湿砂型铸铁件的粘砂缺陷--湿砂型铸铁件缺陷讲座(一)
引用本文:于震中,龚出群. 湿砂型铸铁件的粘砂缺陷--湿砂型铸铁件缺陷讲座(一)[J]. 现代铸铁, 2004, 24(3): 55-58
作者姓名:于震中  龚出群
作者单位:1. 清华大学,北京,100084
2. 中国一拖集团公司,第二铸铁厂,河南,洛阳,471004
摘    要:介绍湿砂型铸铁件机械粘砂和化学粘砂的区分方法,各种因素对机械粘砂的影响,包括:砂型紧实度、浇注温度、型砂的粒度和透气性、砂型涂料等。煤粉是防止粘砂和改善表面光洁度的主要型砂加入物。对煤粉的质量、有效煤粉含量、煤粉的代用品以及煤粉的补加量等问题进行了详细的的分析讨论。

关 键 词:湿砂型 粘砂 煤粉
文章编号:1003-8345(2004)03-0055-04
修稿时间:2003-11-17

Penetration/Burn-in Defects of Green Sand Mold Iron Castings
YU Zhen-zhong,GONG Chu-qun. Penetration/Burn-in Defects of Green Sand Mold Iron Castings[J]. Modern Cast Iron, 2004, 24(3): 55-58
Authors:YU Zhen-zhong  GONG Chu-qun
Abstract:The methods to differentiate between the penetration defect and burn-in defect of green sand mold iron castins were introduced, and influences of some process factors on penetration defect were described including:mold density,pouring temperature, sand grain size and permeability,paintings of the mold, and so on .The coal dust is the main mold sand additive to prevent penetration/burn-in and improve the surface fineness. Some problems such as quality of coal dust, active coal dust content, substitute for coal dust,and supplementary addition amount were analyzed and discussed in detail.
Keywords:green sand mold  penetration/burn-in  coal dust