共查询到19条相似文献,搜索用时 15 毫秒
1.
《钢铁冶炼》2013,40(3):204-210
AbstractA design method of a cascaded whole-leaf spring mechanism is proposed, which is a new oscillation guidance device for the mould in continuous casting. Then its prototype designed in this paper is produced in the lab, of which kinematics and dynamics simulations are carried out based on the rigid–flexible coupling virtual model. Simulation curves of the displacement and velocity of the mould are almost consistent with the ideal ones, which verifies the model built in this paper is rational. Furthermore, natural frequencies and mode shapes of the mechanism are calculated by dynamics simulation, and forces applied on leaf springs and revolute joints are analysed and effects of the basic parameters on these forces are also studied, which establish the basis for further studies and next application of this mechanism. 相似文献
2.
《钢铁冶炼》2013,40(2):135-143
AbstractMould flux samples from an operating continuous caster showed a steady state increase in titanium oxide content of 3–4% for a titanium stabilised ferritic stainless steel and about 6% for a titanium stabilised austenitic stainless steel. Owing to the reduction of silica the flux basicity increased from 0.8 to 0.9, and from 0.95 to 1.2, for the ferritic and austenitic steels, respectively. Similar changes in composition were found for mould shims, which had been recovered from the mould after casting the ferritic steel. The increased titanium oxide content caused a decrease in the flux viscosity, for the original basicity. However, when the flux basicity was increased from 0.95 to 1.2, the apparent viscosity of the mould flux of the austenitic steel increased markedly, for 10% TiO2 and temperatures of 1250°C and below. Precipitation of perovskite was found to be responsible for the higher apparent viscosity. 相似文献
3.
《钢铁冶炼》2013,40(5):364-370
AbstractThe thermal behaviour of the continuous casting mould has a critical influence on strand surface quality, casting productivity and operating safety. voestalpine Stahl GmbH has long been interested in the field of research into mould behaviour, and began with the investigation of heat flux in 1995, and then of thermal variability in 1999. Since 2000, an online mould thermal monitoring system for heat flux density, thermal variability and friction has been installed. The heat flow density in the mould is determined by measuring the inflow and outflow temperatures and the throughflow volume of the primary cooling water. Temperature as measured by a thermocouple based breakout detection system in the mould copper plate is used to investigate the thermal variability. These online measured values have been employed to examine the influence of casting parameters, steel analysis and casting powder on the heat flux and thermal variability, and the relationship between these variables and cracking. The knowledge gained through these wide ranging plant based investigations has been used as a major tool in the diagnosis of problems (such as breakout and sticking), for optimisation of the process, particularly in the field of casting powders, and for control of slab quality. In particular, this knowledge has been incorporated into online mould thermal monitoring. 相似文献
4.
《钢铁冶炼》2013,40(5):396-398
AbstractThe form of fluorine in Na2O-NaF-SiO2 slags has been investigated using Fourier transform infrared spectroscopy. Additions of NaF shifted absorption peaks for stretching modes of Si O bonds to higher wavenumbers, where the basicity of (mol-%Na2O)/ (mol-%SiO2 ) was kept constant, and the shift became larger with an increase in the concentration of NaF. This shift can be explained by the change from Si-O to Si-F bonds, with reference to harmonic oscillation theory of diatomic molecules. It is likely that added NaF depolymerises the silicate network to form Si-F bonds in Na2O-NaF-SiO2 slags. 相似文献
5.
《钢铁冶炼》2013,40(5):357-363
AbstractCorus R,D&T at Teesside Technology Centre has developed over a number of years a mould thermal monitoring (MTM) system based on an array of thermocouples in the mould copper plates. The system is installed on the Corus slab casters in the UK, on slab casters at Outokumpu (UK), Sidmar (Belgium) and Kosice (Slovakia) and, at the time of the 4th European Continuous Casting Conference, was also on the medium thickness slab caster at Tuscaloosa (USA), which was sold to Nucor in 2004. The MTM system was also under development on the thin slab caster at Trico (USA) before plant closure (subsequently bought by Nucor), and aspects are currently being developed on the Corus DSP (direct sheet plant) thin slab caster at IJmuiden (The Netherlands). While a prime function is detection and prevention of sticker type breakouts, the MTM system allows real time assessment of thermal conditions, provides a valuable input for online grading and, most important, enables modifications to mould powder practices to be assessed. The present paper briefly outlines recent developments to the MTM system and presents examples of the use of the system to assist mould powder developments. 相似文献
6.
《钢铁冶炼》2013,40(8):610-614
AbstractInfrared transmittance of glassy and crystalline mould fluxes was measured using a Fourier transform infrared spectrometer at room temperature. Radiation heat transfer from the steel shell to the mould was calculated by a model. The results indicate that transition metal oxides MnO, FeO and TiO2 have a marked negative effect on infrared transmittance and radiation heat flux of glassy samples. With MnO, FeO and TiO2 added, the reductions of radiation heat flux in glassy samples are 19–25%, 34–36%, 6–29% respectively. X-ray diffraction results indicated that the crystalline phase in transition oxides free samples was mainly Ca4Si2O7F2. After transition oxides MnO, FeO and TiO2 added, Mn2SiO4, Fe2SiO4, CaTiO3, Ca2SiO4 and other minor phases were also precipitated in mould fluxes. On account of strong refraction and scattering, the negative effect on radiation heat flux in crystalline samples was much larger than that in the glassy ones. 相似文献
7.
《钢铁冶炼》2013,40(4):283-287
AbstractThe tools and techniques used within Corus UK to improve mould powder performance and product quality are reviewed. Mould thermal monitoring, which allows real time assessment of heat transfer, is a critical tool in the development of mould powders. Thermal analysis, viscosity measurements, flux–mould plate interactions, steel velocity profiles in the mould and slag film properties also play a part in continuing studies. Case studies of improvements in process performance achieved using these methods are presented. 相似文献
8.
《钢铁冶炼》2013,40(5):380-386
AbstractTwo-dimensional finite element heat transfer models have been developed to predict temperature distribution in beam blank moulds with large and small hole water cooling channels. The effects of water channel design and grinding thickness on transverse temperature profile in meniscus region were analysed in detail. The effects of both moulds during plant trials are also compared. The results show that the peak temperature is found in the fillet area of the large hole mould and is 20°C higher than that of the small hole mould. With increasing grinding thickness, peak temperature in both moulds decreases linearly, and when the grinding thickness reaches 9 mm, the peak temperature of the small hole mould exceeds that of the large hole mould. The transverse temperature uniformity of the hole mould is superior to that of the large hole mould. It is also found that longer mould life, better strand surface quality and more homogeneous surface microstructure are obtained when using the small hole mould. 相似文献
9.
《钢铁冶炼》2013,40(1):33-38
AbstractA water modelling experiment was conducted to study the meniscus instability in a continuous thin slab casting mould using particle image visualisation. The results show that the level fluctuation, circulation centre position and jet impinging depth are unsteady and periodic with a similar period. The probability distributions of the fluctuating meniscus and wave height have been obtained with the highest frequency near the average position. The flow pattern and meniscus profile may be momentarily asymmetrical, and the phase difference of level fluctuation in the two sides of mould centreline is a half period. The average meniscus profile, the highest and lowest meniscus positions are generally symmetrical about the mould centreline. The wave height mainly depends on the jet impinging depth and circulation centre position. The wave height increases as the jet impinging position rises and the circulation centre approaches to the submerged entry nozzle. 相似文献
10.
《钢铁冶炼》2013,40(5):341-346
AbstractThe dynamic strain aging behaviour of a niobium microalloyed steel has been examined. Hot tensile testing was carried out on heat treated and as received specimens. Heat treated specimens were austenitised at 1000°C for 1 h, and then cooled in air or in a stainless steel cylinder to obtain various amounts of free or uncombined interstitial solutes in solid solution, to examine the effect on the dynamic strain aging behaviour of the steel. It was found that dynamic strain aging takes place in niobium microalloyed steel during tensile testing at temperatures ranging from ambient temperature to 450°C at a crosshead displacement rate of 2 mm min-1. As a result, the ultimate tensile strength and initial work hardening rate exhibit maximum values at temperatures between 200 and 350°C. Also, load-extension graphs for tested specimens show serrated behaviour and yield points at 200, 250, and 300°C. It is believed that dynamic strain aging in niobium steel is caused by interaction between dislocations and interstitial solutes (nitrogen and carbon) or solute pairs consisting of one interstitial and one substitutional solute atom (for example Mn-C and Mn-N). 相似文献
11.
《钢铁冶炼》2013,40(2):149-156
AbstractHeat transfer between mould and strand has a critical influence on billet quality, caster productivity and operating safety. It is very important to obtain the correct distributions of temperature and heat flux, and many studies are made on the calculation methods of heat transfer between strand and mould, aiming to reduce the computation time and improve the calculation accuracy. In the present paper, based on measured data of temperature and heat flux during round billet continuous casting, the calculation method which combines the online measurement data and numerical simulation was investigated. Through identifying the local thermal resistance and its distribution between the mould and the strand by an inverse heat transfer model, the heat flux and shell thickness profiles were calculated. To avoid the iterative solution by inverse model, a faster alternative model using an artificial neural network was developed to predict the thermal resistance from the measured temperature. After training, there is an exact correspondence between the observed temperature values and the thermal resistance. The calculation results obtained by the combination of neural network and numerical simulation can correctly reflect the characteristics of non-uniform heat transfer around the mould circumference, which provides a worthwhile and applicable method for online calculation and visual technology of heat transfer and solidification in continuous casting mould. 相似文献
12.
《钢铁冶炼》2013,40(1):76-82
AbstractIn high speed continuous casting, optimisation of mould taper is key for intensifying heat transfer and for improving the quality of the cast products. Mathematical modelling has been carried out by combining heat transfer, steel shrinkage and parabolic continuous taper model in order to optimise the mould taper profile. These models have been assembled to a set of software, the inputs of which include the steel grade, casting speed, casting temperature, length and the cross-section of mould tube, while the outputs consist of surface temperature of the strand, thickness of solidified shell, thermal linear expansion coefficient, steel shrinkage, distortion of the mould tube wall, the actual air gap, total taper and the continuous taper profile. Optimum mould taper has a parabolic profile which is tapered inwards that changes continuously along the length of the strand in order to achieve reduction in air gap while avoiding distortion of the mould tube. 相似文献
13.
《钢铁冶炼》2013,40(2):120-124
AbstractVacuum degassing processes are now an integral part of secondary steelmaking operations and besides the more obvious benefits of steel chemistry control to precise specifications, they also reduce the number of non-metallic inclusions. Care has to be taken, however, that the change in steel composition through loss of C, O, Mn, etc. does not result in a deleterious change in the composition of the remaining inclusions. Attempts in the past to determine the effect of vacuum on inclusion compositions have been through the use of thermodynamic models, following the inclusion engineering approach. The calculated inclusion compositions do not, however, compare well with the inclusions as analysed in samples taken from the liquid steel after the degassing operation. Clearly, it is important to take into account time dependent effects during degassing and this has been achieved by the development of a combined fluid flow-thermodynamic model. Using the computational fluid dynamics model, CFX, to establish the temperature, flow and species contours in a two-dimensional steel ladle under the influence of natural convection, the results are transferred as start conditions in a three-dimensional RH degasser model. A body force is then applied to simulate the argon bubbles that are injected into the up-leg of the degasser and changes in flow, temperature and species concentrations are calculated. Allowing for additions made during the process, the composition of the top slag and any local inclusions within the steel is predicted. The influence on top slag and inclusion chemistry of any glaze on the snorkels of the degasser is also taken into account. 相似文献
14.
《钢铁冶炼》2013,40(2):112-118
AbstractIt is very important to obtain reliable lubrication from casting powder both at the meniscus and in the gap between strand and mould as it affects slab surface quality and caster productivity. With knowledge of mould friction, a quantitative insight into the behaviour of powder during caster operation is possible. In the present research, the friction was studied based on a slab continuous caster equipped with hydraulic oscillators. The effects of mould oscillation and the abrupt change of casting speed on mould friction force were evaluated, and the characteristics of lubrication behaviour in a casting sequence were investigated. In particular, a comparison between the mould friction force between sinusoidal oscillation mode and non-sinusoidal oscillation mode was made. Finally, the characteristics of friction before a breakout are discussed. The experimental and analytical results may contribute to the development of mould friction online measurement and more clearly learn the lubrication behaviour in different conditions. 相似文献
15.
《钢铁冶炼》2013,40(6):503-510
AbstractIn continuous casting, heat flow optimisation in the mould is key to improving the quality of the product and production savings. The heat flow influences, and is influenced by, several phenomena of a mechanical or metallurgical nature, so its optimisation should include these. In particular, shrinkage of the strand and solid phase formation are among the most influencing factors affecting the cooling of the solidifying product. The present paper describes a model implemented by a software tool that can carry out simulation of shell formation of carbon steel within the mould, for rectangular shapes. The first aim of the software is to simulate formation of the solid shell in the strand and the deformations to which this solid is subjected. Deformations are a result of both thermal shrinkage, related to phase changes, and stresses caused by metallostatic pressure or the mould-shell interaction. The output of the model consists of temperature maps of the strand, maps of formation of the shell and the ideal mould contour. 相似文献
16.
《钢铁冶炼》2013,40(5):360-368
AbstractThis paper is the second of a series of two describing abnormal transient phenomena observed during online monitoring of a billet continuous casting machine. Special attention is paid in Part 2 to in mould solidification. A mould heat flux drift phenomenon (HFD) has been detected, but only for mould powder basicities larger than 0·8. The HFD is related to a decrease of the heat flux in the lower part of the mould and an increase in both the billet-mould friction force and mould thermocouple variability. Results of tests changing the mould powder grade during casting have provided help in explaining the HFD. The probable reason for the HFD is crystallisation of the glassy slag layer. The heat flux ratio parameter (HFR), defined as the ratio between the heat flux in the lower part of the mould and the heat flux in the upper part of the mould, has proved to be a good tool for judging the casting performance of a mould powder. 相似文献
17.
《钢铁冶炼》2013,40(2):138-143
AbstractIn the present paper, based on the two-phase model (Eulerian model), the two-dimensional fluid flow in air stirred water systems is simulated, and the effect of interphase lift force on the fluid flow is specially discussed. In the Eulerian two-phase model, the gas and liquid phases are considered to be two different continuous fluids interacting with each other through the finite interphase areas. The exchange between the phases is represented by source terms in conservation equations. Turbulence is assumed to be a property of the liquid phase. The k–? model is used to describe the behaviour of the liquid phase. The dispersion of phases due to turbulence is represented by introducing a diffusion term into the mass conservation equation. The contribution of bubble movement to the turbulent energy and its dissipation rate are taken into account by adding extra volumetric source terms to the equations of turbulent energy and its dissipation rate. Comparison between the mathematical simulation and experimental data indicates that the interphase lift force has a strong effect on flow behaviour, and considering both drag force and lift force as interphase forces is important to accurately simulate the gas–water two-phase fluid flow in air stirred systems. The interphase lift force makes bubbles move away from the centreline; the gas concentration decreases near the centreline, and increases near the wall. The lift force is smaller than the drag force at the same place, especially far away from the centreline. 相似文献
18.
《钢铁冶炼》2013,40(8):623-630
AbstractTransformation induced plasticity steel with a high content of Al (Al-TRIP) is an advanced high strength steel. The reaction between Al and SiO2 would lead to compositional changes in mould fluxes, which results in a decrease in SiO2 content and an increase in Al2O3 content, and influences the physical properties of the molten fluxes. In the present study, the changes of viscosities of a series of mould fluxes with different additives and addition amounts were examined by a rotating viscometer and the crystals in the D series mould fluxes were analysed by scanning electron microscopy and X-ray diffraction. The results show that (a) the Al2O3 in mould fluxes containing Li2O presents amphoteric characteristic; (b) the viscosity of the fluxes with 8% B2O3 decreases with the increase in w(Al2O3)/w (SiO2) ratio, the result shows that the Al2O3 presents alkaline; (c) the viscosity of flux containing both 4% Li2O and 5% B2O3 changes a little with the increase in w(Al2O3)/w(SiO2) ratio. When the Al2O3 content is 30%, the viscosity is 0·204 Pa s and the break temperature is 1130°C; (d) mould fluxes used for Al-TRIP steel precipitate CaF2 crystals; (e) base on the Riboud model, a suitable viscosity mathematical model for the mould fluxes with high Al2O3 content is established. 相似文献
19.
通过建立保护渣道压力计算模型,研究了保护渣道压力随结晶器振动的周期性变化规律以及保护渣道形状参数、连铸工艺参数和保护渣黏度对渣道压力的影响.结果表明:结晶器达到最大上振速度和最大下振速度时,渣道压力分别达到最大负压和最大正压;保护渣道形状参数对渣道压力有重要影响,渣道入口宽度和出口宽度增加,渣道正负压力都明显下降,而渣道长度增加,渣道正负压力最大值都增加;拉坯速度与结晶器振动速度都影响渣道压力,拉坯速度增加,渣道最大负压增加,而最大正压减小;结晶器振动速度和保护渣黏度增加,使渣道最大正负压力都增加. 相似文献