The through-thickness variation in the porosity of structural foam material is known to result in different “material properties” when mechanics based on homogeneous materials is used to interpret data from standard tensile and bend tests. Unresolved issues relating to structural design include the specification of the most useful test specimen, the identification of useful material properties, and the application of these properties to part design and analysis. This paper develops procedures for determining the mechanical properties of rigid thermoplastic structural foams, and for the application of these properties to the design of load-bearing components. Rather than molded specimens, it is suggested that specimens cut from large, edge-gated plates be used for determining mechanical properties of structural foams. By modeling foams as continuous but nonhomogeneous materials, it is shown that data from simple tensile and flexural tests can be used in structural analysis to systematically account for the through-thickness variation of material properties.  相似文献   

2.
Choonghee Jo 《Polymer》2007,48(11):3349-3360
A constitutive model for tensile behavior of high density polyethylene (HDPE)/clay nanocomposite foams was proposed. The elastic modulus of HDPE/clay nanocomposite was developed using micromechanics theory, and the modulus for foams was obtained by using representative volume element (RVE) concept. In order to describe the tensile behavior of the foams, a constitutive equation obtained from a viscoelastic model was proposed. The constitutive model was expressed in terms of microstructural properties of polymer, and physical properties of the foams. The effects of the material parameters and processing conditions on the foam morphologies and mechanical properties of HDPE/clay nanocomposite foams were investigated. Microcellular closed-cell nanocomposite foams were manufactured with HDPE, where the nanoclay loadings of 0.5, 1.0, and 2.0 wt% were used. The effect of clay loading and foaming conditions on the volume expansion ratio, elastic modulus, tensile strength, and elongation at break was investigated. Except for the elongation at break, the mechanical properties were improved with nanoclay loading. The tensile experimental data of the foams were compared with the prediction by the theoretical model. It was demonstrated that the tensile behaviors of HDPE/clay nanocomposite foams were well described by the constitutive model.  相似文献   

3.
Composite syntactic foams with different densities were fabricated with hollow phenolic microspheres, a phenolic resin binder, and a small addition of chopped carbon fibers. Compressive, shear, and tensile properties were studied for the syntactic foams with and without carbon fibers. Two fiber layer orientations, either parallel (P‐type) or perpendicular (N‐type) to the loading direction, were considered in the mechanical testing. For N‐type foams, mechanical properties were weakly dependent on foam density. For P‐type foams, the mechanical properties of the foams were strongly dependent on the strength of the supporting matrix. The specific strength and specific stiffness of the P‐type foams were significantly enhanced compared with the neat foams. These findings indicate that fiber reinforcement is an effective way to enhance the mechanical performance of syntactic foams, and the enhanced performance should lead to applications as a foam core material for sandwich structures. POLYM. COMPOS., 2010. © 2009 Society of Plastics Engineers  相似文献   

4.
Because of the nonhomogeneous morphology of rigid structural foams, the elastic moduli determined from tension and bend tests are different, the latter being larger. These moduli also depend on the geometry of the specimen. In general, the elastic bending stiffness of foams is determined by the rigidity tensor, which combines geometry and material information. Although the bending problem for nonhomogeneous materials is more complex than the equivalent homogeneous problem, the analysis simplifies considerably for thin-walled beams. The effective flexural modulus for a thin-walled foam beam is shown to be the tension modulus that would be measured on a flat foam specimen of the same thickness. The flexural modulus measured by bend tests on flat bars is shown to have very little effect on the stiffness of most thin-walled sections. This conclusion is independent of how the “true” material modulus varies across the thickness of the foam part.  相似文献   

5.
Choonghee Jo  Hani E. Naguib 《Polymer》2005,46(25):11896-11903
Constitutive equations for nonlinear tensile behavior of PMMA foams were studied. Five viscoelastic models composed of elastic and viscous components were accounted for the modeling of the constitutive equations. The developed constitutive equations are expressed in terms of material properties and foam properties such as strain, strain rate, elastic modulus, relative density of foam, and relaxation time constant. It was found that the stress-strain behaviors by Generalized Maxwell model, Three Element model and Burgers model could be described by the constitutive equation obtained from the Maxwell model. For the verification of the constitutive model, poly(methyl methacrylate) (PMMA) microcellular foams were manufactured using batch process method, and then uniaxial tensile tests were performed. The stress-strain curves by experiment were compared with the theoretical results by the constitutive equation. It was demonstrated that nonlinear tensile stress-strain behaviors of PMMA foams were well described by the constitutive equation.  相似文献   

6.
In this study, a benign process was used to successfully produce low density foam from poly(arylene ether sulfone) (PAES). Both carbon dioxide (CO2) and water as well as nitrogen and water were used as physical blowing agents in a one‐step batch process. A large amount of blowing agents (up to 7.5%) was able to diffuse into the PAES resin in a 2‐h saturation time. Utilizing water and CO2 as the blowing agents yielded foam with better properties than nitrogen and water because both the water and CO2 are plasticizers for the PAES resin. PAES foam produced from CO2 and water had a large reduction in foam density (~80%) and a cell size of ~50 μm, while maintaining a primarily closed cell structure. The small cell size and closed cell structure enhanced the mechanical properties of the foam when compared with the PAES foam produced from nitrogen and water. The tensile, compressive, and notched izod impact properties of the PAES foams were examined, and the compressive properties were compared to commercially available structural foams. With reduced compression strength of 39 MPa and reduced compression modulus of 913 MPa, the PAES foam is comparable to polyetherimide and poly(vinylchloride) structural foams. POLYM. ENG. SCI., 2009. © 2008 Society of Plastics Engineers  相似文献   

7.
This study examines the effect of foam thickness on impact damping properties of closed-cell cross-linked polyethylene foams of different densities. Compression tests and falling weight impact tests were performed to detect the most important mechanisms, which affect the mechanical properties of the foams. The results showed that impact damping properties are significantly influenced by foam thickness, while energy-absorbing capability primarily depends on foam density. The average cell diameter was determined with a scanning electron microscope, which proved that the mechanical properties are mostly influenced by cell structure because higher density foams have smaller cells and thicker cell walls. Other important conclusion is that a foam thickness limit can be determined for a given load level to avoid excessive compaction of the cells and maximize the shock absorption of the foam.  相似文献   

8.
Assessing a full set of mechanical properties is a rather complicate task in the case of foams, especially if material models must be calibrated with these results. Many issues, for example anisotropy and heterogeneity, influence the mechanical behavior. This article shows through experimental analyses how the microstructure affects different experimental setups and it also quantifies the degree of anisotropy of a poly(vinyl chloride) foam. Monotonic and cyclic experimental tests were carried out using standard compression specimens and non‐standard tensile specimens. Results are complemented and compared with the aid of a digital image correlation technique and scanning electron microscopy analyses. Mechanical properties (e.g., elastic and plastic Poisson's ratios) are evaluated for compression and tensile tests, for two different material directions (normal and in‐plane). The material is found to be transversely isotropic. Differences in the results of the mechanical properties can be as high as 100%, or even more depending on the technique used and the loading direction. Also, the experimental analyses show how the material's microstructure behavior, like the evolution of the herein identified “yield fronts” and a “spring back” phenomenon, can influence the phenomenological response and the failure mechanisms as well as the hardening curves. POLYM. ENG. SCI., 2012. © 2012 Society of Plastics Engineers  相似文献   

9.
Several polymers were evaluated as candidates for the production of high‐performance microcellular closed‐cell foams. The polymers involved were a polysulfone, a polyethersulfone, a polyphenylsulfone, a polyetherimide, and a poly(ether ketone ketone), and their suitability was gauged by measuring rates at which they could be impregnated with carbon dioxide under pressure at room temperature. This step is essential to the subsequent step of heating the impregnated samples at various temperatures to create foamed structures. The present study focused primarily on the use of the polysulfone in this regard. Microcellular foams of this polymer were found to have average cell sizes in the range 1–10 μm and cell densities on the order of 1010–1014 cells/cm3. The microstructures of these foamed samples were controlled through careful choices of the foaming temperature and the foaming speed to produce a wide range of foam densities. Since these materials were prepared for possible use as structural materials, tensile tests were conducted to investigate the dependence of some of their mechanical properties on the foam densities (relative to those of the unfoamed polymer). The results indicated that the tensile moduli of these polysulfone foams increased with the square of their relative densities, and the tensile strengths were proportional to these densities. Both of these experimental findings are in agreement with theory. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 1692–1701, 2002  相似文献   

10.
Microcellular ethylene-propylene-diene monomer (EPDM) foams derived from miniaturizing the cellular structure can improve mechanical properties of traditional EPDM foams. It is a current challenge that microcellular EPDM foams prepared by supercritical CO2 foaming technology cannot undergo the post-crosslinking process due to the disappearance of cellular structure, which strongly restricts the development of the mechanical properties of EPDM foams. Hence, a scalable and blending route by selecting the silicone rubber (SR) with different crosslinking temperature compared to EPDM is developed to improve mechanical properties of EPDM foams. During the pre-crosslinking process of EPDM, SR forms a complete crosslinking network, which can make up for the strength of EPDM without the post-crosslinking. Meanwhile, the silica can reduce the domain size of SR and enhance the compatibility between EPDM and SR. As expected, the addition of SR improves the storage modulus, viscosity and matrix strength of EPDM, which shows enhanced mechanical properties of EPDM foams. When the foam density is basically the same, the tensile strength and compressive strength of SR/EPDM foam are increased by 461% and 283% respectively compared with that of EPDM foam. Finally, the maximum tensile strength and compressive strength (40% strain) of SR/EPDM foam achieves 3.58 MPa and 0.59 MPa, respectively.  相似文献   

11.
Epoxy syntactic foams were prepared with diglycidyl ether of bisphenol‐A (DGEBA) epoxy resin, 2.4.6‐tri(dimethylaminomethyl)phenol (DMP‐30), coupling treated microsphere and short carbon fiber. The density of the foam was maintained between 0.56 and 0.91 g/cm3 for all compositions. Compressive, flexural, tensile and dynamic mechanical properties of the foams were investigated with respect to hollow glass microsphere (HGM) and carbon fiber (CF) content. A considerable improvement in the mechanical properties viz. compressive, flexural and tensile strengths was observed for the foams on incorporation of a small quantity of CF. The storage modulus were higher for the foam composites containing CF. The presence of HGM has significant influence on Tg of the syntactic foams, spherical filler diminished the Tg of the syntactic foams due to the plasticizing effect of the coupling treatment of HGM, that is helpful for enhancing damping properties of syntactic foams. POLYM. COMPOS., 37:1960–1970, 2016. © 2015 Society of Plastics Engineers  相似文献   

12.
Polyurethane (PU) is one of the most important polymers with a global production of 17.565 million tons, which makes its recycling an urgent task. Besides, the main goal of PU recycling is to recover constituent polyol as a valuable raw material that allows to obtain new PU with suitable properties. Split‐phase glycolysis can be considered the most interesting PU recycling process since provides high‐quality recovered products in terms of polyol purity. The aim of this work was to evaluate several recovered polyols as replacement of the raw flexible polyether polyol in the synthesis of new flexible PU foams. These recovered polyols come from the split‐phase glycolysis of different types of PU foams and employing as cleavage agents diethylene glycol or crude glycerol (biodiesel byproduct). The influence of the foam waste type and of the cleavage agent on the foams properties was analyzed. The recovered polyols were evaluated by performing several foaming tests according to the method of free expansion foaming of conventional flexible foam. Synthesized flexible foams containing different proportions of recovered polyols were characterized by means of scanning electron microscopy, density and tensile properties; obtaining similar and sometimes even better values compared to the foams manufactured from commercial polyols. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017 , 134, 45087.  相似文献   

13.
The objectives of this work were to seek a simple method for preparation of poly(lactic acid) (PLA) foams and evaluate properties of these foams for scaffold application. Using a typical blowing agent and compression molding, biocomposite foams were successfully prepared from a PLA/rubber wood sawdust (PLA/RWS) blend. Selection of RWS for the biocomposites was based on particle size. RWS particles in two size ranges were used: 212–600 μm and ≤75 μm. Alkaline and silane treatments were applied to the RWS before blending with PLA. The tensile properties, Izod impact strength, foam morphology, and thermal degradation of the biocomposite foams were evaluated. Cytotoxicity and in vitro degradation were tested to determine the potential of the biocomposite foam for use as a scaffold in tissue engineering. Silane treatment improved mechanical properties by increasing the interfacial adhesion between PLA and RWS. The density and void fraction of the foam samples had a greater effect on mechanical properties than pore size. Proliferation of MG-63 cells increased with culture time, indicating that the foam samples were not cytotoxic. Promising samples were tested for degradation in a lysozyme/phosphate-buffered saline and showed a slow rate of in vitro degradation. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019 , 136, 48259.  相似文献   

14.
This study shows the development of new polymeric open‐cell foams from polypropylene (PP) and polylactide (PLA) resins with a focus on sound absorption properties and modeling of these foams. The objective is to develop new environmentally friendly foams to replace the existing non‐recyclable Polyurethane foams are currently used for sound insulation in industry. Through this research, open‐cell foams of about 90% porosity were fabricated from PP and PLA. These resins were selected since PP is a recyclable thermoplastic polymer, and PLA is a bio‐based thermoplastic polymer made from renewable resources. Polyurethane (PU) foam which is currently used for sound absorption and noise control in industry was compared to the fabricated PP and PLA foams. As the first attempt to fabricate environmentally friendly acoustic foams, the resulting foam structures show improved properties as compared to the existing materials. The average absorption of PP and PLA foams fabricated is in the range of 0.42–0.55 which is comparable or even higher than the average absorption of PU foam. To better understand the effect of structural and material properties on sound absorption and further improve the acoustic performance of bio‐based foams, an analytical model based on Johnson–Champoux–Allard model was used to numerically simulate the acoustic performance of foams under study. POLYM. ENG. SCI., 2013. © 2013 Society of Plastics Engineers  相似文献   

15.
Novel flexible polyurethane foams were successfully prepared from a renewable source, hydroxytelechelic natural rubber (HTNR) having different molecular weights (1000–3400 g mol?1) and variation of epoxide contents (EHTNR, 0–35% epoxidation) by a one‐shot technique. The chemical and cell structures as well as physico‐mechanical, thermal, and acoustic properties were characterized and compared with commercial polyol analogs. The obtained HTNR based foams are open cell structures with cell dimensions between 0.38 and 0.47 mm. The HTNR1000 based foam exhibits better mechanical properties but lower elongation at break than those of commercial polyol analog. However, the HTNR3400 based foam shows the best elastic properties. In a series of EHTNR based foams, the tensile and compressive strengths show a tendency to increase with increasing epoxide content and amount of 1,4‐butanediol (BD). The HTNR based foams demonstrate better low temperature flexibility than that of the foam based on commercial polyol. Moreover, the HTNR based polyurethane foams was found to be an excellent absorber of acoustics. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

16.
以大豆分离蛋白、高活性聚醚、聚合物多元醇、交联剂、发泡剂、泡沫稳定剂和混合异氰酸酯为原料,自由发泡、常温熟化制备了大豆蛋白基高回弹聚氨酯软泡。研究了大豆蛋白质(SPI)对聚氨酯泡沫物理性能、力学性能、孔结构和热性能的影响。结果表明:SPI添加量对泡沫物理和力学性能影响最大。随着SPI含量增加,泡沫的密度、尺寸稳定性提高,压陷硬度和舒适因子提高增大;回弹率下降,断裂伸长率减小,而拉伸强度先增大后减小。SPI能够提高聚氨酯的热稳定性,但最好低于150℃使用。  相似文献   

17.
采用新型高活性聚合物多元醇GPOP-H45为原料,制备出机械性能良好的高回弹泡沫制品。讨论了影响泡沫性能的主要因素及国外同类产品发泡情况和制品性能的比较。结果发现,在发泡中加入GPOP-H45,可显著提高泡沫制品的承载性及开孔性,同时改进了其机械性能。  相似文献   

18.
In this article, mechanical behavior under compression loads of an innovative adsorbent material, based on silicone composite foams filled with SAPO 34 zeolite, is presented. The innovative composite foams were obtained profiting by the dehydrogenative coupling of siloxane constituents. These new adsorbent systems have been proposed to overcome to the low mechanical stability of conventional SAPO‐34 coating for adsorption chiller. In this concern, static and cyclic compressive tests at room temperature have been carried out. Samples at increasing content of SAPO 34 zeolite were tested to evaluate the influence of the filler content on the mechanical behavior of the composite foam. The results showed that the presence of zeolite reduces the elastic limit of the foam and increases the strength. The foams evidenced also acceptable mechanical stability to cyclic compressive loads. The encouraging results confirm the possible use of these new composite foams as adsorbent materials for cyclic adsorption heat pumps. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018 , 135, 46145.  相似文献   

19.
Bio-based polyurethane (PU) foams were developed from bio-polyol (castor oil-based) in the presence of selective catalyst, surfactant, and blowing agent. Bentonite nanoclay (NC) was incorporated into the bio-polyol mixture as nano-reinforcement, while, triethyl phosphate was used as flame-retardant agent. After fabrication, these bioengineered foam nano-composites were studied for microstructural, mechanical and thermal characterizations. Fourier transform infrared spectroscopy analysis indicated the presence of characteristic functionalities within biopolyol segments, which was influenced by reactant activity within the polyurethane (PU) foams. Scanning electron microscopy revealed the cellular morphology of the foam. Thermogravimetric analysis enabled the study of foam decomposition behavior for different sample compositions. Incorporation of NC into pristine foam was found to delay the onset degradation temperature. Flammability studies depicted significant enhancement of flame retardancy with incorporation of NC up to a certain loading level. Compression tests demonstrated that significant improvement of compressive strength properties of foams could be achieved by incorporating bentonite nanoclay, owing to nucleation effect of nanoclay and corresponding enhanced structural integrity. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019 , 136, 47063.  相似文献   

20.
在聚氨酯泡沬中添加竹炭微粒,运用一步发泡法制备了不同竹炭含量的软质泡沫塑料,测试了该泡沫塑料的密度、力学性能、色差、负离子释放能力及远红外发射率。结果表明,该泡沫塑料的密度、负离子释放能力、回弹率、远红外发射率均随着复合竹炭粉含量的增加而增加;而拉伸强度、断裂伸长率、撕裂强度却随着复合竹炭粉含量的增加而减少;复合竹炭粉含量为8%(质量分数,下同)时的聚氨酯泡沫塑料的拉伸强度、断裂伸长率、撕裂强度分别为纯聚氨酯泡沫塑料的63.87%、57.04%、55.32%;当复合竹炭粉含量≤2%时,制备的竹炭聚氨酯泡沫塑料达到GB/T 10802—2006标准要求。  相似文献   