Influence of Rare Earth Elements on Microstructure and Mechanical Properties of Mg-Li Alloys 总被引:6,自引:1,他引:6
Mg-Li alloy , which is also called superlight al-loy ,has many advantages ,such as lowdensity ,highstiffness-to-weight ratio , superior strength-to-weightratio ,good deformation ability ,good damping ability ,and high energetic particle penetration resistance[1 ,2].These advantages provide promising applicationsintheaerospace , electronic industry , and military field[3].Mg-Li alloys ,such as LA141 , LA191 ,and LAZ933were developed and have been usedfor components insatellites and aircrafts… 相似文献
2.
3.
采用铜模浇铸法制备了Al63Cu27Zn10、Al56Cu24Zn20、Al49Cu21Zn30和Al42Cu18Zn40非晶合金.X射线衍射谱图表明Al56Cu24Zn20和Al49Cu21Zn30为完全金属玻璃,而Al63Cu27Zn10和Al42Cu18Zn40为部分非晶合金.得到了合金的玻璃化转变温度(Tg)、晶化温度(Tx)以及过冷液相区宽度(△Tx=Tx-Tg),推断出zn元素的加入降低了体系的非晶形成能力(GFA).从得到的硬度值可知,非晶合金的显微硬度值高于相同成分的结晶合金. 相似文献
4.
采用铜模浇铸法制备了Al63Cu27Zn10、Al56Cu24Zn20、Al49Cu21Zn30和Al42Cu18Zn40非晶合金。x射线衍射谱图表明Al56Cu24Zn20和Al49Cu21Zn30为完全金属玻璃,而Al63Cu27Zn10和Al42Cu18Zn40为部分非晶合金。得到了合金的玻璃化转变温度(t)、晶化温度(t)以及过冷液相区宽度(△Tx=Tx-Tg),推断出Zn元素的加入降低了体系的非晶形成能力(GFA)。从得到的硬度值可知,非晶合金的显微硬度值高于相同成分的结晶合金。 相似文献
5.
Several Mg-xLi-3Al-lCe alloys were prepared by vacuum induction heating. These alloys are Mg-5Li-3Al-lCe, Mg-8Li-3Al-lCe and Mg-14Li-3Al-1C e, respectively. The microstructure and phase composition of these alloys were analyzed by optical microscopy, scanning electron microscopy, energy dispersive X-ray spectroscopy and X-ray diffractometry. The mechanical properties of these alloys were measured with tensile tester. The results show that, Mg-5Li-3Al-1Ce has a single phase (α) structure, Mg-8Li-3Al-lCe has a double phases (α+β) structure, Mg-14Li-3Al-1Ce has a single phase (β) structure. And some compounds distribute in the matrix. After being rolled, the grain size of all the alloys is refined. Under the condition of the same content of other alloying elements, the mechanical properties of Mg-5Li-3Al-1Ce are relatively high. With increasing Li content, the strength of both as-cast and as-rolled alloy decrease. For the as-cast alloys, with increasing Li content, the elongation increases. While for the as-rolled alloys, with increasing Li content, the elongation decreases. Ce has refining effect on these alloys. 相似文献
6.
7.
8.
采用氩气保护、真空熔炼的方法制备了Mg-xLi-3Al-2Zn-0.7Re(x=8~14,wt%)镁锂合金。研究了合金的显微组织及力学性能,结果表明:当锂的含量为12(wt)%时,合金在室温时具有较好的强度和变形能力,具有最佳的综合力学性能。 相似文献
9.
10.
采用粉末冶金技术制备了不同孔隙率的空心球/铝基复合泡沫材料,对其进行T7热处理,并开展了不同孔隙率材料压缩性能及隔声性能的测试。结果表明,制备的泡沫材料中空心球均匀分布于基体内,且空心球与基体之间形成明显的过渡层;空心球/铝合金基复合泡沫材料的压缩应力-应变曲线呈现线弹性、应力平台、致密化3个阶段。随着孔隙率的增加,空心球/铝合金基复合泡沫材料的压缩峰值应力、平台应力及能量吸收能力均呈先上升后下降的变化趋势;随着孔隙率的增加,复合泡沫材料隔声性能逐渐下降。 相似文献