We report a systematic investigation on the structure–property relationships in glycerol-plasticized poly(vinyl alcohol) (PVA)/cassava starch blends prepared via solution casting. In particular, PVA mixed with native, low-oxidized, high-oxidized, and pregelatinized cassava starches were characterized by means of SEM, XRD, FTIR, thermal analysis and mechanical testing and the immiscible systems were received. Burial tests over a period of several days suggested the preferential degradation of the starch and glycerol component (as indicated by the absence of FTIR signatures of those components) and the amorphous phase of PVA (as indicated by the enhanced crystallinity index of the degraded samples). The rheological properties of the blends seem to dictate their morphological characteristics that, in turn, have a profound impact on their mechanical properties. In that sense, the study highlights promising strategies for the development of a new family of polymeric materials that combine their biodegradable nature within superior mechanical properties. © 2020 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2020 , 137, 48848.  相似文献   
2.
Tough biodegradable films were prepared using a poly(vinyl alcohol) (PVA)/poly(vinyl pyrrolidone) (PVP) (1:1) blend with plasticizers of glycerol (GLY), sorbitol (SOR), and their (one to one) mixture. We studied the effect of plasticization on the structural, thermal, and mechanical properties of the PVA/PVP blend films. Fourier transform infrared spectra indicated good miscibility of the two components due to the H‐bonding between the PVA and PVP molecules. The addition of plasticizers reduced the interaction between PVA and PVP, evidenced by an increase in the intensity of PVA diffraction peaks observed in the X‐ray diffraction (XRD) characterization. Thermal degradation of the blends increased as a function of the plasticizer used. GLY affected thermal degradation more than SOR and the mixtures. The incorporation of the plasticizers promoted the growth of PVA crystals as evidenced by XRD patterns and the enthalpy of fusion (ΔHf) obtained by differential scanning calorimetry measurements. The introduction of SOR to the binary blend increased toughness seven times and imparted simultaneous and pronounced improvements to maximum tensile stress and elongation at break. This behavior holds out great promise for the development of a new generation of mechanically robust, yet thoroughly biodegradable materials that could effectively supplant conventional polymers in demanding applications. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018 , 135, 46406.  相似文献   
1
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号