摘    要:Ti61.57Zr17.15Ni14.80Cu6.38(atom fraction, %) metallic glass has applications in brazing. Using the hammer-and-anvil technique, Ti61.67Zr17.15Ni14.80Cu6.38 metallic glass was prepared. The crystallization behavior for this metallic glass was investigated by differential scanning calorimetry(DSC), X-ray diffractometry (XRD) and transmission electron microscopy(TEM). There are three stages in DSC curves of crystallization. The reduced glass temperature Trg is 0.42. The kinetic parameters of crystallization were calculated by a set of equations of the maximum crystallization rate. The crystalline phase formed in the MSⅠ(Metastable stage D is Zr2Cu, in the MSII is α-Ti and in the MSⅢ is Ti2Ni. This kind of alloy has lower glass forming ability, and the Ti61.67Zr17.15Ni14.80Cu6.38 metallic glass has lower thermal stability.

关 键 词:钛合金 非晶合金 晶化 动力学 TEM DSC XRD

Crystallization behavior of Ti61.67Zr17.15Ni14.80Cu6.38 glass-forming alloy
FAN Jin duo ,GAO Yi qun ,LI Shi zeng. Crystallization behavior of Ti61.67Zr17.15Ni14.80Cu6.38 glass-forming alloy[J]. Transactions of Nonferrous Metals Society of China, 2004, 14(1): 156-160
Authors:FAN Jin duo   GAO Yi qun   LI Shi zeng
Affiliation:FAN Jin duo 1,GAO Yi qun 2,LI Shi zeng 3
Abstract:Ti61.67 Zr17.15 Ni14.80 Cu6.38 (atom fraction,%) metallic glass has applications in brazing. Using the hammer-and-anvil technique, Ti61.67 Zr17.15 Ni14.80 Cu6.38 metallic glass was prepared. The crystallization behavior for this metallic glass was investigated by differential scanning calorimetry (DSC), X-ray diffractometry (XRD) and transmission electron microscopy(TEM). Th ere are three stages in DSC curves of crystallization. The reduced glass temperature Trg is 0.42. The kinetic parameters of crystallization were calculated by a set of equations of the maximum crystallization rate. The crystalline phase formed in the MSI(Metastable stage Ⅰ) is Zr2Cu, in the MSⅡ is α-Ti and in the MSⅢ is Ti2 Ni. This kind of alloy has lower glass forming ability, and the Ti61.67 Zr17. 15 Ni14. 80 Cu6.38 metallic glass has lower thermal stability.
Keywords:Ti61.67 Zr17. 15 Ni14.80 Cu6.38 metallic glass  crystallization behavior  glass forming ability  brazing