1.
针对维西含硫磷铁矿,采取弱磁-强磁流程,可在75%-200目的细度下,实现铁的富集,铁品位达56%以上,回收率在80%以上,硫、磷含量分别降至0.5%和0.05%.  相似文献   

2.
湖北某低品位贫铁矿原矿含铁18.56%(S0.42%,P0.16%),通过采用阶磨阶选磁选工艺流程,在一段磨矿细度-74mm69.4%、二段磨矿细度-43um84.4%条件下,通过一粗一扫一精磁选工艺流程,最终获得铁精矿品位62.41%,回收率69.27%的选矿指标(S0.13%,P0.082%,有害杂质含量均未超标)。  相似文献   

3.
滇西某铁矿Fe品位为13.66%,且主要以嵌布粒度细的磁铁矿形式存在。针对原矿品位低及矿物嵌布粒度细等特点,采用"粗磨-弱磁粗选-粗精矿再磨-弱磁精选"的工艺流程。可获得铁精矿Fe品位64.47%,回收率56.87%的指标,为此类矿石的选别提供参考。  相似文献   

4.
昆明钢铁总公司某铁矿选矿流程试验研究   总被引:1,自引:0,他引:1  
对以磁铁矿和赤铁矿为主的混合型铁矿,采用弱磁和强磁相结合的磁选工艺进行试验研究,重点进行了SLon脉动高梯度磁选的不同工艺条件试验以及连续磨选和阶段磨选两种流程的比较试验,确定合理选别流程,并获得高品位铁精和高回收率指标。  相似文献   

5.
为了综合回收利用徐州铁矿集团有限公司镇北矿区磁铁矿和赤褐铁矿混合矿资源,采用磁选-强磁选-焙烧磁选工艺对其进行了试验研究,结果表明:可获得铁品位65.46%.回收率93.95%的综合铁精矿品位,精矿产率约提高7%左右,原矿铁品位下降10%左右。  相似文献   

6.
针对某铁矿尾矿中赤、褐铁矿含量较高,矿物嵌布颗粒微细,试验探索不同解决方案,最终试验结果表明磁选尾矿再磨-溜槽重选流程,可获得铁精矿产率40.89%,品位TFe 52.65%的选别指标,而且回收率达50.9%,选别成本低、无环境污染。  相似文献   

7.
某铁矿选矿试验研究   总被引:3,自引:0,他引:3  
针对某铁矿矿石主要为磁铁矿和赤铁矿,采用弱磁-强磁-反浮选的磁浮联合工艺流程,获得了弱磁精矿品位为66.07%,回收率为50.79%;强磁-反浮选精矿品位为61.37%,回收率为29.22%,总回收率为80.01%的试验指标。  相似文献   

8.
郭丽东  朱磊 《包钢科技》2018,44(3):27-30
某磁铁矿石矿物组成复杂,为了充分利用其中的矿物资源,进行了该铁矿物的工艺矿物学研究及选矿工艺试验研究。结果表明该矿石具有钙镁高、硅铝低的特点,属碱性矿石的范畴;矿石中可供选矿回收的主要组分是铁。通过阶段磨矿阶段选别—中磁选回收流程可获得产率34.01%、品位65.36%、回收率72.50%的铁精矿;通过阶段磨矿阶段选别—强磁选回收流程可获得产率38.93%、品位59.62%、回收率75.69%的铁精矿。  相似文献   

9.
陕西某矿区钒钛磁铁矿为低品位钒钛磁铁矿,钒钛磁铁矿共生有铁、钛、钒三种主要元素及其他有价金属,为减少资源浪费,更好地实现钒钛磁铁矿资源综合利用,提高选矿金属回收率。根据矿石性质特点,选用预先抛尾、两段磨选“阶磨阶选”的选矿工艺流程对该矿石进行选矿试验的相关研究,为指导生产、优化选矿工艺参数提供依据。  相似文献   

10.
河北某复杂低品位铅锌铁矿石,含铅锌铁品位分别为0.51%、2.92%和11.88%,通过浮选法回收铅锌+磁选回收铁的联合工艺流程,获得了理想的选矿工艺指标。采用捕收性和选择性好的乙硫氮作为铅捕收剂,实现了铅与锌的优先浮选分离,获得了含铅品位49.37%,回收率71.81%的铅精矿;采用丁基黄药作为锌捕收剂,获得了含锌品位56.21%,回收率79.19%的锌精矿;采用湿式弱磁选,获得了含铁66.78%,回收率60.21%的铁精矿。  相似文献   

11.
刘学胜  刘洁 《有色矿冶》2004,20(3):26-29
针对矿石中硅线石微细嵌布,铁矿物嵌布亦较细。且有近二分之一铁在非金属矿物晶格之中,除铁难的特点,通过试验研究对比采用一段磨矿磁选除铁后磁尾浮选富集硅线石.浮选精矿再磨后酸浸再除铁的工艺方法,获得了理想的除铁效果,使硅线石精矿质量达到较高品质。  相似文献   

12.
甘肃某公司所属的锑矿主要可回收金属矿物为辉锑矿,辉锑矿粒度范围较宽,大都与脉石矿物较好解离,少量较难解离。针对矿石性质,进行了选矿试验研究,研究结果表明采用原矿磨矿→一次粗选→两次精选→一次扫选的浮选工艺流程可有效的回收该矿石中的辉锑矿,获得的锑精矿锑品位为56.32%、锑回收率为94.37%。  相似文献   

13.
陈磊  马亮 《铜业工程》2021,(4):47-51
The copper grade the low-grade copper-molybdenum ore in Shaanxi is 0.32% and the molybdenum grade is 0.048%.The copper and molybdenum minerals mainly exist in the form of sulfide ore. The properties are complex that there are many kinds of minerals in the ore, which are closely distributed and fine dissemination size. According to the properties of the ore, the technological process of bulk flotation and separation of copper and molybdenum was adopted in the experiment. With lime as regulator and reagent L03 as collector, the mixed concentrate of copper and molybdenum was obtained by the bulk flotation which flow-sheet is one roughing, three refining and two scavenging process. Then regrinding the mixed concentrate, use sodium sulfide as inhibitor of copper minerals, sodium silicate as slurry dispersant and inhibitor of silicate gangue minerals , kerosene as collector, can separate copper and molybdenum with the flow-sheet which one roughing, five refining and three scavenging. The copper concentrate with copper grade of 18.82% and copper recovery rate of 85.35% and molybdenum concentrate with molybdenum grade of 47.14% and molybdenum recovery rate of 79.24% were obtained by the final closed-circuit flotation test process, the indicator is nearly ideal.  相似文献   

14.
某钼、钨多金属矿石的选矿试验研究   总被引:1,自引:0,他引:1  
某钼、钨多金属矿石,有用矿物主要有辉钼矿、黄铁矿和黑钨矿。根据其矿石性质,对钼浮选过程中脉石矿物抑制机理进行了分析,提出"依次浮选-强磁选"的工艺流程,获得了钼精矿品位45.33%、回收率80.49%,硫精矿品位45.83%、回收率92.74%,钨精矿品位58.67%、回收率74.63%的良好指标。  相似文献   

15.
介绍了国内外尤其是国内铁矿选矿(包括磁铁矿和赤铁矿等)主要磁选设备类型及应用现状,归纳、总结了磁选设备的发展趋势,并就提高我国磁选装备水平的重要意义以及如何推动我国磁选设备的发展的措施阐述了作者的观点。  相似文献   

16.
对甘肃某白钨矿的矿石性质进行了分析研究,根据物质成分的研究结果和各种矿物的特点,首先进行了预选试验,确定了小型选矿流程试验,进一步进行了扩大连续选矿流程试验研究,最终试验结果为:白钨精矿产率为0.94%,品位WO365.07%,回收率78.18%,细泥白钨精矿产率为0.10%,品位WO332.29%,回收率4.19%。试验结果可以作为建厂设计的技术依据。  相似文献   

17.
根据湖南某低品位细粒磁铁矿的矿石性质,在原矿全铁含量为16.68%、磁性铁含量为8.28%的条件下,采用阶段磨矿、阶段磁选工艺,获得不同品位的铁精矿产品。  相似文献   

18.
对两家单位选矿试验报告在粗选pH值、粗选捕收剂的种类以及钼精矿再磨等方面进行了详细的分析,为确定更优的工艺流程、达到较高的选矿指标提供依据。  相似文献   