1.
Atactic poly(3‐hydroxybutyrate) (a‐PHB) and block copolymers of poly(ethylene glycol) (PEG) with poly(ε‐caprolactone) (PCL‐b‐PEG) were synthesized through anionic polymerization and coordination polymerization, respectively. As demonstrated by differential scanning calorimetry (DSC) and dynamic mechanical thermal analysis (DMTA) measurements, both chemosynthesized a‐PHB and biosynthesized isotactic PHB (i‐PHB) are miscible with the PEG segment phase of PCL‐b‐PEGs. However, there is no evidence showing miscibility between both PHBs and the PCL segment phase of the copolymer even though PCL has been block‐copolymerized with PEG. Based on these results, PCL‐b‐PEG was added, as a compatibilizer, to both the PCL/a‐PHB blends and the PCL i‐PHB blends. The blend films were obtained through the evaporation of chloroform solutions of mixed components. Excitingly, the improvement in mechanical properties of PCL/PHB blends was achieved as anticipated initially upon the addition of PCL‐b‐PEG. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 80: 2600–2608, 2001  相似文献   

2.
A series of poly(ether–ester) copolymers were synthesized from poly(2,6 dimethyl‐1,4‐phenylene oxide) (PPO) and poly(ethylene terephthalate) (PET). The synthesis was carried out by two‐step solution polymerization process. PET oligomers were synthesized via glycolysis and subsequently used in the copolymerization reaction. FTIR spectroscopy analysis shows the coexistence of spectral contributions of PPO and PET on the spectra of their ether–ester copolymers. The composition of the poly(ether–ester)s was calculated via 1H NMR spectroscopy. A single glass transition temperature was detected for all synthesized poly(ether–ester)s. Tg behavior as a function of poly(ether–ester) composition is well represented by the Gordon‐Taylor equation. The molar masses of the copolymers synthesized were calculated by viscosimetry. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci, 2006  相似文献   

3.
A polyblend of poly(ortho esters)–poly(ethylene glycol) (POE–PEG) was prepared. The release behavior of the acetanilide‐loaded film of the POE–PEG polyblend was studied. Blending POE with water‐soluble PEG can promote the release of drug in pH 7.4 PBS buffer at 37°C, while POE has plasticizing effect on PEG. Infrared and X‐ray diffraction studies reveal that there is some interaction between POE and acetanilide. The SEM micrographs disclose that the porosity of the drug‐loaded film enhances with an increase immersing time. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 71: 303–309, 1999  相似文献   

4.
Poly(ethylene glycol) (PEG) and end‐capped poly(ethylene glycol) (poly(ethylene glycol) dimethyl ether (PEGDME)) of number average molecular weight 1000 g mol?1 was melt blended with poly(ethylene terephthalate) (PET) oligomer. NMR, DSC and WAXS techniques characterized the structure and morphology of the blends. Both these samples show reduction in Tg and similar crystallization behavior. Solid‐state polymerization (SSP) was performed on these blend samples using Sb2O3 as catalyst under reduced pressure at temperatures below the melting point of the samples. Inherent viscosity data indicate that for the blend sample with PEG there is enhancement of SSP rate, while for the sample with PEGDME the SSP rate is suppressed. NMR data showed that PEG is incorporated into the PET chain, while PEGDME does not react with PET. Copyright © 2005 Society of Chemical Industry  相似文献   

5.
Novel amphiphilic star‐shaped terpolymers comprised of hydrophobic poly(?‐caprolactone), pH‐sensitive polyaminoester block and hydrophilic poly(ethylene glycol) (Mn = 1100, 2000 g mol?1) were synthesized using symmetric pentaerythritol as the core initiator for ring‐opening polymerization (ROP) reaction of ?‐caprolactone functionalized with amino ester dendrimer structure at all chain ends. Subsequently, a second ROP reaction was performed by means of four‐arm star‐shaped poly(?‐caprolactone) macromer with eight ‐OH end groups as the macro‐initiator followed by the attachment of a poly(ethylene glycol) block at the end of each chain via a macromolecular coupling reaction. The molecular structures were verified using Fourier transform infrared and 1H NMR spectroscopies and gel permeation chromatography. The terpolymers easily formed core–shell structural nanoparticles as micelles in aqueous solution which enhanced drug solubility. The hydrodynamic diameter of these agglomerates was found to be 91–104 nm, as measured using dynamic light scattering. The hydrophobic anticancer drug curcumin was loaded effectively into the polymeric micelles. The drug‐loaded nanoparticles were characterized for drug loading content, encapsulation efficiency, drug–polymer interaction and in vitro drug release profiles. Drug release studies showed an initial burst followed by a sustained release of the entrapped drug over a period of 7days at pH = 7.4 and 5.5. The release behaviours from the obtained drug‐loaded nanoparticles indicated that the rate of drug release could be effectively controlled by pH value. Altogether, these results demonstrate that the designed nanoparticles have great potential as hydrophobic drug delivery carriers for cancer therapy. © 2015 Society of Chemical Industry  相似文献   

6.
A series of poly(?‐caprolactone)‐b‐poly(ethylene glycol) (PCL‐b‐PEG) block copolymers with different molecular weights were synthesized with a salicylaldimine‐aluminum complex in the presence of monomethoxy poly(ethylene glycol). The block copolymers were characterized by 1H NMR, GPC, WAXD, and DSC. The 1H NMR and GPC results verify the block structure and narrow molecular weight distribution of the block copolymers. WAXD and DSC results show that crystallization behavior of the block copolymers varies with the composition. When the PCL block is extremely short, only the PEG block is crystallizable. With further increase in the length of the PCL block, both blocks can crystallize. The PCL crystallizes prior to the PEG block and has a stronger suppression effect on crystallization of the PEG block, while the PEG block only exerts a relatively weak adverse effect on crystallization of the PCL block. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007  相似文献   

7.
A polyelectrolyte complex (PEC) was formed by mixing aqueous solutions of the polyanion poly(sodium phosphate) with the polycation poly(2‐vinylpyridinium chloride). Conductometric and potentiometric titrations indicated the electrochemical end point of each titration. In all cases the end point occurred at a unit molar ratio of polyanionic to polycationic groups that was approximately one. The stoichiometry was also confirmed by analysis of the supernatant liquid in conjunction with the weights of the initial components and complex. An analysis showed that the starting materials were regenerated after dissolution of the complex with a 2M HCl solution. The interaction of the bivalent cupric ions with PEC were also investigated. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 83: 3022–3028, 2002; DOI 10.1002/app.2332  相似文献   

8.
The crystallization kinetics of poly(butylene terephthalate) (PBT), poly(ethylene terephthalate) (PET), and their copolymers poly(1,4‐butylene‐co‐ethylene terephthalate) (PBET) containing 70/30, 65/35 and 60/40 molar ratios of 1,4‐butanediol/ethylene glycol were investigated using differential scanning calorimetry (DSC) at crystallization temperatures (Tc) which were 35–90 °C below equilibrium melting temperature . Although these copolymers contain both monomers in high proportion, DSC data revealed for copolymer crystallization behaviour. The reason for such copolymers being able to crystallize could be due to the similar chemical structures of 1,4‐butanediol and ethylene glycol. DSC results for isothermal crystallization revealed that random copolymers had a lower degree of crystallinity and lower crystallite growth rate than those of homopolymers. DSC heating scans, after completion of isothermal crystallization, showed triple melting endotherms for all these polyesters, similar to those of other polymers as reported in the literature. The crystallization isotherms followed the Avrami equation with an exponent n of 2–2.5 for PET and 2.5–3.0 for PBT and PBETs. Analyses of the Lauritzen–Hoffman equation for DSC isothermal crystallization data revealed that PBT and PET had higher growth rate constant Go, and nucleation constant Kg than those of PBET copolymers. © 2001 Society of Chemical Industry  相似文献   

9.
The miscibility of high molecular weight poly(ethylene oxide) blends with poly(3‐hydroxypropionic acid) and poly(3‐hydroxybutyric acid) (P(3HB)) has been investigated by differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA) and high‐resolution solid state 13C nuclear magnetic resonance (NMR). The DSC thermal behaviour of the blends revealed that the binary blends of poly(ethylene oxide)/poly(3‐hydroxypropionic acid) (OP blends) were miscible over the whole composition range while the miscibility of poly(ethylene oxide)/poly(3‐hydroxybutyric acid) blends (OB blends) was dependent on the blend composition. OB blends were found to be partly miscible at the middle P(3HB) contents (25 %, 50 %) and miscible at other P(3HB) contents (10 %, 75 % and 90 %). Single‐phase behaviour for OP blends and phase separation behaviour for OB blends were observed from DMTA. The results from NMR spectroscopy revealed that the two components in the OP50 blend were intimately mixed on a scale of about 35 nm, while the domain sizes in the OB blend with a P(3HB) content of 50 % were larger than about 32 nm. © 2000 Society of Chemical Industry  相似文献   

10.
Microparticles formed by poly(lactic acid) (PLA) and poly(ethylene glycol) (PEG) diblock copolymers containing fluorescein grafted to the polymer chain were synthesized by a Ugi four‐component condensation (UFCC) reaction. To synthesize these copolymers, lactide was first polymerized by a ring‐opening polymerization with alcohol initiators containing functional groups to give carboxyl‐ and aldehyde‐end‐functionalized PLA. Two different fluorescent block copolymers (FCPs) of PEG–PLA conjugated to fluorescein (FCP 1 and FCP 2) were then synthesized by UFCC; they gave yields in the range 65–75%. These copolymers were characterized well according their chemical structures and thermal properties, and we prepared fluorescent microspheres (FMSs) from them with the single emulsion–solvent evaporation method (FMS 1 and FMS 2). A new application of UFCC in the preparation of biomasked drug‐delivery systems is proposed. © 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016 , 133, 42994.  相似文献   

11.
Two series of thermoplastic poly(ester–siloxane)s, based on poly(dimethylsiloxane) (PDMS) as the soft segment and poly(butylene terephthalate) as the hard segment, were synthesized by two‐step catalyzed transesterification reactions in the melt. Incorporation of soft poly(dimethylsiloxane) segments into the copolyester backbone was accomplished in two different ways. The first series was prepared based on dimethyl terephthalate, 1,4‐butanediol and silanol‐terminated poly(dimethylsiloxane) (PDMS‐OH). For the second series, the PDMS‐OH was replaced by methyl diesters of carboxypropyl‐terminated poly(dimethylsiloxane)s. The syntheses were optimized in terms of both the concentration of catalyst, tetra‐n‐butyl‐titanate (Ti(OBu)4), and stabilizer, N,N′‐diphenyl‐p‐phenylene‐diamine, as well as the reaction time. The reactions were followed by measuring the inherent viscosities of the reaction mixture. The molecular structures of the synthesized poly(ester–siloxane)s were verified by 1H NMR spectroscopy, while their thermal properties were investigated using differential scanning calorimetry. © 2001 Society of Chemical Industry  相似文献   

12.
Poly(3‐hydroxy octanoate) (PHO), poly(3‐hydroxy butyrate‐co‐3‐hydroxyvalerate) (PHBV), and linoleic acid were grafted onto chitosan via condensation reactions between carboxylic acids and amine groups. Unreacted PHAs and linoleic acid were eliminated via chloroform extraction and for elimination of unreacted chitosan were used 2 wt % of HOAc solution. The pure chitosan graft copolymers were isolated and then characterized by FTIR, 13C‐NMR (in solid state), DSC, and TGA. Microbial polyester percentage grafted onto chitosan backbone was varying from 7 to 52 wt % as a function of molecular weight of PHAs, namely as a function of steric effect. Solubility tests were also performed. Graft copolymers were soluble, partially soluble or insoluble in 2 wt % of HOAc depending on the amount of free primary amine groups on chitosan backbone or degree of grafting percent. Thermal analysis of PHO‐g‐Chitosan graft copolymers indicated that the plastizer effect of PHO by means that they showed melting transitions Tms at 80, 100, and 113°C or a broad Tms between 60.5–124.5°C and 75–125°C while pure chitosan showed a sharp Tm at 123°C. In comparison of the solubility and thermal properties of graft copolymers, linoleic acid derivatives of chitosan were used. Thus, the grafting of poly(3‐hydroxyalkanoate) and linoleic acid onto chitosan decrease the thermal stability of chitosan backbone. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 103:81–89, 2007  相似文献   

13.
Poly(p‐dioxanone)–poly(ethylene glycol)–poly(p‐dioxanone) ABA triblock copolymers (PEDO) were synthesized by ring‐opening polymerization from p‐dioxanone using poly(ethylene glycol) (PEG) with different molecular weights as macroinitiators in N2 atmosphere. The copolymer was characterized by 1H NMR spectroscope. The thermal behavior, crystallization, and thermal stability of these copolymers were investigated by differential scanning calorimetry and thermogravimetric measurements. The water absorption of these copolymers was also measured. The results indicated that the content and length of PEG chain have a greater effect on the properties of copolymers. This kind of biodegradable copolymer will find a potential application in biomedical materials. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102:1092–1097, 2006  相似文献   

14.
The present work provides improved recycled high molecular weight poly(ethylene terephthalate) (PET) by chain extension using 2,2′‐(1,4‐phenylene)bis(2‐oxazoline) (PBO) as the chain extender. PBO is a very reactive compound toward macromolecules containing carboxyl end groups but not hydroxyl end groups. In the case of PET, where both species are present, for even better results, phthalic anhydride (PA) was added in the initial sample, before the addition of PBO. With this technique, we succeeded in increasing the carboxyl groups by reacting PA with the hydroxyl terminals of the starting polymer. From this modification of the initial PET sample, PBO was proved an even more effective chain extender. So, starting from a recycled PET with intrinsic viscosity [η] = 0.78, which would be [η] = 0.69 after the aforementioned treatment without a chain extender or n = 19,800, we prepared a PET grade having [η] = 0.85 or n = 25,600 within about 5 min. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 77: 2206–2211, 2000  相似文献   

15.
The miscibility of poly(3‐hydroxyvalerate) (PHV)/poly(p‐vinyl phenol) (PVPh) blends has been studied by differential scanning calorimetry (DSC) and Fourier transform infrared (FTIR) spectroscopy. The blends are miscible as shown by the existence of a single glass transition temperature (Tg) and a depression of the equilibrium melting temperature of PHV in each blend. The interaction parameter was found to be −1.2 based on the analysis of melting point depression data using the Nishi–Wang equation. Hydrogen‐bonding interactions exist between the carbonyl groups of PHV and the hydroxyl groups of PVPh as evidenced by FTIR spectra. The crystallization of PHV is significantly hindered by the addition of PVPh. The addition of 50 wt % PVPh can totally prevent PHV from cold crystallization. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 74: 383–388, 1999  相似文献   

16.
Aromatic polyesters were prepared and used to improve the brittleness of bismaleimide resin, composed of 4,4′‐bismaleimidodiphenyl methane and o,o′‐diallyl bisphenol A (Matrimid 5292 A/B resin). The aromatic polyesters included PEPT [poly(ethylene phthalate‐co‐ethylene terephthalate)], with 50 mol % of terephthalate, PEPB [poly(ethylene phthalate‐co‐ethylene 4,4′‐biphenyl dicarboxylate)], with 50 mol % of 4,4′‐biphenyl dicarboxylate, and PEPN [poly(ethylene phthalate‐co‐ethylene 2,6‐naphthalene dicarboxylate)], with 50 mol % 2,6‐naphthalene dicarboxylate unit. The polyesters were effective modifiers for improving the brittleness of the bismaleimide resin. For example, inclusion of 15 wt % PEPT (MW = 9300) led to a 75% increase in fracture toughness, with retention in flexural properties and a slight loss of the glass‐transition temperature, compared with the mechanical and thermal properties of the unmodified cured bismaleimide resin. Microstructures of the modified resins were examined by scanning electron microscopy and dynamic viscoelastic analysis. The toughening mechanism was assessed as it related to the morphological and dynamic viscoelastic behaviors of the modified bismaleimide resin system. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 81: 2352–2367, 2001  相似文献   

17.
The aim of the study was to investigate the mechanical properties and biodegradability of poly(trimethylenecarbonate‐ε‐caprolactone)‐block‐poly(p‐dioxanone) [P(TMC‐ε‐CL)‐block‐PDO] in comparison with poly(p‐dioxanone) and poly(glycolide‐ε‐caprolactone) (Monocryl®) monofilaments in vivo and in vitro. P(TMC‐ε‐CL)‐block‐PDO copolymer and poly(p‐dioxanone) were prepared by using ring‐opening polymerization reaction. The monofilament fibers were obtained using conventional melt spun methods. The physicochemical and mechanical properties, such as viscosity, molecular weight, crystallinity, and knot security, were studied. Tensile strength, breaking strength retention, and surface morphology of P(TMC‐ε‐CL)‐block‐PDO, poly(p‐dioxanone), and Monocryl monofilament fibers were studied by immersion in phosphate‐buffered distilled water (pH 7.2) at 37°C and in vivo. The implantation studies of absorbable suture strands were performed in gluteal muscle of rats. The polymers, P(TMC‐ε‐CL)‐block‐PDO, poly(p‐dioxanone), and Monocryl, were semicrystalline and showed 27, 32, and 34% crystallinity, respectively. Those mechanical properties of P(TMC‐ε‐CL)‐block‐PDO were comparatively lower than other polymers. The biodegradability of poly(dioxanone) homopolymer is much slower compared with that of two copolymers. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 737–743, 2006  相似文献   

18.
The synthesis of two low molecular weight linear unsaturated oligoester precursors, poly(propylene fumarate‐co‐sebacate) (PPFS) and poly(ethylene fumarate‐co‐sebacate) (PEFS), are described. PPFS, PEFS, and poly(ethylene glycol) are then used to prepare poly(propylene fumarate‐co‐sebacate)‐co‐poly(ethylene glycol) (PPFS‐co‐PEG) and poly(ethylene fumarate‐co‐sebacate)‐co‐poly(ethylene glycol) (PEFS‐co‐PEG) block copolymers. The products thus obtained are investigated in terms of the molecular weight, composition, structure, thermal properties, and solubility behavior. A number of design parameters including the molecular weights of PPFS, PEFS, and PEG, the reaction time in the polymer synthesis, and the weight ratio of PEG to PPFS or to PEFS are varied to assess their effects on the product yield and properties. The hydrolytic degradation of PPFS‐co‐PEG and PEFS‐co‐PEG in an isotonic buffer (pH 7.4, 37°C) is investigated, and it is found that the fumarate ester bond cleaves faster than does the sebacate ester bond. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 295–300, 2004  相似文献   

19.
A comparison of the thermal properties of two classes of poly(D,L ‐lactic‐glycolic acid) multiblock copolymers is reported. In particular, the results of differential scanning calorimetry, and thermogravimetric analysis of copolymers containing poly(ethylene glycol) (PEG) or diol‐terminated poly(ϵ‐caprolactone) (PCDT) segments are described. The influence of the chemical structure and the length of PEG and PCDT on thermal stability, degree of crystallinity and glass transition temperature (Tg ) is discussed. Finally, an evaluation of the hydrolytic behavior in conditions mimicking the physiological environment is reported. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 78: 1721–1728, 2000  相似文献   

20.
The physical properties of poly(vinyl chloride) (PVC) and poly(N‐isopropylacrylamide) [poly(NIPAAm)] blend systems, and their corresponding graft copolymers such as PVC‐g‐NIPAAm, were investigated in this work. The compatible range for PVC–poly(NIPAAm) blend systems is less than 15 wt % poly(NIPAAm). The water absorbencies for the grafted films increase with increase in graft percentage. The water absorbencies for the blend systems increase with increase in poly(NIPAAm) content within the compatible range for the blends, but the absorbencies decrease when the amount of poly(NIPAAm) is more than the compatible range in the blend system. The tensile strengths for the graft copolymers are larger than the corresponding blends. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 76: 170–178, 2000  相似文献   