Bio‐inspired layered ceramic‐polymer composites with high strength and toughness were prepared from sintered aluminum oxide ceramic sheets and cationically curing epoxy resins toughened with poly(ε‐caprolactone) (PCL). The architecture of the composite is inspired by nacre but is arranged on a larger scale. Ceramic sheets with a nominal thickness of 250 μm were assembled into composite plates by adhesive layers with a nominal thickness of 20 μm. Before the manufacturing of the composites, the stress‐strain properties of the polymer component were tailored by the variation in the PCL content between 0 and 39 wt%. For composites with 4 and 15 ceramic layers, the bending strengths achieved 327 MPa and 376 MPa, which are higher than that of pure ceramic sheets. Moreover, composites with 15 ceramic layers show a 16 times higher toughness compared to that of the pure ceramic sheets. The results indicate that the toughness of the layered composites increases significantly with the number of layers. Inspired by the geometrical ratio of the natural sheet composite nacre, we have achieved a similar strength but a 2 times higher toughness than nacre by only adding up to 6 vol% of the polymer.  相似文献   

2.
In this study, the effects of mixed‐acid oxidation on the contents of surface elements, morphology, fiber fineness, mechanical properties, mass change rate, chemical structure, and microaggregate structure of dry‐spun Suplon polyimide (PI) fibers were systematically investigated with wet chemical treatment with HNO3/H2SO4. Experiments investigating both the improvement in the O/C ratio of the fiber surface elements and the changes in other performance features were conducted through the functional modification of the fibers. Meanwhile, the causes of specific changes in the mechanical properties of the oxidized PI‐fiber‐reinforced polypropylene‐resin‐based composites were studied and are discussed. The results of this study demonstrate that the treatment of the fibers with HNO3/H2SO4 mixed‐acid oxidation resulted in significant changes in the properties of the fibers; these changes included an uneven surface, increased specific surface area and surface roughness, a locally etched surface, increased surface energy and O/C ratio, an enhanced wettability, an increased fiber fineness, reduced mechanical properties, and a mass gain in the fibers. Although the chemical structures of the fibers treated by oxidized HNO3/H2SO4 were not significantly changed compared to those of the untreated fibers, the microscopic aggregation of the treated fibers changed to some degree, and the ratio of the amorphous regions significantly increased. Taken together, the functional modification of the PI fiber surface was achieved efficiently through the use of a suitable HNO3/H2SO4 oxidation process and with other performance features of the fibers taken into account. This was favorable for the enhancement of the interfacial properties of the polypropylene fibers and the matrix resins, and thus, the modification improved the mechanical properties of the composites. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017 , 134, 44932.  相似文献   

3.
A dual‐curable epoxyacrylate (EA) oligomer with one epoxide group and one vinyl group at each end was synthesized for the application as adhesive sealant in the liquid crystal display panels. However, after UV and thermal cure, the EA resin was brittle with a poor resistance to crack initiation and propagation. Liquid rubbers with different functional end groups were thus tried as toughening agents for the EA resin. Among all the rubber‐toughened EAs, the EA‐V5A5 added with vinyl‐terminated and amino‐terminated butadiene‐acrylonitrile copolymers (VTBN and ATBN) each at 5 phr had the highest fracture toughness, tensile strength, and elongation at break but a lower initial modulus. To raise the modulus, submicron‐sized silica particles (∼170 nm) with surface vinyl functional groups were further added to the EA‐V5A5 to prepare the hybrid composites. Because of interfacial chemical bonding provided by the surface vinyl functional groups, both modulus and fracture toughness were increased by adding silica particles, without any appreciable decrease in extensibility. For the hybrid composite at 20 phr silica particles, the initial modulus, fracture toughness, and fracture energy were raised by 10.3, 100, and 267%, respectively, when compared to the neat epoxyacrylate. Owing to their strong interfacial bonding, the increase of fracture toughness was mainly due to the crack deflection and bifurcation on silica particles, in addition to the rubber particle bridging and tearing as evidenced by SEM pictures on the fracture surface. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015 , 132, 41820.  相似文献   

4.
This research work investigates the tensile strength and elastic modulus of the alumina nanoparticles, glass fiber, and carbon fiber reinforced epoxy composites. The first type composites were made by adding 1–5 wt % (in the interval of 1%) of alumina to the epoxy matrix, whereas the second and third categories of composites were made by adding 1–5 wt % short glass, carbon fibers to the matrix. A fourth type of composite has also been synthesized by incorporating both alumina particles (2 wt %) and fibers to the epoxy. Results showed that the longitudinal modulus has significantly improved because of the filler additions. Both tensile strength and modulus are further better for hybrid composites consisting both alumina particles and glass fibers or carbon fibers. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014 , 131, 39749.  相似文献   

5.
This study focuses on the performance characteristics of wood/short carbon fiber hybrid biopolyamide11 (PA11) composites. The composites were produced by melt‐compounding of the fibers with the polyamide via extrusion and injection molding. The results showed that mechanical properties, such as tensile and flexural strength and modulus of the wood fiber composites were significantly higher than the PA11 and hybridization with carbon fiber further enhanced the performance properties, as well as the thermal resistance of the composites. Compared to wood fiber composites (30% wood fiber), hybridization with carbon fiber (10% wood fiber and 20% carbon fiber) increased the tensile and flexural modulus by 168% and 142%, respectively. Izod impact strength of the hybrid composites exhibited a good improvement compared to wood fiber composites. Thermal properties and resistance to water absorption of the composites were improved by hybridization with carbon fiber. In overall, the study indicated that the developed hybrid composites are promising candidates for high performance applications, where high stiffness and thermal resistance are required. © 2016 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016 , 133, 43595.  相似文献   

6.
The effect of basalt fibre sizing on the mechanical and interphase properties of fibre‐reinforced composites was studied. Two different chemical preparations of the fibre surface (PBT‐compliant and PP‐compliant) were used. The polymer matrix was prepared from polypropylene/poly(butylene terephthalate) (PP/PBT) immiscible polymer blend and the effect of different compatibilizers on the composite properties was evaluated. SEM hints at improved fibre adhesion to the polymer matrix when a PP‐compliant sizing is applied. SEM also reveals improved compatibilization effects when block copolymer instead of multiblock copolymer is used for the PP/PBT blend preparation. The pull‐out test was applied to quantitatively evaluate the interface adhesion between the fibres and matrices. It showed a high value of the interfacial shear strength between basalt fibres modified with PP‐compliant sizing and polymer blend compatibilized by block copolymer, thus confirming good adhesion. One possible explanation of such good mechanical properties can be related to the chemical interactions between functional groups, mainly maleic anhydride on basalt fibres and the polyolefin component (PP) of the polymer matrix. © 2017 Society of Chemical Industry  相似文献   

7.
Nano‐/microcomposites based on polypropylene/montmorillonite/calcium carbonate were prepared by melt mixing. Their structures and properties were characterized by small‐angle X‐ray diffraction, thermal analysis, and rheological measurements. The intercalation degree was found to be dependent on the compatibilizer content and the processing temperature. The addition of the organoclay slightly increased the melt crystallization temperature of polypropylene, acting as nucleating agents, and improved the degree of crystallinity. The rheological tests showed that nanocomposites increased the complex viscosity when compared with the microcomposites with the same filler content and exhibited a pronounced shear‐thinning behavior in the low frequency range. A Carreau‐Yasuda model was used to model the rheological behavior of these materials. The nano‐/microcomposites showed a significant improvement (about 50%) of the Young's modulus when compared with microcomposites with the same filler content due to the intercalation or exfoliation of the organoclay and the enhanced degree of crystallinity. Moreover, some formulations showed an enhancement of elongation at break and ultimate strength. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

8.
Composites based on phenolic matrices and both untreated and alkali and ionized air–treated jute fibers were prepared. Different fiber lengths and fiber content were used to reinforce the phenolic matrices. The jute fibers were characterized with respect to lignin, holocellulose, ash, and humidity contents and also to the crystallinity index. The mechanical properties of fibers were investigated by means of tensile analysis and the morphology by SEM. The untreated and treated jute fiber–reinforced composites were characterized as to water absorption. The mechanical property and morphological aspects of the composites were evaluated by impact strength and photomicrographs obtained from SEM. Among the jute fiber treatments considered in the present work, the treatment with a solution of 5% NaOH presented the best results because: (1) the fiber presented a higher tensile strength, and a larger percentage of elongation at break; (2) the composite reinforced with this fiber presented the highest impact strength results when this was the unique treatment (20% of fiber), as well as when it was combined with ionized air (30% of fiber); and (3) the composite that presented the lowest water uptake was that reinforced with this fiber. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 1077–1085, 2004  相似文献   

9.
Hybrid composites based on bisphenol‐C‐formaldehyde resin and jute mat with rice, wheat, sugar cane, and jamun husks have been fabricated at 150°C under 30.4 MPa pressure for 2 h. The resin content in composites was 50% of fibers. Tensile strength, flexural strength, electric strength, and volume resistivity of hybrid composites have been evaluated and compared with those of jute‐bisphenol‐C‐formaldehyde composites. It is observed that the tensile strength of composites is found to decrease by 53–72%, which is mainly due to random orientation of sandwiched fibers. Flexural strength has increased by 53–153% except jute–rice husk composite for which it is decreased by 26%. A little change in dielectric breakdown strength (1.89–2.11 kV/mm) is found but volume resistivity of Jute–wheat husk and Jute–jamun husk composites has improved by 437–197% and it is slightly decreased(2.3–25.2%) for the remaining two composites. Thus, hybrid composites possess good mechanical and electrical properties signifying their importance in low strength and light weight engineering applications as well as low cost housing units such as partition and hard boards. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1754–1758, 2006  相似文献   

10.
Natural rubber was reinforced with untreated sisal and oil palm fibers chopped to different fiber lengths. The influence of fiber length on the mechanical properties of the hybrid composites was determined. Increasing the fiber length resulted in a decrease in the properties. The effects of concentration on the rubber composites reinforced with sisal/oil palm hybrid fibers were studied. Increasing the concentration of fibers resulted in a reduction in the tensile strength properties and tear strength but an increase in the modulus of the composites. Fiber breakage analysis was evaluated. The vulcanization parameters, processability characteristics, and stress–strain properties of these composites were analyzed. The extent of fiber alignment and the strength of the fiber–rubber interface adhesion were analyzed from the anisotropic swelling measurements. Scanning electron microscopy studies were performed to analyze the fiber/matrix interactions. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 93: 2305–2312, 2004  相似文献   

11.
In this investigation, the influence of filler type and filler content on the mechanical properties of nylon‐6 is investigated. The mineral fillers were selected on the basis of their shape and size: flake‐like kaolin and talc, spherical glass beads or fibrous wollastonite. These fillers were added to nylon‐6 individually or in mixed combinations. They were added at different percentages varying between 10 and 30% w/w. Samples of the composites were prepared by the injection moulding process. Uniaxial tensile, Izod impact and flexural tests were carried out. Tensile strength, elongation at break, modulus of elasticity and impact energy were obtained and compared. In case of single fillers the results showed that the tensile strength, modulus of elasticity and their flexural values for nylon‐6 composite improve with the increase in filler content while mixed compounds showed no significant changes above 15% + 15% w/w filler. However, for single and mixed filler up to 10% w/w, the impact strength and maximum elongation at break showed significant decrease. In general, the maximum improvement in mechanical the addition of 10–15% w/w filler. Copyright © 2003 Society of Chemical Industry  相似文献   

12.
Lignocellulosic materials can be used for the development of bio‐based composites. This study explores the potential of long bamboo fiber bundles extracted directly from bamboo stems using the novel mechanical method and bamboo‐based fiber composites (BFC) fabricated using long bamboo fiber bundles and phenolic resins via cold pressing and thermal cure process. The microstructure, mechanical properties, and durability of BFC were evaluated, results being compared with raw bamboo and other commercialized bamboo fiber composites. The mechanical properties of BFC reinforced with 87% (w/w) long bamboo fiber bundles increased more than 50% than those of raw bamboo and were significantly higher than those of other bamboo‐based composites. Lower water absorption and thickness swelling were obtained in the case where bamboo fiber bundles with the small fineness. Higher tensile strength was obtained in the case where bamboo fiber bundles with large sizes of bamboo fiber bundles. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014 , 131, 40371.  相似文献   

13.
Hollow microspheres (HM) of ceramic, silica, and glass‐filled silicone rubber (SR) composites were prepared, and the effects of hybrid HM on thermal and mechanical properties of composites were investigated. The results indicate that hybrid HM can effectively improve the thermal insulation property of HM/SR composites. Especially, for sample 15S, the thermal conductivity and thermal degradation temperature reached 0.1273 W/m K and 521 °C (45 °C higher than that of neat SR), respectively. Besides, thermal insulation performance was improved, showing as a temperature of 103.2 °C after 15 min heating, which is 37.8 °C lower than that of SR. The tensile strength of composites was enhanced from 1.92 MPa at 11.56 vol % hollow silica microspheres (HSM) loading to 3.08 MPa at 21.88 vol % HSM loading. Moreover, the compressive strength was improved from 3.33 to 5.68 MPa by introducing more hollow ceramic microspheres into the matrix, in this case, from 7.79 to 15.33 vol %. Furthermore, the failure mechanism was analyzed. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018 , 135, 46025.  相似文献   

14.
Composites consisting of a conjugated linseed or soybean oil‐based thermoset reinforced with wood flour and wood fibers have been prepared by free radical polymerization. The thermoset resin consists of a copolymer of conjugated linseed oil (CLO) or conjugated soybean oil (CSO), n‐butyl methacrylate (BMA), divinylbenzene (DVB), and maleic anhydride (MA). The composites were cured at 180°C and 600 psi and postcured for 2 h at 200°C under atmospheric pressure. The effect of varying filler load, time of cure, filler particle size, origin of the fillers, and resin composition has been assessed by means of tensile tests, DMA, TGA, Soxhlet extraction followed by 1H‐NMR spectroscopic analysis of the extracts, and DSC. The best processing conditions have been established for the pine wood flour composites. It has been observed that the addition of MA to the resin composition improves the filler‐resin interaction. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012  相似文献   

15.
This study was conducted due to the necessity for improving the processability of commingled yarns during textile processing, in particular dense 3D preform weaving. Open structure of the commingled yarns caused higher production stops. As a possible solution, GF/PP commingled yarns with different twisting levels were produced. Effect of twisting on the mechanical properties of commingled yarns and on their compression molded UD composites are determined. Further tests were executed about yarn/yarn and yarn/metal friction of twisted commingled yarns, which are important properties during textile processing. Theoretical approaches such as a yarn model with linear bar elements and lamina equation with an equivalent angle distortion of over‐delivery proved useful to relate the structural parameters and mechanical properties. As a result, twisting did not significantly affect the modulus of elasticity of UD‐composites, however, the tensile strength of UD‐composites were reduced by further processing even without twisting. Therefore, small twisting levels can be applied on commingled yarns to improve processability of dense preforms without significantly affecting the mechanical performance. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

16.
In this work, high‐performance multifunctional composites were obtained by melt blending silver deposited tetrapod‐like zinc oxide whiskers (Ag‐ZnOw) with polystyrene (PS). The chemical, spectroscopic, antibacterial, mechanical, and morphological properties of the PS/Ag‐ZnOw composites were carefully investigated and discussed. The obtained PS/Ag‐ZnOw composites characterized remarkable antibacterial activity against Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus). Moreover, it is found that impact strength of the composite increase with increasing nanofiller concentration (up to 0.25 wt %). Morphological characterization of the impact fractured surface of composites revealed that toughening was achieved through uniform filler distribution in the polymer matrix, and anchoring effect was imparted by the tetrapod‐like shape of ZnO whiskers. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014 , 131, 40900.  相似文献   

17.
Short‐glass‐fiber (SGF)‐reinforced polypropylene (PP) composites toughened with a styrene/ethylene butylene/styrene (SEBS) triblock copolymer were injection molded after extrusion. Furthermore, a maleic anhydride (MA)‐grafted SEBS copolymer (SEBS‐g‐MA) was used as an impact modifier and compatibilizer. The effects of the processing conditions and compatibilizer on the microstructure and tensile and impact performance of the hybrid composites were investigated. In the route 1 fabrication process, SGF, PP, and SEBS were blended in an extruder twice, and this was followed by injection molding. In route 2, or the sequential blending process, the elastomer and PP were mixed thoroughly before the addition of SGF. In other words, either PP and SEBS or PP and SEBS‐g‐MA pellets were premixed in an extruder. The produced pellets were then blended with SGF in the extruder, and this was followed by injection molding. The SGF/SEBS‐g‐MA/PP hybrid fabricated by the route 2 process exhibited the highest modulus, yield stress, tensile stress at break, Izod impact energy, and Charpy drop weight impact strength among the composites investigated. This was due to the formation of a homogeneous SEBS elastomeric interlayer at the SGF and matrix interface of the SGF/SEBS‐g‐MA/PP hybrid. This SEBS rubbery layer enhanced the interfacial bonding between SGF and the matrix of the SGF/SEBS‐g‐MA/PP hybrid. The correlations between the processing, microstructure, and properties of the hybrids were investigated. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 88: 1384–1392, 2003  相似文献   

18.
Short ramie fiber (RF) was used to reinforce the polypropylene (PP). The composites were prepared in a twin‐screw extruder followed by injection molding. The experimental results showed that both the strength and the modulus of the composites increase considerably with increasing RF content. The tensile strength and flexural strength are as high as 67 and 80 MPa by the incorporation of ramie up to 30 wt %. To the best of our knowledge, this is one of the best results for short natural fiber‐reinforced PP composites. However, the preparation method in this study is more simple and economic. This short RF‐reinforced PP composites extend the application field for short‐nature fiber‐reinforced PP composites. Morphological analysis revealed that it is the high aspect ratio of the fiber and good interfacial compatibility that result in the high performance of the composites. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

19.
The reinforcement mechanics of viscose‐fiber‐reinforced polypropylene (PP) composites were studied. The effect of the coupling agent, maleated polypropylene (MAPP), was of special interest. The fibers, coupling agent, and PP were extruded and injection‐molded. The composition, mechanical properties, fracture morphology, and dispersion of the composites were examined. Thermogravimetric analysis showed that the fiber content in the tensile specimens varied slightly with the sample location; however, the differences in the values were within 1.0%. Scanning electron microscopy images of the fracture surfaces of the composites showed that the surfaces of the composites without MAPP were covered with fibers pulled out from the matrix. A lack of adhesion further appeared as a cracked matrix–fiber interface. A new scanning thermal microscopy method, microthermal analysis, was used to study the dispersion of the fibers in the composites. Local thermal analyses gave further information about the location of the fibers. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 2676–2684, 2004  相似文献   

20.
Multiwalled carbon nanotube (MWCNT)‐welded carbon fibers (CFs) were prepared by a three‐step process, which included polyacrylonitrile (PAN) coating, MWCNT absorption, and heat treatment. The structure of these materials was characterized by scanning electron microscopy, Fourier‐transform infrared spectroscopy, and Raman spectroscopy. The MWCNTs were uniformly assembled on the surface of the PAN‐coated CFs and welded by a PAN‐based carbon layer after heat treatment. The contact angle of the MWCNT‐welded CFs in the epoxy resins was 41.70°; this was 22.35% smaller than that of the unsized CFs. The interfacial shear strength (IFSS) of the MWCNT‐welded CF–epoxy composite was 83.15 MPa; this was 28.89% higher than that of the unsized CF–epoxy composite. The increase in the IFSS was attributed to the enhancement of adhesions between the CFs and polymer matrix through the welding of the MWCNTs on the CFs. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017 , 134, 45027.  相似文献   