以四乙氧基硅烷(TEOS)作为主要前驱体,通过改变溶胶-凝胶工艺参数制得了结构和形态各异的丙烯酸酯聚氨酯/SiO2纳米复合涂层,利用TEM、SAXS等手段表征涂层的结构与形态,由洗刷前后涂层的失光率来表征耐刮伤性,详细探讨了纳米复合涂层耐刮伤性与SiO2相特征、有机无机相作用力及SiO2质量分数之间的关系。研究表明:丙烯酸酯聚氨酯涂层中引入纳米SiO2相后,耐刮伤性明显提高。有机相与SiO2相之间的作用力是影响涂层耐刮伤性的最重要因素,作用力越强,耐刮伤性越好。网络状纳米SiO2与颗粒状纳米SiO2相比,更有利于耐刮伤性的提高,且网络状纳米SiO2质量分数越大,耐刮伤性越佳,但SiO2相的致密度和尺寸对耐刮伤性影响较小。对于颗粒状胶体SiO2,在15~160 nm范围内,粒径对耐刮伤性没有明显影响;随着胶体SiO2粒子的质量分数增加,耐刮伤性先增大后减小。 相似文献
2.
3.
Phase Partition of Acrylonitrile (AN) in Vinylidene Chloride (VDC)/Water System and Its Effect on VDC-AN Copolymer Composition 下载免费PDF全文
phase partition of acrylvnitrile in the vlnylidene chloride/water system at different temperature and under pressure was studied, A calculation method for average VDC-AN copolymer compeeition with AN phmm partition considered was proposed. The conversion results are in good agreement with the experimental data nearly the entire conversion rauge. VDC-AN copolymer with narrower composltion distribution can be prepared in the suspension process and interpreted with dynamic equilibrium of AN between the oil and water phases continuously. 相似文献
4.
5.
本文研究了以偶氮二异丁腈(AIBN)引发的偏氯乙烯(VDC)-丙烯腈(AN)-苯乙烯(St)悬浮聚合颗粒的粒径及其分布。实验发现在该体系中存在两种成粒机理:单体液滴的珠状成粒和水相聚合沉淀成粒。水相聚合是由于AN的水溶性增加了AIBN在水中的溶解度所致。加入亚硝酸钠(NaNO2)可以有效减少水相聚合生成物,使悬浮颗粒的粒径分布变窄。 相似文献
6.
用DSC法研究了VDC-AN悬浮共聚物的玻璃化转变和热熔融行为,并用Barton方程定量关联了Tg与组成的关系,用TGA法研究了共聚物的热分解行为,结果表明,AN单元对与其相邻连拉的VDC单元脱HC1有诱导催化作用,由DCS法和X射线衍射法得到高VDC含量的共聚物结晶度与AN含量成线性关系,而在高AN含量时则与AN组成成三次多项式关系。 相似文献
7.
8.
9.
10.
丙烯酸酯/纳米SiO2复合乳液的制备和表征 总被引:25,自引:0,他引:25
通过原位聚合、高速剪切法分散共混和球磨法分散共混等三种方法制备丙烯酸酯/纳米SiO2复合乳液,以相同的方法制备丙烯酸酯/微米SiO2复合乳液,并利用电子拉力机(Instron)、动力学粘弹谱(DMA)、紫外可见光分光光度计(UV-VIS)和透射电子显微镜(TEM)考察了复合物的各种力学和光学性能。结果发现,共混法制得的纳米复合物的拉抻强度、断裂伸长度和玻璃化转变温度(Tg)随纳米二氧化硅含量的增加先上升然后逐渐下降,而通过原位聚合制得的纳米复合物的这些性能均低于未加纳米SiO2的丙烯酸酯。涂层对紫外光的吸收和透过随纳米SiO2含量的增加分别呈上升和下降趋势,而微米SiO2复合的丙烯酸酯乳液,其涂层对紫外光的吸收和透过率基本保持不变。 相似文献