Affiliation:1.Research Unit Vascular Biology of Oral Structures (VABOS), Department of Cranio-Maxillofacial Surgery, University Hospital Muenster, 48149 Münster, Germany; (S.J.); (M.M.M.); (J.K.);2.Private Practice, 48165 Muenster, Germany;3.Center of Dentistry, Department of Prosthetic Dentistry, University of Ulm, 89081 Ulm, Germany
Abstract:Gingivafibroblasts were cultured on lithium disilicate, on zirconia dioxide, and on titanium with two different surface roughnesses (0.2 µm and 0.07 µm); Proliferation (MTT), Living/Dead staining, cytotoxicity (LDH), proliferation (FGF2), and inflammation (TNFα) were analyzed after 1 day and 21 days. Furthermore, alteration in cell morphology (SEM) was analyzed. The statistical analysis was performed by a Kruskal–Wallis test. The level of significance was set at p < 0.05. There were no distinct differences in cellular behavior between the tested roughness. There were slight differences between tested materials. Cells grown on zirconia dioxide showed higher cytotoxic effects. Cells grown on lithium disilicate showed less expression of TNFα compared to those grown on zirconia dioxide or titanium. These effects persisted only during the first time span. The results indicate that the two tested high-strength ceramics and surface properties are biologically suitable for transmucosal implant components. The findings may help clinicians to choose the most appropriate biomaterial as well as the most appropriate surface treatment to use in accordance with specific clinical dental applications.
Keywords:dental implants   gingivofibroblasts   surface roughness   lithium disilicate   zirconium dioxide   titanium
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号