摘    要:An environment-friendly cerium-based sealing treatment was developed to improve the surface integrity and corrosion resistance of Mg–Al hydrotalcite film on AZ91D magnesium alloy. The cerium dioxide was generated through three stages namely nucleation, growth and dissolution, modifying the surface of AZ91D Mg alloy, and the hydrotalcite film became integral after being treated for 30 min. The results of polarization curves showed that the anti-corrosive performance of the hydrotalcite film was enhanced by the sealing treatment. Moreover, the immersion tests and electrochemical impedance spectrum measurements also demonstrated that the sealed hydrotalcite film provided a longer-term protection of magnesium alloy from corrosion as compared to the unsealed one.

收稿时间:2016-03-31

Cerium-Based Sealing Treatment of Mg-Al Hydrotalcite Film on AZ91D Magnesium Alloy
Authors:Qiang-Sheng Dong  Zhi-Xin Ba  Zhang-Zhong Wang  Juan Kuang  Zheng-Yang Cai  Chen Yuan
Affiliation:1.School of Materials Science and Engineering, Nanjing Institute of Technology, Nanjing 211167, China2 Jiangsu Key Laboratory of Advanced Structural Materials and Application Technology, Nanjing 211167, China
Abstract:An environment-friendly cerium-based sealing treatment was developed to improve the surface integrity and corrosion resistance of Mg-Al hydrotalcite film on AZ91D magnesium alloy. The cerium dioxide was generated through three stages namely nucleation, growth and dissolution, modifying the surface of AZ91D Mg alloy, and the hydrotalcite film became integral after being treated for 30 min. The results of polarization curves showed that the anti-corrosive performance of the hydrotalcite film was enhanced by the sealing treatment. Moreover, the immersion tests and electrochemical impedance spectrum measurements also demonstrated that the sealed hydrotalcite film provided a longer-term protection of magnesium alloy from corrosion as compared to the unsealed one.
Keywords:AZ91D magnesium alloy  Mg-Al hydrotalcite film  Sealing treatment  Ce-containing solution  Corrosion resistance  
本文献已被 CNKI 等数据库收录!
点击此处可从《金属学报(英文版)》浏览原始摘要信息
点击此处可从《金属学报(英文版)》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号