排序方式: 共有14条查询结果,搜索用时 15 毫秒
1.
用阳极电沉积技术在304不锈钢基体上制备CeO2薄膜,用扫描电子显微镜(SEM)和X射线衍射(XRD)等手段探讨不同配体阳离子种类、配体浓度和O2对镀层表面结构的影响规律。结果表明,CH3COONH4配体中的铵离子(NH4+)对CeO2薄膜晶粒的细化具有重要作用,镀液中高CH3COONH4配体浓度及镀液的脱氧作用有利于阳极电沉积CeO2薄膜的致密化;在镀液组成为0.1 mol/L Ce(NO3)3和0.2 mol/LCH3COONH4、且镀液脱氧的实验条件下,获得了平整致密的纳米晶CeO2薄膜,其晶粒粒径范围为5~10 nm。 相似文献
2.
耐候钢在2.0%NaCl中性溶液中的腐蚀过程 总被引:3,自引:0,他引:3
采用电化学阻抗谱技术研究了耐候钢Q400NQR1和09CuPCrNi在2.0%NaCl中性溶液中的腐蚀行为,建立了其腐蚀等效电路模型并分析了其相关电化学参数随时间的演化规律,结果表明,两种耐候钢的溶液腐蚀过程均可以分为四个阶段,即点蚀诱导期、点蚀发展期、腐蚀中期和腐蚀后期;Q400NQR1较09CuPCrNi具有较高的抗溶液腐蚀能力,前者在腐蚀的中期生成保护性较强的内层锈层,而后者形成的内层锈层难以稳定且易于出现均匀腐蚀的现象。 相似文献
3.
4.
5.
6.
In-situ monitoring of nickel electrodeposit structure using electrochemical noise technique 总被引:1,自引:1,他引:1
The nickel electroplating process was investigated by means of electrochemical noise(EN), cyclic voltammetry in conjunction with the scanning electron microscopy(SEM) technique. The results show that, in the experimental conditions and with the increase of current density, the growth mechanism of nickel crystallites changes from 2-D to 3-D with the potential turning point of about - 1.15 V, and the potential for the onset of diffusion control of the ensemble nickel electroplating process was about --1.4 V. In the case of activation-control, the two-dimensional (2-D) nucleation / growth process of nickel often results in the electrocrystallization EN features of only slowly small positive potential drift and the corresponding compact layer-by-layer deposit structure, and the maximum relative energy of the RP-EDP (re-plotted relative energy distribution plot), which is obtained from wavelet analysis, defmed in the region with smaller scales. While under the diffusion-control, the three-dimensional (3-D) nucleation / growth process of nickel, often results in the electrocrystallization EN features of both the fast positive potential drift and subsequent remarkable negative potential drift and the corresponding dentritic/large conglomerate structure of nickel deposit, and the maximum relative energy of the RP-EDP defined in the region with larger scales. The electroplating time affects the nickel deposit structure mainly through its influence on the growth rate of crystallites and the Ni^2+ ions diffusion process around each crystallite. 相似文献
7.
8.
9.
10.
为了开发新型环境友好的天然缓蚀剂,采用索氏提取法提取马齿苋中的有效成分,采用失重法、动电位极化曲线和交流阻抗研究了不同浓度马齿苋提取液在1.0 mol/L盐酸溶液中对Q235碳钢的缓蚀作用及机理。结果表明:马齿苋提取液在盐酸介质中对碳钢具有良好的缓蚀效果,缓蚀效率随缓蚀剂浓度增大而升高,30℃下当提取液的浓度达到0.16 g/m L时,其缓蚀效率可达91%以上;随温度升高,马齿苋提取液对碳钢的缓蚀效率降低;马齿苋提取液是一种抑制阴阳极反应的混合型缓蚀剂,有效成分吸附在碳钢表面形成一层保护膜,吸附过程遵循Langmuir等温方程式,其在碳钢表面的吸附属于自发过程,是以化学吸附为主的物理和化学吸附共同作用的过程。 相似文献