首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 93 毫秒
1.
采用ER50-6焊丝对NM450耐磨钢板进行了CO_2气体保护焊,研究了接头的显微组织、力学性能,以及焊接冷裂纹敏感性。结果表明:焊缝组织为块状铁素体+针状铁素体,热影响区粗晶区和正火区的组织分别为板条马氏体和铁素体+渗碳体;焊缝区、粗晶区、正火区和不完全重结晶区的硬度分别为220,412,234,386HV,马氏体分解导致正火区和不完全重结晶区硬度降低;接头的抗拉强度为768 MPa,焊缝中心、影响区和母材的-20℃夏比冲击吸收功分别为110,140,88J;此钢有一定的冷裂纹敏感性,在环境温度32.6℃、不预热焊接时不会产生裂纹,在环境温度-1.4℃、不预热焊接时,接头根部裂纹率和截面裂纹率均为100%,80℃预热焊接则不会产生焊接裂纹。  相似文献   

2.
为满足X80管线钢的焊接需要,开发了以BaF2为主的低碱性渣系Mn-Ni-Mo-Ti-B合金系自保护药芯焊丝,并对采用该焊丝焊接后此钢接头的显微组织及力学性能进行了分析。结果表明:X80管线钢接头焊缝显微组织为针状铁素体、粒状贝氏体以及少量的M-A岛,热影响区的组织主要为粒状贝氏体、贝氏体铁素体;焊接接头的抗拉强度为711 MPa,屈服强度为565.7 MPa,室温冲击功为155J,-20℃冲击功为144.7J,完全能满足石油管道建设的标准要求。  相似文献   

3.
利用光学显微镜、拉伸试验机、冲击试验机及维氏硬度计等对X100管线钢埋弧焊焊接接头的组织及性能进行了研究。结果表明:X100管线钢焊接接头粗晶区组织为粗大的先共析铁素体和粒状贝氏体,细晶区主要为细小的铁素体,不完全重结晶区为细晶铁素体、粗晶针状铁素体和粒状贝氏体混合组织;接头的抗拉强度平均值为576MPa,达到母材的80%,拉伸试样断裂于焊缝处;接头焊缝、热影响区的冲击功分别为198J和259J;焊缝区最高硬度为316HV,在临界温度热影响区(ICHAZ)和亚临界温度热影响区(SCHAZ)之间存在软化现象。  相似文献   

4.
利用光学显微镜、拉伸和冲击试验机、显微硬度计等对高温运行前后12Cr1MoV钢焊接接头的组织及力学性能进行了研究。结果表明:高温运行后,焊接接头组织中除了原始组织中的铁素体和珠光体外,还出现颗粒状析出物,热影响区和焊缝处组织中出现了贝氏体;焊接接头的屈服强度和抗拉强度分别由高温运行前的455,625MPa下降为430和583MPa,平均冲击功从160J下降为124J;冲击断口上有许多裂纹,裂纹上有明显的台阶,断裂方式为塑性断裂;高温运行后母材和焊缝区的硬度分别为190,265HV,焊缝的硬度符合供货方技术要求,而母材硬度超标。  相似文献   

5.
采用MAG(熔化极活性气体保护焊)对25mm厚10Ni5CrMoV钢进行了焊接,观察了接头显微组织与冲击断口形貌,并对其硬度、冲击性能和拉伸性能进行了研究。结果表明:接头焊缝区组织主要为板条马氏体/贝氏体+粒状贝氏体,且存在较多的沿奥氏体晶界分布的M-A组元,硬度接近于母材,冲击韧性较低,-50℃时的平均冲击功为42J;随着距焊缝中心距离的增大,热影响区组织依次为淬火马氏体、板条马氏体/贝氏体+铁素体+粒状贝氏体,且临界区碳化物积聚并长大,硬度先升高后降低,最低硬度为286.4HV,冲击韧性较高,-50℃时的平均冲击功为188J;焊接接头的平均抗拉强度达到920 MPa,拉伸试样的断裂位置均在母材;M-A组元及碳化物是影响接头性能的主要因素。  相似文献   

6.
热输入对焊接接头组织与力学性能有重要影响。采用激光-电弧复合焊接方法,研究了不同电弧能量和激光能量下的接头组织、焊缝氮含量、拉伸与冲击性能及接头显微硬度。研究表明:焊缝组织为奥氏体+少量δ铁素体,焊缝中析出的δ铁素体随热输入加大而增多;当电流达到200A后,熔池液态金属中氮的溶解近于饱和,即使焊接电流增大,焊缝氮含量依然趋于恒定;而当激光功率增至2.0kW后,焊接过程中的匙孔维持在稳定状态,焊缝氮含量也近于恒定;拉伸断裂位置均在焊缝区,当焊接电流为200A时,平均拉伸强度最高,达到967.58MPa,当激光功率为1.6kW时,平均拉伸强度可达962.88MPa;焊缝冲击功随激光功率的增大呈先降低后升高的变化趋势,但随电流的增大其变化趋势相反;熔合线的冲击功随着焊接参数的变化呈现出相同的变化趋势,焊缝和熔合线的最大平均冲击功分别为47.60J和62.85J;拉伸和冲击的断裂形式均为韧性断裂;焊缝区显微硬度最低,导致拉伸测试时均断裂于焊缝区。  相似文献   

7.
用药芯焊丝CO2气体保护焊焊接Domex700MC低合金高强钢,用光学显微镜、硬度计和冲击试验机等对焊接接头的显微组织和力学性能进行了分析。结果表明:焊缝金属晶粒细小且分布均匀,有较多针状铁素体,但熔合区组织比较粗大,使熔合区附近塑性降低,为焊接接头的薄弱部位;焊缝金属显微硬度较高,为315HV,而在热影响区为225HV,出现软化现象;焊接接头力学性能优良,具有较高的抗拉强度(630.94MPa)和冲击功(135.34J)。  相似文献   

8.
对D406钢和20钢进行了角焊接,研究了异质钢焊接接头的显微组织和力学性能,此外还研究了D406钢对接接头的力学性能。结果表明:此异质钢焊接接头D406钢侧焊缝区的显微组织主要以板条马氏体为主,熔合区主要是针状马氏体,该区是接头中最易产生裂纹的区域;D406A钢侧焊接接头热影响区靠近焊缝处的硬度最大,约为659 HV;20钢侧焊接接头焊缝区的最高硬度约为350HV,低于D406A钢侧的最高硬度,因而D406A钢侧热影响区的淬硬倾向相对较大;D406A钢对接接头熔合区的冲击功小于母材和焊缝区的冲击功,该焊接接头的拉伸试样均断裂于在焊缝区,抗拉强度的平均值为679 MPa,这与其焊缝区的组织为板条马氏体有很大关系。  相似文献   

9.
用自行设计的锰镍钼硼合金系焊丝对低碳贝氏体钢进行双面焊;利用光学显微镜、扫描电子显微镜、拉伸和冲击试验机以及显微硬度计等研究了焊接接头的显微组织和力学性能。结果表明:焊缝和热影响区显微组织都主要是针状铁素体和粒状贝氏体;HAZ区组织粗大,存在软化问题;在较小的焊接线热输入条件下,焊接接头强韧性匹配较好,抗拉强度为803.63 MPa,焊缝和热影响区冲击韧性分别为193J和232J。  相似文献   

10.
采用埋弧焊对DH32高强度船板钢进行了焊接,通过扫描电镜、拉伸和冲击试验机等测试了焊接接头的力学性能并分析了其冲击断口形貌。结果表明:该钢10道次埋弧焊焊接接头的拉伸断裂位置均在靠近热影响区的母材区,接头的抗拉强度与母材的相当,没有出现明显的软化现象;焊缝、熔合区、热影响区试样的平均冲击功分别为55,58,75J,均满足冲击功不小于34J的要求;随着距焊缝中心距离的增大,焊接接头冲击断口中的纤维区面积增大,接头基本不存在韧性最差区。  相似文献   

11.
In a recent paper, the Ritz method with simple algebraic polynomials as trial functions was used to obtain an eigenvalue equation for the free vibration of a class of homogeneous solids with cavities. The method presented is here extended to the study of a class of non-homogeneous solids, in which each solid is composed of a number of isotropic layers with different material properties. The Cartesian coordinate system is used to describe the geometry of the solid which is modelled by means of a segment bounded by the yz, zx and xy orthogonal coordinate planes and by two curved surfaces which are defined by fairly general polynomial expressions in the coordinates x, y and z. The surface representing the interface between two material layers in the solid is also described by a polynomial expression in the coordinates x, y and z. In order to demonstrate the accuracy of the approach, natural frequencies are given for both a two- and three-layered spherical shell and for a homogeneous hollow cylinder, as computed using the present approach, and are compared with those obtained using an exact solution. Results are then given for a number of two- and three-layered cylinders and, to demonstrate the versatility of the approach, natural frequencies are given for a five-layered cantilevered beam with a central circular hole as well as for a number of composite solids of more general shape.  相似文献   

12.
以叶切面最大厚度的数值计算方法为基础,探讨叶切面最大厚度计算的计算机实现,介绍叶切面厚度数值计算法的应用实例.  相似文献   

13.
通过分析膨胀套在实际使用产生滑移受阻现象、卡死现象原因的实质,并在分析产生问题原因的基础上提出了改进措施即:增加导向机构。  相似文献   

14.
介绍了双丝杠驱动机构工作原理,论述了双丝杠运动产生不同步的原因以及如何判定与解决同步问题。  相似文献   

15.
刘素山 《机械制造》2022,60(1):62-63,80
设计了磨粉机快辊轴承座的加工工艺和具体的工装夹具.利用卧式加工中心加工磨粉机快辊轴承座,辅以能够高效快速夹紧的夹具,既可以保证加工精度,又能够提高加工效率.  相似文献   

16.
一种涡旋压缩机径向随变机构的设计   总被引:1,自引:0,他引:1  
刘涛  邬再新 《流体机械》2001,29(7):17-19
详细介绍了运用随变原理设计的一种新型径向密封机构的结构特点,工作原理及主要参数的确定方法,该机构可补偿由于涡旋体加工精度不高而造成的功率损失,适用于涡旋压缩机的批量生产。  相似文献   

17.
Specific features of operation of one- and two-capacitor microelectromechanical converters (MEMC) of energy of mechanical microscopic vibrations into electric energy with a modulated electrode-gap magnitude and with allowance for the mutual influence of electrical and elastic forces are analyzed, and the characteristics of these two devices are compared. The main factors restricting the increase in MEMC power are demonstrated to be the effects of “collapsing” and the condition of conservation of positive rigidity of the system. Expressions for estimating the limiting MEMC parameters are derived. The possibility of electrical energy generation in the presence of “real“ sources of wide-spectrum microscopic vibrations is considered.  相似文献   

18.
针对目前市场对工业设计人才的需求,本文论述了我校在工业设计教育方面的改革措施,着重介绍了我校工业设计教育在软件和硬件方面所进行的一系列的改革。  相似文献   

19.
飞机起落架减振支柱在飞机起落和滑跑时,吸收撞击能量,对飞机安全起降的意义重大.减振筒是减振支柱中的重要部件,本文从工艺流程、理化分析、外场使用和腐蚀机理分析等方面,对减振支柱减振筒内壁的腐蚀原因及危害进行了综合分析,并提出了相应措施.  相似文献   

20.
本文以某些积算和双笔记录仪产品为例说明由于仪表功能设计的不合理或选型不当,影响了仪表的正常使用,制造厂和用户应关注这类问题。  相似文献   