排序方式: 共有41条查询结果,搜索用时 15 毫秒
31.
用活性炭可从含金浸化物溶液中吸附金。在室温(20-35℃);C:Au=0.7g:1mg;溶液pH<6;溶液中化钠浓度小于0.2mol.L^-^1;适当搅拌下;吸附4h,金金吸附率可达95%以上。吸附反应为溶液,金扩散过程所控制。-dc/dt-kc;k=0.0353min^-^1。吸附等温线可用朗格公尔缪式表示q=q∞ac/(1+ac),q∞≈335mg.g^-^1,a≈0.0562L.mg^-^1 相似文献
32.
The newly developed green leaching processes for chromium, lead and gold extraction from ores or concentrates are described. The chromium is extracted from the iron chromite ore with fused sodium hydroxide at 500---550~C as sodium chromate. The galena in lead sulfide concentrate is converted into lead carbonate in ammonium or sodium carbonate solution at 50---80℃ followed by the separation of lead carbonate formed from the unconverted sulfide ores by flotation. Gold associated with sulfide ore (such as pyrite and chalcopyrite) can be extracted into sodium thiceulfate solution without any pretreatment such as roasting, high pressure aqueous oxidation or bacteria pre-leaching. 相似文献
33.
34.
本文提出了一个简便的检验金矿的方法和还原型金矿的新概念。在拿到磨细矿石后一天内就可判断出这种矿石是易处理矿,还是难处理矿,是需要在酸性介质中处理还是需要在碱性介质中处理,以及选择多大氧化能力的氧化剂。本文建议把那些既不是氧化型金矿又不属硫化金矿,并能消耗大量氧化剂的金矿石称还原型金矿。并认为要从还原型金矿中提金,首先要使矿石从还原型转变为氧化型。 相似文献
35.
36.
应用旋转环盘电极研究了方铅矿在碳酸铵溶液中直接转化为碳酸铅的反应机理.并根据所拟定的机理,对稳态极化曲线进行了数学模拟.实验指出,当以10mV.s~(-1)扫描速度作暂态极化曲线时,在0.49,0.86及1.19V(SHE)三处出现氧化峰,第一峰产物为PbCO_3及S°,第二峰产物可能为PbCO_■及PbSO_4,第三峰产物可能含有PbO_(2(?))反应过程中经历了一系列硫的中间价态化合物.当以0.2mV.s~(-1)扫描速度作稳态极化曲线时,仅在0.28V处出现一个峰.根据拟定的反应机理进行数学模拟,推导出动力学关系式. 相似文献
37.
39.
甲酸还原硅钼酸—动力学分光光度法测定硫代硫酸盐浸取液中金 总被引:1,自引:0,他引:1
本文采用甲酸还原硅钼酸——动力学分光光度法测定硫代硫酸盐浸取液中金.对硫代硫酸盐浸取用液以及浸取后液中杂质对金测定的影响进行了考察.方法标准偏差0.76%,变异系数24.5‰.为硫代硫酸盐法提金动力学实验提供了有效的分析方法. 相似文献