This work provides an estimation procedure to determine J-resistance curves for pin-loaded and clamped SE(T) fracture specimens using the unloading compliance technique and the η-method. A summary of the methodology upon which J and crack extension are derived sets the necessary framework to determine crack resistance data from the measured load vs. displacement curves. The extensive plane-strain analyses enable numerical estimates of the nondimensional compliance, μ, and parameters η and γ for a wide range of specimen geometries and material properties characteristic of structural and pipeline steels. Laboratory testing of an API 5L X60 steel at room temperature using pin-loaded SE(T) specimens with side-grooves provide the load-displacement data needed to validate the estimation procedure for measuring the crack growth resistance curve for the material. The results presented here produce a representative set of solutions which lend further support to develop standard test procedures for constraint-designed SE(T) specimens applicable in measurements of crack growth resistance for pipelines.  相似文献   

2.
This work focuses on an evaluation procedure to determine the elastic?Cplastic J-integral and Crack Tip Opening Displacement (CTOD) fracture toughness based upon the ??-method for C(T) fracture specimens made of homogeneous and welded steels. The primary objective of this investigation is to enlarge on previous developments of J and CTOD estimation procedures for this crack configuration while, at the same time, addressing effects of strength mismatch on the plastic ??-factors. The present analyses enable the introduction of a larger set of factors ?? for a wide range of crack sizes (as measured by the a/W-ratio) and material properties, including different levels of weld strength mismatch, applicable to pipeline and pressure vessel steels. Very detailed non-linear finite element analyses for plane-strain and 3-D models of C(T) fracture specimens with centerline-cracked welds provide the evolution of load with increased load-line and crack mouth opening displacement required for the estimation procedure. Overall, the present study, when taken together with previous investigations, provides a fairly extensive body of results to determine parameters J and CTOD for different materials using C(T) specimens with varying overmatch conditions.  相似文献   

3.
This work examines the effect of weld strength mismatch on fracture toughness measurements defined by J and CTOD fracture parameters using single edge notch bend (SE(B)) specimens. A central objective of the present study is to enlarge on previous developments of J and CTOD estimation procedures for welded bend specimens based upon plastic eta factors (η) and plastic rotational factors (r p ). Very detailed non-linear finite element analyses for plane-strain models of standard SE(B) fracture specimens with a notch located at the center of square groove welds and in the heat affected zone provide the evolution of load with increased crack mouth opening displacement required for the estimation procedure. One key result emerging from the analyses is that levels of weld strength mismatch within the range ±20% mismatch do not affect significantly J and CTOD estimation expressions applicable to homogeneous materials, particularly for deeply cracked fracture specimens with relatively large weld grooves. The present study provides additional understanding on the effect of weld strength mismatch on J and CTOD toughness measurements while, at the same time, adding a fairly extensive body of results to determine parameters J and CTOD for different materials using bend specimens with varying geometries and mismatch levels.  相似文献   

4.
This paper describes enhanced J‐integral estimation schemes for pipes with circumferential semi‐elliptical cracks subjected to tensile loading, global bending and internal pressure. These schemes are given in two different forms to cover the wide ranges of geometries and material parameters; the modified GE/EPRI method and the modified reference stress method. In the former method, new plastic influence functions for fully plastic J‐integral estimation are developed based on extensive three‐dimensional finite element calculations. In the latter method, new optimized reference loads are suggested and utilized to predict the J values. To verify the feasibility of these two schemes, J‐integral values obtained from further detailed FE analyses are compared to those from the proposed schemes. Because the estimated J‐integrals agree fairly well with the detailed FE analysis results, the new solutions can be applied for accurate structural integrity assessment of different size pipes with a circumferential surface crack.  相似文献   

5.
This paper provides approximate J estimates for off-centred, circumferential through-wall cracks in cylinders under bending and under combined tension and bending. The proposed method is based on the reference stress approach, where the dependence of elastic and plastic influence functions of J on the cylinder/crack geometry, the off-centred angle and strain hardening is minimised through the use of a proper normalising load. Based on published limited FE results for off-centred, circumferential through-wall cracks under bending, such normalising load is found, based on which the reference stress based J estimates are proposed for more general cases, such as for a different cylinder geometry and for combined loading. Comparison of the estimated J with extensive FE J results shows overall good agreements for different crack/cylinder geometries and for combined tension and bending, which provides sufficient confidence in the use of the proposed method for fracture mechanics analyses of off-centred circumferential cracks. Furthermore, the proposed method is simple to use, giving significant merits in practice.  相似文献   

6.
This study describes an extensive set of 3-D analyses conducted on conventional fracture specimens, including pin-loaded and clamped SE(T) specimens, and axially cracked pipes with varying crack configurations. The primary objective is to examine 3-D effects on the correlation of fracture behavior for the analyzed crack configurations using the J-Q methodology. An average measure of constraint over the crack front, as given by an average hydrostatic parameter, denoted Qavg, is employed to replace the plane-strain measure of constraint, Q. Alternatively, a local measure of constraint evaluated at the mid-thickness region of the specimen, denoted QZ0, is also utilized. The analysis matrix considers 3-D numerical solutions for models of SE(T) fracture specimens with varying geometries (i.e., different crack depth to specimen width ratio, a/W, as well as different loading point distance, H) and test conditions (pin-loaded ends vs. clamped ends). The 3-D numerical models for the cracked pipes cover different crack depth to pipe wall thickness ratio, a/t, and a fixed crack depth to crack length ratio, a/c. The extensive 3-D numerical analyses presented here provide a representative set of solutions which provide further support for using constraint-designed SE(T) specimens in fracture assessments of pressurized pipes and cylindrical vessels.  相似文献   

7.
A new methodology for predicting the location of maximum crack extension along a surface crack front in ductile materials is presented. Three-dimensional elastic-plastic finite element analyses were used to determine the variations of a constraint parameter (αh) based on the average opening stress in the crack tip plastic zone and the J-integral distributions along the crack front for many surface crack configurations. Monotonic tension and bending loads are considered. The crack front constraint parameter is combined with the J-integral to characterize fracture, the critical fracture location being the location for which the product h is a maximum. The criterion is verified with test results from surface cracked specimens.  相似文献   

8.
Extensive finite element analyses have been conducted to obtain solutions of the A-term, which is the second parameter in three-term elastic-plastic asymptotic expansion, for test specimens. Three mode I crack plane-strain test specimens, i.e. single edge cracked plate (SECP), center cracked plate (CCP) and double edge cracked plate (DECP) were studied. The crack geometries analyzed included shallow to deep cracks. Solutions of A-term were obtained for material following the Ramberg-Osgood power law with hardening exponent of n = 3, 4, 5, 7 and 10. Remote tension loading was applied which covers from small-scale to large-scale yielding. Based on the finite element results, empirical equations to predict the A-terms under small-scale yielding (SSY) to large-scale yielding conditions were developed. In addition, by using the relationships between A and other commonly used second fracture parameters such as Q factor and A2-term, the present solutions can be used to calculate parameters A2 and Q as well. The results presented in the paper are suitable to calculate the second elastic-plastic fracture parameters for test specimens for a wide range of crack geometries, material strain hardening behaviors and loading conditions.  相似文献   

9.
Contrary to the previous work that successfully applied the constant CTOD/CTOA fracture criteria to relatively thin structures, this paper demonstrates that the initial non-constant portion of the CTOD/CTOA plays an essential role in predicting fracture behavior under plane-strain conditions. Three- and two-dimensional finite element analyses indicate that a severe underestimation of the load would occur as the crack extends if a constant CTOD/CTOA criterion were used. However, the use of a simplified, bilinear CTOD/CTOA criterion to approximate its non-constant portion will closely duplicate the test data. Furthermore, using the experimental data from J-integral tests with various crack length to specimen width ratios (a/W), it is demonstrated that the critical CTOD/CTOA is crack tip constraint dependent. The initial high values of the CTOD/CTOA are in fact a natural consequence of crack growth process that is reflected by, and consistent with, the J-resistance (J-R) curve and its slope (tearing modulus).  相似文献   

10.
Piping elbows under bending moment are vulnerable to cracking at crown. The structural integrity assessment requires knowledge of the J-integral. The J-integral values for axially through-wall cracked thick elbows are not available in the open literature over a certain range. This paper presents a closed form expression for elastic J-integral for 90°, long radius elbows subjected to bending moment. The expression is derived, based on the results of a large number of finite element analyses covering a wide range of standard geometries. The analyses were performed using WARP3D software. The present study enables the estimation of the elastic J-integral over a range of Rm/t from 5 to 25 (Rm/t = 5, 6, 7.5, 9, 12, 15, 20 and 25) and thus extends the range of earlier solution towards the thicker elbows used in nuclear industry. The crack angles considered were 9°, 18°, 27° and 36°.  相似文献   

11.
Leak-before-break (LBB) assessment of primary heat transport piping of nuclear reactors involves detailed fracture assessment of pipes and elbows with postulated throughwall cracks. Fracture assessment requires the calculation of elastic-plastic J-integral and crack opening displacement (COD)1 for these piping components. Analytical estimation schemes to evaluate elastic-plastic J-integral and COD simplify the calculations. These types of estimation schemes are available for pipes with various crack configurations subjected to different types of loading. However, no such schemes are available for throughwall circumferentially cracked elbow (or pipe bend), an important component for LBB analysis. In this paper, simple J and COD estimation schemes are proposed for throughwall circumferentially cracked elbow subjected to closing bending moment. The ovalisation of elbow cross-section has a significant bearing on its fracture behavior. Therefore, unlike conventional deformation theory plasticity analysis, incremental flow theory is adopted considering both material and geometric non-linearities in the development of the proposed estimation schemes. Although it violates Ilyushin’s theorem, it has been shown that the resulting estimation schemes is still reasonably accurate for engineering purposes. Finally, experimental/numerical validation has been provided by comparing the J-integral and COD between numerical/test data and predictions of the proposed estimation schemes.  相似文献   

12.
The present work proposes a method for elastic-plastic fracture mechanics analysis of the circumferential through-wall crack in weldment joining elbows and attached straight pipes, subject to in-plane bending. Heterogeneous nature of weldment is not explicitly considered and thus, the proposed method assumes cracks in homogeneous materials. Based on small strain finite element limit analyses using elastic-perfectly plastic materials, closed-form limit loads for circumferential through-wall cracks between elbows and straight pipes under bending are given. Then applicability of the reference stress-based method to approximately estimate J and crack opening displacement (COD) is evaluated. It was found that the limit moments for circumferential cracks between elbows and attached straight pipes can be much lower than those for cracks in straight pipes, particularly for a crack length of less than 30% of the circumference; this result is of great interest in practical cases. This result implies that, if one assumes that the crack locates in the straight pipe, limit moments could be overestimated significantly, and accordingly, reference stress-based J and COD could be significantly overestimated. For the leak-before-break analysis, accurate J and COD estimation equations based on the reference stress approach are proposed.  相似文献   

13.
This paper presents plastic limit loads and approximate J estimates for axial through-wall cracked pipe bends under internal pressure and in-plane bending. These loads and estimates are based on small strain finite element limit analyses using elastic-perfectly plastic materials. Geometric variables associated with the crack and pipe bend are systematically varied, and three possible crack locations (intrados, crown and extrados) are considered. Effects of the bend and crack geometries on plastic limit loads are quantified, and closed-form limit load solutions are given. Based on the proposed limit load solutions, a reference stress based the J estimation scheme for axial through-wall cracked pipe bends under internal pressure and in-plane bending is proposed.  相似文献   

14.
Using large deformation FEM analyses in SA333Gr.6 carbon steel material, the present study demonstrated the assessment of SZWc value that leads to JSZWc and finally compares with the respective experimental results. It also includes numerical prediction of specimen J-R curve using Gurson-Tvergaard-Needleman parameters obtain from tensile specimen tests. Using numerically predicted results, the crack initiation and instability stages in circumferentially through-wall cracked elbows is finally predicted and compares with experimental results. The present study gives evidence that the non-linear FEM analysis supported with proper tensile test data can be helpful in assessing the safety of bend pipes with through-wall crack.  相似文献   

15.
In this paper, surface cracked plates under biaxial tension are studied. Three-dimensional elastic-plastic finite element analyses have been carried out to calculate the J-integral for surface cracked plate for a wide range of geometry, biaxiality and material properties. Fully plastic J-integral solutions along the front of the surface cracks are presented for Ramberg-Osgood power law hardening material of n = 3, 5, 10 and 15. Geometries considered are a/c = 0.2, 1.0 and a/t = 0.2, 0.4, 0.6 and 0.8 and the biaxial ratios of 0, 0.5 and 1. Based on these results, the J-integral along the crack front for general elastic-plastic loading conditions can be estimated using the EPRI scheme. These solutions are suitable for fracture analyses for surface cracked plates under biaxial loading.  相似文献   

16.
Crack resistance curves of GLARE laminates by elastic compliance   总被引:1,自引:0,他引:1  
The objective of this work was to study the applicability of the elastic compliance technique for crack resistance curves evaluation of commercial GLARE laminates using small SE(B) and C(T) specimens. The experimental evaluation of R-curves of 25.0 mm wide SE(B) specimens of unidirectional GLARE 1 3/2 0.3 and 50.0 mm wide C(T) specimens of bidirectional GLARE 3 5/4 0.3 was performed. Fracture toughness was measured through a recently proposed experimental methodology based on standardized specimens and elastic-plastic methodologies (J-integral and CTOD δ5), whereas crack growth was measured optically and estimated by elastic compliance. According to the results the elastic compliance technique seemed to be applicable to GLARE laminates, accurately predicting stable crack growth during the tests.  相似文献   

17.
Proceeding from the experimentally vindicated basis that circumferential growth of a through-wall crack in a circular cylindrical Type 304 stainless steel pipe subject to bending loads is associated with a constant crack tip opening angle, an earlier paper has predicted the shape of the JR curve in terms of geometrical and material parameters. The predictions compare favourably with experimental results for 4 in. (~ 10 cm.) diameter pipes containing circumferential through-wall cracks with different sizes. In this paper, the implications of the geometry dependence of the JR curve are considered in relation to the criterion for the instability of circumferential crack growth. Limitations of the tearing modulus approach are accordingly highlighted, particularly if it is used for a material with a low crack growth resistance.  相似文献   

18.
Leak-before-break (LBB) assessment of primary heat transport piping of nuclear reactors involves detailed fracture assessment of pipes and elbows with postulated throughwall cracks. Fracture assessment requires the calculation of elastic–plastic J-integral and crack opening displacement (COD)1 for these piping components. Analytical estimation schemes to evaluate elastic–plastic J-integral and COD simplify the calculations. These types of estimation schemes are available for pipes with various crack configurations subjected to different types of loading. However, such schemes for elbow (or pipe bend), which is one of the important components for LBB analyses, is very meager. Recently, elastic–plastic J and COD estimation scheme has been developed for throughwall circumferentially cracked elbow subjected to closing bending moment. However, it is well known that the elbow deformation characteristics are distinctly different for closing and opening bending modes because the ovalisation patterns of elbow cross section are different under these two modes. Development of elastic–plastic J and COD estimation scheme for an elbow with throughwall circumferential crack at intrados subjected to opening bending moment forms the objective of the present paper. Experimental validation of proposed J-estimation scheme has been provided by comparing the crack initiation, unstable ductile tearing loads and crack extension at instability with the test data. The COD estimation scheme has been validated by comparing the COD of test data with the predictions of the proposed scheme.  相似文献   

19.
This paper provides engineering J and crack opening displacement (COD) estimation equations for through-wall cracked (TWC) pipes under internal pressure and under combined internal pressure and bending. Based on selected 3-D FE calculations for the TWC pipe under internal pressure using power law materials, elastic and plastic influence functions for fully plastic J and COD solutions are tabulated as a function of the normalised crack length and the mean radius-to-thickness ratio. These developed GE/EPRI-type solutions are then re-formulated based on the reference stress concept. Such re-formulation not only provides simpler equations for J and COD estimation, but also can be easily extended to combined internal pressure and bending. The proposed reference stress based J and COD estimation equations are compared with elastic-plastic 3-D FE results using actual stress-strain data for Type 316 stainless steels. The FE results for both internal pressure cases and combined internal pressure and bending cases compare very well with the proposed J and COD estimates.  相似文献   

20.
Working conditions of casing pipes in drilling rigs can significantly influence the initiation and development of damage in the material, and therefore also the safe service of the entire system. In this work, an integrity assessment of a pipe with initial defect (machined surface crack) is presented. The position of this defect is on the external surface; unlike transport pipes, where internal surface is often endangered due to the contact with the fluid, casing pipes are also often exposed to damages at the external surface. A pipe segment exposed to internal pressure is examined experimentally and numerically, using the finite element method. Experimental setup included tracking of crack mouth opening displacement (CMOD) values, as well as J integral. Criteria for pipe failure are determined on the finite element (FE) models of the pipe; fracture initiation and plastic collapse are considered as failure mechanisms. Several 3D models with different crack sizes are evaluated. 2D plane strain models are also examined, to determine the applicability limits of this simplified approach. Integrity assessment criteria for the analysed geometries are discussed. Assessment of fracture resistance of the pipeline material is also considered in this work. Besides the standard SENB specimens, Ring specimens cut from the pipe are tested, and the results are compared. Both specimen geometries are modelled using local approach to fracture, by application of the micromechanical Complete Gurson model (CGM), developed by Z.L. Zhang. It is shown that the Ring specimens have similar fracture conditions under bending load as SENB specimens. Since they are much simpler to fabricate from the pipe than standard specimens, it is concluded that they can be used for assessment of fracture of the pipes with axial cracks.  相似文献   