排序方式: 共有3条查询结果,搜索用时 0 毫秒
1
1.
Strontium iron holmium niobate (Sr(Fe1?xHox)0.5Nb0.5O3) ceramics were synthesized via a solid-state reaction technique. The undoped ceramic showed an orthorhombic phase, but it transformed to a pseudocubic phase for higher Ho concentrations. A low solubility limit of Ho in SFN caused a formation of second phase for the x=0.15 ceramic. Dielectric behavior of undoped ceramic exhibited high dielectric constant over a wide temperature range. However, the doping shifted this region to a higher temperature. The doping also shifted the peak of dielectric loss to a higher temperature. Activation energy of dielectric relaxation increased with increasing Ho concentration. In addition, complex impedance analysis was applied to determine the behaviors of grain boundary and grain after doping. 相似文献
2.
Pakpoom Jarupoom Pharatree Jaita Ratabongkot Sanjoom Chamnan Randorn Gobwute Rujijanagul 《Ceramics International》2018,44(8):8768-8776
In this research, the effects of La0.7Sr0.3MnO3 additive on the phase evolution, microstructure, dielectric, ferroelectric and magnetic properties of BaZr0.07Ti0.93O3 ceramics were systematically investigated. The (BaZr0.07Ti0.93O3)/x(La0.7Sr0.3MnO3) or BZT/xLSM (where x?=?0, 5, 10 and 20?mol%) ceramics were prepared via a solid state reaction method. A pure perovskite phase is observed for the samples of x?≤?10?mol%. The M-H hysteresis loops also show an improvement in the magnetic behavior for higher LSM content samples as well as the modified ferroelectric properties. However, the 5?mol% sample exhibited the optimum ferroelectric and ferromagnetic properties with remnant magnetization (Mr) and remanent polarization (Pr) of 2.38?emu/g and 10.5?µC/cm2, respectively. The dielectric-temperature curves show that the two phase-transition temperatures as observed for the unmodified BZT ceramic merges into a single phase-transition temperature for the 5?mol% sample and then become flat curves for the 10?mol% sample. In addition, the mechanical properties i.e. Knoop hardness and Young's modulus values increase with increasing LSM content, where Knoop hardness and Young's modulus values for the 20?mol% sample are increased by ~ 45% and ~ 104%, respectively, as compared to the unmodified sample. 相似文献
3.
Pharatree Jaita Lalita Tawee Ratabongkot Sanjoom Chamnan Randorn Komsanti Chokethawai Gobwute Rujijanagul 《Journal of Electroceramics》2018,41(1-4):50-59
The (1-x)Ba(Zr0.25Ti0.75)O3-xSr(Fe0.5Nb0.5)O3 or (1-x)BZT-xSFN ceramics have been fabricated via a solid-state reaction technique. All ceramics exhibit a pure phase perovskite with cubic symmetry. The addition of a small amount of SFN (x?=?0.1) produces an obvious change in dielectric behavior. Very high dielectric constants (εr?>?164,000 at 1 kHz and temperature?>?150°C) are observed and the value is obviously higher than dielectric constants for Ba(Zr0.25Ti0.75)O3 and Sr(Fe0.5Nb0.5)O3 ceramics. The ferroelectric measurement data suggests that the unmodified sample exhibited a ferroelectric behavior. However, a transformation from a ferroelectric to a relaxor-like behavior is noted with increasing x concentration. Impedance Spectroscopy (IS) analysis indicates that the presence of excellent dielectric constants is due to the heterogeneous conduction in the ceramics after adding SFN, which can be explained in terms of the Maxwell-Wagner polarization mechanism. 相似文献
1