排序方式: 共有25条查询结果,搜索用时 0 毫秒
1.
2.
陈月顺 《武汉理工大学学报(材料科学英文版)》2007,22(2):354-357
The influence of reinforced bar corrosion on the bond degradation in lightweight concrete was studied. Accelerated constant current corrosion tests were performed on lightweight reinforced concrete samples, and the influential factors, such as protective layer thickness, reinforced bar diameter and corrosive level were investigated. The constant current step method was used to measure the electric resistance of the concrete protective cover, which was used to characterize the corrosion level of the rebar. Experimental results indicated that the corrosive resistance increased with increasing the cover dimension and decreasing the reinforced bar diameter, and the rate of decrease in the specimen impedance after cracking depended on the cover dimension. A new medium was offered for the further research on the performance degradation of corrosion lightweight concrete. 相似文献
3.
4.
5.
通过模型试验,测定了张拉时U形曲线预应力筋中有效应力沿预应力筋的分布以及混凝土中的有效应力的分布情况,并比较了在相同条件下,直线预应力筋与曲线预应力筋的孔道摩阻的不同分布规律,为更好地弄清U形曲线预应力筋孔道摩阻的作用机理提供了试验依据。 相似文献
6.
钢筋混凝土锈胀开裂临界锈蚀率模型研究 总被引:2,自引:0,他引:2
基于弹塑性理论,在考虑了钢筋直径、保护层厚度、钢筋间距、混凝土材料性能的基础上,提出钢筋的锈胀填充膨胀率参数,建立了钢筋混凝土保护层锈胀开裂的临界锈蚀率模型,并研究了各因素对模型影响的敏感性。所建模型通过试验数据得到了验证,钢筋的锈胀填充膨胀率n=1.2。 相似文献
7.
探地雷达作为近10几年来新兴起来的进行地下探测和混凝土无损检测的一种高新技术,具有操作简单,结果稳定的优点。采用劳雷SIR-20型地质雷达,对某轨道梁的混凝土完整性进行检测,同时与完好梁的检测结果进行对比,该梁混凝土完整性较好。 相似文献
8.
借助足尺模型试验,测定了三种形式的预应力筋张拉过程中的孔道摩阻损失。试验结果表明,直线型和小曲率预应力筋孔道的摩阻损失较小,而大曲率情况的孔道摩阻损失超过30%。引入非线性摩擦的概念,建立了预应力摩阻损失模型,并将模型计算结果与试验结果进行比较,摩擦模量取1011N/mm时二者符合较好。 相似文献
9.
10.
为完善和发展锈蚀钢筋混凝土结构的计算方法,基于混凝土结构中钢筋锈蚀后,锈蚀钢筋的截面损失、力学性能下降,钢筋和混凝土之间的粘结性能退化,钢筋锈胀力导致混凝土锈胀开裂等因素,将造成钢筋混凝土梁的承载能力及整体刚度都会有所下降的事实。借鉴已有的研究成果,得到了钢筋不同锈蚀率对钢筋混凝土梁中钢筋与混凝土间协同工作的影响公式,并结合现有的关于钢筋混凝土梁抗弯承载力的规范计算方法,建立了锈蚀双筋混凝土梁抗弯承载力的计算模型。最后,利用所建立的计算模型对已有的试验成果进行了验证分析,结果表明,所建立的的计算模型能够与试验结果较好地吻合。 相似文献