1.
Natural rubber (NR), epoxidized natural rubber (ENR), and chlorosulfonated polyethylene (CSM) composites filled with conductive carbon black and aluminum powder have been prepared by using a two‐roll mill. An electromagnetic interference shielding effectiveness of those rubber composites was carried out in the frequency range of 8–12GHz (X‐band microwave). The increase of filler loading enhanced shielding effectiveness of the rubber composites. Conductive carbon black was more effective in shielding than aluminum powder. Binary filler‐filled rubber composites showed higher shielding effectiveness than that of single filler‐filled rubber composites. It has been observed that the shielding effectiveness of these rubber composites could be ranked in the following order: ENR ≥ CSM > NR, whereas the mechanical properties of the rubber composites were in the order of CSM > ENR > NR. The correlation between shielding effectiveness and electrical conductivity as well as mechanical properties of the rubber composites are also discussed. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007  相似文献   

2.
This study aims to investigate the viability of employing corn-based fillers (powdered corn grain [CG], corn flour [CF] and cornstarch [CS]) to improve the biodegradability of natural rubber latex (NRL) composites by varying filler loading from 0 to 50 phr. Notable variation in both physical and mechanical properties were observed for the different filler types, with CG-filled NRL demonstrating the better adhesion with NRL. Thus, CG-filled composites were selected for investigation of biodegradability. Increased CG loading in NRL compounds enhanced biodegradation; with over 70% degradation observed for 50 phr CG loading upon 15 weeks of soil burial. However, the trade-off between mechanical properties and biodegradability limits the CG loading in the NRL matrix to 20 phr for manufacturing NRL-based products. It was observed that NRL with CG filler loading of 20 phr conforms to the ASTM D3578 standard for manufacturing rubber gloves; with 50% biodegradation upon 15 weeks of soil burial.  相似文献   

3.
The effects of filler loading on the curing characteristics, swelling behavior, and mechanical properties of natural rubber compounds were studied using a conventional vulcanization system. Recycle rubber powder (RRP), carbon black (CB) (N550), and calcium carbonate (CaCO3) were used as fillers and the loading range was from 0 to 50 phr. Results show that the scorch time, t 2, and cure time, t 90, decrease with increase in filler loading. At a similar filler loading, RRP shows shortest t 2 and t 90 followed by CB and calcium carbonate. The tensile strength, tensile modulus, and hardness increase with increase in CB loading, whereas elongation at break, resilience, and swelling properties show opposite trend. For RRP and calcium carbonate filled natural rubber compounds, the tensile strength increases up to 10 phr and starts to deteriorate at higher filler loading. The other properties such as tensile modulus, hardness, elongation at break, resilience, and swelling percentage show a small change (increase or decrease) with increase in RRP and calcium carbonate loading in natural rubber compounds. Overall results indicate that RRP can be used as a cheapener to replace calcium carbonate in natural rubber compounds where improved mechanical properties are not critical.  相似文献   

4.
The purpose of this work is to study the reinforcement effect of modified coal gangue (CG) on natural rubber (NR); carbon black (CB) was taken as reference filler. The addition of CG and CB to NR with the total filler loading fixed at 35 phr. The orthogonal experiment was employed to reveal the modification conditions on reinforcing properties. The results show that modification conditions such as weight ratio of coupling agent (CA), calcining temperature (CT), and calcining time (CM) affect the strengthening properties of CG, and CA is the most important factor influencing the tensile strength of NR, the order of influence can be expressed as CA > CT > CM. The optimum modification conditions are CT 800°C, CM 1 hr, and CA 2%. 300% modulus of NR composites filled with modified CG (17.5 phr)/CB (17.5phr) hybrid filler is similar to NR filled with CB alone at same filler loading, while elongation at break increases significantly for existent of CG. The effect of heat treatment and modification conditions of CG were tested by particle size distribution, scanning electron microscopy, Fourier transform infrared spectra, and X‐ray diffraction. The results show that the specific surface area of CG increased and hydroxyl group in crystal structure of CG removed under heat treatment. Dynamic mechanical analysis results show that the storage modulus and tan δ of CG filled NR composites are higher while Tg is less than that of CB, indicating the existence of a strong and stiff interface between filler and NR matrix. POLYM. COMPOS., 35:1911–1917, 2014. © 2014 Society of Plastics Engineers  相似文献   

5.
Abstract

The effect of carbon black on nanoclay filled polychloroprene (CR) composites has been investigated. The nanoclay loading is fixed at 5 part per hundred rubbers (phr), and carbon black loading varied from 5 to 20 phr in rubber compounds. The rubber nanocomposites are prepared in laboratory by mixing in two-roll mill. The addition of nanoclay enhances mechanical properties especially tear strength and decreases water absorption without change in electrical properties compared to gum rubber vulcanisates. Wide angle X-ray diffraction and transmission electron microscopy are used to study the microstructure of CR nanocomposites. The addition of 5 parts of nanoclay to 15 phr carbon black filled samples shows synergistic effect between the fillers and suggests that the reinforcement is due to a more developed filler network formation in hybrid filler system than that in single phase filler. Significant improvement in mechanical, electrical and low water absorption properties has been obtained with these nanoclay and carbon black filled rubber nanocomposites. The paper concludes that nanocomposites containing a mixture of organoclay and carbon black in right proportion can be a substitute for rubber components used in underwater cable and device encapsulation applications.  相似文献   

6.
《Polymer Composites》2017,38(11):2594-2602
Novel rice bran carbon (RBC) filled styrene butadiene rubber (SBR) composites were fabricated by latex compounding method (LCM). The chemical structure determination and the static precipitation experiments definitely authenticated the hydrophilicity of RBC, which enables RBC to be uniformly dispersed in water without surface modification and thereby compounded with rubber latex directly. The SBR/RBC composites prepared by LCM exhibited homogeneous filler dispersion state and superior mechanical properties compared with those compounded by solid compounding method (SCM). The vulcanization properties, mechanical properties, thermal stabilities, and swelling properties of SBR/RBC composites prepared by LCM were studied. It was revealed that the tensile strength, modulus, and tear strength of SBR/RBC composites increased correspondingly as the RBC loading increased from 0 to 80 phr. The decomposition temperature would stop rising when the filler loading exceeded 40 phr. The significant increases of the crosslink density with increasing filler volume content indicated the reinforcement effect of RBC. POLYM. COMPOS., 38:2594–2602, 2017. © 2015 Society of Plastics Engineers  相似文献   

7.
Nickel zinc ferrite (Ni-ZnFe2O4)-filled natural rubber (NR) composite was prepared at various loading of ferrite. The tensile properties included in this study were tensile strength, tensile modulus and elongation at break. The tensile strength and elongation at break of the composites increased up to 40 parts per hundred rubber (phr) of ferrite and then decreased at higher loading whereas the tensile modulus was increased gradually with increasing of ferrite loading. Scanning electron microscopy (SEM) was used to determine the wettability of filler in rubber matrix. From the observation, the increase of filler loading reduced the wettability of the filler. Thermal stability of the composites was conducted by using a thermogravimetry analyser (TGA). The incorporation of ferrite in NR composites enhanced the thermal stability of NR composites. The swelling test results indicate that the swelling percentage of the composites decreased by increasing of ferrite loading. The initial permeability, μi and quality factor, Q of magnetic properties of NR composites achieved maximum value at 60 phr of ferrite loading for frequency range between 5000–40,000 kHz. The maximum impedance, Z max of the NR composites was at the highest value at 80 phr ferrite loading for frequency range between 200–800 MHz.  相似文献   

8.
3-Octanoylthio-1-propyltriethoxysilane (a new silane) grafted styrene butadiene rubber/ silica composites were prepared in the present work, where grafting weight percentage of the base rubber (0%, 2%, 4%, and 6%) and filler content of the composites (0, 5, 15, 35, and 50 phr) were varied to investigate dispersion of the filler in the rubber. A detailed quantitative study of morphology-physical property relationship of the composites using dispersion degree parameter was carried out. Pronounced improvement of dispersion was observed with increasing grafting weight percentage of the base rubber. A mechanism of polymer to filler interaction was shown by Fourier transform infrared spectroscopy. The dispersion rate constant from the torque-time curve increased with the grafting percentage. Bound rubber content and Payne effect measurement indicated improved rubber-filler interaction for the grafted rubber compound. A relation between low strain modulus of the composites and grafting percentage was proposed. The nanoindentation studies gave further insight into the results. Other physico-mechanical properties at different grafting weight percentages at particular filler loading (50 phr) and at different filler loadings at a particular grafting weight percentage (4%) were evaluated. The improved mechanical and dynamic mechanical properties with increasing grafting weight percentage are an indication that this methodology could be used in green tire application.  相似文献   

9.
The fluorine rubber nanocomposites were prepared by using the silane‐coupling agents treated silica and diatomite, in which 3‐amino propyltriethoxysilane (KH550), 3‐mercapto‐propyl trimethoxysilane (KH590), and bis‐(γ‐triethoxysilylpropyl)‐tetrasulfide (Si69) of the coupling agent were used as the filler modifiers to increase the compatibility between filler and fluorine rubber. The structure and morphology of the composites were investigated by Fourier transform infrared spectroscopy and scanning electron microscopy. The Tg and thermal stability of the composites were investigated by dynamic mechanical analysis and thermogravimetric analysis. The results showed that the best coupling agent was KH550 and 2 phr (parts per hundred rubber). The KH550‐modified compound filler was crosslinked with fluorine rubber, and the compatibility between filler and fluorine rubber was improved and further confirmed to improve the thermal properties of fluorine rubber with the KH550‐modified filler. J. VINYL ADDIT. TECHNOL., 26:55–61, 2020. © 2019 Society of Plastics Engineers  相似文献   

10.
The grafting of poly(2-hydroxyethyl acrylate) onto natural rubber (NR-g-PHEA) was used to compatibilize NR composites with silica filler. The NR/silica compounds were prepared with various grafting percentages of NR-g-PHEA (0, 6.5, 10.5, and 14.5%) and fixed amounts of 3 parts per hundred of rubber (phr) NR-g-PHEA and 20 phr silica. The cure characteristics were examined using a moving die rheometer. The physicomechanical properties of NR/silica composites were determined in terms of tensile strength, bound rubber content, and dynamic mechanical analysis. Thermal properties were assessed with thermogravimetric analysis. The results showed that scorch time and cure time tend to decrease with the level of grafting in NR-g-PHEA. The NR-g-PHEA decreased tan δ, whereas bound rubber content in NR/silica compounds increased, which indicates improved silica dispersion in the NR matrix. The mechanical properties improved with level of grafting in NR-g-PHEA. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2020 , 137, 48738.  相似文献   

11.
The dispersion of filler and interfacial interaction are crucial in determining the properties of rubber composites. Aiming to improve the dispersion and filler–rubber interaction, we introduce rubber graft bearing oniums in a rubber/silica composite. To fulfill this goal, the graft, which is prepared via thio-ene click reaction between 1-methylimidazolium mercaptopropionate (MMP) and the pendent vinyl groups of a solution-polymerized styrene-butadiene rubber (SSBR), is introduced into the silica-filled styrene-butadiene rubber (SBR) composite. The dispersion of silica and interfacial interaction are improved via hydrogen bonding interaction. Moreover, the graft exhibits catalytic effect toward the silanization, which can improve interfacial interaction in the composites with bis [3-(triethoxysilyl) propyl] tetrasulfide. With 2 phr of the graft, the tensile modulus (stress at 300% strain) is increased by 18% and the abrasion loss is decreased by 31%. This study opens a new attempt to improve the filler dispersion and filler–rubber interaction in the composites with onium-bearing polymers. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019 , 136, 48243.  相似文献   

12.
Styrene–butadiene rubber (SBR) composites filled with hemp hurd powder (HP) were prepared with bis(3‐triethoxysilylpropyl) tetrasulfide (Si69) as a coupling agent. The effects of the filler content and coupling agent on the curing characteristics and dynamic mechanical properties of the composites were studied. The results indicate that with increasing filler loading, the torque values increased and the curing time decreased. The mechanical properties improved with increasing filled HP content up to 60 phr. Usually, long fibers led to a sharp decrease in the toughness of the composites, whereas short fibers, such as HP, had a positive effect on the elongation at break within the loading range studied. The extent of the filler–matrix interaction and the scanning electron micrographs of the fractured surfaces confirmed that the addition of Si69 improved the interfacial interaction between HP and the SBR matrix, which led to an increase in the maximum torque and the mechanical properties. Moreover, the coupling agent was helpful in dispersing the filler in the rubber matrix. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

13.
New technology is constantly required for updating new generation flexible devices, such as stretchable sensors, flexible electronics, and actuators. In the present study, a stretchable strain sensor, and actuator were developed based on room-temperature-vulcanized (RTV) silicone rubber reinforced with carbon nanotubes (CNTs), nanographite (GR), and CNT-GR hybrids. A CNT-based strain sensor developed for RTV silicone rubber showed improved stiffness and brittleness. For example, at 5 phr of filler loading, the compressive and tensile modulus for the CNT-reinforced RTV silicone matrix improved by 287% and 240%, respectively. Similarly, the improvements in the compressive and tensile modulus were moderate for the CNT-GR hybrid (210% and 235%) and low for GR (135% and 125%). The improved brittleness resulted in a higher fracture strain of 170% and 155% for the CNT-GR hybrid and GR, respectively. The improved mechanical properties were tested in real-life applications of actuation. The actuation displacement at a filler loading of 2 phr increased to 1.65 mm (CNT), 1.25 mm (CNT-GR), and 0.08 mm (GR). From 2 to 8 kV, the actuation displacement increased by 825% (CNT), 830% (CNT-GR), and 32% (GR). The strain sensor showed a stretchability of >100% (CNT) and >100% (CNT-GR). In addition, the gauge factor was higher for the CNT-GR hybrid composites. The durability measurements showed that the change in resistance was negligible for up to 5000 cycles in both the CNT and CNT-GR rubber composites. A series of experiments confirmed that compared to the composite based on RTV silicone rubber and CNT, the CNT-GR hybrid showed a robust flexibility and stretchability as a piezo-resistive strain sensor and actuator.  相似文献   

14.
Vulcanized composites of chloroprene rubber (CR) with cellulose II (Cel II) as a filler were investigated. Cel II, obtained by the coagulation of cellulose xanthate, was incorporated in the rubber by the traditional method. The filler content varied from 0 to 30 phr. For comparison purposes, carbon black (CB)–CR composites were also studied. The CB amount varied from 0 to 45 phr. The mechanical and dynamic mechanical properties were determined, and the CR composite containing 20 phr of Cel II showed the best set of properties. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 2425–2430, 2004  相似文献   

15.
Natural rubber (NR) vulcanizates exhibit good mechanical properties compared to vulcanizates of synthetic rubbers. Incorporation of a conventional filler at higher loadings to NR enhances its modulus, while reduction in tensile strength and elongation. This paper presents a new strategy for development of a NR‐clay nanocomposite with enhanced mechanical properties by incorporation of lower loadings (2–8 phr) of cetyl trimethyl ammonium bromide modified montmorillonite clay (OMMT‐C) under acid‐free environment. The effect of OMMT‐C loading on cure characteristics, rubber‐filler interactions, crosslink density, dynamic mechanical thermal properties, and mechanical properties were evaluated. Incorporation of OMMT‐C accelerated the vulcanization process and enhanced mechanical properties. X‐ray diffraction analysis and scanning electron microscopy images revealed that the formation of intercalated clay structures at lower OMMT‐C loadings, and clay aggregates at higher loadings. A nanocomposite at OMMT‐C loading of 2 phr exhibited the best balanced mechanical properties, and was associated with highest crosslink density and rubber–filler interactions. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018 , 135, 46502.  相似文献   

16.
Bio‐waste materials such as eggshell (ES) and fishbone (FB) were used as new fillers compared with commercial calcium carbonate (CC) in natural rubber composite. The effect of their presence in the rubber mix on the rheometric study, morphology, mechanical properties, hardness, and abrasion resistance has been investigated at constant filler content (30 phr). The filler and their composites were characterized by Fourier‐transform infrared, X‐ray diffraction, thermogravimetric analysis, and scanning electron microscope (SEM). The results showed that the cure time and scorch time of the composites filled with CC and ES are lower than the composites filled FB filler. On the other hand, composites with ES and CC showed enhanced values of tensile, modulus at 100% and 300% elongation, hardness, and abrasion resistance. The morphological data revealed that CC and ES fillers are better dispersed in the rubber matrix than FB filler. J. VINYL ADDIT. TECHNOL., 26:309–315, 2020. © 2019 Society of Plastics Engineers  相似文献   

17.
Natural rubber is one of the most potential electro-active polymers for sensors, actuators, and energy harvesting applications. Enhancing the characteristic properties of polymers by reinforcing with fillers that possess multifunctional attributes have attracted considerable attention. In the present study, barium titanate reinforced natural rubber composite is prepared by using two-roll mill mixing. Afterwards, mechanical, electrical, and electromechanical properties of the composites are extensively analyzed by reinforcing different amounts of barium titanate into the matrix of natural rubber. The fabricated dielectric composite shows excellent properties such as high dielectric constant, low dielectric losses, high dielectric breakdown strength, and extreme stretchability. It is observed that as the filler loading reaches the value of 11 parts per hundred rubber (phr), maximum agglomeration of the particles occurs. Maximum stretchability and highest ratio of dielectric constant to elastic modulus are obtained at 8 phr of barium titanate fillers and at the loading, a maximum actuation strain of 11.24% is achieved. This study provides a simple, economical, and effective method for preparing enhanced mechanical, electrical, and electromechanical properties of natural rubber composites, facilitating the wide applications of dielectric materials as actuators and generators.  相似文献   

18.
《Polymer Composites》2017,38(5):870-876
Thermally conductive fillers are usually employed in the preparation of rubber composites to enhance thermal conductivity. In this work, ethylene‐propylene‐diene monomer rubber (EPDM)/expanded graphite (EG) and EPDM/graphite composites with up to 100 phr filler loading were prepared. Compared to EPDM/graphite compounds with the same filler loading, stronger filler network was demonstrated for EPDM/EG compounds. Thermal conductivity and mechanical properties of EPDM/graphite and EPDM/EG composites were compared and systematically investigated as a function of the filler loading. The thermal conductivity of both EPDM/graphite and EPDM/EG composites increased with increasing volume fraction of fillers, and could be well fitted by Geometric Mean Model. The thermal conductivity as high as 0.910 W · m−1 · K−1 was achieved for the EPDM/EG composite with 25.8 vol% EG, which was ∼4.5 times that of unfilled EPDM. Compared to EPDM/graphite composites, EPDM/EG composites exhibited much more significant improvement in thermal conductivity and mechanical properties, which could be well correlated with the better filler‐matrix interfacial compatibility and denser structure in EPDM/EG composites, as revealed in the SEM images of tensile fracture surfaces. POLYM. COMPOS., 38:870–876, 2017. © 2015 Society of Plastics Engineers  相似文献   

19.
Curing characteristics, tensile properties, morphological studies of tensile fractured surfaces using scanning electron microscopy (SEM), and the extent of rubber filler interactions of rattan‐powder‐filled natural rubber (NR) composites were investigated as a function of filler loading and silane coupling agent (CA). NR composites were prepared by the incorporation of rattan powder at filler loading range of 0–30 phr into a NR matrix with a laboratory size two roll mill. The results indicate that in the presence of silane CA, scorch time (ts2), and cure time (t90) of rattan‐powder‐filled NR composites were shorten, while, maximum torque (MH) increased compared with NR composites without silane CA. Tensile strength and tensile modulus of composites were enhanced whereas elongation at break reduced in the presence of silane CA mainly due to increase in rubber‐filler interaction. It is proven by SEM studies that the bonding between the filler and rubber matrix has improved. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012  相似文献   

20.
Biocomposites of styrene butadiene rubber (SBR) reinforced with silane-treated peanut shell powder (SPSP) of different filler loadings and particle sizes were prepared by two roll mixing mills with sulfur as a vulcanizing agent. The cure characteristics of composites were studied, and they vulcanized at 160 °C. Test samples were prepared by compression moulding, and their physicomechanical properties, such as tensile strength tear strength, modulus, hardness, and abrasion resistance of SBR vulcanizates, were studied with filler loading 0, 5, 10, 15, and 20 parts per hundred rubber (phr). Composites with 10 phr filler having small particle size exhibited better properties. The interfacial adhesion between filler and matrix has a major role in the properties of composites. Surface modification of PSP was done by silane coupling agent to improve the interfacial adhesion and it characterised by FTIR, XRD, TGA, UV, and SEM. Better properties are shown by the composites with SPSP. Thermal stability of the composites was also determined using thermogravimetric analysis.  相似文献   