1.
ADM1023是由美国ANALOG DEVICES公司生产的温度监视芯片,该芯片具有高精度,双通道工作等特点,文中详细讨论了ADM1023的主要参数,结构性能,工作原理及应用设计等问题。  相似文献   
2.
Ti-1023合金铸锭铁偏析控制   总被引:1,自引:0,他引:1  
在工业化生产条件下,分析并阐述了Ti-1023合金铁组元偏析的特点及其影响因素,探索了铁偏析规律,提出了控制铁偏析的措施。  相似文献   
3.
PRO teolysis TA rgeting C himeras (PROTACs) promote the degradation, rather than inhibition, of a drug target as a mechanism for therapeutic treatment. Bifunctional PROTAC molecules allow simultaneous binding of both the target protein and an E3-Ubiquitin ligase, bringing the two proteins into close spatial proximity to allow ubiquitinylation and degradation of the target protein via the cell's endogenous protein degradation pathway. We utilized native mass spectrometry (MS) to study the ternary complexes promoted by the previously reported PROTAC GNE-987 between Brd4 bromodomains 1 and 2, and Von Hippel Lindeau E3-Ubiquitin Ligase. Native MS at high resolution allowed us to measure ternary complex formation as a function of PROTAC concentration to provide a measure of complex affinity and stability, whilst simultaneously measuring other intermediate protein species. Native MS provides a high-throughput, low sample consumption, direct screening method to measure ternary complexes for PROTAC development.  相似文献   
4.
Ti-1023合金超塑性压缩时的流动应力及显微组织   总被引:5,自引:0,他引:5  
在α+β两相区和β单相区对Ti-1023合金进行了恒应变速率等温超塑性压缩试验,实测得到了一组流动应力-应变曲线。实验结果表明:应变速率对Ti-1023合金的流动应力有显著影响,变形温度对流动应力的影响程度与应变速率大小密切相关;较低温度快速压缩时易得到均匀细小的等轴α相组织,慢速压缩时组织有一定粗化。较佳超塑性压缩温度为760℃~740℃,应变速率可根据锻件成形、组织性能及生产率的需要在一定范围内选取。  相似文献   
5.
Leucine-rich repeat kinase 2 (LRRK2) is a large protein involved in the pathogenesis of Parkinson's disease (PD). It has been demonstrated that PD is mainly conferred by LRRK2 mutations that bring about increased kinase activity. As a consequence, selective inhibition of LRRK2 may help to recover the normal functions of LRRK2, thereby serving as a promising alternative therapeutic target for PD treatment. The mapping of LRRK2 by positron emission tomography (PET) studies allows a thorough understanding of PD and other LRRK2-related disorders; it also helps to validate and translate novel LRRK2 inhibitors. However, no LRRK2 PET probes have yet been reported in the primary literature. Herein we present a facile synthesis and preliminary evaluation of [11C]GNE-1023 as a novel potent PET probe for LRRK2 imaging in PD. [11C]GNE-1023 was synthesized in good radiochemical yield (10 % non-decay-corrected RCY), excellent radiochemical purity (>99 %), and high molar activity (>37 GBq μmol−1). Excellent in vitro binding specificity of [11C]GNE-1023 toward LRRK2 was demonstrated in cross-species studies, including rat and nonhuman primate brain tissues by autoradiography experiments. Subsequent whole-body biodistribution studies indicated limited brain uptake and urinary and hepatobiliary elimination of this radioligand. This study may pave the way for further development of a new generation of LRRK2 PET probes.  相似文献   
6.
Deformation behavior and mechanisms of Ti- 1023 alloy   总被引:1,自引:0,他引:1  
1 Introduction Beta titanium alloys offer a variety of microstructural morphologies and associated mechanical property variations thus giving considerable latitude in microstructure design. They are the most versatile class of titanium alloys and offer th…  相似文献   
7.
等温锻造过程中Ti-1023合金的本构关系   总被引:3,自引:2,他引:3  
采用Thermecmaster-Z型热加工模拟实验机对Ti-1023合金进行了等温恒应变速率压缩试验,变形温度范围为:740-820℃;变形速率为:0.001~1s^-1。在对试验数据进行系统分析的基础上,全面揭示了Ti-1023合金在等温锻造条件下的热态变形行为。分析了锻造热力参数对流动应力的影响,提出了以Zener-Hollomn参数表征的Ti-1023合金本构方程。并初步分析了Ti-1023合金等温锻造过程中显微组织演化规律。根据分析结果,Ti-1023合金等温锻造宜在略低于相变点温度下以相对高的变形速率进行。  相似文献   
8.
通过室温拉伸性能测试、断口分析和显微组织分析,研究了淬火转移时间对Ti-1023合金组织演变和力学性能的影响规律和机理。结果表明,随淬火转移时间的增加,淬火转移过程中过饱和β相中析出α相,导致等轴α相含量增加,过饱和β相基体的相对含量降低,时效析出的次生αs相含量和弥散程度下降,致使合金强度降低、塑性提高。对于厚80 mm的Ti-1023合金板材或锻件,将淬火转移时间控制在120 s之内,合金组织性能不会受到明显的影响。  相似文献   
9.
10.
研究了工业化制备的超大规格Ti-1023合金铸锭在不同磁场强度下的纵向凝固组织和Fe元素成分分布,并对其影响进行了探讨。结果表明:当磁场强度为10Gs和30Gs时,铸锭组织主要由粗大柱状晶,竹节状的小柱状晶和等轴晶组成;当磁场搅拌强度为20Gs时,凝固组织转变为由底部粗大柱状晶和细小等轴晶组成。Ti-1023合金铸锭中Fe元素在不同磁场强度下遵循正偏析规律,沿铸锭长度方向Fe元素含量从底部到顶部逐渐增加,沿径向从边缘到中心逐渐增加。随着磁场强度从10Gs增加到30Gs,合金元素Fe的宏观偏析率先减小后增大。  相似文献   