朱振峰  蔺华妮 《陶瓷》2011,(5):18-20
以二水合乙酸锌提供锌源,氨水调节pH值,聚乙二醇-2000为改性剂,采用沉淀法在一定的工艺条件下得到了花状ZnO粉体。并以SEM、TEM及XRD等测试手段对产物的形貌及结构方面进行了表征。利用X射线衍射仪进行结晶结构分析,表明花状ZnO为六方纤锌矿结构;利用场发射电子扫描电镜进行样品形貌分析,表明花状结构ZnO是由纺锤状棒状结构组成,棒的长径比为2.10;利用场发射透射电镜进行结晶结构分析,表明花状ZnO是单晶与多晶的混合体,室温光致发光谱表明花状ZnO在380nm左右存在紫外发射峰。  相似文献   

2.
以[Bmim]Cl、[Bmim]BF_4、[C_2OH]mimCl和[C_2OHmim]BF_4四种室温离子液体为模板,采用微波加热前驱体Zn(OH)_4~(2-)溶液的方法制备了多形貌纳米/微米ZnO.采用XRD、SEM、TEM对实验样品进行了结构和形貌表征,通过SEM照片分析了不同合成条件对产物形貌的影响.结果表明:合成产物为结晶良好,具有六方纤锌矿结构的ZnO;不同离子液体中合成了鳞状、片状、棒状、锥状纳米ZnO晶体单元,大量ZnO晶体聚集成微米球、花簇;随着前驱体原料配比增大,[0001]方向择优生长明显;随温度从80 ℃增加到95 ℃,ZnO纳米锥生长趋势总体趋于明显, 长径比增大,同时产物形貌的规整性也明显变好;探讨了多形貌纳米/微米ZnO的生长机理;采用室温下光致发光(PL)光谱对多形貌纳米ZnO的光学性能研究表明,多形貌纳米ZnO具有较强的紫外发射和相对较弱的蓝绿发射,离子液体[Bmim]Cl中合成的ZnO纳米锥在387 nm处紫外发射峰强度最大,离子液体[C_2OHmim]Cl 中合成的ZnO纳米片在497 nm处有较强的绿光发射峰.  相似文献   

3.
以氢氧化钠和氢氧化锂作为助熔剂,采用常压混合碱液法成功生长了各种形貌的ZnO晶体。以Bravais-Friedel-Donnay-Harker法则为指导,获得了ZnO晶体的几种理论结构晶形;在考虑晶体内部结构和生长实验中外部生长条件下,得到了晶体的实验晶形。采用光学显微镜、扫描电子显微镜和原子力显微镜对六方片状晶体的表面形貌进行了研究。结果表明:晶体的理论结构晶形和实验晶形吻合良好;晶体具有二维螺旋生长的机制。此外,晶体在325 nm光激发的室温光致发光光谱显示,在380 nm处存在1个强的紫外发射峰和位于652 nm处的弱且窄的红光发射峰,说明生长的六方片状ZnO晶体结晶质量优良。  相似文献   

4.
王文忠  赵建华 《陶瓷》2011,(9):18-20
以二水合乙酸锌提供锌源,氨水调节pH值,聚乙二醇-2000为改性剂,采用沉淀法在一定的工艺条件下得到了花状ZnO粉体。并以SEM、TEM及XRD等测试手段对产物的形貌及结构方面进行了表征。利用X射线衍射仪进行结晶结构分析,表明花状ZnO为六方纤锌矿结构;利用场发射电子扫描电镜进行样品形貌分析,表明花状结构ZnO是由纺锤状棒状结构组成,棒的长径比为2.10;利用场发射透射电镜进行结晶结构分析,表明花状ZnO是单晶与多晶的混合体,室温光致发光谱表明花状ZnO在380nm左右存在紫外发射峰。  相似文献   

5.
以二水合乙酸锌提供锌源,氨水调节pH值,聚乙二醇-2000为改性剂,采用沉淀法在一定的工艺条件下得到了花状ZnO粉体。并以SEM、TEM及XRD等测试手段对产物的形貌及结构方面进行了表征。利用X射线衍射仪进行结晶结构分析,表明花状ZnO为六方纤锌矿结构;利用场发射电子扫描电镜进行样品形貌分析,表明花状结构ZnO是由纺锤状棒状结构组成,棒的长径比为2.10;利用场发射透射电镜进行结晶结构分析,表明花状ZnO是单晶与多晶的混合体,室温光致发光谱表明花状ZnO在380nm左右存在紫外发射峰。  相似文献   

6.
丁红霞 《广东化工》2014,(9):205-206,212
采用紫外可见光谱作为检测2,4-二硝基苯酚的方法,pH6或pH3时,2,4-二硝基苯酚的特征吸收峰分别为370 nm及260 nm处;在pH 3~6之间,两特征峰共存。文章提出一种简单的归一拟合方法,首先推导出260 nm处的吸收值与浓度的线性关系,再将pH不同的2,4-二硝基苯酚在370 nm处的吸收值校正到260 nm处。开发了一种简单快捷无需调节pH测定2,4-二硝基苯酚浓度的方法。  相似文献   

7.
高定向ZnO纳米棒阵列膜的制备及其光学性能   总被引:3,自引:1,他引:3  
采用阴极恒电位沉积方法,在Zn(NO3)2溶液中,用六亚甲基四胺作为形貌控制试剂,直接在氧化铟锡玻璃衬底上制备出透明致密的ZnO纳米棒阵列膜。通过X射线衍射、扫描电镜和能量色散谱表征了薄膜的形貌和结构,测量了ZnO纳米棒阵列膜的光学透射谱和光致发光谱。结果表明:所制备的具有c轴高度择优取向的ZnO纳米棒为高纯单晶纤锌矿结构,粒径约为200nm,膜的结晶度和表面平整度明显提高。ZnO薄膜在可见光区具有高透射率(80%)和陡峭的吸收边缘,室温光致发光谱显示,在380nm处存在一个尖锐的强紫外发射峰和在510nm处存在一宽带弱绿光发射峰。  相似文献   

8.
采用水相化学沉淀法合成ZnS∶Mn2+纳米量子点时,反应条件的变化会直接影响量子点的荧光特性。文中通过调节三聚磷酸钠(STPP)的加入量,改变反应介质酸碱度,成功获得了不同荧光颜色的ZnS∶Mn2+纳米量子点。研究结果表明:反应介质酸碱度的变化只改变了ZnS∶Mn2+量子点的发射光谱,而没有改变其激发光谱。分别加入0.17,0.16 g/mL的STPP,pH值控制在7.5,8.0时,合成的量子点发射峰出现在425 nm和475 nm,呈蓝色荧光;当加入0.15 g/mL的STPP,pH值控制在8.5时,量子点发射峰在485 nm,有微弱橙红色荧光;加入0.10,0.02 g/mL的STPP,pH值控制在9.0或9.5时,在580 nm处有单一发射峰,呈现较强的橙红色荧光。其中pH值为9.5时,荧光强度最高,所合成的ZnS∶Mn2+量子点直径为3.5 nm,且均匀分散。荧光光谱分析证明,随着介质pH值的增大,ZnS∶Mn2+量子点的发射峰逐渐红移,而pH值达到10.0时,发射峰又回到470 nm,橙红色荧光消失,呈蓝色。  相似文献   

9.
陈爱珍 《农药》1992,31(4):30-30
一、实验部分1.定量波长及溶剂的确定选用一系列溶剂,在波长375纳米的紫外区,测定氟乐灵的溶剂吸收值,以正己烷、丙酮为好。氟乐灵以正己烷为溶剂,在375纳米处有最大特征吸收峰;以丙酮为溶剂在390纳米处有最大特征吸收峰。2.展开剂的选择为了更好地将氟乐灵和杂质分离,对不同  相似文献   

10.
固相反应法制备高浓度掺杂Nd:YAG激光透明陶瓷及其性能   总被引:3,自引:0,他引:3  
用固相反应和真空烧结技术,成功制备了高质量的4.0%(摩尔分数)Nd:YAG透明陶瓷,并对样品的显微结构、光学透过率、光谱性能和激光性能进行了表征.结果表明:样品的平均晶粒尺寸约为10 μm;样品(厚度为2.8 mm)在1 064 nm处的透过率高达79.5%;主吸收峰位于807 nm处,峰值吸收系数为13.9 cm-1,激光波长1 064 nm处的吸收系数为0.2 cm-1;主荧光发射峰位于1 064 nm处,荧光寿命为102 μs.用激光二极管(808 nm)端面泵浦Nd:YAG陶瓷样品(泵浦源最大输出功率为1 000 mW),获得了波长为1 064 nm的连续激光输出,输出功率17 mW(最大泵浦吸收功率为998 mW),斜率效率为6.1%,激光阈值约733 mW.  相似文献   

11.
Solid solutions of diphosphates of zinc and copper and of zinc and cobalt were synthesized from mixtures of pure diphosphates at temperatures up to 1000°C. Their X-ray diffractometry patterns varied continuously from one end member to the other. Solid solutions of orthophosphates of composition Zn3−xCox(PO4)2, with x = 0.4–1.6, were formed at temperatures up to 950°C; all exhibited the structure of γ-Zn3(PO4)2. Solid solutions of orthophosphates of composition Zn3−xCux(PO4)2 exhibited more-complex behavior. At 1000°C and copper contents of 20–80 mol%, a phase that is related to Cu3(PO4)2, termed here the "ε-phase," predominated. At 850°–950°C and in the region from 20 mol% to ∼33 mol% of copper, the solid solutions (the "η-phase") adopted the structure of graftonite. At 800°–900°C and 10–15 mol% of copper, the solid solutions exhibited a new structure (the "δ-phase"), which we found to be related to the mineral sarcopside. At temperatures 950°C, the solutions that contained 5–15 mol% of copper (the "β-phase") had the structure of β-Zn3(PO4)2, whereas at 800°–850°C, solutions with 5 mol% of copper (the "-phase") exhibited the structure of γ-Zn3(PO4)2. Attempts to synthesize Cu+ZnPO4 and Cu+Cu2+Zn3(PO4)3 were unsuccessful.  相似文献   

12.
油气储运系统已经与保障国家经济的发展息息相关,介绍了油气储运系统中油气回收问题及腐蚀与防护问题,并提出了相应的解决措施。  相似文献   

13.
Gemini型表面活性剂的结构和性质与传统的表面活性剂有很大的不同,例如Gemini型表面活性剂可以视为两个普通表面活性剂在亲水基或者靠近亲水基处由连接基团通过化学键连接而成;Gemini表面活性剂的C20值和cmc值都比传统表面活性剂的值要低很多。着重介绍了Gemini型表面活性剂的特性,结构与表面活性的关系以及应用。  相似文献   

14.
为了提高油田的生产效率,设计最佳的油气集输处理的工艺流程,更好地完成油气水分离处理的任务。对油气集输工艺技术进行优化,发挥高效油气水分离处理设备的优势,提高油气水处理的质量,保证油气集输工艺顺利实施,获得最佳的油田产量外输。  相似文献   

15.
建设创新型国家是我们中华民族的历史责任。“自主创新、重点突破、支撑发展、引领未来”的16字方针应当成为我们未来创新活动的指南。建设创新型国家把自主创新放在首位,并提出了引领未来的高标准要求。钢铁科技创新必须突出重点,抓住创新成果产业化这个关键,支撑起行业和国民经济的发展。  相似文献   

16.
相比已经完善丰富的开采和勘探技术,油气的运输以及储存却仍然存在不足之处。我国对能源安全提出更加严格要求的同时,对区域经济的发展规划也有足够重视。因此,保障油气管道的安全则成为了我国能源安全战略的重中之重。在阐释油气管道现阶段在储运安全保障技术发展状况的基础上,分析了现存的问题及解决问题的手段,并指出未来可能使用的目标策略,为今后研究者提供一定程度上的借鉴经验。  相似文献   

17.
石油天然气的地质勘探开发目的是为了获得最佳的油气产能而进行的地质研究工作。石油天然气地质勘探工作具有非常重要的意义,通过地质勘探获得有价值的地层信息资料,对储层油气的显示进行评价和分析,确定具有工业开采价值,才能投入开发生产,为油田创造最佳的经济效益。  相似文献   

18.
膜的污染和劣化及其防治对策   总被引:25,自引:0,他引:25  
较为系统地介绍了膜污染和劣化的定义和特点,因膜污染和劣化而造成的膜性能变化,以及如何预防、减少或清除膜污染和劣化的一些通用方法。  相似文献   

19.
20.
Gel permeation chromatographic (GPC) and thin-layer chromatographic (TLC) studies of polystyrene, polybutadienes (BR), and their copolymers (SBR) have been carried out. GPC primarily separates them on the basis of molecular size, and TLC, on the basis of composition. Methods of obtaining absolute molecular weight distributions for BR and SBR based upon variations of the Strasbourg Universal Calibration procedure are described. In particular, [η]–M relationships in both the GPC solvent (THF) and in a second solvent (toluene) were used; in addition, results of statistical mechanical calculations for \documentclass{article}\pagestyle{empty}\begin{document}$\overline {s^2 }$\end{document} (based on the assumption of negligible steric hindrance and freely rotating bonds) were applied. An experimental comparison of these methods was carried out, and use of the [η]–M relationships for both solvents was found to give satisfactory results. The predictions of the statistical theory were too low. A detailed study of polymer–solvent–gel interaction in the GPC unit was made through investigation of ternary phase equilibrium in the (polystyrene)–THF–(polymer) system. The polymers studied included BR and SBR with varying styrene contents. Experimental techniques for TLC separations of BR, SBR, and polystyrene according to the composition are described.  相似文献   