1.
2.
Silicon-on-insulator (SOI) materials have a number of inherent advantages over bulk silicon substrates owing to their high speed, low power complementary metal-oxide-semiconductor (CMOS) integrated circuits, such as immunity to radiation hardness, high speed, and high tem-perature tolerance [1]. Separation by implantation of oxygen (SIMOX), bonding and etch back (BESOI) and Smart-Cut are the leading technologies for SOI material fabrication. Transitional metal impurities such as Cu, F… 相似文献
3.
本文研究不同金属薄膜结构形成的超薄CoSi2膜的高温稳定性.采用离子束溅射和反应磁控溅射技术制备Co/Si、TiN/Co/Si、Co/Ti/Si、TiN/Co/Ti/Si不同结构,在高纯氮气下进行快速热退火(RTA),形成CoSi2薄膜.应用四探针薄层电阻测试、扫描电子显微镜(SEM)、透射电子显微镜(TEM)进行测试.实验结果表明:TiN覆盖层和Co/Ti/Si三元固相反应都是有利于形成具有良好高温稳定特性的CoSi2薄膜的有效方法,有望应用于深亚微米接触和互连技术中. 相似文献
4.
等离子体浸没离子注入(PIII)为解决束线离了注入所难以解决的圆筒状零件内表面注入处理问题提供了新要可能途径,但在应用中却受到注入能量和注入剂量偏代的限制,本文针对这一问题了偏转电场法用以提高内表面注入的能量和注入剂量,实验结果表明,采用这一方法可以有效地改善圆筒状零件内表面注入的注入情况,注论述工提高了25%~100%,注入剂量提高了73%~113%,注入脉冲宽度的延有利于注入离子向部深入,利于 相似文献
5.
钛合金微弧氧化陶瓷膜微观特性的分析 总被引:5,自引:0,他引:5
微弧氧化膜存在微米量级宏孔,这些宏孔对氧化膜特征的研究非常重要.研究了微弧氧化中电流密度对微弧氧化膜的生长速率、结构形貌及相组成的影响,并对氧化膜进行了离子束抛光处理,分析了氧化膜和微孔的组织结构.研究表明:电源频率固定为1 500 Hz/5 μs和氧化膜厚为10 μm时,随着氧化电流密度的增大,氧化膜的生成速度和孔径都随之增大,但同一膜厚的氧化层组成成分金红石型TiO2和锐钛矿型TiO2的相对含量无明显变化;离子束抛光后的氧化膜膜层外疏内密,放电通道内表面更是淀积了电解液溶质、氧化膜颗粒及基材等多种物质的纳米微颗粒. 相似文献
6.
7.
磁控溅射Zr-Ti薄膜的组织结构与血液相容性 总被引:1,自引:0,他引:1
通过直流平衡磁控溅射法在NiTiSMA表面生成Zr-Ti膜,用SEM、XRD和XPS分析证实制备的Zr-Ti膜呈现晶带T型结构,组织保持了细小致密的纤维状特征,与基底结合良好,并且出现了少量生物惰性ZrO2和TiO2陶瓷相。通过测定溶血率研究血小板黏附行为,评估血液相容性。结果表明,与NiTi基底相比,Zr-Ti膜的溶血率更低,表面黏附的血小板数量减少,能够改善NiTiSMA基底的血液相容性。最后,对磁控溅射沉积Zr-Ti膜的成膜机理进行了探讨。 相似文献
8.
9.
A modified advanced oxidation process(AOP) utilizing a UV/electrochemically-generated peroxide system was used to fabricate titania films on chemically polished NiTi shape memory alloy(SMA). The microstructure and biomedical properties of the film were characterized by scanning electron microscopy(SEM), X-ray photoelectron spectroscopy(XPS), inductively-coupled plasma mass spectrometry(ICPMS), hemolysis analysis, and blood platelet adhesion test. It is found that the modified AOP has a high processing effectiveness and can result in the formation of a dense titania film with a Ni-free zone near its top surface. In comparison, Ni can still be detected on the outer NiTi surface by the conventional AOP using the UV/H2O2 system. The depth profiles of O, Ni, Ti show that the film possesses a smooth graded interface structure next to the NiTi substrate and this structure enhances the mechanical stability of titania film. The titania film can dramatically reduce toxic Ni ion release and also improve the hemolysis resistance and thromboresistance of biomedical NiTi SMA. 相似文献
10.
用于加工Inconel718的切削刀具发展现状 总被引:1,自引:0,他引:1
镍基高温合金Inconel718具有熔点高、热传导率低、加工硬化现象严重的特点,被认为是最难加工的金属材料之一。近年来,随着航空航天、能源动力技术的飞速发展,Inconel718高温合金的应用越来越多,其高速、高效切削的加工需求也日益扩张,其切削工艺的制定、尤其是切削刀具的选择越来越重要。本文综述了常用于加工In-conel718的刀具(高速钢、硬质合金、陶瓷、立方氮化硼)及其涂层刀具的加工性能,分析了不同涂层对于刀具寿命和工件表面质量的影响,对硬质合金刀具和陶瓷刀具作了详尽的对比分析。最后,对高速钢、陶瓷、硬质合金和立方氮化硼刀具切削Inconel718的应用情况进行了总结,给出了Inconel718高温合金切削加工刀具选择的有益参考。 相似文献