The custom design of protein–dendron amphiphilic macromolecules is at the forefront of macromolecular engineering. Macromolecules with this architecture are very interesting because of their ability to self-assemble into various biomimetic nanoscopic structures. However, to date, there are no reports on this concept due to technical challenges associated with the chemical synthesis. Towards that end, herein, a new chemical methodology for the modular synthesis of a suite of monodisperse, facially amphiphilic, protein–dendron bioconjugates is reported. Benzyl ether dendrons of different generations (G1–G4) are coupled to monodisperse cetyl ethylene glycol to form macromolecular amphiphilic activity-based probes (AABPs) with a single protein reactive functionality. Micelle-assisted protein labeling technology is utilized for site-specific conjugation of macromolecular AABPs to globular proteins to make monodisperse, facially amphiphilic, protein–dendron bioconjugates. These biohybrid conjugates have the ability to self-assemble into supramolecular protein nanoassemblies. Self-assembly is primarily mediated by strong hydrophobic interactions of the benzyl ether dendron domain. The size, surface charge, and oligomeric state of protein nanoassemblies could be systematically tuned by choosing an appropriate dendron or protein of interest. This chemical method discloses a new way to custom-make monodisperse, facially amphiphilic, protein–dendron bioconjugates. 相似文献
The cover image is based on the Research Article V2O5/RGO/Pt nanocomposite on oxytetracycline degradation and pharmaceutical effluent detoxification by Mohan, H et al., DOI: 10.1002/jctb.6238 .
The effects produced by annealing Y2O3 nanopowders on their spark plasma sintering (SPS) behavior are systematically investigated in this work. It is found that the annealed powders display higher sinterability with respect to the as‐received ones. Indeed, the maximum densification level reached from pristine powders is about 97.5%, whereas density decreases when further increasing either the sintering temperature or the dwell time. In contrast, the density of SPS products obtained from pretreated powder monotonically increases with temperature and processing time, thus leading to fully dense materials in 30 min at 1050°C and 60 MPa. Correspondingly, it is found that the annealing treatment markedly inhibits grain coarsening during SPS. Thus, dense translucent samples with grain size below 100 nm can be attained from annealed powders. On the other hand, white‐opaque specimens with significantly coarser microstructures (up to 1‐μm‐sized grains) are obtained when pristine powders are directly processed under the same sintering conditions. Furthermore, it is observed that the annealing treatment of SPS samples in air allows for graphite contamination removal, whereas no improvement in term of light transmittance is produced. 相似文献