Structure and catalytic properties of Co/ porcelain in the synthesis of 2,3‐dihydrofuran
Authors:Vladislavs Stonkus  Ludmila Leite  Anton Lebedev  Edmunds Lukevics  Augusts Ruplis  Jerzy Stoch  Maciej Mikolajczyk
Abstract:The cyclodehydration of 1,4‐butanediol over cobalt catalysts in the liquid phase is used for the production of 2,3‐dihydrofuran. The catalyst preparation parameters considered were the metal loading, precipitation pH and reduction temperature of cobalt salt. It was found that the use of Co(NO3)2 together with Na2CO3 in a 1:1 ratio yielded better catalysts. Under the conditions used in this study the optimum cobalt loading for the selective production of 2,3‐dihydrofuran is in the range 15–50 wt%. The optimum reduction temperature of Co/porcelain catalyst depends on cobalt loading. The optimum reduction temperatures for 15 and 50 wt% cobalt loading are 773 and 723 K (reduction time 20 min), respectively. © 2001 Society of Chemical Industry
Keywords:2  3‐dihydrofuran  1  4‐butanediol  cyclodehydration  cobalt porcelain catalyst
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号