The frequency dependency of Rayleigh surface wave is investigated indirectly by measuring the angular dependency of the backward
radiation of the incident ultrasonic wave in two kinds of degraded specimens by scuffing or corrosion. Then, the frequency
dependency is compared with the residual stress distribution or the corrosion-fatigue characteristics for the scuffed or corroded
specimens, respectively. The width of the backward radiation profile increases with the increase of the variation in residual
stress distribution for the scuffed specimens. In the corroded specimens, the profile width decreases with the increase of
the effective aging layer thickness and is inversely proportional to the exponent, m, in the Paris’ law that can predict the
crack size increase due to fatigue. The result observed in this study demonstrates high potential of backward radiated ultrasound
as a tool for nondestructive evaluation of subsurface gradient of material degradation generated by scuffing or corrosion. 相似文献
Behaviour of a series of lubricant oils and the effect of a non stoichiometric inorganic compound, as solid extreme pressure additive, on rolling fatigue life are studied using the rolling four-ball accelerated service simulation test proposed by Barwell and Scott. The results show, in all tested cases, the remarkable efficacy of this type of additive. The Total Acidity Number (tan) was found to increase with performance time for the case of the base lubricant, while for the oils with additives, it remained at its constant low value. This led to a proposal of a possible mechanism of the additive performance in the rolling process. 相似文献
Hydroprocessing catalysts based on Ni, Co, Mo and W are used in various refinery processing applications where several deactivation mechanisms become of importance (coke formation, active phase sintering, metals deposition, poisoning) in the catalyst's life cycle. The life cycle of commercial hydroprocessing catalysts is very complex and includes the catalyst production, sulfidation, use, oxidative regeneration followed by re-sulfidation and reuse or, if reuse is not possible, recycling or disposal. To understand the changes in catalyst properties taking place during a life cycle, the catalyst quality in the different stages can be best monitored by using advanced analytical techniques. The catalyst's life cycle is further complicated by numerous technical, environmental and organizational issues involved. In principle, different companies can be involved in each of the life cycle steps. Leading catalyst manufacturers, together with specialized firms, offer refineries a total catalyst management concept, starting with the purchase of the fresh catalyst and ending with its final recycling or disposal. Total catalyst management includes a broad range of services, ensuring optimal timing during the change-out process, reliable, smooth and safe operations, minimal downtime and maximum catalyst and unit performance. 相似文献
Home storage is the final step of the frozen foods distribution chain, and little is known on how it affects the products quality. The present research describes frozen green beans (Phaseolus vulgaris, L.) quality retention profile during the recommended ‘star marking’ system dates, at the storage temperatures of +5, −6, −12 and −18 °C (along 1, 4, 14 and 60 days, respectively).
The quality profile was assessed by a simulation system. Simulations were set by a response surface methodology to access the effect of different packaging materials (thermal conductivities and thickness), surface heat transfer coefficient, and refrigerator dynamics (effect of refrigeration cycles at the different storage temperatures) on the average retentions of Ascorbic Acid, total vitamin C, colour and flavour.
Green beans quality losses along frozen storage are significantly influenced by temperature, refrigerator dynamics and kinetic properties. Quality is also highly dependent on packaging materials thermal insulation (e.g. at temperatures above the melting point). Temperature cycles inside frozen chambers have a long term effect, and at the higher storage temperatures (e.g. T>−6 °C) are detrimental to frozen green beans quality after shorter periods. 相似文献
The procedure for calculating the life of header – steam generator connector weld joints is proposed. It allows for running out the material plasticity reserve upon static cyclic elastoplastic loading as well as operating conditions, local stress concentrations, and residual stresses after welding. 相似文献