The current investigation focuses on the determination of the strength of adhesive-bonded single lap joints under impact with the use of a split Hopkinson pressure bar (Kolsky bar). For this, experiments were conducted at different loading rates, for identical metallic adherends bonded by a two-part epoxy adhesive. Four different types of specimens were adopted, all with a given adhesive thickness. The length of overlap and the width of the adherends were varied resulting in four different areas of overlap. It was found that the average strength, as calculated from the readings obtained from a Kolsky bar, increases with decrease of overlap area. An elastodynamic model for the shear strain of the adhesive-bonded single lap joint was developed to investigate this drastic effect of overlap area on the average strength of the joint. The mathematical model was found to be dependent on both the material properties of the adherend and adhesive, as well as the structural properties of the joint, viz. the width and the thickness of the adhesive layer. A combined experimental-numerical technique was used to predict the strain distribution over the length of the bond in the adhesive. It was found that the edges of the adhesive were subjected to maximum strain, while a large part of the adhesive was found to exhibit zero shear strain. The effect of the lap length and the width was studied individually. The cumulative effect of averaging the strain over the entire overlap area, was decreased shear strain for an increased overlap area. The Kolsky bar was identified to give conservative values of the shear strength of an adhesive bonded lap joint under high rates of loading.  相似文献   

2.
In this paper we examine the effect on joint strength of depleting the bond line of a relatively flexible adhesive (polyethylene) while maintaining a constant adhesive film thickness. It is shown that the tensile shear strength of a lap specimen is not governed by edge effects but rather by the bonded area. By using limit analysis of the plasticity theory, we demonstrate why the tensile shear strength of the joint is insensitive to stress concentrations at the bonding defects.  相似文献   

3.
Adhesively bonded composite single lap joints were experimentally investigated to analyze the bondline stress concentrations and characterize the influence of adhesive ductility on the joint strength. Two epoxy paste adhesives—one with high tensile strength and low ductility, and the other with relatively low tensile strength and high ductility—were used to manufacture composite single lap joints. Quasi-static tensile tests were conducted on the single lap joints to failure at room temperature. High magnification two-dimensional digital image correlation was used to analyze strain distributions near the adhesive fillet regions. The failure mechanisms were examined using scanning electron microscopy to understand the effect of adhesive ductility on the joint strength. For a given surface treatment and laminate type, the results show that adhesive ductility significantly increases the joint strength by positively influencing stress distribution and failure mechanism near the overlap edges. Moreover, it is shown that high magnification two-dimensional digital image correlation can successfully be used to study the damage initiation phase in composite bonded joints.  相似文献   

4.
This paper discusses the static and fatigue behavior of adhesively bonded single lap joints in SMC-SMC composites. Effects of lap length and adhesive thickness on the static and fatigue strength of SMC-SMC adhesive joints are studied. Effects of SMC surface preparation and test speed on the joint performance are evaluated. Finally, the effect of water exposure on the joint durability is also investigated. Results show that the static behavior of adhesive joints in SMC-SMC composites is significantly influenced by the lap length and adhesive thickness. With an increase in lap length from 12.7 mm to 38.1 mm, the joint failure load increases by 37%. The joint failure load also increases with the adhesive thickness, but it reaches a maximum at an adhesive thickness of 0.33 mm and then decreases. However, lap length and adhesive thickness have negligible effect on the ratio of fatigue strength to static strength. The fatigue strength at 106 cycles is approximately 50% to 54% of the static strength for various adhesive thicknesses and lap lengths investigated in this study. Adhesive failure, fiber tear or combination of these two failure modes are observed during both static and fatigue tests.  相似文献   

5.
The strength of adhesive bonded joints is investigated both analytically and experimentally. The deformed states of lap joints under tensile shear loading are analysed by the finite element method on the assumption of elastic deformation. A method of using the adhesive strength law is proposed to estimate the joint strength. The adhesive strength law is experimentally determined by subjecting butt joints of two thin-walled tubes to combined axial load and torsion. The strength of lap joints is determined by adopting the adhesive strength law to the adhering interface as well as the strength law of adherend and adhesive resin. The calculated strain distribution and strength of the joints are compared with the experimental results. The effects of the joint configurations on the deformation and strength are discussed. It is shown that the proposed method is useful to predict the joint strength.  相似文献   

6.
The strength of adhesive bonded joints is investigated both analytically and experimentally. The deformed states of lap joints under tensile shear loading are analysed by the finite element method on the assumption of elastic deformation. A method of using the adhesive strength law is proposed to estimate the joint strength. The adhesive strength law is experimentally determined by subjecting butt joints of two thin-walled tubes to combined axial load and torsion. The strength of lap joints is determined by adopting the adhesive strength law to the adhering interface as well as the strength law of adherend and adhesive resin. The calculated strain distribution and strength of the joints are compared with the experimental results. The effects of the joint configurations on the deformation and strength are discussed. It is shown that the proposed method is useful to predict the joint strength.  相似文献   

7.
In order to improve the tensile lap shear strength of adhesively bonded joints, nano-particles were dispersed in the adhesive using a 3-roll mill. The dispersion states of nano-particles in the epoxy adhesive were observed with TEM (Transmission Electron Microscopy) with respect to the mixing conditions, and the effect of nano-particles on the mechanical properties of the adhesive was measured with respect to dispersion state and weight content of nano-particles. Also the static tensile load capability of the adhesively bonded double lap joints composed of uni-directional glass/epoxy composite and nano-particle-reinforced epoxy adhesive was investigated to assess the effect of nano-particles on the lap shear strength of the joint. From the experimental and FE analysis results, it was found that the nano-particles in the adhesive improved the mechanical properties of the adhesive. Also the increased failure strain and the reduced CTE (coefficient of thermal expansion) of the nano-particle-reinforced adhesive improved the lap shear strength of adhesively bonded joints.  相似文献   

8.
通过理论分析和计算确定了动车组空调通风口部件与铝合金车体胶接用胶粘剂的强度指标。介绍了胶粘剂的选择及胶接结构的设计原则,考查了搭接长度、搭接宽度、胶层厚度和被粘接材料厚度等对胶接件粘接强度的影响。结果表明:车体与空调通风口部件的胶接接头选择受剪切应力作用的搭接接头较适宜,并且搭接接头的承载能力随搭接长度或宽度增加呈先快速上升后趋于稳定态势;当搭接长度为10 mm、胶层厚度为6 mm、铝合金板厚度为5 mm且常温湿固化型单组分PU(聚氨酯)胶粘剂的剪切强度超过0.23 MPa时,搭接接头的承载能力相对最大。  相似文献   

9.
When an adhesively bonded joint is exposed to a high environmental temperature, the tensile load capability of the adhesively bonded joint decreases because the elastic modulus and failure strength of the adhesive decrease. In this paper, the elastic modulus and failure strength of the adhesive as well as the tensile load capability of the tubular single lap adhesively bonded joint were experimentally and theoretically investigated with respect to the volume fraction of filler and the environmental temperature. Two types of fillers - Al2O3 (alumina) and chopped fiber E glass - were used. From the experiment, it was found that the elastic modulus and failure strength of the adhesive increased in accordance with the increase of volume fraction of the filler and decreased with the environmental temperature rise. It was also found that the tensile load capability of the tubular single lap adhesively bonded joint decreased as the environmental temperature increased; however, it had no correlation with the volume fraction of filler because of the effect of the fabrication thermal residual stresses generated by the CTE difference between the adherend and adhesive.  相似文献   

10.
An experimental study was conducted on the strength of adhesively bonded steel joints, prepared epoxy and acrylic adhesives. At first, to obtain strength characteristics of these adhesives under uniform stress distributions in the adhesive layer, tensile tests for butt, scarf and torsional test for butt joints with thin-wall tube were conducted. Based on the above strength data, the fracture envelope in the normal stress-shear stress plane for the acrylic adhesive was compared with that for the epoxy adhesive. Furthermore, for the epoxy and acrylic adhesives, the effect of stress triaxiality parameter on the failure stress was also investigated. From those comparison, it was found that the effect of stress tri-axiality in the adhesive layer on the joint strength with the epoxy adhesive differed from that with the acrylic adhesive. Fracture toughness tests were then conducted under mode l loading using double cantilever beam (DCB) specimens with the epoxy and acrylic adhesives. The results of the fracture toughness tests revealed continuous crack propagation for the acrylic adhesive, whereas stick-slip type propagation for the epoxy one. Finally, lap shear tests were conducted using lap joints bonded by the epoxy and acrylic adhesives with several lap lengths. The results of the lap shear tests indicated that the shear strength with the epoxy adhesive rapidly decreases with increasing lap length, whereas the shear strength with the acrylic adhesive decreases gently with increasing the lap length.  相似文献   

11.
Abstract

Adhesive bonding is the best alternative to riveting in aircraft structures but the strength of the adhesive bonded joint is low and is limited by strength of adhesive. Strengthening of adhesive bonding is an important requirement. In this work, an attempt has been made to strengthen the adhesive bonding by mixing different quantities of brittle adhesive in the ductile adhesive and vice-versa. Two different adhesives, one brittle (AV138) and another ductile (Araldite-2015) adhesive have been considered. Initially single lap joint has been constructed between the CFRP and aluminium with individual adhesives, then the mixture of adhesives have been used in the bonded region in varied proportions. The X-ray radiography and ultrasonic testing have been performed to check the quality of bonding. Uniaxial tensile tests have been conducted on the lap joints along with Digital Image Correlations (DIC) to obtain the individual and mixed adhesive bond strength. The failure patterns have been identified using optical and scanning electron microscope. These studies indicate that strengthening of the adhesive bonding achieved by mixing of two adhesives and highest bond strength obtained when the mixture of AV138 and Araldite-2015 adhesives are used in equal proportions.  相似文献   

12.
The goal of this research was to experimentally demonstrate the correlations between processing variables (adhesive type, bondline thickness, adherend thickness, surface pretreatment, overflow fillet) and effective strength in adhesively bonded single lap joints. While generalizations between effective strength and individual joint design parameters have been assumed for decades, the multifaceted interplay between parameters is complex and remains difficult to understand. Traditionally reported studies of the adhesive bond strength of single lap joints are often limited in the sample size populations needed to statistically probe concurrent design variables. To overcome sample size limitations a test matrix of 1200 single lap joints, partitioned by 96 unique fabrication conditions, was processed and tested using a workflow protocol orchestrated through a relational database. The enhanced pedigree and integrity enabled by using a relational database centered workflow allowed for multivariate principal component analysis of the joint design parameters, with all experimental data input available for peer audit. The results of this study revealed that the adhesive type biases the remaining joint configuration variables towards more influence with respect to either mechanical load or displacement to failure.  相似文献   

13.
Single-lap band adhesive joints of dissimilar adherends subjected to external bending moments are analyzed as a four-body contact problem using a two-dimensional theory of elasticity (plane strain state). In the analysis, the upper and lower adherends and the adhesive which are bonded in two regions are replaced by finite strips. In the numerical calculations, the effects of the ratio of Young's moduli of the adherends, the ratio of the adherend thicknesses, and the ratio of the band length to the half lap length on the stress distributions at the interfaces are examined. A method for estimating the joint strength is proposed using the interface stress and strain obtained by the analysis. An elasto-plastic finite element analysis (EP-FEA) was conducted for predicting the joint strength more exactly. Experiments to measure strains and the joint strength were also carried out. The results show that the strength of a single-lap band adhesive joint is almost the same as that of a single-lap adhesive joint in which the two adherends are completely bonded at the interfaces. Thus, the single-lap band adhesive joints are useful in the design of single-lap joints.  相似文献   

14.
An experimental–computational fracture-mechanics approach for the analysis and design of structural adhesive joints under static loading is demonstrated by predicting the ultimate fracture load of cracked lap shear and single lap shear aluminum and steel joints bonded using a highly toughened epoxy adhesive. The predictions are then compared with measured values. The effects of spew fillet, adhesive thickness, and surface roughness on the quasi-static strength of the joints are also discussed. This fracture-mechanics approach is extended to characterize the fatigue threshold and crack growth behavior of a toughened epoxy adhesive system for design purposes. The effects of the mode ratio of loading, adhesive thickness, substrate modulus, spew fillet, and surface roughness on the fatigue threshold and crack growth rates are considered. A finite element model is developed to both explain the experimental results and to predict how a change in an adhesive system affects the fatigue performance of the bonded joint.  相似文献   

15.
Too often adhesive thickness, adherend thickness and other geometric factors are not explicitly considered in adhesive joint design. This study includes experimental and computational research exploring the means of enhancing the engineering design process for adhesive lap joints to include such effects. It clearly demon-strated that both the cleavage stresses and the shear stresses, near the bond termini, play important roles in lap 'shear' joint failure. Finite Element and Fracture Mechanics analyses were used to examine the energy release rate applied to growth of cracks in adhesive lap joints. Lap joints with similar geometries to those analyzed were designed, fabricated and tested. In a separate set of experiments the bond termini were constrained in the direction normal to the uniaxial loading. If the strength of lap shear joints is dominated by the adhesive shear strength, then constraining the lateral motion of the bond termini should have little or no effect on the overall shear strength of the adhesive joint. This work clearly demonstrates that this is not the case. If cleavage stresses are important in lap joints then constraining the bond termini, in a direction normal to the bond area, should have a commensurate effect on the overall strength of the lap joint. None of the ASTM standardized 'lap shear tests' provide any insight into this premise. This paper also presents analyses and experimental results for lap joints to which several methods of lateral constraint were applied near the bond termini. The analytical and numerical methods described and used for explaining and predicting such effects might be a useful adhesive joint design tool.  相似文献   

16.
The two types of joint discussed in this paper are a thick adherend symmetrical lap joint, and a symmetrical double lap joint. The effect of varying adherend and adhesive thicknesses on the stress distribution in the thin adhesive layer is discussed. These analyses were used in the design on a lap shear test to characterize certain aerospace adhesives used in bonded repair of structural components. An alternative analytical approach for the estimation of the load-carrying capacity of the double lap joint is also presented.  相似文献   

17.
The stress distributions in adhesive lap joints of dissimilar hollow shafts subjected to tensile loads have been analyzed by the elastoplastic finite element method, taking the nonlinear behaviors of the adhesive and the hollow shafts into consideration. A prediction method for the joint strength has been proposed based on the Mises equivalent stress distribution in the adhesive and the frictional resistance between the adhesive and the shaft after rupture of the adhesive. In the experiments, three different kinds of adhesive lap joints were made, i.e. the inner and outer hollow shafts were aluminum alloy/aluminum alloy, steel/steel, and steel/aluminum alloy combinations, and the tensile strength of each joint was measured. From the numerical calculations, in the case of the two hollow shafts made of the same material, the tensile strength increases with an increase of Young's modulus of the shaft and in the case of the two hollow shafts made of different materials, the tensile strength increases when the inner hollow shaft of larger Young's modulus is bonded to the outer one of smaller Young's modulus. Also, the effects of the overlap length and the inner diameter of the inner shaft on the tensile strength of the joint are discussed. By comparing the predicted values of the tensile strength with the experimental results, it was shown that the proposed prediction method could estimate the tensile strength of the adhesive lap joints of hollow shafts within an error of about 15%.  相似文献   

18.
刘刚  游敏  曹平  陈习坤 《粘接》2005,26(3):16-18
采用自制的装置研究了磁场对由环氧胶层连接的钢制单搭接接头剪切强度的影响,结果表明.在所采取的试验条件下.试样叠合后立即施加的磁场可显著影响接头的强度;垂直于胶层的磁场提高接头的剪切强度效果高于平行磁场,磁场处理的时间以4h左右为宜。  相似文献   

19.
Calculated torque transmission capability of adhesively bonded tubular lap joints using linear elastic material properties is usually much less than the experimentally-determined one because the majority of the load transfer of the adhesively bonded joints is accomplished by the nonlinear behavior of rubber-toughened epoxy adhesives.

Although the adhesively bonded tubular double lap joint has better torque transmission capability and reliability than the single lap joint, the nonlinear analytic or numerical analysis for the adhesively bonded tubular double lap joint has not been performed because of numerical complications.

An iterative solution that includes the nonlinear shear behavior of the adhesive was derived using the analytic solution. Since the iterative solution can be obtained very quickly due to the simplicity of the algorithm, it is an attractive method of designing adhesively bonded tubular single and double lap joints.  相似文献   

20.
The application of a fracture criterion, formulated in terms of material-induced stress/strain singularities at the terminus of an adhesive joint, to cohesive fracture in a single lap joint is presented. The criterion can be interpreted physically in terms of the elastic strain energy density. The strength of the singularities depends on the elastic properties of the adhesive and adherends and the geometry of the bond terminus, but is independent of loading and global geometry. A finite element method is used to predict the limit load of an adhesively bonded single lap joint from a known value of Qcrit, the critical singular intensity factor. This method may be applicable to general joint geometries.  相似文献   