排序方式: 共有3条查询结果,搜索用时 0 毫秒
1
1.
A selective chemical etching was used to fabricate fiber probes for the photon scanning tunneling microscope (PSTM). The cladding diameter of the fiber probe was controlled by varying the first-step etching time. The cone angle of the fiber probe tip was controlled by varying the doping ratio of the fiber and the composition of the etching solution. A cladding diameter of 8 μm and a tip diameter of about 3 nm were fabricated. The smallest cone angle was 14°. 相似文献
2.
3.
A selective chemical etching was used to fabricate fiber probes for the photon scanning tunneling microscope (PSTM). The cladding diameter of the fiber probe was controlled by varying the first-step etching time. The cone angle of the fiber probe tip was controlled by varying the doping ratio of the fiber and the composition of the etching solution. A cladding diameter of 8 μm and a tip diameter of about 3 nm were fabricated. The smallest cone angle was 14°. 相似文献