采用高温固相法合成了系列红色荧光粉Li2Y4–xEux(MoO4)7。合成样品的最佳烧结温度和时间分别为850℃和4h。X射线衍射显示样品为纯相Li2Y4(MoO4)7四方晶系晶体结构。光致发光光谱表明,该样品能够被395nm的近紫外光和465nm的可见光有效激发,主发射峰位于615nm附近,对应于Eu3+的5D0→7F2跃迁,显色性能好,可作为白光发光二极管用红色荧光粉;且Eu3+的掺杂量x为2.8时,样品Li2Y1.2Eu2.8(MoO4)7的相对发光强度达到最大值。 相似文献
2.
3.
Li2Y4-xEux(WO4)7-y(MoO4)y red-emitting phosphors were synthesized by solid state reaction and characterized by powder X-ray diffraction (XRD) and photoluminescence (PL) spectrum. The excitation spectra showed that the phosphors could be efficiently excited by near-UV light of 395 nm. When the relative molar ratio of Mo/W was 7:0, and the optimum doped concentration of Eu3+was 2.8 mol, the phosphor showed strong red emission lines at 615 nm corresponding to the forced electric dipole 5D0→7F2 transition of Eu3+. Compared with Na2Y2Eu2(MoO4)7 and K2Y2Eu2(MoO4)7, the fluorescence intensity of Li2Y1.2Eu2.8(MoO4)7 phosphor was the strongest. The CIE chromaticity coordinates of Li2Y1.2Eu2.8(MoO4)7 phosphor was calculated to be (0.66, 0.34). 相似文献