The objective of this study is to investigate the feasibility of developing cellulose acetate (CA) membranes to partially immobilize Pseudomonas putida (ATCC 49451) and to evaluate the inhibitory effect of phenol on the immobilized bacteria by monitoring their growth in partially immobilized and free-suspension systems. The cellulose acetate membranes used in this study were wet spun from 20 wt % of CA in 1-methyl-2-pyrrolidone (NMP)/acetone (30 : 70) solvent using water as the bore fluid as well as the external coagulant. Scanning-electron microscopy (SEM) characterization of the newly developed CA hollow fibers suggests that the fiber cross section consists of multilayer microporous structures useful for cell immobilization. Experiments were conducted using the bacteria to degrade phenol at initial phenol concentrations of 300 mg/L and 1000 mg/L. In a free suspension (no membrane) system, it was observed that the bacteria were able to grow optimally at 300 mg/L of phenol, and degraded phenol almost completely in about 26 h. However, neither cell growth nor phenol degradation occurred when initial concentration of phenol was increased to 1000 mg/L. In a cell-immobilized membrane system, the cell growth and phenol concentration profiles in the medium were very similar to those obtained in a free suspension culture if phenol concentration was 300 mg/L. However, when the initial phenol concentration was increased to 1000 mg/L, data obtained in a cell-immobilized membrane system were discernibly different from that obtained in the suspension culture. In the former case, phenol concentration decreased in the beginning of test, indicating that the carbon source has been consumed and immobilized cells within the membrane had begun to multiply. As soon as the phenol concentration decreased to about 700 mg/L (at which concentration, substrate inhibition was not as severe as 1000 mg/L), partial immobilization occurred when some cells diffused out of the membrane into the medium and optical density became measurable in the medium. It was found that cell growth continued for the next 32 h, reaching an optical density in the medium of 0.42 absorbance units and a significant amount of phenol was degraded. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 68: 1677–1688, 1998  相似文献   

2.
Polysulfone (PSf) asymmetric hollow‐fiber membranes, which have a dense outer layer but a loose inner layer, were tentatively fabricated by coextrusion through a triple‐orifice spinneret and a dry/wet‐phase inversion process. Two simple polymer dopes were tailored, respectively, for the dense outer layer and the porous inner layer according to the principles of the phase‐inversion process. By adjusting the ratio of the inner/outer extrusion rate, the hollow‐fiber membranes with various thicknesses of outer layers were achieved. The morphology of the hollow‐fiber membranes was exhibited and the processing conditions and the water permeability of the membrane were investigated. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 94: 259–266, 2004  相似文献   

3.
Through the use of thermal polymerization, poly(vinylidene fluoride) (PVDF) hollow‐fiber membranes modified by a thin layer of molecularly imprinted polymers (MIPs) were developed for the selective separation of levofloxacin. To demonstrate the changes induced by thermal polymerization, PVDF hollow‐fiber membranes with different modification degrees by repeated polymerization were weighed. The total weight of the imprinted membranes increased by 14 μg/cm2 after a five‐cycle polymerization. An increase in the membrane weight indicated the deposition of an MIP layer on the external surface of PVDF hollow‐fiber membranes during each polymerization cycle, which was also characterized by scanning electron microscopy. MIP membranes with different degrees of surface modification provided highly selective binding of levofloxacin. Both hollow‐fiber MIP membranes and nonimprinted membranes showed enhanced adsorption of levofloxacin and ofloxacin gradually with an increase in the modification degrees of PVDF hollow‐fiber membranes to a maximum value followed by a decrease. These results indicate that thermal polymerization indeed produces an MIP layer on the external surface of PVDF hollow‐fiber membranes and that it is feasible to control the permeability by repeated polymerization cycles. Different solvent systems in the permeation experiments were used to understand the hydrophobic interaction as one of the results of the binding specificity of MIP membranes. Selective separation was obtained by multisite binding to the template via ionic, hydrogen‐bond, and hydrophobic interactions. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007  相似文献   

4.
Outer‐selective thin‐film composite (TFC) hollow fiber membranes offer advantages like less fiber blockage in the feed stream and high packing density for industrial applications. However, outer‐selective TFC hollow fiber membranes are rarely commercially available due to the lack of effective ways to remove residual reactants from fiber's outer surface during interfacial polymerization and form a defect‐free polyamide film. A new simplified method to fabricate outer‐selective TFC membranes on tribore hollow fiber substrates is reported. Mechanically robust tribore hollow fiber substrates containing three circular‐sector channels were first prepared by spinning a P84/ethylene glycol mixed dope solution with delayed demixing at the fiber lumen. The thin wall tribore hollow fibers have a large pure water permeability up to 300 L m?2 h?1 bar?1. Outer‐selective TFC tribore hollow fiber membranes were then fabricated by interfacial polymerization with the aid of vacuum sucking to ensure the TFC layer well‐attached to the substrate. Under forward osmosis studies, the TFC tribore hollow fiber membrane exhibits a good water flux and a small flux difference between active‐to‐draw (i.e., the active layer facing the draw solution) and active‐to‐feed (i.e., the active layer facing the feed solution) modes due to the small internal concentration polarization. A hyperbranched polyglycerol was further grafted on top of the newly developed TFC tribore hollow fiber membranes for oily wastewater treatment. The membrane displays low fouling propensity and can fully recover its water flux after a simple 20‐min water wash at 0.5 bar from its lumen side, which makes the membrane preferentially suitable for oil‐water separation. © 2015 American Institute of Chemical Engineers AIChE J, 61: 4491–4501, 2015  相似文献   

5.
For the purpose of separating aqueous alcohol by the use of pervaporation technique, a composite membrane of chitosan (CT) dip‐coated cellulose acetate (CA) hollow‐fiber membranes, CT‐d‐CA, was investigated. The effects of air‐gap distance in the spinning of CA hollow‐fiber membranes, chitosan concentration, and sorts of aqueous alcohol solutions on the pervaporation performances were studied. Compared with unmodified CA hollow‐fiber membrane, the CT‐d‐CA composite hollow‐fiber membrane effectively increases the permselectivity of water. The thickness of coating layer increases with an increase in chitosan concentration. As the concentration of chitosan solution increased, the permeation rate decreased and the concentration of water in the permeate increased. In addition, the effects of feed composition and feed solution temperature on the pervaporation performances were also investigated. The permeation rate and water content in permeate at 25°C for a 90 wt % aqueous isopropanol solution through the CT‐d‐CA composite hollow‐fiber membrane with a 5‐cm air‐gap distance spun, 2 wt % chitosan dip‐coated system were 169.5 g/m2 h and 98.9 wt %, respectively. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 94: 1562–1568, 2004  相似文献   

6.
We have investigated the feasibility of developing polysulfone (PS) membranes to partially immobilize Pseudomonas and to evaluate the inhibitory effect of phenol on immobilized Pseudomonas by monitoring their growths in partially immobilized cell and free-suspension systems. The polysulfone membranes used in this study were wet spun from 20 wt % of PS in 1-methyl-2-pyrrolidone (NMP) solvent using water as the bore fluid as well as the external coagulant. Scanning electron microscopy (SEM) characterization of the newly developed PS hollow fibers suggests that fiber cross-section consists of multilayer microporous structures useful for cell immobilization. Experiments were conducted using Pseudomonas bacteria to remove phenol with initial phenol concentrations of 300 mg/L and 1000 mg/L. In a free suspension (no membrane) system, it was observed that the bacteria were able to grow optimally at 300 mg/L of phenol and degraded phenol almost completely in about 26 h. However, neither cell growth nor phenol degradation occurred when initial concentration of phenol was increased to 1000 mg/L. In a cell-immobilized membrane system, the cell growth and phenol concentration profile in the medium were very similar to those obtained in a free-suspension culture if phenol concentration was 300 mg/L. However, when the initial phenol concentration was increased to 1000 mg/L, data obtained in a cell-immobilized membrane system was discernibly different from that obtained in the suspension culture. In the former case, phenol concentration decreased in the beginning of the test, indicating that the carbon source has been consumed and immobilized cells within the membrane had begun to multiply. As soon as the phenol concentration decreased to about 600 mg/L (at which concentration, substrate inhibition was not as severe as 1000 mg/L), partial immobilization occurred when some cells diffused out of the membrane into the medium and optical density became measurable in the medium. It was found that cell growth continued for the next 28 h, reaching a maximum optical density in the medium of 0.610 absorbance units, and phenol was also completely degraded. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 70: 2585–2594, 1998  相似文献   

7.
Poly(vinylidene fluoride‐co‐hexafluoropropylene) (PVDF‐co‐HFP) hollow fiber membranes were prepared by using the phase inversion method. The effect of polyethylene glycol (PEG‐600Mw) with different concentrations (i.e., 0, 5, 7, 10, 12, 15, 18, and 20 wt %) as a pore former on the preparation and characterization of PVDF‐co‐HFP hollow fibers was investigated. The hollow fiber membranes were characterized using scanning electron microscopy, atomic force microscopy, and porosity measurement. It was found that there is no significant effect of the PEG concentration on the dimensions of the hollow fibers, whereas the porosity of the hollow fibers increases with increase of PEG concentration. The cross‐sectional structure changed from a sponge‐like structure of the hollow fiber prepared from pure PVDF‐co‐HFP to a finger‐like structure with small sponge‐like layer in the middle of the cross section with increase of PEG concentration. A remarkable undescribed shape of the nodules with different sizes in the outer surfaces, which are denoted as “twisted rope nodules,” was observed. The mean surface roughness of the hollow fiber membranes decreased with an increase of PEG concentration in the polymer solution. The mean pore size of the hollow fibers gradually increased from 99.12 to 368.91 nm with increase of PEG concentration in polymer solution. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

8.
A novel braid‐reinforced (BR) poly(vinyl chloride) (PVC) hollow fiber membrane was fabricated via dry‐wet spinning process. The mixtures of PVC polymer solutions were uniformly coated on the tubular braid which contained polyester (PET) and polyacrylonitrile (PAN) fibers. The influences of braid composition on structure and performance of BR PVC hollow fiber membranes were investigated. The results showed that the prepared BR PVC hollow fiber membranes were composed of two layers which contained separation layer and tubular braid supported layer when the PET and PET/PAN hybrid tubular braids were used as the reinforcement. But the sandwich structure appeared when the PAN tubular braid was used as the reinforcement, which revealed outer separation layer, tubular braid supported layer and the inner polymer layer. The BR PVC hollow fiber membranes that prepared by PET/PAN hybrid tubular braid had favorable interfacial bonding state compared with the membrane prepared by pure PET or PAN tubular braid. The pure water flux of the BR PVC hollow fiber membranes that prepared by the PET/PAN hybrid tubular braid were lower than that prepared by pure PET or PAN tubular braid, but the rejection of Bovine serum albumin was opposite. The tensile strength of prepared BR PVC hollow fiber membrane was higher than 50 MPa. Both of the tensile strength and elongation at break decreased with the increase of the PAN filaments in the PET/PAN hybrid tubular braid. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017 , 134, 45068.  相似文献   

9.
Phenol degradation at high concentrations was investigated under continuous operation in an immobilized‐cell hollow fiber membrane bioreactor. Pseudomonas putida ATCC49451 was immobilized in asymmetric polysulfone hollow fiber membranes through entrapment within the porous regions and through attachment on the membrane surfaces. Bioreactor performance was assessed based on the startup period, the effect of feed rate (ranging from 21 to 120 mL/h), the relative contribution of the lumen and the shell sides to phenol degradation, the effect of feed phenol concentration (1000–2000 mg/L) and the long‐term operation of the bioreactor. The bioreactor startup was very short, and steady state was accomplished within 160 h. An optimum degradation capacity with respect to phenol loading rate was observed because of the tradeoff in the amount of phenol degraded against the increase in feed rate. It was also found that at higher feed rate, the shell side contributed to a larger proportion of the total phenol degraded compared with the lumen. On the basis of these results, it was found that options abound for the operating conditions of the bioreactor. These can be chosen depending on whether complete phenol degradation or high degradation capacity is desirable. Finally, long‐term sustainable continuous operation of the bioreactor was demonstrated without significant biofilm fouling on the membranes. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007  相似文献   

10.
The molecular design of nanoporous membranes with desired morphology and selectivity has attracted significant interest over the past few decades. A major problem in their applications is the trade‐off between sieving property and permeability. Here, we report the discovery of elongation‐induced nano‐pore evolution during the external stretching of a novel polyamide‐imide nanofiltration hollow fiber membrane in a dry‐jet wet‐spinning process that simultaneously leads to a decreased pore size but increased pure water permeability. The molecular weight cutoff, pore size, and pore size distribution were finely tuned using this approach. AFM and polarized FTIR verified the nano‐pore morphological evolution and an enhanced molecular orientation in the surface skin layer. The resultant nanofiltration membranes exhibit highly effective fractionation of the monovalent and divalent ions of NaCl/Na2SO4 binary salt solutions. More than 99.5% glutathione can be rejected by the nanofiltration membranes at neutral pH, offering the feasibility of recovering this tripeptide. © 2009 American Institute of Chemical Engineers AIChE J, 2010  相似文献   

11.
Emission of sulfur compounds to the atmosphere is universally recognized as one key target to be reduced. For membrane pervaporation which is considered as a potential purification process of fuels, dual‐layer polyurethane (PU)/polyethersulfone hollow‐fiber membranes were prepared. A novel fabrication technique is proposed using a quadruple spinneret to produce the fiber with such morphology by simultaneous spinning of two polymer solutions in the presence of two corresponding precipitation media. Activated carbon was added into the PU solution to improve the transport properties of the selective layer. Resulting hollow‐fiber membranes showed very good adhesion between the selective layer and its support, in addition to an effective removal of a sulfur compound such as 2‐methyl thiophene from a typical model fuel, an indication of good prospects for both the fabrication technique and for sulfur removal by pervaporation of fuels.  相似文献   

12.
Polydimethylsiloxane (PDMS) hollow‐fiber membranes grafted with 1H,1H,9H‐hexadecafluorononyl methacrylate (HDFNMA), which is a fluoroalkyl methacrylate, using a 60Co irradiation source, were characterized and applied to pervaporation. The PDMS hollow‐fiber membranes were filled with N2 gas and sealed. The membranes and the HDFNMA solution were then irradiated simultaneously. In the HDFNMA solution, graft polymerization was performed. The degree of grafting of the outside surface of the hollow fiber was greater than that in the inside surface of the hollow fiber. In the grafted PDMS hollow‐fiber membranes, the best separation performance was shown due to the introduced hydrophobic polymer, poly(HDFNMA). The grafted membrane had a microphase‐separated structure, that is, a separated structure of PDMS and graft‐polymerized HDFNMA. The permeability of molecules in the poly(HDFNMA) phase was so low that the diffusion of molecules was prevented in the active layer with many poly(HDFNMA) domains, as the feed solution was introduced through the inside of the hollow fibers and the outside was vacuumed. As the feed solution was introduced through the outside of the hollow fibers and the inside was vacuumed, the diffusion of molecules was not prevented in the active layer with few poly(HDFNMA) domains. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 88: 1573–1580, 2003  相似文献   

13.
Poly(4‐methyl‐1‐pentene) (PMP) hollow fibers were prepared and fabricated into gas separation or microporous membranes by the melt‐spun and cold‐stretched method. PMP resin was melt‐extruded into hollow fibers with cold air as the cooling medium. The effects of take‐up speed and thermotreatment on the mechanical behavior and morphology of the fibers were investigated. Scanning electronic microscope (SEM) photos were used to reveal the geometric structure of the section and surface of the hollow fibers. It was found that the original fiber had an asymmetric structure. A “sandwich” mode was used to describe the formation of this special fine structure. And a series of PMP hollow‐fiber membranes were prepared by subsequent drawing, and it was found that there was a “skin–core” structure on the cross section of these hollow‐fiber membranes. Asymmetric or microporous PMP hollow‐fiber membranes could be obtained by controlling posttreatment conditions. The morphology of these membranes were characterized by SEM, and the gas (oxygen, nitrogen, and carbon dioxide) permeation properties of the membranes was measured. The results indicate that the annealing time of the original fiber and the stretching ratio were the key factors influencing the structure of the resulting membrane. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 2131–2141, 2006  相似文献   

14.
Multilayer membranes constructed layer‐by‐layer (LbL) is finding increasing importance in many separation applications. The efficient construction of LbL multilayer on to hollow fiber substrates may offer many new opportunities for industrial applications. An organic–inorganic composite hollow fiber membrane has been developed using a dynamic LbL self‐assembly. This poly(acrylic acid)/poly(ethyleneimine) multilayer was dynamically assembled onto the inner surfaces of ceramic hollow fiber porous substrates pretreated by Dynasylan Ameo silane coupling agents. The hollow fibers were subsequently heat crosslinked to obtain stable permselective membranes. The formation of multilayers on the hollow fibers was characterized with a SEM, EDX, an electrokinetic analyzer and IR spectra. The effects of layer number, feed temperature and water content in the feed on the pervaporation performance have been investigated. To the best of our knowledge, this is the first report of LbL assembly of polymer building blocks onto ceramic hollow fiber porous substrates. © 2011 American Institute of Chemical Engineers AIChE J, 58: 3176–3182, 2012  相似文献   

15.
Hollow‐fiber carbon membranes were prepared and used as support media for a platinum catalyst. The platinum metal was deposited onto the surface of the hollow‐fiber carbon membranes by three different techniques: solution coating with chloroplatinic acid, which is the commonly used technique; vapor deposition, involving the sublimation of the platinum metal; and magnetron sputter coating, the most effective method. The hollow‐fiber carbon membranes coated with a chloroplatinic acid solution were studied with scanning electron microscopy (SEM) and energy‐dispersive X‐ray analysis (EDAX). The platinum coating grew on the surface, unevenly, in the form of small crystals. The percentage of platinum on the surface was too low to be detected by EDAX. The high‐vacuum evaporation coating of the membranes with platinum was also studied with both SEM and EDAX. Again, because of the low percentage of platinum, EDAX did not reveal any platinum on the surfaces of the membranes. The magnetron sputter coating of platinum onto the membranes was performed and studied with SEM. The thickness of the coated platinum could be varied through variations in the coating time. The cavities observed in the micrographs were formed during the coating operations by the presence of dust particles on the membranes. An SEM micrograph of a hollow‐fiber carbon membrane, produced from a polyacrylonitrile‐based precursor, spun with a low amount of dimethyl sulfoxide in the bore fluid, and coated with platinum, showed a skin on the outside and a porous elongated structure inside the skin. The distance between the inner and outer skins contained fingerlike pores of various sizes. The largest pores were found near the inside skin, whereas the smallest pores were next to the outside skin. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 87: 1051–1058, 2003  相似文献   

16.
Polyethersulfone (PES) hollow‐fiber membranes were fabricated using poly(ethyleneglycol) (PEG) with different molecular weights (MW = PEG200, PEG600, PEG2000, PEG6000, and PEG10000) and poly(vinyl pyrrolidone) PVP40000 as additives and N‐methyl‐2‐pyrrolidone (NMP) as a solvent. Asymmetric hollow‐fiber membranes were spun by a wet phase‐inversion method from 25 wt % solids of 20 : 5 : 75 (weight ratio) PES/PEG/NMP or 18 : 7 : 75 of PES/(PEG600 + PVP40000)/NMP solutions, whereas both the bore fluid and the external coagulant were water. Effects of PEG molecular weights and PEG600 concentrations in the dope solution on separation properties, morphology, and mechanical properties of PES hollow‐fiber membranes were investigated. The membrane structures of PES hollow‐fiber membranes including cross section, external surface, and internal surface were characterized by scanning electron microscopy and the mechanical properties of PES hollow‐fiber membranes were discussed. Bovine serum albumin (BSA, MW 67,000), chicken egg albumin (CEA, MW 45,000), and lysozyme (MW 14,400) were used for the measurement of rejection. It was found that with an increase of PEG molecular weights from 200 to 10,000 in the dope solution, membrane structures were changed from double‐layer fingerlike structure to voids in the shape of spheres or ellipsoids; moreover, there were crack phenomena on the internal surfaces and external surfaces of PES hollow‐fiber membranes, pure water permeation fluxes increased from 22.0 to 64.0 L m?2 h?1 bar?1, rejections of three protein for PES/PEG hollow‐fiber membranes were not significant, and changes in mechanical properties were decreased. Besides, with a decrease of PEG600 concentrations in the dope solution, permeation flux and elongation at break decreased, whereas the addition of PVP40000 in the dope solution resulted in more smooth surfaces (internal or external) of PES/(PEG600 + PVP40000) hollow‐fiber membranes than those of PES/PEG hollow‐fiber membranes. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 91: 3398–3407, 2004  相似文献   

17.
An external loop airlift bioreactor with a small amount (99% porosity) of stainless steel mesh packing inserted in the riser section was used for bioremediation of a phenol‐polluted air stream. The packing enhanced volatile organic chemical and oxygen mass transfer rates and provided a large surface area for cell immobilization. Using a pure strain of Pseudomonas putida, fed‐batch and continuous runs at three different dilution rates were completed with phenol in the polluted air as the only source of growth substrate. 100% phenol removal was achieved at phenol loading rates up to 33 120 mg h?1 m?3 using only one‐third of the column, superior to any previously reported biodegradation rates of phenol‐polluted air with 100% efficiency. A mathematical model has been developed and is shown to accurately predict the transient and steady‐state data. Copyright © 2006 Society of Chemical Industry  相似文献   

18.
Dual‐layer acetylated methyl cellulose (AMC) hollow fiber membranes were prepared by coupling the thermally induced phase separation (TIPS) and non‐solvent induced phase separation (NIPS) methods through a co‐extrusion process. The TIPS layer was optimized by investigating the effects of coagulant composition on morphology and tensile strength. The solvent in the aqueous coagulation bath caused both delayed liquid–liquid demixing and decreased polymer concentration at the membrane surface, leading to porous structure. The addition of an additive (triethylene glycol, (TEG)) to the NIPS solution resolved the adhesion instability problem of the TIPS and NIPS layers, which occurred due to the different phase separation rates. The dual‐layer AMC membrane showed good mechanical strength and performance. Comparison of the fouling resistance of the AMC membranes with dual‐layer polyvinylidene fluoride (PVDF) hollow fiber membranes fabricated with the same method revealed less fouling of the AMC than the PVDF hollow fiber membrane. This study demonstrated that a dual‐layer AMC membrane with good mechanical strength, performance, and fouling resistance can be successfully fabricated by a one‐step process of TIPS and NIPS. © 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015 , 132, 42715.  相似文献   

19.
A thin layer of star‐shaped poly(ethylene oxide) (PEO) (starPEO), on the polydimethylsiloxane (PDMS) membrane was prepared by a simple immobilization procedure. Photoreactive molecules were introduced on the surface of the polymeric support to achieve the formation of thin starPEO film from the materials having no functional groups. This novel technique enabled us to immobilize any kind of chemical, especially one that had no functional groups, and readily to control the amount of immobilization. The gas permeation properties of the starPEO‐immobilized PDMS membranes were investigated for pure propane and propylene. The permeance of gases were found to decrease in the starPEO‐immobilized PDMS membranes, although the ideal separation factors for propylene/propane were increased with the loading amount of silver ions, because of the facilitation action of silver ions in the immobilized PEO unit on the PDMS membranes, as propylene carriers. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 83: 2369–2373, 2002  相似文献   

20.
ZIF‐8/6FDA‐DAM, a proven mixed‐matrix material that demonstrated remarkably enhanced C3H6/C3H8 selectivity in dense film geometry, was extended to scalable hollow fiber geometry in the current work. We successfully formed dual‐layer ZIF‐8/6FDA‐DAM mixed‐matrix hollow fiber membranes with ZIF‐8 nanoparticle loading up to 30 wt % using the conventional dry‐jet/wet‐quench fiber spinning technique. The mixed‐matrix hollow fibers showed significantly enhanced C3H6/C3H8 selectivity that was consistent with mixed‐matrix dense films. Critical variables controlling successful formation of mixed‐matrix hollow fiber membranes with desirable morphology and attractive transport properties were discussed. Furthermore, the effects of coating materials on selectivity recovery of partially defective fibers were investigated. To our best knowledge, this is the first article reporting successful formation of high‐loading mixed‐matrix hollow fiber membranes with significantly enhanced selectivity for separation of condensable olefin/paraffin mixtures. Therefore, it represents a major step in the research area of advanced mixed‐matrix membranes. © 2014 American Institute of Chemical Engineers AIChE J, 60: 2625–2635, 2014  相似文献   