1.
The pitting corrosion of SUSU304 steel can be suppressed by the application of a 19.5 kHz ultrasound (US) in 3.5% NaCl aqueous solution. At a constant vibrator-to-specimen distance of d = 76 mm equal to the wavelength, the suppression effect increased with the input power to vibrator and the largest effect was obtained at the power of I = 8. At constant input powers of I = 2 or 8, the suppression effect decreased with the increase in the vibrator-to-specimen distance, but the largest effect was obtained at d = 68 mm in each case of I = 2 and 8.  相似文献   

2.
The change of polarization curves and surface morphologies of SUS304 stainless steel was investigated in 3.5 mass% NaCl solution with or without the application of ultrasound (US). As the result, both the pitting corrosion and the crevice corrosion were largely suppressed by the application of US. The reason is attributed to the decrease in the concentration of hydrogen and chloride ions in pits or in the crevice by removing the corrosion product and stirring the liquid there.  相似文献   

3.
Measurements of pitting corrosion by potentiodynamic method and also by acoustic emission technique were carried out simultaneously. Cumulative distribution function of pitting corrosion (CDFP) occurrence was determined based on the results of potentiodynamic measurements. Independently cumulative distribution function of acoustic events (CDFAE) was found. The correlation analysis of both distributions was also performed. The occurrence of pitting corrosion was checked by metallographic observation. The measurements proved that observable acoustic activity is an effect of hydrogen evolution inside the pits. The random character of acoustic events during polarization, statistical analysis and existence of pits are good confirmation.  相似文献   

4.
Employing electrochemical frequency modulation for pitting corrosion   总被引:1,自引:0,他引:1  
By using the electrochemical frequency modulation (EFM) technique, the non-linear behavior of a corroding system is measured. This non-linear behavior is likely to be different for a system undergoing uniform or pitting corrosion. The implementation of the EFM technique to detect pitting corrosion has been investigated by observing the fluctuations in the so-called causality factors. These causality factors, resulting from an EFM test and in the ideal case having values of 2 and 3, respectively, are normally used for quality and data validation purposes. While investigating pitting corrosion, they show different behavior leading to the CPT (critical pitting temperature) detection.  相似文献   

5.
In the simulated heat affected zone of 2205 duplex stainless steels, effects of large welding heat inputs on the microstructure and corrosion behaviour were investigated. Reformed austenite content increased with the coarsening of grain boundary austenite (GBA) and the growth of intragranular austenite (IGA) and Widmanstatten austenite (WA), thus improving the low temperature toughness and affecting corrosion state. Reduction of chromium nitrides contributed to better resistance to pitting corrosion. Moreover, the pitting corrosion and intergranular corrosion were improved resulting from the formation of more GBA and WA. The specimen with a Δt8/5 of 100 s presents better comprehensive performance.  相似文献   

6.
During the drying stage of the cyclic corrosion test on ferritic stainless steels in the NaCl environment, the current abruptly increased and then decreased to nearly zero, indicating that pits are initiated as the salt concentration is increased, which are then repassivated when the surface is completely dry. During the wet stage, the current remained high, suggesting that pits mainly propagate during the wet stage. In contrast, in the cyclic corrosion test in the CaCl2 environment, the current was highest during the drying stage, indicating that the electrolyte is not completely dried and corrosion mainly propagates during the drying stage.  相似文献   

7.
Pitting corrosion of stainless steel has been investigated with high-resolution in situ X-ray microtomography. The growth of pits at the tip of stainless steel pins has been observed with 3D microtomography under different conditions of applied current and cell potential. The results demonstrate how pits evolve in stainless steel, forming a characteristic “lacy” cover of perforated metal. In addition, it is shown how the shape of pits becomes modified by MnS inclusions.  相似文献   

8.
The present investigation was undertaken to analyze the effects of isothermal ageing treatments, carried out between 700 and 900 °C for a variety of times up to two weeks and followed by water quenching, on the microstructure and on the localized corrosion resistance of a superduplex stainless steel, SAF 2507.The quantitative metallography coupled with X-ray diffraction techniques was adopted to follow the microstructural evolution, together with SEM microscopy.Electrochemical potentiodynamic tests, as cyclic polarization curves recorded in sodium chloride solutions, together with weight loss measurements were employed to evaluate the susceptibility of the aged specimens to pitting corrosion.The influence of the transformation of ferrite into secondary austenite and sigma phase and of other microstructural variations, as chromium nitrides precipitation, on the stability of the passive film is shown. The susceptibility of the aged alloy to pitting corrosion phenomena, is related to sigma phase precipitation in association to the secondary austenite formation, which lead to a noticeable Cr depletion at grain boundaries.  相似文献   

9.
The microstructure of grade X4CrNiMo16.5.1 stainless steel was studied at different scales. The chemical composition of the native passive film formed on the different phases was then determined at the microscale. The degree of homogeneity of the native passive film is discussed. Subsequently, the susceptibility to pitting corrosion of X4CrNiMo16.5.1 was quantified using the electrochemical microcell technique. The nature of precursor sites and the morphology of pits were investigated by combining scanning electron microscopy with Electron BackScatter Diffraction and potentiostatic pulse tests. The role of the microstructure and the cold-worked layer generated by polishing in pitting is discussed.  相似文献   

10.
Intergranular corrosion (IGC) of type 409L ferritic stainless steel (FSS) was investigated. A free-exposure corrosion and a double loop electrochemical potentiokinetic reactivation (DL-EPR) tests were conducted to examine IGC of the FSS. IGC occurred in the specimens aged at the temperature range of 400–600 °C that has the sensitization nose located around 600 °C. The critical Ir/Ia value was determined to be about 0.03 above which IGC occurred. Based on the analysis of the intergranular precipitates by an energy dispersive spectroscopy (EDS) and a transmission electron microscopy (TEM), IGC was induced by the Cr depletion zone formation due to Cr segregation around intergranular TiC.  相似文献   

11.
Mn and Mo were introduced in AISI 304 and 316 stainless steel composition to modify their pitting corrosion resistance in chloride-containing media. Corrosion behaviour was investigated using gravimetric tests in 6 wt.% FeCl3, as well as potentiodynamic and potentiostatic polarization measurements in 3.5 wt.% NaCl. Additionally, the mechanism of the corrosion attack developed on the material surface was analysed by scanning electron microscopy (SEM), X-ray mapping and energy dispersive X-ray (EDX) analysis. The beneficial effect of Mo additions was assigned to Mo6+ presence within the passive film, rendering it more stable against breakdown caused by attack of aggressive Cl ions, and to the formation of Mo insoluble compounds in the aggressive pit environment facilitating the pit repassivation. Conversely, Mn additions exerted an opposite effect, mainly due to the presence of MnS inclusions which acted as pitting initiators.  相似文献   

12.
R. Oltra 《Corrosion Science》2007,49(1):158-165
Local probe techniques have been largely applied to predict the spatial distribution of the electrochemical reactions and to quantify the corrosion rate. These local probe techniques are now being developed to capture the temporal information, in-situ and in real-time. Nevertheless only few works have been devoted to investigate with these local probes the role of stress on pitting sensitivity on passive materials. In this paper, a part of the most recent studies based on combination of local electrochemical measurements with finite element mapping of surface stress gradients are reported illustrating the role of inclusions under straining and the mechanical effect of surface preparation on pitting sensitivity of stainless steels.  相似文献   

13.
Electrochemical noise measurements on anodically polarised type 304 stainless steel surfaces in contact with buffer solutions of neutral pH were performed to study the effect of chloride ions in the nucleation of pitting corrosion. Passive layer stability and susceptibility to pitting corrosion after pickling and passivation at different environmental conditions were also investigated by means of electrochemical current noise measurements under cathodic and anodic polarisation. According to the obtained experimental results pits nucleate independently on the presence of chloride ions. It has been also shown that protectiveness of stainless steel surfaces after pickling strongly depends on the relative humidity of the environment in which the surface is subsequently passivated.  相似文献   

14.
An investigation has been undertaken to establish the effect of surface preparation method on the susceptibility of a 304 stainless steel to stress corrosion cracking under simulated atmospheric corrosion conditions. MgCl2 was deposited onto four-point bend specimens, which were then placed in a chamber with a relative humidity of 45% and temperature of 60 °C. These test conditions were designed to reflect external exposure of stainless steel components in industrial plant, including nuclear reactor components, situated in a coastal region, but with the severity of the exposure conditions enhanced to allow discrimination of the effect of surface preparation in a short timescale (up to 1500 h). Four surface preparation methods were evaluated: transverse grinding, longitudinal grinding, transverse dressing using an abrasive flap wheel, and transverse milling. For each case, surface topography, surface defect mapping, near-surface microhardness mapping, residual stress and electron back-scattered diffraction measurements were undertaken. Stress corrosion cracks were observed for the ground and milled specimens but not for the dressed specimens, with cracks apparently originating at corrosion pits. The density of cracks increased in the order: transverse ground, milled and longitudinal ground, with the cracks notably much smaller in length for the transverse ground condition. The propensity for cracking could be linked to the high residual stress and apparent nanocrystalline microstructure at the surface. There was a greater propensity for pitting to initiate at local defect sites on the surface (laps, deeper grooves). However, the tendency was not overwhelming, suggesting that other factors such as more general roughness or the distribution of MnS inclusions had an influence, perhaps reflecting the severity of the environment.  相似文献   

15.
Pitting corrosion was studied in welded joints of supermartensitic stainless steels. The electrochemical behavior of three different weldment zones (weld metal (WM), parent metal (PM) and heat affected zone (HAZ)) was characterized independently using an electrochemical minicell through potentiodynamic and potentiostatic techniques. The minicell design selected for this work has the additional advantage of showing promise for service application. Macro-electrochemical characterization was also used to provide a basis for comparison and check the effectiveness of minicell techniques in characterizing the corrosion resistance of welded super martensitic stainless steels. Minicell experiments exhibit a great capacity to discriminate between the different welding zones. The electrochemical response can be correlated with the microstructure of the different zones. Thermal cycles resulting from the welding procedure do not have an important effect on the amount of retained austenite or on the values of the pitting potential EP in the HAZ.  相似文献   

16.
The effect of microplasma arc welding (MPAW) on the electrochemical and corrosion behaviour of AISI 316L stainless steel tubes has been studied. Scanning electrochemical measurements were performed in sodium chloride to evaluate the difference in the electrochemical activity of base (non-welded) and welded samples. Oxygen reduction rates increase in AISI 316L due to the heat treatment effect induced by welding, indicating a higher electrochemical activity in the welded samples. Additionally, the use of MPA weldments in lithium bromide (LiBr) absorption machines was also analysed at typical operating temperatures and Reynolds numbers. The welding process increases corrosion rates, hinders passivation and increases the susceptibility to pitting attack in LiBr. However, zero-resistance ammeter and localization index measurements show that the galvanic pair generated between the base and welded alloys is weak, both electrodes being in their passive state. Temperature greatly affects the corrosion process.  相似文献   

17.
Acoustic emission (AE) during pitting corrosion of 304 stainless steel (304 SS) in H2SO4 solutions with different pH values and Cl concentrations was studied. Two types of AE signals are detected in all solutions. Each type of signals is characterized by AE parameters (rise time, counts number, duration and amplitude) and waveform carefully. It is believed that the hydrogen bubbles evolution inside the pits is the AE source.  相似文献   

18.
The microstructure and properties of UNS S31803 duplex stainless steel had been investigated following isothermally aging in a temperature range of 450–1000 °C for 10 min, which simulates a fairly long time relative to a weld thermal cycle. The results showed that specimens aged between 600 and 950 °C are subjected to precipitation of secondary phases, such as Cr2N, σ and χ. And the most significant reduction in pitting corrosion resistance and impact energy occurs at 850 °C. Moreover, at aging temperatures below 600 °C, austenite is the preferred site for pitting initiation, which changes to precipitates modified ferrite phase at higher temperatures above 600 °C.  相似文献   

19.
PM 304L and 316L stainless steel have been compacted at 400, 600 and 800 MPa and sintered in vacuum and in nitrogen-hydrogen atmosphere. Postsintered heat treatments (annealing solution and ageing at 375, 675 and 875 °C) have been applied. Pitting corrosion resistance has been studied using anodic polarization measurements and the ferric chloride test. Anodic polarization curves reveal that densities and atmospheres are relevant on anodic behaviour. Pitting resistance is higher for PM 316L and for higher densities and vacuum as sintered atmosphere. Ageing heat treatments at medium and high temperatures are detrimental to passivity although susceptibility to pitting corrosion barely changes. But heat treatments at 375 °C even show certain improvement in pitting corrosion resistance. The results were correlated to the presence of precipitates and mainly to the lamellar constituent which appears in some samples sintered in nitrogen-hydrogen atmosphere. The role of nitrogen on the samples sintered under nitrogen-hydrogen atmosphere and its relation to the microstructural features was described.  相似文献   

20.
Pitting corrosion is difficult to detect, predict and design against. Modeling and simulation can help to increase the knowledge on this phenomenon as well as to make predictions on the initiation and progression of it. A cellular automaton based model describing pitting corrosion is developed based on the main mechanisms behind this phenomenon. Further, a sensitivity analysis is performed in order to get a better insight in the model, after which the information gained from this analysis is employed to estimate the model parameters by means of experimental time series for a metal electrode in contact with different chloride concentrations.  相似文献   