Calcined kaolin/TiO2 composite particle material (CK/TCPM) was prepared with TiO2 coating on the surfaces of calcined kaolin particles by the mechano-chemical method. X-ray diffraction (XRD) and scanning
electron microscope (SEM) were used to investigate the microstructures and morphologies, respectively. The mechanism of the
mechano-chemical reaction between calcined kaolin and TiO2 was studied by infrared spectra (IR). The results show that TiO2 coats evenly on the surfaces of calcined kaolin particles by Si-O-Ti and Al-O-Ti bonds on their interfaces. The hiding power
and whiteness of CK/TCPM are 17.12 g/m2 and 95.7%, respectively, presenting its similarity to TiO2 in pigment properties. 相似文献
2.
3.
煅烧高岭土-TiO_2复合材料的制备及表征 总被引:1,自引:1,他引:0
以煅烧高岭土和TiO2为原料,采用机械力化学法制备煅烧高岭土-TiO2复合材料。以遮盖力和吸油量为指标,优化煅烧高岭土-TiO2复合材料的制备工艺,并表征其颜料性能。结果表明:复合过程中共混研磨时间、球料质量比和搅拌磨转速对复合材料的颜料性能影响显著。制备的煅烧高岭土-TiO2复合材料遮盖力为纯钛白粉的88.4%,白度也与其接近,且吸油量适中。该材料用于内墙涂料显示出较好的颜料性能,能以一定比例替代钛白粉使用。 相似文献
4.
利用废弃物制备白炭黑的研究现状及发展趋势 总被引:2,自引:0,他引:2
本文详细阐述了利用废弃物制备白炭黑的研究现状,重点介绍利用农业固体废物、矿山尾矿和工业废渣、废水等回收白炭黑,探讨了其发展趋势。 相似文献
5.
以高岭土为载体,采用机械力化学法制备了TiO2/高岭土复合光催化剂。以甲基橙溶液的光催化降解率作为评价指标,采用正交实验法,研究了纳米TiO2和高岭土混合研磨体系中固体浓度、球料比、复合研磨时间以及纳米TiO2的含量对复合材料光催化降解率的影响。实验结果表明,采用机械球磨技术可以制备具有光催化性能的TiO2/高岭土复合光催化剂。当高岭土湿磨时间为60min,纳米TiO2和高岭石混合研磨体系中固体浓度20%、球料比5∶1、复合研磨时间30min、纳米TiO2的含量为33.3%时,该复合材料对甲基橙的光催化降解率为69%,高于纯TiO2的光催化降解率。 相似文献
6.
本文详细阐述了利用废弃物制备白炭黑的研究现状,重点介绍利用农业固体废物、矿山尾矿和工业废渣、废水等回收白炭黑,探讨了其发展趋势。 相似文献
1