铝铸轧带坯冷轧时表面"黑花"的原因探讨
引用本文:刁普.铝铸轧带坯冷轧时表面"黑花"的原因探讨[J].有色金属加工,2007,36(5):29-30,41.
作者姓名:刁普
作者单位:西南铝业集团有限责任公司压延厂,重庆九龙坡,401326
摘    要:结合生产实际,采用8种方案分别在不同生产条件下进行轧制试验,探讨带材表面“黑花”的原因及影响因素。结果表明,铸轧带坯、轧辊粗糙度、乳液润滑剂对带材表面质量都有不同程度的影响。通过调整工艺参数和控制生产要素,问题得以解决。

关 键 词:铝带材  热轧带坯  铸轧带坯  表面质量  乳液
文章编号:1671-6795(2007)05-0029-03
修稿时间:2007-05-18

Causes of Black Pattern on Surface of Strip Cold-Rolled with Aluminum Casting-Rolling Strip
DIAO Pu.Causes of Black Pattern on Surface of Strip Cold-Rolled with Aluminum Casting-Rolling Strip[J].Nonferrous Metals Processing,2007,36(5):29-30,41.
Authors:DIAO Pu
Affiliation:Southwest Aluminum Group Co. , Ltd. , Chongqing, 401326, China
Abstract:The eight rolling schemes were tested under for seeking the causes of black pattern on the surface of cold rolled strip with aluminum casting-roiling strip, the results show that all the quality of casting-rolling strip, roughness of rolls and water soluble oil solution have influences to varying degrees on the surface quality of cold rolled strip. The problem has been solved by adjusting the process parameters and controlling the production conditions.
Keywords:aluminum strip  hot rolled strip  casting-rolling strip  surface quality  water soluble oil solution