首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到16条相似文献,搜索用时 0 毫秒
1.
A new bioactive diacid monomer, 5‐(2‐phthalimidoethanesulfonamido) isophthalic acid ( 6 ), was synthesized in three steps. This monomer can be regarded as biologically active aromatic diacid and may be used in the design of biodegradable and biological materials. This monomer was polymerized with several aromatic diamines by step‐growth polymerization to give a series of biodegradable and highly thermally stable polyamides (PAs) with good yield (70–82%) and moderate inherent viscosity between 0.38–0.68 dL/g in a system of triphenylphosphite/pyridine/N‐methyl‐2‐pyrolidone/CaCl2. The new aromatic diacid 6 and all of the PAs derived from this diacid and aromatic diamines were characterized by Fourier transform infrared, 1H‐NMR, 13C‐NMR, and elemental analysis techniques. The thermal stability of the PAs was determined by thermogravimetric analysis and differential scanning calorimetry techniques under a nitrogen atmosphere, and we found that they were moderately stable. The soil biodegradability behavior of 6 and all of the PAs derived from this diacid and aromatic diamines were investigated in culture media, and we found that the synthesized diacid 6 and all of the PAs were biodegradable under a natural environmental. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

2.
A new class of optically active poly(amide‐imide‐urethane) was synthesized via two‐step reactions. In the first step, 4,4′‐methylene‐bis(4‐phenylisocyanate) (MDI) reacts with several poly(ethylene glycols) (PEGs) such as PEG‐400, PEG‐600, PEG‐2000, PEG‐4000, and PEG‐6000 to produce the soft segment parts. On the other hand, 4,4′‐(hexafluoroisopropylidene)‐N,N′‐bis(phthaloyl‐L ‐leucine‐p‐amidobenzoic acid) (2) was prepared from the reaction of 4,4′‐(hexafluoroisopropylidene)‐N,N′‐bis(phthaloyl‐L ‐leucine) diacid chloride with p‐aminobenzoic acid to produce hard segment part. The chain extension of the above soft segment with the amide‐imide 2 is the second step to give a homologue series of poly(amide‐imide‐urethanes). The resulting polymers with moderate inherent viscosity of 0.29–1.38 dL/g are optically active and thermally stable. All of the above polymers were fully characterized by IR spectroscopy, elemental analyses, and specific rotation. Some structural characterization and physical properties of this new optically active poly(amide‐imide‐urethanes) are reported. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 2288–2294, 2004  相似文献   

3.
Epiclon [3a,4,5,7a‐tetrahydro‐7‐methyl‐5‐(tetrahydro‐2,5‐dioxo‐3‐furanyl)‐1,3‐isobenzofurandione] or [5‐(2,5‐dioxotetrahydrofurfuryl)‐3‐methyl‐3‐cyclohexyl‐1,2‐dicarboxylic acid anhydride] (1) was reacted with L ‐isoleucine (2) in acetic acid and the resulting imide acid (3) was obtained in high yield. The diacid chloride (4) was obtained from diacid derivative (3) by reaction with thionyl chloride. The polycondensation reaction of diacid chloride (4) with several aromatic diamines such as 4,4′‐sulfonyldianiline (5a), 4,4′‐diaminodiphenyl methane (5b), 4,4′‐diaminodiphenylether (5c), p‐phenylenediamine (5d), m‐phenylenediamine (5e), 2,4‐diaminotoluene (5f), and 4,4′‐diaminobiphenyl (5g) was developed by using a domestic microwave oven in the presence of a small amount of a polar organic medium such as o‐cresol. The polymerization reactions were also performed in two other different methods: low‐temperature solution polycondensation and reflux conditions. A series of optically active poly(amide imides) with inherent viscosity of 0.12–0.30 dL/g were obtained. All of the above polymers were fully characterized by IR, elemental analyses, and specific rotation techniques. Some structural characterizations and physical properties of these optically active poly(amide imides) are reported. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 93: 2218–2229, 2004  相似文献   

4.
Polyamides (PAs) containing fluorene, oxyether, and diphenyl‐silane moieties in the repeating unit were synthesized in > 85% yield by direct polycondesation between a diamine and four dicarboxylic acids. Alternatively, one PA was synthesized from an acid dichloride. The diamine 4‐[4‐[9‐[4‐(4‐aminophenoxy)‐3‐methyl‐phenyl]fluoren‐9‐yl]‐2‐methyl‐phenoxy]aniline ( 3 ) was obtained from the corresponding dinitro compound, which was synthesized by nucleophilic aromatic halogen displacement from p‐chloronitrobenzene and 9,9‐bis (4‐hydroxy‐3‐methyl‐phenyl)fluorene ( 1 ). Monomers and polymers were characterized by FTIR and 1H, 13C, and 29Si‐NMR spectroscopy and the results were in agreement with the proposed structures. PAs showed inherent viscosity values between 0.14 and 0.43 dL/g, indicative of low molecular weight species, probably of oligomeric nature. The glass transition temperature (Tg) values were observed in the 188–211°C range by DSC analysis. Thermal decomposition temperature (TDT10%) values were above 400°C due to the presence of the aromatic rings in the diamine. All PAs showed good transparency in the visible region (>88% at 400 nm) due to the incorporation of the fluorene moiety. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

5.
A pyromellitic dianhydride (benzene‐1,2,4,5‐tetracarboxylic dianhydride) was reacted with L ‐isoleucine in acetic acid, and the resulting imide acid [N,N′‐(pyromellitoyl)‐bis‐L ‐isoleucine] (4) was obtained in a high yield. 4 was converted into N,N′‐(pyromellitoyl)‐bis‐L ‐isoleucine diacid chloride by a reaction with thionyl chloride. The polycondensation reaction of this diacid chloride with several aromatic diamines, including 1,4‐phenylenediamine, 4,4′‐diaminodiphenyl methane, 4,4′‐diaminodiphenylsulfone (4,4′‐sulfonyldianiline), 4,4′‐diaminodiphenylether, 2,4‐diaminotoluene, and 1,3‐phenylenediamine, was developed with two methods. The first method was polymerization under microwave irradiation, and the second method was low‐temperature solution polymerization, with trimethylsilyl chloride used as an activating agent for the diamines. The polymerization reactions proceeded quickly and produced a series of optically active poly(amide imide)s with good yields and moderate inherent viscosities of 0.17–0.25 dL/g. All of the aforementioned polymers were fully characterized by IR, elemental analyses, and specific rotation. Some structural characterization and physical properties of these optically active poly(amide imide)s are reported. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 951–959, 2004  相似文献   

6.
A series of polyamides were synthesized by the direct polycondensation of 2,2‐bis[4‐(4‐amino‐2‐fluorophenoxy)phenyl]hexafluoropropane with various commercially available dicarboxylic acids such as terephthalic acid, isophthalic acid, 5‐t‐butyl isophthalic acid, and 2,6‐naphthalene dicarboxylic acid. The synthesized polyamides were soluble in several organic solvents such as N,N‐dimethylformamide, N,N‐dimethylacetamide, dimethyl sulfoxide, tetrahydrofuran, and chloroform, and they exhibited inherent viscosities of 0.42–0.59 dL/g. The polyamides exhibited weight‐average molecular weights of up to 26,000, which depended on the exact repeating unit structure. These polyamides showed good thermal stability up to 440°C for a 10% weight loss in synthetic air. The polyamides synthesized from 5‐t‐butyl isophthalic acid and isophthalic acid exhibited glass‐transition temperatures of 217 and 185°C, respectively (by differential scanning calorimetry) in nitrogen. The polyamides synthesized from terephthalic acid and 2,6‐naphthalene dicarboxylic acid showed melting temperatures of 319 and 385°C, respectively. The polyamides films were pale yellow, with tensile strengths of up to 82 MPa, moduli of elasticity of up to 2.3 GPa, and elongations at break of up to 9%, which depended on the exact repeating unit structure. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 89: 691–696, 2003  相似文献   

7.
A new class of optically active poly(amide imide)s were synthesized via direct polycondensation reaction of diisocyanates with a chiral diacid monomer. The step‐growth polymerization reactions of monomer bis(p‐amido benzoic acid)‐N‐trimellitylimido‐L‐leucine (BPABTL) (5) as a diacid monomer with 4,4′‐methylene bis(4‐phenylisocyanate) (MDI) (6) was performed under microwave irradiation, solution polymerization under gradual heating and reflux condition in the presence of pyridine (Py), dibuthyltin dilurate (DBTDL), and triethylamine (TEA) as a catalyst and without a catalyst, respectively. The optimized polymerization conditions according to solvent and catalyst for each method were performed with tolylene‐2,4‐diisocyanate (TDI) (7), hexamethylene diisocyanate (HDI) (8), and isophorone diisocyanate (IPDI) (9) to produce optically active poly(amide imide)s by the diisocyanate route. The resulting polymers have inherent viscosities in the range of 0.09–1.10 dL/g. These polymers are optically active, thermally stable, and soluble in amide type solvents. All of the above polymers were fully characterized by IR spectroscopy, 1H NMR spectroscopy, elemental analyses, specific rotation, and thermal analyses methods. Some structural characterization and physical properties of this new optically active poly(amide imide)s are reported. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 93: 1647–1659, 2004  相似文献   

8.
4‐(4′‐Aminophenyl)urazole (AmPU) was prepared from 4‐nitrobenzoic acid in six steps. The reaction of AmPU with acetyl chloride was performed in N,N‐dimethylacetamide solutions at different ratios, and the resulting disubstituted and trisubstituted amide derivatives were obtained in high yields and were used as models for polymerization reactions. Polycondensation reactions of AmPU with succinyl chloride, suberoyl chloride, and sebacoyl chloride were performed with conventional solution polymerization techniques in the presence of different catalysts, such as pyridine, triethylamine, and dibutyltin dilaurate, and led to the formation of novel aliphatic polyamides. The resulting novel polyamides had inherent viscosities of 0.11–0.22 dL/g in dimethylformamide or H2SO4 at 25°C. These polyamides were characterized with IR, 1H‐NMR, elemental analysis, and thermogravimetric analysis. Some physical properties and structural characterization of these novel polyamides are reported. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 3173–3185, 2004  相似文献   

9.
Pyromellitic dianhydride (1,2,4,5‐benzenetetracarboxylic acid 1,2,4,5‐dianhydide) was reacted with L ‐valine in a mixture of acetic acid and pyridine (3:2) at room temperature, and then was refluxed at 90–100 °C, N,N′‐(pyromellitoyl)‐bis‐L ‐valine diacid was obtained in quantitative yield. The imide–acid was converted to N,N′‐(pyromellitoyl)‐bis‐L ‐valine diacid chloride by reaction with thionyl chloride. Rapid and highly efficient synthesis of a number of poly(amide–imide)s was achieved under microwave irradiation using a domestic microwave oven by polycondensation of N,N′‐(pyromellitoyl)‐bis‐L ‐valine diacid chloride with six different derivatives of 5,5‐disubstituted hydantoin compounds in the presence of a small amount of a polar organic medium that acts as a primary microwave absorber. A suitable organic medium was o‐cresol. The polycondensation proceeded rapidly, compared with conventional melt polycondensation and solution polycondensation and was almost completed within 8 min, giving a series of poly(amide–imide)s with inherent viscosities in the range 0.15–0.36 dl g?1. The resulting poly(amide–imide)s were obtained in high yield and are optically active and thermally stable. All of the above compounds were fully characterized by Fourier‐transform infrared (FT‐IR) spectroscopy, elemental analysis, inherent viscosity (ηinh) measurements, solubility testing and specific rotation measurements. The thermal properties of the poly(amide–imide)s were investigated by using thermogravimetric analysis. Copyright © 2004 Society of Chemical Industry  相似文献   

10.
Pyromellitic dianhydride (benzene‐1,2,4,5‐tetracarboxylic dianhydride) (1) was reacted with L‐phenylalanine (2) in a mixture of acetic acid and pyridine (3 : 2) and the resulting imide‐acid [N,N′‐(pyromellitoyl)‐bis‐L‐phenylalanine diacid] (4) was obtained in quantitative yield. The compound (4) was converted to the N,N′‐(pyromellitoyl)‐bis‐L‐phenylalanine diacid chloride (5) by reaction with thionyl chloride. A new facile and rapid polycondensation reaction of this diacid chloride (5) with several aromatic diols such as phenol phthalein (6a), bisphenol‐A (6b), 4,4′‐hydroquinone (6c), 1,8‐dihydroxyanthraquinone (6d), 4,4‐dihydroxy biphenyl (6e), and 2,4‐dihydroxyacetophenone (6f) was developed by using a domestic microwave oven in the presence of a small amount of a polar organic medium such as o‐cresol. The polymerization reactions proceeded rapidly and are completed within 20 min, producing a series of optically active poly(ester‐imide)s with good yield and moderate inherent viscosity of 0.10–0.26 dL/g. All of the above polymers were fully characterized by IR, elemental analyses, and specific rotation. Some structural characterization and physical properties of these optically active poly(ester‐imide)s are reported. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 2211–2216, 2002  相似文献   

11.
Rapid and highly efficient synthesis of novel poly(amide‐imide)s (PAIs) were achieved under microwave irradiation by using a domestic microwave oven from the polycondensation reactions of 4,4′‐carbonyl‐bis(phthaloyl‐L ‐alanine) diacid chloride [N,N′‐(4,4′‐carbonyldiphthaloyl)] bisalanine diacid chloride (1) with six different derivatives of tetrahydropyrimidinone and tetrahydro‐2‐thioxopyrimidine compounds (2a–2f) in the presence of a small amount of a nonpolar organic medium that acts as a primary microwave absorber. Suitable organic media was o‐cresol. The polycondensation proceeded rapidly and was almost completed within 10 min, giving a series of PAIs with inherent viscosities of about 0.25–0.45 dL/g. The resulting PAIs were obtained in high yield and are optically active and thermally stable. All of the above compounds were fully characterized by means of Fourier transform infrared spectroscopy, elemental analyses, inherent viscosity (ηinh), solubility test, and specific rotation. Thermal properties of the PAIs were investigated using thermogravimetric analysis. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 80: 2416–2421, 2001  相似文献   

12.
Pyromellitic dianhydride (1,2,4,5‐benzenetetracarboxylic acid 1,2,4,5‐dianhydide) (1) was reacted with L‐phenylalanine (2) in a mixture of acetic acid and pyridine (3 : 2) at room temperature, then was refluxed at 90–100°C and N,N′‐(Pyromellitoyl)‐bis‐L ‐phenylalanine diacid (3) was obtained in quantitative yield. The imide‐acid (3) was converted to N,N′‐(Pyromellitoyl)‐bis‐L ‐phenylalanine diacid chloride (4) by reaction with thionyl chloride. Rapid and highly efficient synthesis of poly(amide‐imide)s (6a–f) was achieved under microwave irradiation by using a domestic microwave oven from the polycondensation reactions of N,N′‐(Pyromellitoyl)‐bis‐L ‐phenylalanine diacid chloride (4) with six different derivatives of 5,5‐disubstituted hydantoin compounds (5a–f) in the presence of a small amount of a polar organic medium that acts as a primary microwave absorber. Suitable organic media was o‐cresol. The polycondensation proceeded rapidly, compared with the conventional melt polycondensation and solution polycondensation, and was almost completed within 10 min, giving a series of poly(amide‐imide)s with inherent viscosities about 0.28–0.44 dL/g. The resulting poly(amide‐imide)s were obtained in high yield and are optically active and thermally stable. All of the above compounds were fully characterized by means of FTIR spectroscopy, elemental analyses, inherent viscosity (ηinh), solubility test and specific rotation. Thermal properties of the poly(amide‐imide)s were investigated using thermal gravimetric analysis (TGA). © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 516–524, 2004  相似文献   

13.
A new kind of aromatic unsymmetrical diamine monomer containing thiazole ring, 2‐amino‐5‐(4‐aminophenyl)‐thiazole (AAPT), was synthesized. A series of novel polyimides were prepared by polycondensation of AAPT with various aromatic dianhydrides by one‐step polyimidation process. The synthesized polyimides had inherent viscosity values of 0.36–0.69 dL/g and were easily dissolved in highly dipolar solvents. Meanwhile, strong and flexible polyimide films were obtained, which have good thermal and thermo‐oxidative stability with the glass transition temperatures (Tg) of 276.7–346.1°C, the temperature at 5% weight loss of 451–492°C in nitrogen and 422–440°C in air, as well as have outstanding mechanical properties with the tensile strengths of 94–122 MPa, elongations at breakage of 5–18%. These films also had dielectric constants of 3.12–3.38 at 10 MHz. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008  相似文献   

14.
Polycondensation‐type poly(amic acid) (PAA) was synthesized with 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride as a dianhydride monomer and 4,4′‐diaminodiphenylmethane and 4,4′‐oxydianiline as diamine monomers under microwave irradiation in dimethylformamide. Then, PAA was used to make polyimide (PI) by imidization at a low temperature. The structure and performance of the polymers were characterized with Fourier transform infrared (FTIR), proton nuclear magnetic resonance (1H‐NMR), viscosity, X‐ray diffraction (XRD), and thermogravimetry (TG) curve analyses. The FTIR spectra of the polymers showed characteristic peaks of PI around 1779 and 1717 cm?1. The 1H‐NMR spectrum of PAA indicated a singlet at 6.55 ppm assigned to ? NHCO? and a singlet at 10.27 ppm assigned to carboxylic acid protons. The XRD spectrum demonstrated that the obtained PI had a low‐order aggregation structure with a d‐spacing of 0.5453 nm. The TG results revealed that the PI was thermally stable with 10% weight loss at 565°C in an N2 atmosphere. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2008  相似文献   

15.
A new class of optically active poly(amide–imide–urethane)s (PAIUs) was synthesized via a two‐step diisocyanate route under microwave irradiation. In these reactions, 4,4′‐methylene‐bis(4‐phenylisocyanate) was reacted with bis(p‐amido benzoic acid)‐N‐trimellitylimido‐L ‐leucine and poly(ethylene glycol diol)s (PEGs), such as PEG‐400, PEG‐600, PEG‐1000, and PEG‐2000, to furnish a series of new PAIUs. The effects of different reaction conditions, such as the method of preparation (polyol or acid chain extension), the prepolymerization step (NCO‐terminated oligoamide or NCO‐terminated polyether polyol), the irradiation time and power, the reaction solvent, the soft‐segment length, and the presence or absence of reaction catalysts (e.g., triethylamine, pyridine, and dibutyltin dilaurate), on the properties of the copolymers, including the solubility, viscosity, and thermal behavior, were investigated. The resulting multiblock copolymers had inherent viscosities of 0.15–0.53 dL/g. These multiblock copolymers were optically active, thermally stable, and soluble in amide‐type solvents. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 98: 1781–1792, 2005  相似文献   

16.
N,N′‐(Pyromellitoyl)‐bis‐(L ‐leucine) diacid was reacted with ethyl chloroformate in the presence of triethylamine followed by reaction with activated sodium azide and gave N,N′‐(pyromellitoyl)‐bis‐(L ‐leucine) diacylazide in high yield. This diacylazide was heated in dry benzene and gave the unstable N,N′‐(pyromellitoyl)‐bis‐(L ‐leucine) diisocyanate ( 5 ) in quantitative yield. Thus, diisocyanate 5 was generated in situ and polycondensation reaction of this monomer with several aromatic diols, such as 4,4′‐dihydroxybiphenyl, 1,4‐hydroquinone, bisphenol A, phenolphthalein and 1,4‐dihydroxyanthraquinone, was performed in dry toluene under refluxing in the presence of 1,4‐diazabicyclo[2.2.2]octane (triethylenediamine) as a catalyst. The polymerization reactions proceeded within 48 h, producing a series of optically active poly(imide–urethane)s with good yield and moderate inherent viscosity in the range 0.18–0.28 dl g?1. All of the above polymers were fully characterized by infrared spectra, elemental analyses and specific rotation. Some structural characterization and physical properties of these optically active poly(imide–urethane)s are reported Copyright © 2003 Society of Chemical Industry  相似文献   