首页 | 本学科首页   官方微博 | 高级检索  
文章检索
  按 检索   检索词:      
出版年份:   被引次数:   他引次数: 提示:输入*表示无穷大
  收费全文   141篇
  免费   0篇
  国内免费   1篇
综合类   3篇
化学工业   18篇
金属工艺   64篇
机械仪表   5篇
能源动力   3篇
轻工业   2篇
无线电   2篇
一般工业技术   36篇
冶金工业   2篇
自动化技术   7篇
  2022年   1篇
  2021年   3篇
  2019年   2篇
  2015年   1篇
  2014年   3篇
  2013年   116篇
  2012年   1篇
  2011年   1篇
  2010年   2篇
  2008年   1篇
  2007年   3篇
  2006年   1篇
  2004年   3篇
  2002年   2篇
  2001年   1篇
  1997年   1篇
排序方式: 共有142条查询结果,搜索用时 15 毫秒
1.
2.
Abstract

Polyethylene terephthalate (PET) film drilling using a 248 nm excimer laser through photomask projection is presented. The parameter effects of laser fluence, shot number and repetition rate on the processing results are examined. A high quality microhole array with 50 μm thick PET film is fabricated. When the projection process is carried out, the diameter differences in the microhole in the front and back side of PET are observed. This causes a conical shape in the kerf. The formation of this conical shape in terms of the laser process parameters is discussed. The process parameter effects are investigated and characterised to improve the PET microhole laser machining quality.  相似文献   
3.
4.
We have investigated the adhesion properties of microcrystalline diamond thin films on Ti-Al-V alloy, Co-Cr-Mo alloy and steel. Microcrystalline diamond possesses high hardness, a low coefficient of friction, extreme chemical inertness and biocompatibility; these properties can enhance the performance of metal alloys used in medical implants and in machine tools. We have adopted three methods for improving the adhesion of microcrystalline diamond to commonly used metal alloys: (1) by alloying the substrate surface to minimize graphitization; (2) by employing appropriate buffer layers between the diamond film and the substrate; and (3) by creating functionally gradient diamond-(titanium carbide, tungsten carbide, titanium nitride and aluminum nitride) composites. We have demonstrated that functionally gradient discontinuous buffer layers of titanium carbide, titanium nitride, aluminum nitride and tungsten carbide are able to control stress and graphitization in microcrystalline diamond thin films. This work on buffer layers and functionally gradient coatings should allow the development of more adherent crystalline diamond films for medical and tribological applications.  相似文献   
5.
Research on Laser Direct Deposition Process of Ti-6Al-4V Alloy   总被引:2,自引:0,他引:2  
Laser direct deposition (LDD) of metallic components is an advanced technology of combining CAD/CAM (computer aided design/computer aided manufacturing), high power laser, and rapid prototyping. This technology uses laser beam to melt the powders fed coaxiaUy into the molten pool by the laser beam to fabricate fuUy dense metallic components. The present article mainly studies the LDD of Ti-6Al-4V alloy, which can be used to fabricate aircraft components. The mechanical properties of the Ti-6Al-4V alloy, fabricated by LDD, are obtained using the tension test, and the oxygen content of used powders and deposited specimens are measured. In the present article, it can be seen that the mechanical properties obtained using this method are higher than the ones obtained by casting, and equal to those got by wrought anneal. One aircraft part has been made using the LDD process. Because of this aircraft part, with sophisticated shape, the effect of the laser scanning track on the internal soundness of the deposited part was discussed.  相似文献   
6.
Abstract

The highly crack susceptible magnesium alloy ZK60 plates of 2 mm thickness were successfully welded by laser beam welding (LBW) with filler strip, which has the advantages of low heat input and capability of adjusting the compositions of weld metal to a less susceptible level. The effects of the compositions of filler strips on the microstructures and mechanical properties of the joints were investigated. Compared with autogenous LBW, LBW with filler strip can produce a narrower joint and avoid the cracks and pits, which severely worsen mechanical properties of the joints. When the filler strip of ZK40 alloy is employed, the grains in fusion zone can be refined, and a high quality joint, with the ultimate tensile strength of 322 MPa up to 90·7% of the base metal, is obtained.  相似文献   
7.
Abstract

In order to obtain a robust dissimilar joint of Al/Ti alloys, a filler wire of Al–12 wt-%Si and 45° V shape groove on the base metal were used during CO2 laser welding. Heat input had evident influence on the interfacial reaction mode. It was found that a dissolution mode for low heat input and a melting mode for high heat input exist at the joint interface, which was analysed from thermodynamic point of view. Tensile strength of the joints in the dissolution mode reached as high as 296 MPa, which was significantly higher than that in the melting mode.  相似文献   
8.
Abstract

The main objective of the paper is to outline the 'bridges' existing between the outcomes of fundamental researches and the results of investigations in the field of industrial laser materials processing (LMP). An analysis is presented on the models based on non-stationary hydrodynamic phenomena caused by deeply penetrating high power CW laser beam into materials. This is typical of laser welding (LW) and laser cutting (LC). A physical analysis pertaining to melt removal and melt layer instability mechanisms of gas jet assisted CW–CO2 laser fusion cutting is presented. The models deliberated here are melt squeezing out by gas pressure gradient, melt dragging by the friction force between melt surface and gas flow, formation of moving shelves at the cutting front. In case of high laser intensity, radiative flux interacts with material causing dynamical thermal transport onto the surface and phase transition at solid–liquid–gas interfaces. The solution is based on the non-stationary variables. Under these conditions the Mach number varies significantly due to laser intensity associated with laser flux energy instabilities. The connection among material surface temperature, laser intensity, laser flux and pressure in the plasma cloud is brought out. In addition, novel mechanisms based on hydrodynamics are proposed.  相似文献   
9.
10.
Removing particles with nanometer scale diameters from substrates is a challenging task with numerous critical applications. A novel removal method for nanoparticles is developed and tested. The technique, which is dry and non-contact, takes advantages of shock wavefronts initiated by plasma formation under a focused laser beam pulse and its interaction with the substrate. Experimental results indicate that silica particles down to 500 nm on silicon wafers can be removed without substrate damage. In the reported experiments, a Q-switched Nd : YAG pulsed laser with a 5-ns pulse width and 360-mJ pulse energy at 1064 nm wavelength is employed as a plasma generation source. It is reported that the traditional dry laser cleaning method based on the rapid thermal expansion under direct laser irradiation often results in surface damage in the nanometer scale due to light diffraction around nanoparticles and/or stress localization in the thermal skin. This occurs when the characteristic dimensions of the particles are comparable to the wavelength of incident beam. In the laser plasma method, various mechanisms are responsible for the removal effect. The strong shock wave in air generates complex pressure wavefields resulting in both drag/lift on the particle and acceleration of the substrate. However, shock waves are not transmitted to the solid substrate due to a large difference between the relevant wave phase speeds in the two media. The effects of the number of shots and the distance between the surface and the plasma boundary on the removal efficiency are reported.  相似文献   