ABSTRACT This study investigates the effects of strain, strain rates, and forming directions (RD-rolling direction, TD-transverse direction, and ND-normal direction) on adiabatic shear, via dynamic impact compression tests using the Split Hopkinson Pressure Bar (SHPB) apparatus. A modified Johnson-Cook (J-C) constitutive model is proposed, which used to analyse the influence of the constitutive parameters on the sensitivity of adiabatic shear, employing a finite element software. The different sensitivities of adiabatic shear under different directions are explained by combining microscopic analysis and results from mechanical responses. The results show that the sensitivity of adiabatic shear can be related to the time of stress collapse in the following trend: ND?>?TD?>?RD; the sensitivities of these constitutive parameters on adiabatic shear are calculated and compared. 相似文献
In this paper, cenosphere particles embedded in AA2014 aluminium matrix are used to fabricate syntactic foam by stir casting method. The particle size is about 100?µm and foam density is about 1990?kg?m?3. Compression tests at strain rate 0.001/s are performed on foam samples to characterise their mechanical properties which are then used in numerical analysis on commercial finite element analysis software ABAQUS/CAE with isotropic elastic-plastic material model. Experimental and numerical results show good conformity in deformation behaviour with elastic and plateau zones showing average deviations less than 5% and 20%, respectively. Foams showed high yield stress and energy absorption capabilities that can be useful in making blast and impact resistant structures. 相似文献
Abstract— The behaviour of fatigue cracks in an Al-alloy under cyclic compression, either with or without overloads, was studied. For constant-amplitude compressive cycling, a non-catastrophic (saturation) character of the fatigue crack behaviour was confirmed, with the final depth of a crack depending on the applied load level. Single (tensile or compressive) intermittent overloads were shown to re-activate a previously arrested crack while reversed (tensile—compressive or compressive—tensile) ones were also shown to maintain continual fatigue crack extension under otherwise fully compressive cycling. 相似文献
Filiform corrosion is mainly considered as a cosmetic attack and is undesirable in most applications. The initiation and propagation of the filaments are related to different parameters such as the presence of defects, the permeability of the coating to water and oxygen, the adherence of the paint system and the presence of salts.
The aim of this work is to study the behaviour of painted aluminium samples towards filiform corrosion or delamination. The 6082 Aluminium alloy was selected and the samples were covered with a cataphoretic epoxy primer without lead (PPG Industries France). Prior to the application of the electrocoat, the samples were pre-treated by a commercial Zr/Ti or chromate conversion treatment or simply etched with a commercial acid etching product.
Filiform corrosion was studied by the normalized test (ISO/DIS 4623): painted and scratched samples were inoculated in HCl and exposed in a constant humidity chamber at 40 °C and 82% RH for 3 weeks. After exposure the samples were subjected to a visual and optical microscopic examination.
Electrochemical impedance spectroscopy was used to study the sensitivity to filiform corrosion. The operating mode of this test is similar to the normalized one. The samples were scratched before inoculation for 1 h in HCl and then exposed to the humidity chamber for a maximum of 4 days. The samples were tested by EIS in an acidified 0.1 M Na2SO4 electrolyte solution. The resulting impedance spectra were analyzed with an appropriate equivalent electrical circuit which allows the evaluation of the exposed metallic surface area, directly related to the extent of filiform corrosion or delamination. Different parameters were varied: the exposure time in the humidity chamber; the immersion time in the electrolyte sulphate solution as well as its pH and the coating thickness. 相似文献
This paper presents the results obtained at three Antarctic test sites participating in the “Ibero-American Map of Atmospheric Corrosiveness” (MICAT), a project on atmospheric corrosion carried out during the period 1988–1994 at some 70 sites distributed across 12 countries of the Latin-American region, Spain and Portugal. The three Antarctic sites are located near the coastline.The singular climatic characteristics of Antarctic regions are related with the purity of the air, the absence of rainfall and the formation of ice on the metallic surface during an important part of the exposure time. However, electrochemical activity is possible below ice layers. This situation affects the structure and morphology of corrosion product films and the resulting corrosion rates of metallic surfaces. 相似文献
The influence of mechanical deformation and heating on the protective performance of a chromium-free conversion treatment for aluminium alloys has been assessed by polarisation and AC impedance measurements. Protection is unlikely to be seriously compromised by typical production operations. 相似文献
This paper highlights the possibility of inverse gas chromatography for the surface characterization of common fillers (CaCO3, talc, SiO2,) for paints and coatings. Divided solids are described, on the one hand, by the dispersive component of their surface energy and, on the other, by a specific parameter indicating their acid-base interaction potential. The role of the surface morphology at a molecular level is also examined. It is demonstrated that steric effects play an important role in the adsorption of probes on lamellar solids like talc. The consequences of surface treatments as well as examples of practical applications are also reported. 相似文献
High-density structures with relatively well-ordered nanopore arrays have been obtained by the self-ordering growth of nanopores occurring during anodisation of aluminium in sulphuric acid. The resulting array of well-ordered nanopores strongly depends on an applied voltage of anodising, temperature and a procedure of synthesis. Regular arranged hexagonal arrays on aluminium with a relatively uniform pore diameter, interpore distance, and depth of pores exceeding 90 μm, can be formed by the self-ordering two-step anodising at 1 °C. The interpore distance and the pore diameter were evaluated on anodised aluminium layers obtained at different cell potentials ranging from 15 to 25 V. The detailed analyses of their uniformity were performed from SEM images. The analysis of a pore arrangement defects was made from SEM top view images taken on samples anodised at various cell potentials. The defect maps, known as Delaunay triangulations, of the arrangement of about 1000 pores were constructed for different applied anodising potentials. The percentage of pores that are not six-fold coordinated by the neighbouring pores indicates the percentage of defected surface. 相似文献
During homogenisation of AA 6xxx aluminium alloys, the platelike β-AlFeSi intermetallic phase will transform to a less Si-rich and more spheroidised α-Al(FeMn)Si phase which is more favourable for extrusion. In this study, several quantitative methods, which determine the relative volume fraction of α-Al(FeMn)Si and β-AlFeSi, are compared and an assessment of each method is made. The methods used are optical microscopy, scanning electron microscopy (SEM) in combination with electron dispersive X-ray (EDX) using polished samples, and X-ray diffraction (XRD) on intermetallics, extracted through selective dissolution of the Al matrix. The highest accuracy is obtained by using SEM/EDX analysis and applying two criteria. 相似文献
In this work, the filiform corrosion behaviour of powder painted aluminium profiles was studied, and the coating barrier properties together with adhesion to the substrate were analysed. Samples coated with a traditional painting procedure (one powder layer application followed by curing), and other samples coated using a special cycle to obtain wood grain effect were compared using accelerated filiform corrosion tests. Moreover, in order to better understand the degradation mechanisms of painted metal substrates, thermal stresses were applied to accelerate the natural weathering. The effects of the thermal aging were analysed by electrochemical impedance spectroscopy. 相似文献