In the oxidation of TiAl alloys, the role of scale-growth stresses formed during oxidation has, thus far, been unknown. In the present paper the oxide-growth stresses were investigated by the deflection-test method in monofacial oxidation (DTMO) accompanied by acoustic-emission measurements. On unmodified surfaces the growth stresses are compressive and reach levels of around –100 MPa. At the same time, significant acoustic emission occurs indicating that even under isothermal conditions, stresses are relieved by a scale-cracking mechanism. For oxide scales on TiAl surfaces, which had been ion implanted with chlorine before oxidation, a very thin protective alumina layer is formed which, however, develops growth stresses in the range of several GPa, accompanied by intensive acoustic emission. In all stress–time curves, a dynamic situation is observed. This consists of phases of stress relief by scale microcracking and phases of stresses increase due to crack healing and further oxide growth. As a result, the level of stress as a function of oxidation time, is characterized by an oscillating course. 相似文献
Based on an idea introduced by Benjamin and Cornell (1970. Probability, statistics and decision for civil engineers. New York: McGaw Hill) and previous works by the authors it is demonstrated how condition indicators may be formulated for the general purpose of quality control and for assessment and inspection planning in particular. The formulation facilitates quality control based on sampling of indirect information about the condition of the considered components. This allows for a Bayesian formulation of the indicators whereby the experience and expertise of the inspection personnel may be fully utilized and consistently updated as frequentistic information is collected. The approach is illustrated on an example considering a concrete structure subject to corrosion. It is shown how half-cell potential measurements may be utilized to update the probability of excessive repair after 50 years. Furthermore in the same example it is shown how the concept of condition indicators might be applied to develop a cost optimal maintenance strategy composed of preventive and corrective repair measures. 相似文献
GENIUS-TF (Nucl. Instr. and Meth. A 511 (2003) 341; Nucl. Instr. and Meth. A 481 (2002) 149.) is a test-facility for the GENIUS project (GENIUS-Proposal, 20 November 1997; Z. Phys. A 359 (1997) 351; CERN Courier, November 1997, 16; J. Phys. G 24 (1998) 483; Z. Phys. A 359 (1997) 361; in: H.V. Klapdor-Kleingrothaus, H. Pas. (Eds.), First International Conference on Particle Physics Beyond the Standard Model, Castle Ringberg, Germany, 8–14 June 1997, IOP Bristol (1998) 485 and in Int. J. Mod. Phys. A 13 (1998) 3953; in: H.V. Klapdor-Kleingrothaus, I.V. Krivosheina (Eds.), Proceedings of the Second International Conference on Particle Physics Beyond the Standard Model BEYOND’ 99, Castle Ringberg, Germany 6–12 June 1999, IOP Bristol (2000) 915), a proposed large scale underground observatory for rare events which is based on operation of naked germanium detectors in liquid nitrogen for an extreme background reduction. Operation of naked Ge crystals in liquid nitrogen has been applied routinely already for more than 20 years by the CANBERRA Company for technical functions tests (CANBERRA Company, private communication, 5 March 2004.), but it never had found entrance into basic research. Only in 1997 first tests of application of this method for nuclear spectroscopy have been performed, successfully, in Heidelberg (Klapdor-Kleingrothaus et al., 1997, 1998; J. Hellmig and H.V. Klapdor-Kleingrothaus, 1997).
On May 5, 2003 the first four naked high-purity germanium detectors (total mass 10.52 kg) were installed in liquid nitrogen in the GENIUS Test Facility at the Gran Sasso underground laboratory. Since then the experiment has been running continuously, testing for the first time the novel technique in an underground laboratory and for a long-lasting period.
In this work, we present the first analysis of the GENIUS-TF background after the completion of the external shielding, which took place in December 2003. We focus especially on the background coming from 222Rn daughters. This is found to be at present by a factor of 200 higher than expected from simulation. It is still compatible with the scientific goal of GENIUS-TF, namely to search for cold dark matter by the modulation signal, but on the present level would cause serious problems for a full GENIUS—like experiment using liquid nitrogen. 相似文献
LiFePO4 is a potential candidate for the cathode material of the lithium secondary batteries. A co-precipitation method was adopted to prepare LiFePO4 because it is simple and cheap. Nitrogen gas was needed to prevent oxidation of Fe2+ in the aqueous solution. The co-precipitated precursor shows the high reactivity with the reductive gas, and the single phase of LiFePO4 is successfully synthesized with the aid of carbon under less reductive conditions. LiFePO4 fine powder prepared by co-precipitation method shows high rate capability, impressive specific capacity and cycle property. 相似文献
The transit time of the coolant, and thus its velocity, has been measured using the temperature fluctuation at the outlet of a reactor core. An impulse response function estimation is introduced, which substitutes the widely used cross-correlation measurement technique. It is shown in theory and practice that the time delay estimation is improved when using the impulse response function instead of the cross-correlation function in parameter estimation. Extremely low velocities (down to 2 cm/sec) have been measured in a natural circulation regime in a research reactor. 相似文献
Variable-magnetic-field Hall measurements (0 to 1.5 T) are performed on very-narrow-gap bulk-grown Hg1−xCdxTe single crystals (0.165 ≤ x ≤ 0.2) at various temperatures (10 to 300K). The electron densities and mobilities are obtained
within the one-carrier (electrons) approximation of the reduced-con-ductivity-tensor scheme. The present data together with
the selected data set reported by other workers exhibit a pronounced peak when the electron mobility is plotted against the
alloy composition x-value which has been predicted to be due to the effective-mass minimum at the bandgap-crossing (Eg ≈ 0). The observed position (x ≈ 0.165), height (≈4 x 102 m2Vs), and width (≈0.01 in x) of the mobility-peak can be explained by a simple simulation involving only ionized-impurity scattering.
A lower bound of the effective mass is introduced as a fitting parameter to be consistent with the finiteness of the observed
electron mobility and is found to be of the order of 10−4 of the mass of a free electron. 相似文献
Chemometrics has enjoyed tremendous success in the areas related to calibration of spectrometers and spectroscopy-based measurements. These chemometric-based spectrometers have been widely applied for process monitoring and quality assurance. However, chemometrics has the potential to revolutionize the very intellectual roots of problem solving. Are there barriers to a more rapid proliferation of chemometric-based thinking, particularly in industry? What are the potential effects of chemometrics technology and the New Network Economy (NNE) working in concert? Who will be the winners in the race for faster, better, cheaper systems and products? These questions are reviewed in terms of the principles of the NNE and in the promise of chemometrics for industry. What then is the state of multivariate thinking in industry? Several powerful principles are derived from an evaluation of the NNE and chemometrics which could allow chemometrics to proliferate much more rapidly as a key general problem-solving tool. 相似文献
In this paper, we present the theory for calculating Raman line shapes as functions of the Fermi energy and finite temperatures in zinc blende, n-type GaAs for donor densities between 1016 cm−3 and 1019 cm−3. Compared to other theories, this theory is unique in two respects: 1) the many-body effects are treated self-consistently and 2) the theory is valid at room temperature for arbitrary values of the ratio R = (Q2/α), where Q is the magnitude of the normalized wave vector and α is the normalized frequency used in the Raman measurements. These calculations solve the charge neutrality equation self-consistently for a two-band model of GaAs at 300 K that includes the effects of high carrier concentrations and dopant densities on the perturbed densities of states used to calculate the Fermi energy as a function of temperature. The results are then applied to obtain the carrier concentrations from Fermi energies in the context of line shapes in Raman spectra due to the coupling between longitudinal optical phonons and plasmons. Raman measurements have been proposed as a non-destructive method for wafer acceptance tests of carrier density in semiconductor epilayers. The interpretation of Raman spectra to determine the majority electron density in n-type semiconductors requires an interdisciplinary effort involving experiments, theory, and computer-based simulations and visualizations of the theoretical calculations. 相似文献