倪晓昌 桑丽霞 张洪杰 Anoop Kiliyanamkandy Salvatore Amoruso 王宣 Rosalba Fittipaldi 李彤 胡明列 徐丽娟 《光电子快报》2014,10(1):43-46
Based on the normal pulsed laser ablation method,femtosecond pulsed laser deposition(fs-PLD)is adopted in vacuum for the production of TiO2nanoparticle-assembled films.We study the morphology and electronic characteristics of TiO2nanoparticle-assembled films deposited at different oxygen background gas pressures from high vacuum(~10-4Pa)to 100 Pa and different deposition time.Our results show that TiO2nanoparticle-assembled films obtained in high vacuum present both a mixture with rutile phase and anatase phase and a pure rutile phase.At the same time,there are more mesoporous structures in the film after annealing,which is beneficial for the enhancement of photocatalytic activity.In water splitting experiment,part of the TiO2nanoparticle-assembled films embedded with a small mass fraction of CdS nanoparticles(~5%)present an interesting photocurrent enhancement with a maximum value of~0.2mA/cm2under a solar simulator. 相似文献
13.
由于电解液成分、氧化条件和所制备纳米管尺寸等因素的影响, TiO2纳米管阵列在阳极氧化过程中容易形成纳米草结构, 而利用两步阳极氧化法可制备出表面整洁的TiO2纳米环/纳米管分层结构。实验通过控制氧化时间得到了不同生长阶段的TiO2纳米环/纳米管分层结构, 并对其生长机理及吸光特性展开研究。结果表明, 在第二步阳极氧化过程中, 钛箔表面的周期性六边形纳米洞结构可以使纳米管的生长过程局限于每个纳米洞内部, 从而形成TiO2纳米环/纳米管分层结构。同时, 存在的纳米环可以为其内部的纳米管提供支撑作用, 防止纳米草结构的形成。TiO2纳米环/纳米管分层结构的吸收光谱在可见光区域呈现震荡形态, 这是纳米环顶部反射的光与钛基底反射的光相互干涉导致的。根据震荡峰形状与样品厚度的关系, 可以估算出入射光在TiO2纳米环/纳米管分层结构中的最大穿透深度为2 μm左右。 相似文献
15.
建立含有肋片的微小通道内甲烷/空气燃烧模型,研究了带肋片的导热壁面对微小尺度燃烧和传热特性的影响。结果表明,纵向肋片对于微小通道中的燃烧和传热过程有着非常重要的影响,与没有肋片的光滑通道相比,带有肋片的壁面起到了良好的导热作用,燃烧室内区域的温度分布梯度大幅降低;纵向肋片的数量对燃烧和传热特性的影响作用要优于肋片高度的影响;横向肋片的高度对火焰位置有着很大的影响,肋片高度增加火焰位置后移且流体区域的温度分布梯度加大;横向肋片宽度和肋片位置对微燃烧和传热过程的影响甚小;两个肋片及肋间距大的通道,其微燃烧和传热特性得到了较大的改善。 相似文献
16.
Photocatalytic Degradation of Water-Soluble Dyes by LaCoO3 总被引:4,自引:0,他引:4
Perovskite-type oxides LaCoO3 was prepared by citrate method in granula of 20 - 30 rim. Using a fluorescent Hg lamp or sunlight as irradiator, the degradation experiments of various water-soluble dyes were carried out in the suspension system of LaCoO3. The results show that the perovskite-type oxide LaCoO3 has good photoeatalytic activity. With the study of X-ray photoelectron spectroscopy and photoacoustic spectra, its photoeatalytic activity is mainly related with the factors such as the d-electron structure of ion Co3 , Co-O binding energy and adsorbed oxygen on the surface etc. 相似文献
17.
针对染料和Cd S等量子点敏化剂存在的不足,开发廉价、易合成、无毒无害、催化性能好且带隙较窄的Cu基量子点材料成为敏化剂研究的重点之一.综述了Cu基量子点对Ti O2的敏化方式、Cu基量子点敏化Ti O2的光响应性和电荷传递性能及在不同领域的应用的研究进展,并对Cu基量子点敏化Ti O2在光催化制氢领域的研究重点进行了分析和总结. 相似文献
18.
利用纳米金属的等离激元共振效应可提高光解水效率,但金属Cu易氧化且Cu/TiO2界面间热电子传递过程复杂。本项研究制备了分层的Cu/TiO2纳米碗阵列并在界面间引入SiO2中间层(10~15 nm),实验和模拟相结合研究了光解水性能和等离激元共振效应的作用机制。结果表明:Cu/TiO2中Cu被氧化形成的Cu2O薄膜虽能协助热电子的注入,但对Cu的吸光性有抑制作用;加入SiO2中间层后可增强光吸收和阻隔热电子迁移,且等离激元能量转移作用促使更多的光生电子与空穴对的生成,因此Cu/SiO2/TiO2纳米碗阵列的光电性能相对提高。 相似文献
19.
利用经典分子动力学对锐钛矿型TiO2(101)/(001)羟基化表面与水分子的相互作用进行模拟计算,分析得到表面羟基对TiO2-H2O界面性质的影响.首先,通过TiO2表面钛、氧原子与水中氧、氢原子间的径向分布函数及键长验证得到,所建羟基化TiO2(101)/(001)模型和力场能够很好地模拟TiO2-水体系的结构和相关特性.由分子动力学快照图可知,TiO2表面的O2c吸附位在羟基化前后不发生改变,而完整表面原有的Ti5c吸附位被表面羟基中的氢原子取代.羟基化表面的水分子以氢键作用吸附于TiO2表面引起界面电荷转移,根据水分子密度分布可知TiO2-H2O界面形成内亥姆霍兹层、外亥姆霍兹层和体相3个分层结构.与完整表面比较,羟基使TiO2(101)表面内、外亥姆霍兹层均变窄,而TiO2(001)表面仅内亥姆霍兹层变窄.对水分子的扩散性质和平均速度分布进行分析,相对于TiO2(101)羟基表面,TiO2(001)羟基表面结构更有利于水分子沿表面法线方向移动.最后,由水的电荷密度分布函数得到,表面羟基使得TiO2(101)和(001)表面的电荷波动加剧,正、负电荷密度分布极值的绝对值明显增加.
相似文献20.
TiO2/SiO2及其表面改性光催化剂的分子级分散结构与吸光特性 总被引:1,自引:0,他引:1
以氯化醇钛盐表面反应法制备系列TiO2/SiO2,根据化学分析、XRD、Raman、XPS和DRS表征分析,载体表面具有分子级分散的锐钛矿型TiO2微晶粒子和非晶TiOx物种。与本体TiO2相比,系列TiO2/SiO2的吸收带边显著蓝移,能隙相应增大;随Ti物种载量的增加,TiOx物种的配位数增加,能隙相对减小。当金属M(M:Pd,Cu,Ni)负载于TiO2/SiO2表面,可使其光吸收域扩展到可见光区,并引起吸收带边红移,这取决于金属与界面的相互作用。当金属氧化物MoO3负载于TiO2/SiO2上时,可以调变TiO2/SiO2的吸收带边并增强对可见光的吸收;随MoO3载量的增加,表面物种的相互作用增强,形成一定复合结构并相应改变了其吸光特性。 相似文献