至-74μm占65%时进行磁选,可获得品位为38.33%、回收率为51.14%的硫精矿,而磁选尾矿经铜硫混合-铜硫分离浮选,可分别获得品位为20.06%、回收率为73.12%的铜精矿和品位为35.20%、回收率为42.11%的硫精矿;其中铜硫混合浮选尾矿以碳酸钠为调整剂、水玻璃为抑制剂、731氧化石蜡皂为捕收剂,进行一粗一扫三精白钨常温浮选,可得到WO_3品位为63.93%、回收率为89.60%的白钨精矿,有效地实现了铜硫的分离和白钨矿的回收。  相似文献   

11.
对某铜钼硫多金属矿进行了选矿试验。采用钼铜混合浮选再分离工艺流程,在原矿含 Mo 0.17%、Cu 0.137%、S 5.36%、Pb 0.067%的条件下,获得了含钼49.26%、钼回收率82.66%的钼精矿及含铜15.45%、铜回收率53.52%的铜精矿。实现了钼铜硫矿物与脉石及钼铜硫矿物之间的有效分离,获得了良好的技术指标。  相似文献   

12.
陈磊  马亮 《铜业工程》2021,(4):47-51
The copper grade the low-grade copper-molybdenum ore in Shaanxi is 0.32% and the molybdenum grade is 0.048%.The copper and molybdenum minerals mainly exist in the form of sulfide ore. The properties are complex that there are many kinds of minerals in the ore, which are closely distributed and fine dissemination size. According to the properties of the ore, the technological process of bulk flotation and separation of copper and molybdenum was adopted in the experiment. With lime as regulator and reagent L03 as collector, the mixed concentrate of copper and molybdenum was obtained by the bulk flotation which flow-sheet is one roughing, three refining and two scavenging process. Then regrinding the mixed concentrate, use sodium sulfide as inhibitor of copper minerals, sodium silicate as slurry dispersant and inhibitor of silicate gangue minerals , kerosene as collector, can separate copper and molybdenum with the flow-sheet which one roughing, five refining and three scavenging. The copper concentrate with copper grade of 18.82% and copper recovery rate of 85.35% and molybdenum concentrate with molybdenum grade of 47.14% and molybdenum recovery rate of 79.24% were obtained by the final closed-circuit flotation test process, the indicator is nearly ideal.  相似文献   

13.
西藏某难选铜铅多金属矿石中多种金属矿物密切共生,硫化物之间嵌连关系较为复杂,且含有大量的次生硫化铜及氧化铜矿物,铜铅分选极为困难。针对该矿石特点,进行了铜铅混合浮选—混合精矿分离、优先浮钼、优先浮铜—再浮铅等多种工艺流程探索试验。结果表明:优先浮铜—再浮铅工艺流程可获得较好指标,闭路试验获得铜品位25.01%、铜回收率81.92%、含铅6.71%的铜精矿,铅品位45.89%、铅回收率70.09%、含铜1.69%的铅精矿,实现了矿石中铜铅的有效分离。  相似文献   

14.
对某斑岩型铜钼矿进行了选矿试验研究。采用钼铜等可浮浮选再分离-强化选铜工艺流程,采用CSU31作等可浮浮选捕收剂,在原矿含铜0.49%、含钼0.0115%的条件下,获得了含铜26.71%、总铜回收率86.11%的铜精矿及含钼48.03%、钼回收率83.53%的钼精矿,实现了铜、钼矿物与脉石的有效分离,获得了良好的技术指标。  相似文献   

15.
提高新疆富蕴县索尔库都克铜矿铜钼回收率的有效途径   总被引:1,自引:0,他引:1  
翟东民  汤作锟 《甘肃冶金》2011,33(6):52-55,72
新疆富蕴县索尔库都克铜矿具有我国伴生钼的矽卡岩型铜矿,探讨推进铜钼选矿工艺,从企业经济上和成功技术的应用推广上都具有很重要的意义。本文主要针对该矿石主金属含量低,铜钼矿物嵌布粒度粗细、不均匀,钼矿物与铜矿物及脉石矿物共生密切的特点,采用浮选柱与浮选机联合配置的浮选改进工艺,从原矿磨矿细度、浮选作业浓度、药剂制度等工艺参数的有效控制来介绍提高铜钼回收率的一些要点和方法。  相似文献   

16.
针对某低品位难选铜钼矿,进行了条件试验和全流程闭路试验研究,确定了铜钼的选矿回收工艺流程,在原矿含钼0.065%,含铜0.04%的前提下,得到钼精矿含钼47.87%,钼回收率为81.41%;铜精矿含铜18.84%,铜回收率为70.96%。  相似文献   

17.
青海某矽卡岩型铁铜多金属矿石中矿物嵌布粒度微细,伴生有闪锌矿、磁黄铁矿等矿物,且易泥化的蛇纹石、橄榄石、绿泥石等脉石矿物含量高。针对该矿石特征,进行了综合回收工艺研究。结果表明:采用铜硫混合浮选-中矿再磨-铜硫分离-弱磁选铁工艺流程,以及采用新型捕收剂和抑制剂相结合,在最佳试验条件下,获得了铜回收率75. 28%、全铁回收率73. 12%的较好指标,且伴生元素锌得到了综合回收。  相似文献   

18.
某低品位钼铜矿石选矿试验研究   总被引:1,自引:0,他引:1  
某钼铜矿石是一种以钼为主、并伴生铜矿物的低品位钼铜矿石,原矿含钼仅0.045%、含铜0.025%,无其它有价值的金属元素,试验采用先优先混合浮选将钼铜金属矿物同时富集后,再进行钼铜分离的选矿工艺,取得了钼精矿钼品位53.25%~50.4%(含铜0.30%~1.514%,取决于精选作业次数)、混合浮选开路作业回收率70.09%、分离浮选开路作业回收率55.89%~82.42%、开路作业总回收率为39.17%~57.77%;铜精矿含铜品位22.23%(含钼2.36%)、混合浮选作业回收率46.82%、分离浮选回收率90.45%、开路总回收率为42.35%的较好指标。如果条件允许能够进行闭路浮选试验,可能会取得更好的技术经济指标。  相似文献   

19.
某难选铜钼矿石的选矿试验研究   总被引:11,自引:0,他引:11  
对某铜钼矿石进行了矿物成分考察,针对该矿石中黄铁矿、黄铜矿含量较高,辉钼矿嵌布不均匀,并且解离比较困难的特点,通过铜钼混选-铜钼混精再磨后铜钼分离的选别工艺流程及合理的药剂制度,使辉钼矿和黄铜矿得到充分合理的回收.  相似文献   