1.
抑制剂W—98在翁福磷矿反浮选中的选矿研究   总被引:3,自引:0,他引:3  
根据公司福磷矿的性质,采用反浮选工艺处理胶磷矿,用反浮选高效抑制剂W-98作为磷矿的抑制剂,来抑制磷矿物而浮白云石等脉石,从原矿P2O5品位为27.33%,MgO为6.19%中,获得了磷精矿P2O5品位为37.34%,MgO为0.73%,回收率92.39%的选矿指标。  相似文献   

2.
远安低品位胶磷矿浮选试验研究   总被引:3,自引:0,他引:3  
确定了远安低品位胶磷矿的正-反浮选流程,通过正-反浮选,可获得原矿P2O517.96%,MgO 2.31%,精矿P2O531.21%,MgO 0.84%的良好指标,实现了胶磷矿与石英、白云石等杂质矿物的有效分离。采用十二烷基磺酸钠(SDS)作增效剂可以较大程度提高捕收剂的捕收性能和选择性,提高P2O5品位和回收率。  相似文献   

3.
采用旋流-静态微泡浮选柱对某胶磷矿进行了半工业试验研究,在原矿品位为23.73%P2O5的情况下通过正-反浮选流程获得了精矿P2O5品位29.78%、MgO品位0.29%,回收率82.69%的良好指标,缩短了流程结构.为浮选柱技术的工业应用进行了积极探索.  相似文献   

4.
钙硅质胶磷矿浮选工艺研究   总被引:1,自引:0,他引:1  
针对湖北某中低品位钙硅质胶磷矿,分别进行单一反浮选、双反浮选和常温正反浮选工艺研究及药剂费用对比,结果表明:采用单一反浮选,可得到磷精矿P2O5 30.37%,MgO 0.36%,回收率88.38%的较好指标,且最为经济,每吨原矿药剂费用仅为15.28元;若希望精矿质量更好些,回收率更高些,建议采用双反浮选,可得到磷精矿P2O5 31.60%,MgO 0.43%,回收率90.63%的好指标,每吨原矿药剂费用为23.40元;正反浮选相对来说精矿质量一般、回收率较低、药剂费用较高、磨矿细度较细,指标分别为磷精矿P2O5 30.54%,MgO0.70%,回收率84.62%,每吨原矿药剂费用为26.98元.  相似文献   

5.
以大豆油酸化油为原料,经磺化、皂化等单元反应合成了α-磺酸基油酸皂浮选捕收剂,用于四川某中低品位胶磷矿的浮选试验.结果表明,该捕收剂实现了胶磷矿与白云石的有效分离,入选原矿P2O5品位23.80%,MgO质量分数6.54%;获得磷精矿P2O5品位33.88%,回收率85.37%,MgO含量1.50%.  相似文献   

6.
对宜昌丁东磷矿进行重介质选矿+正—反浮选试验与原矿直接进行正—反浮选试验研究,结果表明,分离密度为2.70时,只抛去17.35%的尾矿,量太少,仍需与正—反浮选联合使用,才能保证精矿品位P2O530%以上,回收率80%以上,MgO低于0.8%的磷精矿指标;而原矿直接进行正—反浮选流程(一粗一精一扫正浮选和一粗一扫反浮选),在不加温条件下,原矿P2O516.83%时,闭路试验可获得P2O531.49%,回收率83.75%,MgO 0.52%,选矿比为2.28的优良指标.可见,宜昌磷矿更适于采用直接正—反浮选流程,从而保证资源的经济、合理、有效利用.  相似文献   

7.
采用反浮选法以油酸盐和烷基胺盐为捕收剂分别除去细粒径磷矿中的碳酸盐和硅质脉石以提高矿石的品位。结果表明:不管是对油酸盐反浮选捕收方解石,还是胺盐反浮选捕收硅石,增加体系的酸性都有利于提高矿石的品位,还能明显提高前者的P2O5回收率。增加捕收剂用量同样可提高矿石品位,但却减少了P2O5回收率。对于2种反浮选过程较适宜的捕收剂用量为0.5 kg/t。抑制剂的添加有利于提高2种反浮选的效果,优化后的抑制剂用量为3.5kg/t。  相似文献   

8.
针对湖北某中低品位钙硅质胶磷矿,分别进行单一反浮选、双反浮选和常温正反浮选工艺研究及药剂费用对比,结果表明:采用单一反浮选,可得到磷精矿P2O530.37%,MgO 0.36%,回收率88.38%的较好指标,且最为经济,每吨原矿药剂费用仅为15.28元;若希望精矿质量更好些,回收率更高些,建议采用双反浮选,可得到磷精矿P2O531.60%,MgO 0.43%,回收率90.63%的好指标,每吨原矿药剂费用为23.40元;正反浮选相对来说精矿质量一般、回收率较低、药剂费用较高、磨矿细度较细,指标分别为磷精矿P2O530.54%,MgO 0.70%,回收率84.62%,每吨原矿药剂费用为26.98元.  相似文献   

9.
脱泥-浮选工艺是针对矿石品位下降,矿物共生关系复杂,回收率低等一系列问题提出来的一整套关于磨矿、浮选的有效解决手段,其特点是:合理利用流程设备,降低能耗及药耗.晋宁中低品位胶磷矿通过该工艺,试验获得P2O5品位为30.92%,MgO为0.18%,R2O3含量为1.73%5回收率为69.16%的优质磷精矿.  相似文献   

10.
某磷矿属海相沉积型磷块岩矿床,磷酸盐矿物主要为泥晶磷灰石(俗称胶磷矿),脉石矿物主要为白云石、石英和粘土矿物,属较难选别磷块岩.本研究依据该胶磷矿的矿石性质,采用重液浮沉—反浮选联合工艺流程,得到磷精矿品位P2O531%以上,MgO 1%左右,回收率88%以上的精矿产品.  相似文献   

11.
利用磷酸分解中低品位磷矿生产湿法磷酸.通过湿法磷酸与有机碱形成复合物沉淀,实现了磷酸与杂质离子的高效分离,从而得到工业级磷酸二铵.本工艺使中低品位磷矿能得到高效利用,为工业磷酸及其磷酸盐的生产提供了一种有效的方法.  相似文献   

12.
采用直接酯化法,以多聚磷酸和脂肪醇醚为原料合成了高含量单醇醚磷酸酯,并设计正交实验考察了合成工艺条件对单酯含量和醇醚转化率的影响;研究了不同单酯含量、p H值和含油率对芳砜纶纤维的抗静电性影响,并利用环境扫描电子显微镜和扫描隧道显微镜对醚磷酸酯钾盐浸丝处理后的芳砜纶纤维表面形貌特征进行了表征.结果表明:醇醚和多聚磷酸酯化反应的最优化条件为投料比3∶1,反应温度80℃,反应时间4h,此时磷酸酯产品中单酯质量分数为91.8%,醇醚转化率为95%;磷酸酯钾盐的单酯含量和纤维表面的含油率比磷酸酯钾盐的p H值对芳砜纶纤维的抗静电性能影响大,综合考虑,纤维最佳含油率为0.3%,磷酸酯钾盐单酯含量越高,纤维的抗静电性能越好.  相似文献   

13.
14.
The phosphate solubilizing characteristics of a strain YC, which was isolated from phosphate mines (Hubei, China), were studied in National Botanical Research Institute’s phosphate (NBRIP) growth medium containing tricalcium phosphate (TCP) as sole phosphorus (P) source. The strain YC is identified as Stenotrophomonas maltophilia (S. maltophilia) based upon the results of morphologic, physiological and biochemical characteristics and 16S rRNA sequences analysis. The results show that the strain S. maltophilia YC can solubilize TCP and release soluble P in NBRIP growth medium. A positive correlation between concentration of soluble P and population of the isolate and a negative correlation between concentration of soluble P and pH in the culture medium are observed from statistical analysis results. Moreover, gluconic acid is detected in the culture medium by HPLC analysis. It indicates that the isolate can release gluconic acid during the solubilizing experiment, which causes acidification of the culture medium and then TCP solubilization. S. maltophilia YC has a maximal TCP solubilizing capability when using maltose as carbon source and ammonium nitrate as nitrogen source, respectively, in NBRIP growth medium. Foundation item: Project(2004CB619201) supported by the Major State Basic Research and Development Program of China; Project(Z200515002) supported by the Key Project Foundation of the Education Department of Hubei Province, China; Project(GCP200801) supported by the Open Research Fund of Key Laboratory for Green Chemical Process of Ministry of Education, China; Project(Q200811) supported by the Youths Science Foundation of Wuhan Institute of Technology, China  相似文献   

15.
聚醚/磷酸酯改性聚硅氧烷的合成   总被引:3,自引:0,他引:3  
以聚醚改性聚硅氧烷与五氧化二磷为主要原料,通过酯化反应和水解反应制备了有效物浓度达8000的液态聚醚/磷酸酯改性聚硅氧烷,并总结出较好的酯化反应条件为:投料比2.5∶1,一次性投料,在80℃下反应4h;水解反应条件是:温度为80℃,时间为2h.  相似文献   

16.
17.
我国磷矿资源丰富,但大多为中低品位沉积型磷块岩,选别难度大. 浮选是磷矿选矿中最主要的分选方法,浮选药剂对浮选指标有着至关重要的影响. 浮选药剂按照所起作用不同分为调整剂、捕收剂、起泡剂三类. 结合近年文献资料分析,发现传统捕收剂存在溶解性差、选择性不强等缺点,提出利用不同药剂分子间协同作用及提高药剂的活性,采用复配及合成方法研发高效低毒、水溶性好、选择性强的抑制剂和捕收剂是实现我国难选性磷矿中与脉石矿物分离的有效途径.  相似文献   

18.
磷酸钛在无机离子交换剂和聚阴离子型锂电池正极材料等领域有着重要应用.随着纳米及多孔材料的发展,各种形貌和结构的磷酸钛合成方法相继报道并逐渐引起人们的广泛兴趣.本文总结国内外关于磷酸钛的合成研究报道,概括地介绍了几种磷酸钛的合成方法,并对磷酸钛在合成和应用领域中存在的问题及研究方向做了简要论述.  相似文献   

19.
研究了富磷培养基中胶质红假单胞菌的摄磷能力以及光照、pH、外加碳源和缺磷环境对胶质红假单胞菌摄磷能力的影响。结果表明,该菌在富磷培养基中具有较强的摄磷能力,在光照、微好氧条件下有较好的摄磷能力,其生长的最适pH在7.2左右,缺磷环境可导致该菌的过量摄磷现象发生。  相似文献   