1.
Studies on impact and tensile properties of binary blend of PP and ABS and ternary blend of PP, ABS, and LDPE are presented. Variation of impact strength and the fracture surface morphology with blend composition is examined and interpreted. Tensile behavior in the yield region is studied and the trends of variation of work of yield and impact strength are compared to ascertain the predominent mechanism of impact toughening in these binary and ternary blends. An analysis of yield–stress data in terms of theoretical models is presented to reveal the differences in these binary and ternary blends, attributable to the role of LDPE component in the ternary blend.  相似文献   

2.
Melt rheological properties of the ternary blend of isotactic polypropylene (PP), styreneethylene–butylene–styrene terpolymer (SEBS), and polycarbonate (PC), PP/SEBS/PC, are studied in a wide range of composition, such that PP is the matrix and SEBS and PC are the minor components, with the proportion of one varying from 0 to 30% at various fixed compositions of the other. The respective binary blends, PP/SEBS and PP/PC, studied as the reference systems for interpretation of results on the ternary blends yielded interesting new information about the morphology development and its correlation with melt rheological properties of these binary blends. The studies include the measurement of melt rheological properties on a capillary rheometer in the shear rate range 101–104 s?1 at a fixed temperature of 240°C. The data presented as conventional flow curves are analyzed for the effect of blend composition and shear rate on pseudoplasticity, melt viscosity, and melt elasticity, and role of each individual component is identified. Morphology of dispersed phases of these blends is studied through scanning electron microscopy of the cryogenically fractured and suitably etched surfaces. Variations of morphology with blend composition and shear rate showed interesting correlation with melt rheological properties, which are discussed in detail. An important finding of the morphological studies is that in the PP/SEBS/PC ternary blend the SEBS phase forms two types of morphologies depending on the blend composition and shear rate: (i) simple droplets and (ii) boundary layer at the surface of the PC droplets. © 1993 John Wiley & Sons, Inc.  相似文献   

3.
Studies are reported on melt rheological behavior of some binary and ternary blends of polypropylene (PP) with one or two of the following polymers: styrene–b-ethylene butylene–b-styrene triblock copolymer (SEBS), polystyrene (PS), and high-density polyethylene (HDPE). Blend composition of the binary blends PP/X or ternary blends PP/X/Y were so chosen that the former represent addition of 10 wt % X to PP while the latter represent 10 wt % addition of X or Y to the PP/Y or PP/X blend of constant composition 90:10 by weight, X/Y being SEBS, PS, or HDPE. Measurements were made on a capillary rheometer using both temperature elevation and constant temperature methods to study the behaviors prior to flow and in the flow region. Flow behavior, measured at a constant temperature (200°C) and varying shear stress (from 1.0 to 5.0 × 106 dyn/cm2) to evaluate melt viscosity and melt elasticity parameters, is discussed for its dependence on the nature of the blend. Extrudate distortion, studied as a function of shear stress to evaluate the critical shear stress for the onset of extrudate distortion, showed differences in the tendency for extrudate distortion or melt fracture of these different blends. Also discussed is the effect of melt viscosity and melt elasticity on extrudate distortion behavior at the critical condition, which showed a unique critical value of the ratio (melt elasticity parameter)1/2 (melt viscosity) for all these blends. Blend morphologies before and after the flow through the capillary are investigated through scanning electron microscopy, and their correlations with rheological parameters of the melt are discussed.  相似文献   

4.
Melt rheological properties of the blend of isotactic polypropylene (PP) and ethylene propylene diene rubber (EPDM) at varying ratios and of the glass fiber (GF) filled PP and PP/EPDM blend by varying both GF loading and blending ratio of the polyblend matrix are studied. Rheological measurements at 220°C in shear rate range 101?104s?1 were made on a capillary rheometer. Scanning electron micrographs of the extrudates are presented to show the morphology and the alignment of the glass fibers with respect to the flow direction. Variations of pseudoplasticity index, melt viscosity, and melt elasticity with EPDM content in PP/EPDM blend, and with varying GF content at any given composition of the matrix in PP/EPDM/GF ternary system, in the studied range are presented and discussed. Resultes on melt viscosity and melt elasticity show (i) reduced effect of GF at high shear rates on these properties and (ii) upward deviation of melt viscosity versus shear rate curve at low shear rates. A change in flow behavior in presence of GF is observed around a critical shear rate 2 × 103 s?1 and is attributed to the difference of interaction of GF and the dispersed rubber droplets at high and low shear rates. Elastic recovery showed nonequilibrium behavior at low shear rates.  相似文献   

5.
Studies on melt rheological properties of blends of low density polythylene (LDPE) with selected grades of linear low density polyethylene (LLDPE), which differ widely in their melt flow indices, are reported. The data obtained in a capillary rheometer are presented to describe the effects of blend composition and shear rate on flow behavior index, melt viscosity, and melt elasticity. In general, blending of LLDPE I that has a low melt flow index (2 g/10 min) with LDPE results in a decrease of its melt viscosity, processing temperature, and the tendency of extrudate distortion, depending on blending ratio. A blending ratio around 20–30% LLDPE I seems optimum from the point of view of desirable improvement in processability behavior. On the other hand, blending of LLDPE II that has a high melt flow index (10g/10 min) with LDPE offers a distinct advantage in increasing the pseudoplasticity of LDPE/LLDPE II blends. © 1996 John Wiley & Sons, Inc.  相似文献   

6.
Polypropylene (PP) and acrylonitrile–butadiene–styrene blends of different composition were prepared using a single‐screw extruder. The binary blend of PP/ABS was observed to be incompatible and shows poor mechanical properties. PP‐g‐2‐hydroxyethyl methacrylate (2‐HEMA) was used as a compatibilizer for the PP/ABS blends. The ternary compatibilized blends of PP/ABS/PP‐g‐2‐HEMA showed improvement in the mechanical properties. Electron micrographs of these blends showed a homogeneous and finer distribution of the dispersed phase. The mechanical performance increased particularly in the PP‐rich blend. The 2.5‐phr (part per hundred of resin) compatibilizer was observed to bring improvement to the properties. The suitability of various existing theoretical models for the predication of the tensile moduli of these blends was examined. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 88: 72–78, 2003  相似文献   

7.
This paper describes a study of melt-rheological properties of the binary blend of isotactic polypropylene (PP) and ethylene–vinyl acetate copolymer (EVA) at varying blending ratios (from 0 to 40 wt % EVA content) and using three samples of EVA containing different vinyl acetate contents (VA %), viz. 9, 12, and 19%. Measurements made on a capillary rheometer at three different temperatures (210, 220, and 230°C) in a shear stress range of 104–106 Pa (shear rate 101–104 s?1) are presented and discussed for the effects of blend composition and shear stress on the flow curves, melt viscosity and melt elasticity. Morphology of the blend studied through scanning electron microscopy revealed distinct differences in size and number density of dispersed EVA droplets, which are discussed in terms of the variation of average size and number density of the dispersed EVA droplets as a function of blend composition and shear stress. Melt-rheological properties and morphology of dispersion are correlated and found quite consistent.  相似文献   

8.
The recycling possibilities of poly(butylene terephthalate)/polycarbonate/acrylonitrile–butadiene–styrene (PBT/PC/ABS) ternary blend with and without glass‐fiber content were investigated using repeated injection molding process. In this study, PBT/PC/ABS ternary blends were reprocessed at five times and the results were presented after each recycling process. The recycling possibility of PBT/PC/ABS ternary blend was evaluated by measuring the mechanical, chemical, thermal, and rheological properties. Mechanical properties were determined by the tensile strength, yield strength, strain at break, elastic modulus, impact strength, flexural strength, and flexural modulus. Chemical and thermal properties were evaluated by Fourier transform infrared spectroscopy, differential scanning calorimetry, thermal gravimetric analysis, and scanning electron microscopy. Rheological properties of the ternary blends were studied by melt flow index measurement. From the results, it was found that mechanical properties of recycled composites were better than virgin PBT/PC/ABS ternary blends. POLYM. COMPOS., 35:2074–2084, 2014. © 2014 Society of Plastics Engineers  相似文献   

9.
The rheological properties and crystalline structure of the polyolefin ternary blends of EPDM/polypropylene/high density polyethylene were studied. Blends were prepared in a laboratory internal mixer by two different methods. In blend–cure process, blending and curing were performed simultaneously and EPDM was cured by dicumyl peroxide (DCP) in the presence of PP/HDPE under shear. The cure–blend was to cure EPDM alone first under shear (dynamic curing) and then mix the cured EPDM with PP and HDPE. The effect of DCP concentration, intensity of the shear mixing, and the rubber/plastic composition were studied using capillary rheometer and X-ray diffractometer. The PP-rich ternary blends showed the effect of the mechanooxidative degradation of PP by shear and peroxide. The melt viscosity increased with increasing DCP concentration in blends of EPDM-rich compositions. X-ray diffraction studies revealed that the inclusion of 25 wt % of linear EPDM in the PP/HDPE mixture for the PP-rich ternary blends changed the crystal structure of polypropylene component in the ternary blends. However, the dynamic curing did not alter the crystal structure of PP or HDPE in the blends.  相似文献   

10.
The melt rheological properties of binary uncompatibilized polypropylene–polyamide6 (PP–PA6) blends and ternary blends compatibilized with maleic anhydride‐grafted PP (PP–PP‐g‐MAH–PA6) were studied using a capillary rheometer. The experimental shear viscosities of blends were compared with those calculated from Utracki's relation. The deviation value δ between these two series of data was obtained. In binary PP–PA6 blends, when the compatibility between PP and PA6 was poor, the deformation recovery of dispersed PA6 particles played the dominant role during the capillary flow, the experimental values were smaller than those calculated, and δ was negative. The higher the dispersed phase content, the more deformed the droplets were and the lower the apparent shear viscosity. Also, the absolute value of δ increased with the dispersed phase composition. In ternary PP–PP‐g‐MAH–PA6 systems, when the compatibility between PP and PA6 was enhanced by PP‐g‐MAH, the elongation and break‐up of the dispersed particles played the dominant role, and the experimental values were higher than calculated. It was observed that the higher the dispersion of the PA6 phase, the higher the δ values of the ternary blends and the larger the positive deviation. Unlike uncompatibilized blends, under high shear stress with higher dispersed phase content, the PP‐g‐PA6 copolymer in compatibilized blends was pulled out from the interface and formed independent micelles in the matrix, which resulted in reduced total apparent shear viscosity. The δ value decreased with increasing shear stress. Copyright © 2006 Society of Chemical Industry  相似文献   

11.
A study of melt rheology of the blend of styrene-acrylonitrile (SAN) and polypropylene (PP) in composition range 0–50 wt % SAN content is presented. Measurements are made on a capillary rheometer at temperatures of 210, 230, and 250°C. The data are presented as flow curves and variations of melt viscosity and melt elasticity as functions of shear rate and blend composition. Scanning electron micrographs are presented to illustrate the dispersion and other characteristics of the SAN droplets. Results of melt rheology are interpreted in terms of the role of SAN droplets in the blend.  相似文献   

12.
Studies are reported on tensile and impact properties of several binary and ternary blends of polypropylene (PP), styrene-b-ethylene-co-butylene-b-styrene triblock copolymer (SEBS), high-density polyethylene (HDPE), and polystyrene (PS). The blend compositions of the binary blends PP/X were 10 wt % X and 90 wt % PP, while those of the ternary blends PP/X/Y were 10 wt % of X and 90 wt % of PP/Y, or 10 wt % Y and 90 wt % PP/X (PP/Y and PP/X were of identical composition 90:10); X, Y being SEBS, HDPE, or PS. The results are interpreted for the effect of each individual component by comparing the binary blends with the reference system PP, and the ternary blends with the respective binary blends as the reference systems. The ternary blend PP/SEBS/HDPE showed properties distinctly superior to those of PP/SEBS/PS or the binary blends PP/SEBS and PP/HDPE. Differences in the tensile yield behavior of the different samples and their correlation with impact strength suggested shear yielding as the possible mechanism of enhancement of impact strength. Scanning electron microscopic study of the impact fractured surfaces also supports the shear yielding mechanism of impact toughening of these blends.  相似文献   

13.
The extrudate swell behavior and extrudate texture of various thermoplastic melts, namely, polystyrene (PS), low‐density polyethylene (LDPE), acrylonitrile‐butadiene styrene (ABS) copolymer, poly(vinyl chloride) (PVC), and their blends, were examined weith a magnetic die system in a constant‐shear‐rate capillary rheometer at a shear rate range 5–28 s?1 and a temperature range 170–230 °C. The extrudate swell results obtained from the magnetic die were then compared with those produced by a nonmagnetic die. The results showed that the extrudate swell increased with shear rate, but decreased with temperature. In a pure polymer system, up to 25% increase in the extrudate swell was observed with the application of the magnetic field to the PS melt, and the effect decreased in the order ABS > LDPE > PVC. The extrudate swell changes were associated with the changes in rheological properties of the melts. The extrudate textures of the ABS and PVC melts were improved by the magnetic field. In PS/LDPE or PS/ABS blend, it was found that the magnetic die resulted in higher values of the extrudate swell than the nonmagnetic die for all blends, the magnetic effect being less as the LDPE or ABS content was increased. For PS/LDPE system, the extrudate swell of the PS melt did not change much with addition of 20% LDPE, but slightly decreased at the LDPE loading of 40%. At higher LDPE loadings, the extrudate swell increased towards the value of the pure LDPE melt. For PS/ABS system, the extrudate swell ratio progressively decreased with increasing ABS content. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 509–517, 2002  相似文献   

14.
15.
Study of melt rheological properties of the blends of polypropylene (PP) with styrene–ethylene butylene–styrene block copolymer (SEBS), at blending ratios 5–20% SEBS, is reported. Results illustrate the effects of (i) blend composition and (ii) shear rate or shear stress on melt viscosity and melt elasticity and the extrudate distortion. In general, blending of PP with SEBS results in a decrease of its melt viscosity, processing temperatures, and the tendency of extrudate distortion. However, the properties depend on blending ratio. A blending ratio around 5–10% SEBS seems optimum from the point of view of desirable improvement in processability behavior.  相似文献   

16.
The ternary powder blends based on low-density polyethylene (LDPE) and two polymers of natural origin poly(lactic acid) (PLA) and starch are obtained in a rotor disperser under conditions of shear deformations. The dependence of the final powder dispersity on the composition is explored. A comparative analysis of the mechanical properties of the ternary blends with those of the LDPE–PLA and PLA–starch binary blends previously obtained has revealed that the presence of two rigid polymers PLA and starch leads to an increase in the elastic modulus and a decrease in the tensile strength and elongation at break. In the study of the blend biodegradability, it is found that the presence of two polymers of natural origin in the system with a total mass fraction of 60% promotes intensive biodegradation.  相似文献   

17.
采用毛细管流变仪和旋转流变仪研究了聚丙烯(PP)纤维专用料/丙烯-乙烯共聚物(PEC)共混体系的流变行为,探究了剪切速率、温度、共混物组成对熔体流变行为的影响。结果表明,随着剪切速率的增加,PP、PP/PEC和PEC均表现出"剪切变稀"行为;随着温度的升高,聚合物的表观黏度逐渐降低,特别是在低剪切速率下的这种现象更明显;随着PEC含量的增加,体系的非牛顿指数增加,黏流活化能降低,黏度对温度的敏感性降低,熔体剪切模量增加,熔体弹性增加。  相似文献   

18.
EPDM/聚烯烃共混型热塑性弹性体的研究   总被引:1,自引:0,他引:1       下载免费PDF全文
龚蓬  张祥福  张隐西 《橡胶工业》1996,43(8):451-457
制备EPDM/聚烯烃简单共混型热塑性弹性体。研究了聚合物种类、橡塑比、二元和三元共混对共混物力学性能的影响。结果表明,部分结晶性EPDM共混物的力学性能比无定形EPDM共混物好,部分结晶性EPDM与LDPE(低密度聚乙烯)共混物的拉伸强度大于两者的加和值,而其它二元共混物的拉伸强度均低于两共混单元的加和值;用LDPE部分替代PP,或用氯磺化聚乙烯(CSM)部分替代结晶性EPDM进行三元共混,能改善部分结晶性EPDM/PP共混物的某些性能。  相似文献   

19.
Branched polyethylenes, low‐density polyethylenes (LDPE1 and LDPE2) or long‐chain‐branched very low density polyethylenes (VLDPE2), were blended with very low density polyethylenes containing short branches (VLDPE1 and VLDPE3). The rheological and thermal measurements of the pure copolymers and their blends (VLDPE1–LDPE1, VLDPE1–LDPE2, VLDPE1–VLDPE2, and VLDPE2–VLDPE3) were taken by controlled stress rheometry and differential scanning calorimetry, respectively. The shear‐thinning effect became stronger with increasing long‐chain‐branched polymer compositions when it was correlated with the flow behavior index, and the extent of shear thinning was different for each blend set. Stronger shear thinning and a linear composition dependence of the zero‐shear viscosity were observed for the VLDPE1–LDPE1 and VLDPE1–LDPE2 blends. These blends followed the log additivity rule, and this indicated that they were miscible in the melt at all compositions. In contrast, a deviation from the log additivity rule was observed for the VLDPE1–VLDPE2 blend compositions with 50% or less VLDPE2 and for the VLDPE3–VLDPE2 blends with 50% or more VLDPE2. The thermal properties of the blends were consistent with the rheological properties. VLDPE1–LDPE1 and VLDPE1–LDPE2 showed that these blends were characteristic of a single‐component system at all compositions, whereas the phase separation (immiscibility) was detected only for VLDPE1–VLDPE2 blends with 50% or less VLDPE2 and for VLDPE3–VLDPE2 blends with 50% or more VLDPE2. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 95: 1549–1557, 2005  相似文献   

20.
Nanofibrous morphology has been observed in ternary blends of low density polyethylene (LDPE), linear low density polyethylene (LLDPE), and isotactic polypropylene (PP) when these were melt‐extruded via slit die followed by hot stretching. The morphology was dependent on the concentration of the component polymers in ternary blend LDPE/LLDPE/PP. The films were characterized by wide angle X‐ray diffraction (XRD), scanning electron microscopy (SEM), and testing of mechanical properties. The XRD patterns reveal that the β phase of PP is obtained in the as‐stretched nanofibrillar composites, whose concentration decreases with the increase of LLDPE concentration. The presence of PP nanofibrils shows significant nucleation ability for crystallization of LDPE/LLDPE blend. The SEM observations of etched samples show an isotropic blend of LDPE and LLDPE reinforced with more or less randomly distributed and well‐defined nanofibrils of PP, which were generated in situ. The tensile modulus and strength of LDPE/LLDPE/PP blends were significantly enhanced in the machine direction than in the transverse direction with increasing LLDPE concentration. The ultimate elongation increased with increasing LLDPE concentration, and there was a critical LLDPE concentration above which it increased considerably. There was a dramatic increase in the falling dart impact strength for films obtained by blow extrusion of these blends. These impressive mechanical properties of extruded samples can be explained on the basis of the formation of PP nanofibrils with high aspect ratio (at least 10), which imparted reinforcement to the LDPE/LLDPE blend. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008  相似文献   