Influence of Ti Powder Characteristics on the Mechanical Properties of Porous Ti Using Space Holder Technique |
| |
Authors: | Boqiong LI Xing LU |
| |
Affiliation: | Liaoning Key Materials Laboratory for Railway, School of Materials Science and Engineering, Dalian Jiaotong University, Dalian, 116028, China |
| |
Abstract: | Porous Ti samples were fabricated by powder metallurgy technique using three kinds of Ti powder and the space holder of polymethyl methacrylate. The final morphological features and mechanical properties were described. Results show that there is only α-Ti phase in porous Ti samples. After sintering, the oxygen content of three porous Ti is increased from the range of 0.34–0.63 wt% to 0.95–1.3 wt%. The porous Ti prepared from the uneven powders with an average particle size of (22.75 ± 11.09) μm presents the largest micro-pore size, grain size, and oxygen content, which lead to the lowest strength and Young’s modulus. |
| |
Keywords: | Porous material Powder metallurgy Microstructure Mechanical property |
本文献已被 CNKI 维普 等数据库收录! |
| 点击此处可从《金属学报(英文版)》浏览原始摘要信息 |
|
点击此处可从《金属学报(英文版)》下载全文 |
|