首页 | 本学科首页   官方微博 | 高级检索  
     

Ti6Al4V钛合金的变形组织及织构
引用本文:杨柳青,杨延清.Ti6Al4V钛合金的变形组织及织构[J].中国有色金属学会会刊,2014,24(10):3103-3110.
作者姓名:杨柳青  杨延清
作者单位:西北工业大学
基金项目:Projects(51071122,51271147)supported by the National Natural Science Foundation of China;Project(B08040)supported by Program of Introducing Talents of Discipline to Universities(“111”Project),China
摘    要:在温度850~930°C、应变速率0.01~1 s-1的条件下,对初始组织为等轴组织的Ti6Al4V钛合金进行变形程度为70%的热压缩变形实验,研究合金的变形组织及织构。结果表明,当温度低于900°C、应变速率高于0.1 s-1时,合金的组织主要是拉长的α晶粒;而在高于900°C以及低应变速率下,则会发生动态再结晶。电子背散射衍射(EBSD)结果显示,合金在再结晶过程中亚晶界吸收位错,最终形成大角晶界。在930°C时动态再结晶已基本完成,水冷至室温时形成针状α相。与原始组织相比,合金在930°C变形时织构得到增强,低于930°C变形时织构变弱。

关 键 词:Ti6Al4V合金  热压缩  动态再结晶  EBSD  织构
收稿时间:20 November 2013

Deformed microstructure and texture of Ti6Al4V alloy
Liu-qing YANG,Yan-qing YANG.Deformed microstructure and texture of Ti6Al4V alloy[J].Transactions of Nonferrous Metals Society of China,2014,24(10):3103-3110.
Authors:Liu-qing YANG  Yan-qing YANG
Affiliation:(State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China)
Abstract:Microstructure and texture evolution during hot compression of Ti6Al4 V alloy with an initial equiaxed microstructure were studied in the temperature range of 850-930 °C, strain rate range of 0.01-1 s-1 and engineering compressive strain of 70%. The results indicate that when temperature is below 900 °C and strain rate is higher than 0.1 s-1, the microstructure is mainly composed of elongated α grains. While deforming at higher temperatures and lower strain rates, dynamic recrystallization takes place. Electron back scattered diffraction(EBSD) result shows that during dynamic recrystallization, subgrain boundaries absorb dislocations and the recrystallized grains with high angle grain boundary form. At 930 °C dynamic recrystallization has basically completed, and needlelike α phase forms after water quenching. Pole figure analysis indicates that compared with the initial specimen, textures below 930 °C are weaker, while at 930 °C they are stronger.
Keywords:Ti6Al4V alloy  hot compression  dynamic recrystallization  EBSD  texture
本文献已被 CNKI 维普 ScienceDirect 等数据库收录!